Duplex 2507/S32750 Stainless Steel Bars and Round Bars China Supplier

Leading stainless steel rod and bar Suppliers in China

    • Daxun Alloy offers Duplex 2507 in Round Bar and Flat Bar forms
    • Available in cold rolled and hot rolled options
    • Composition: 25% chromium, 4% molybdenum, 7% nickel
    • High strength and excellent corrosion resistance
    • Used in chemical processing, petrochemical, and seawater equipment
    • Resistant to chloride stress corrosion cracking
    • Good thermal properties, including low thermal expansion, making it suitable for high-temperature applications

스테인리스 봉 및 원형 막대 제작 서비스 분야의 글로벌 리더

일반 속성

Duplex 2507 (UNS S32750) is a super duplex stainless steel bar. Its composition includes 25% chromium, 4% molybdenum, and 7% nickel. This alloy excels in challenging environments, offering remarkable strength and corrosion resistance. It’s the go-to choice for chemical processing and petrochemical industries. Seawater equipment also benefits from its exceptional properties. Duplex 2507 stands strong against chloride stress corrosion cracking. Its thermal properties are impressive, with high conductivity and low thermal expansion, making it ideal for high-temperature applications. The alloy’s unique blend of elements ensures top-notch corrosion resistance. For tough conditions demanding both strength and durability, Duplex 2507 delivers.

당사의 서비스 센터 네트워크는 일반적인 크기와 합금의 바를 빠르고 준비된 공급을 위해 스테인리스 스틸 바 제품을 보유하고 있으며, 또한 맞춤형 크기의 스테인리스 스틸 막대를 생산하며 수량이 공장 최소 수량 미만인 경우 적시에 빠른 처리를 위해 재고 일정을 조정할 수 있으며, Daxun Alloys는 직경이 1/16 인치에서 26 인치 범위의 스테인리스 스틸 원형 바를 재고하고 있습니다. 원형 바는 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205 및 Alloy 20을 포함한 거의 모든 등급의 스테인리스 스틸로 제공됩니다. 열처리된 스테인리스 스틸 원형 바는 17-4PH, H900 템퍼(요청 시), H1025, H1150, Double H1150 및 H1150M으로 제공됩니다. 요청 시 다른 열처리된 템퍼도 제조할 수 있습니다. 410, 430, 416 등 400 시리즈 스테인리스 스틸을 보유하고 있습니다. 또한 303, 304, 316/L 정밀 및 베어링 품질의 스테인리스 스틸 원형 바도 보유하고 있습니다. 재고의 대부분은 가공성을 높이고 부품당 총 비용을 낮추기 위해 일관된 표준으로 용융된 스테인리스 스틸 원형 봉강인 당사의 고유한 가공 봉강 등급으로 구성되어 있습니다. 당사의 스테인리스 스틸 바 가공 기계를 통해 Daxun Alloys는 고객의 정확한 사양에 따라 생산할 수 있습니다.

