x
오늘 문의 보내기
빠른 견적

Daxun is an experienced manufacturer of CP-Grade 1 titanium plates

중국 최고의 티타늄 및 티타늄 합금 막대 공급업체인 Daxun은 전 세계에 고성능 티타늄 막대를 공급하고 있습니다.
  • Titanium plate Grade:CP-1(1등급)- UNS R50250
  • Titanium plate production types: cold rolling, hot rolling, forging.
  • Titanium plate density The density of grade 1 titanium is 4.51 g/cm3
  • Standards: ASTM B265 Gr 1, ASME SB265, ASTM F67 AMS 4919
  • Features: high specific strength, light weight, corrosion resistance
  • Processing: high ductility, easy to form, easy to process

——Daxun produces titanium sheets in China to meet the diverse and demanding needs of customers!

A global leader in commercially pure titanium sheet fabrication services

DAXUN Alloys is a top global supplier of premium Grade 1 titanium plates. Grade 1 titanium offers great ductility and cold formability, perfect for deep drawing. It is also highly resistant to seawater and various solutions, including chlorides, making it a reliable choice for different environments.

Titanium’s low density, high strength-to-weight ratio, and corrosion resistance make it ideal for tough chemical environments. Commercially pure Grade 1 titanium is the softest and most ductile, offering great cold formability and top-notch corrosion resistance. It also welds easily and has good impact strength. Grade 1 titanium is also used in the aerospace industry for manufacturing airframe components due to its excellent properties.

DAXUN specializes in large and small titanium plate projects. We are your trusted partner, dedicated to providing high-quality titanium plates and ongoing technical support for your business. Our focus is on building long-term relationships through reliability and expertise.

자세히 보기

Technical Data Sheet

Alvac Grade ASTM B265 Grade # Chemistry N C HA HB O Fe Pd Other Elements Each Total Other Elements Ti
30 1 Weight %, maximum 0.03 0.08 0.010 0.0125 0.18 0.20 - 0.05 0.30 Bal.

Unalloyed CP titanium (Grades 1, 2, 3, and 4) generally resist crevice corrosion at temperatures below 80°C (175°F) in any pH-treated solution.

Our technical datasheet pdf provides more information about mechanical properties. If you have any concerns or need more details about our product, please contact us.

Physical Properties & Specifications

ASTM Grades I (ATI 30)

ATI 30: 1,630°F ± 25°F (888°C ± 4°C)

ASTM F 67 – Unalloyed Titanium

ISO 5832-2 – Unalloyed Titanium

열처리

Commercially pure titanium can be annealed by heating to 1,000 – 1,300°F (538 – 704°C) for 1/2 to 2 hours and air cooling.

프로젝트의 성공을 위해 Daxun을 선택하세요.

지금 Daxun에 문의

맞춤 커팅

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • 워터젯 절단
  • 레이저 커팅
  • Plasma cutting
  • Wire cutting
  • Bending
  • Slitting
  • 톱질
지금 Daxun에 문의

Grade1 TItanium sheet FINISHES

#1 – Hot rolled, annealed, and descaled for applications that do not require a smooth decorative finish. #2D – Dull finish achieved through cold rolling, annealing, and descaling. Used for deep-drawn pieces and parts requiring lubricants to be kept during the shaping process.

#2B – Smooth finish achieved through cold rolling, annealing, and descaling. A light, cold rolling pass following annealing results in a brighter finish than 2D.

#BA – Cold rolled, brilliant annealed

#CBA: Coarse bright annealed cold rolled matte finish and bright annealed.

지금 Daxun에 문의

고급 프로덕션

The cold-rolled thickness range for Grade 1 Titanium Plates is 0.3 mm to 6.0 mm, while the hot-rolled range is 4.76 mm to 155 mm. These plates are produced through longitudinal and transverse rolling and are available in hot-rolled or heat-treated conditions.

지금 Daxun에 문의

품질, 검사

Daxun performs a variety of quality assurance tests, including flattening, pitting resistance, mechanical, hardness, material identification, and expansion tests. These tests guarantee that the material meets the required standards for its intended application.

During the production process, we measure the diameter, thickness and surface of the product.

  • 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
  • 고객 테스트를 위한 무료 샘플 지원
  • 현장 또는 비디오 공장 검사 지원
지금 Daxun에 문의

기술 지원

추가 기술 지원이 필요한 경우 금속 전문가와 지식이 풍부한 직원이 기꺼이 도와드릴 것입니다. 또한 Daxun은 다중 금속 및 플라스틱 재고 업계 최초로 인증된 테스트 실험실을 보유하고 있습니다. 이는 품질에 대한 변함없는 헌신과 풀서비스 공급업체로서의 철학을 보여주는 것이라고 생각합니다.

지금 Daxun에 문의

Fast Delivery

We ensure timely delivery of Grade 1 titanium plates, supported by our strong production capacity, seamless information flow, and efficient logistics. Daxun’s order data is instantly integrated with our logistics system, enabling smooth coordination. Our processing center is strategically located near highways, rivers, and ports, allowing for quick scheduling, storage, and transportation. With efficient loading, we guarantee that your goods arrive on time.

We provide different way to ship our product, including FOB, CFR, CIF, DDP and DAP.

배송 시간은 엄격하게 계약에 따릅니다.