자세히 보기

데이터

제품 매개변수: 스테인리스 스틸 로드
사양 ASTM A276, ASME SA276 / ASTM A479 ASME SA479
치수 EN, DIN, JIS, ASTM, BS, ASME, AISI
Duplex 2507- S32750 Round Bars 4mm ~ 500mm 범위의 외경
Duplex 2507- S32750 Round Bars 4mm~100mm 범위의 외경
Duplex 2507- S32750 Round Bars 18mm - 57mm(11/16인치 ~ 2-3/4인치)
완료 블랙, 밝은 광택, 러프 턴, NO.4 마감, 무광 마감, BA 마감
길이 1~6미터, 맞춤형 절단 길이
양식 원형, 정사각형, 육각(A/F), 직사각형, 빌렛, 잉곳, 단조 등.
등급 슈퍼 듀플렉스 2507
유엔 지정 S32750
탄소(C) 최대. 0.03
망간(Mn) 최대. 1.2
인(P) 최대. 0.035
황(S) 최대. 0.02
실리콘(Si) 최대. 0.8
크롬(Cr) 24.0-26.0
니켈(Ni) 6.0-8.0
몰리브덴(Mo) 3.0-5.0
질소(N) 0.24-0.32
철(Fe) Bal.
구리(Cu) 0.5
기타 요소 —
밀도, 파운드/in3 0.28
탄성 계수, psi 29.0x 106
열팽창 계수, 68-212˚F, /˚F 7.5 x 10-6
열 전도성, Btu/ft hr ˚F 8
비열, Btu/lb ˚F 0.12
전기 저항, 마이크로옴인 31.5
슈퍼 듀플렉스 2507 제품군
합금 유엔 지정 Werkstoff NR. 사양*
슈퍼 듀플렉스 2507 S32750                       1.4410 ASTM A276
Stainless Steel 2507/S32750 Bright Bar SS 2507/S32750 Bright Bar
2507/S32750 SS Bright Bar
Stainless Steel 2507/S32750 Bright Bar
UNS S2507/S32750 SS Bright Bar
WERKSTOFF NR. 1.4410 Bright Bar
ASTM A276 2507/S32750 Stainless Steel Bright Bar
Stainless Steel 2507/S32750 Hex Bar SS 2507/S32750 Hex Bar
2507/S32750 SS Hexagonal Bar
2507/S32750 Stainless Steel Hex Bar
UNS S2507/S3275000 SS Hexagonal Bar
ASTM A276 2507/S32750 Stainless Steel Hex Bar
Stainless Steel 2507/S32750 Square Bar SS 2507/S32750 Square Bar
2507/S32750 SS Square Bars
2507/S32750 Stainless Steel Square Bar
UNS S2507/S3275000 SS Square Bar
WERKSTOFF NR. 1.4410 Square Bar
ASTM A479 2507/S32750 Stainless Steel Square Bars
Stainless Steel 2507/S32750 Rectangular Bar SS 2507/S32750 Rectangular Bar
2507/S32750 SS Rectangular Bars
2507/S32750 Stainless Steel Rectangular Bar
UNS S2507/S3275000 SS Rectangular Bars
WERKSTOFF NR. 1.4410 Rectangular Bar
ASTM A276 2507/S32750 Stainless Steel Rectangular Bar
Stainless Steel 2507/S32750 Flat Bars SS 2507/S32750 Flat Bar
2507/S32750 SS Flat Bars
2507/S32750 Stainless Steel Flat Bars
UNS S2507/S3275000 SS Flat Bars
WERKSTOFF NR. 1.4410 Flat Bars
ASTM A276 2507/S32750 Stainless Steel Flat Bars
Stainless Steel 2507/S32750 Polished Bar SS 2507/S32750 Polished Bar
2507/S32750 SS Polished Bars
2507/S32750 Stainless Steel Polished Bar
UNS S2507/S3275000 SS Polished Bars
WERKSTOFF NR. 1.4410 Polished Bar
ASTM A476 2507/S32750 Stainless Steel Polished Bar
Stainless Steel 2507/S32750 Threaded Bar SS 2507/S32750 Threaded Bar
2507/S32750 SS Threaded Bars
2507/S32750 Stainless Steel Threaded Bar
UNS S2507/S3275000 SS Threaded Bar
WERKSTOFF NR. 1.4410 Threaded Bar
ASTM A276 2507/S32750 Stainless Steel Threaded Bar

Daxun을 선택하고 고객을 만족시키세요.

Contact Daxun now-2507 Stainless Steel Rod

빠른 응답

We provide timely and fast delivery of 2507 stainless steel bars for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to ports and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

지금 Daxun에 문의

닥순의 장점

  • 종류: 300 시리즈, 400 시리즈, 600 시리즈 등 다양한 크기와 등급을 제공합니다.
  • 유연성: 열간 압연 또는 냉간 압연 바가 필요하든, 당사의 스테인리스 스틸 바 길이는 특정 프로젝트 요구 사항을 충족하도록 설계되었습니다.
  • Quality Standards: 2507 Stainless Steel Rod meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
  • 맞춤 주문: 특별한 사이즈의 스테인리스 스틸 바를 찾고 계신가요? 경쟁력 있는 가격과 편리한 온라인 주문으로 다양한 스테인리스 스틸 바 맞춤 제작 옵션을 제공합니다.
지금 Daxun에 문의

2507 Stainless Steel Rod packaging

We pay attention to every process to ensure quality. The 2507 round bar packaging we usually adopt is to pack the stainless steel round bars with environmentally friendly plastic bags and then put them into fumigation-free wooden boxes or wooden pallets. Customized packaging, such as OEM, can also be negotiated. We provide almost everything to meet your round bar packaging requirements. We attach great importance to packaging. The round bars are packed in wooden corrugated boxes, wrapped with plastic packaging and bubble film on the outside.

지금 Daxun에 문의

품질, 배송, 검사

  • Daxun은 또한 여러 가지 품질 보증 테스트를 수행합니다. 이러한 테스트에는 평탄화 테스트, 피팅 및 저항 테스트, 기계적 테스트, 경도 테스트, 재료 양성 식별, 팽창 테스트 등이 포함됩니다. 이러한 모든 테스트를 통해 재료가 필요한 용도에 적합한지 확인합니다.
  • 생산 과정에서 제품의 직경, 두께, 표면을 측정합니다. 표준 배송 기간은 7~15일이며, 일부 특수 사이즈 제품을 제외하고는 배송 기간이 20일로 늘어납니다.
    배송 시간은 엄격하게 계약에 따릅니다.
  • 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
  • 고객에게 테스트용 무료 샘플 지원
  • 현장 또는 비디오 공장 검사 지원
지금 Daxun에 문의

기술 지원

추가 기술 지원이 필요한 경우 금속 전문가와 지식이 풍부한 직원이 기꺼이 도와드릴 것입니다. 또한 Daxun은 다중 금속 및 플라스틱 재고 업계 최초로 인증된 테스트 실험실을 보유하고 있습니다. 이는 품질에 대한 변함없는 헌신과 풀서비스 공급업체로서의 철학을 보여주는 것이라고 생각합니다.

지금 Daxun에 문의

2507 Stainless Steel Rod Ordering Information

2507 Round Bar Purchase orders shall include quantity, PSL grade, type or category, API5L reference, diameter, surface finish, length and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish or end treatment. Bars are solution bright annealed.

2507/S32750 Stainless Steel Rod Features

높은 강도
내식성
내열성
저온 저항
환경 보호
용접 성능

Daxun 합금으로 브랜드를 빠르게 향상 시키십시오.

배송 상태 선택 표면 상태
Forged 블랙
광택
열간 압연 블랙
광택
밝음
피클
콜드 드로잉 광택
밝음
참고:
1. 위에 나열된 것과 다른 배송 상태가 필요한 경우 당사에 문의해 주시기 바랍니다.
2. 문의 또는 주문 시 여기에 표시되지 않은 추가 요구 사항이 있으면 친절하게 알려주시기 바랍니다.
용액 어닐링 상태의 재료는 다음과 같이 숙성될 수 있습니다.-*두 배 숙성을 나타냅니다.
조건 H900(H480) H925(H495) H1025(H550) H1075(H580) H1100(H595) H1150(H620) H1150M(H620M)* 플러스 H1150D(H620D)* 플러스
로 가열합니다. ±15oF 900oF 925 oF 1025oF 1075oF 1100oF 1150oF 1400oF 1150oF 1150oF 1150oF
±9oC 480oC 495oC 550oC 580oC 595oC 620oC 760oC 620oC 620oC 620oC
몇 시간 동안 보류 1 4 4 4 4 4 2 4 4 4
아래로 냉각 Air Air Air Air Air Air Air Air Air Air
90oF(32oC)

Types of 2507/S32750 Stainless Steel Rods (6)

참조 및 다운로드 가능한 정보

스테인리스 스틸 로드 생산

Daxun은 신뢰할 수 있는 스테인리스 스틸 막대 및 바 제조업체입니다.

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless rod  are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 2507 Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

최근 인기 있는 사례 프로젝트 및 제품

2507/S32750 stainless steel rod
스테인리스 스틸 로드
대구경 스테인리스 스틸 로드
2507/S32750 stainless steel rod
스테인리스 스틸 광택 막대
스테인리스 스틸 로드
스테인리스 스틸 로드
스테인리스 스틸 로드
2507/S32750 stainless rod
스테인리스 스틸 정밀 로드
스테인리스 스틸 로드
샘플을 받을 수 있나요?

We can provide 2507 Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.

이미 수출한 국가는 어디인가요?

캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.

MOQ는 얼마인가요?

Our MOQ is 1 ton for 2507 Stainless Steel Rod.

배송 시간은 얼마나 걸리나요?

체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.

오늘 문의 보내기