지금 Daxun에 문의

패키징

Daxun pays special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- 상자 및 상자
• Shrinkwrap
- 목재 팔레트
- 나무 상자

Grade 1 Titanium Plate Features

높은 강도
내식성
내열성
저온 저항
환경 보호
경량

Daxun Grade 1 Titanium sheet Let your brand improve rapidly

아래 나열된 제품 외에 사용 가능한 다른 금속 제품은 여기에 나열되어 있지 않습니다. DAXUN이 제조 및 공급할 수 있는 기타 금속 제품으로는 탄탈륨, 니오븀, 지르코늄, 하프늄, 니켈, 구리 등이 있으며 주로 판재, 바, 튜브 형태입니다.
제품/처리 표준 등급/크기
티타늄 플레이트, 시트, 코일- ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(두께:( 0.0197”-6”)최대 폭: 12피트, 최대 길이: 50피트)
AMS-T-9046
티타늄 및 티타늄 합금 시트, 플레이트
상업적으로 순수한 티타늄(CP)
코드 지정 수율 강도
최소, KSI 1 /
CP-1 70
CP-2 55
CP-3 40
CP-4 25
알파 티타늄 합금(A)
코드 지정 구성
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
알파-베타 티타늄 합금(AB)
코드 지정 구성
AB-1 6A1-4V
AB-2 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
베타 티타늄 합금(B)
코드 지정 구성
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
처리 중입니다:
열간 압연 냉간 압연
사용 가능한 성적:
CP 1등급 6Al-2Sn-4Zr-2Mo(6-2-4-2) 등급
CP 2등급 6Al-4V ELI 등급(이전 23등급)
7학년 6Al-6V-2Sn(6-62) 등급
19학년 8알-1모-1V 등급(8-1-1)
5등급(6Al-4V) 9등급(3Al-2.5V)
6등급(5Al-2.5Sn) CP 3등급
애플리케이션
화학 산업 해수 담수화
석유화학 산업 항공우주
기계 가공 분야, 자동차 분야 휴대폰 구성 요소 필드.

Daxun is a professional manufacturer committed to high-quality products. We ensure all our titanium plates meet international standards. This includes certifications from ISO9001, SGS, CE, and OQC. Our strict quality control process minimizes defects.

최근 인기 있는 사례 프로젝트 및 제품

Grade 1 Titanium Plate and sheet
원자력 전기
Grade 1 Titanium Plate and sheet
항공우주
티타늄 플레이트 및 시트
화학 물질
티타늄 플레이트 및 시트
압력 용기
티타늄 플레이트 및 시트
새로운 에너지 산업
티타늄 플레이트 및 시트
해양 엔지니어링
티타늄 플레이트 및 시트
담수화
티타늄 플레이트 및 시트
전력 산업
티타늄 플레이트 및 시트
태양광 에너지
Titanium plate and sheet Grade 1 

We specialize in pure titanium plates. Our products serve both the industrial and aerospace sectors. We excel in meeting customer needs. Our clients trust our capabilities. We consistently deliver the products they require.

DAXUN has always worked with overseas clients. We have strong ties to global titanium industry leaders. Our technology ensures high-quality materials. We meet specific project needs.

We have established supply chains and maintain research laboratories. Alpha-beta alloys, such as Ti 6Al-4V, are heat-treatable and extensively used in various industries, including aerospace and marine applications. We operate through subsidiaries to ensure top-quality production. We adapt to any specific product request. Every order receives our full attention. Quality is our priority from start to finish.

DAXUN values customer service highly. It’s a key part of our business. We provide clear information to customers. Our pricing is comprehensive. We interact closely with our customers and answer their technical questions. Our support goes beyond the product itself.

When you buy from us, you get more. You receive raw materials, of course. But you also get excellent service.

Titanium Plate and sheet Grade 1 Data sheet

ASTM B265 | ASME SB265 | ASTM F67 | ISO 5832-2 | 3.7025 | UNS R50250

Grade 1 pure titanium sheet is highly ductile. It has excellent cold formability, making it ideal for deep drawing. Grade 1 titanium resists corrosion well. It stands up to general corrosion. It also withstands seawater corrosion. The material resists oxidizing media. It handles neutral solutions too. Even mildly reducing media, like chlorides.

Titanium has a low density. It’s about half as dense as nickel-based alloys. Titanium offers a high strength-to-weight ratio. Its corrosion resistance is remarkable.

These properties make titanium versatile. It performs well in harsh chemical conditions. Many industries choose it for demanding applications.

Grade 1 Titanium Plate Features and Corrosion Resistance

High ductility;
Good cold formability and impact strength;
Medium strength;
High corrosion resistance and notched impact strength;
Excellent biocompatibility;
Very easy to weld and not magnetic.

어떤 등급의 티타늄이 가장 좋은가요?

필요한 티타늄 합금의 등급은 각 등급마다 다른 이점이 있으므로 작업 중인 프로젝트에 따라 다릅니다.

All grades of titanium alloy are extremely strong and corrosion-resistant, which means they will continue to work well even in the harshest conditions.

The higher grades of titanium alloy (5-12) are alloys designed for specific benefits. It also knows as beta alloyes for different usage like metal support in human body. For example, grade 12 titanium alloy has excellent heat resistance, making it a perfect choice for shell and tube heat exchangers, hydraulic piping, and chemical industry equipment.

Grades 1-4 are pure titanium grades, and they are a perfect choice if you need a weldable, ductile material for piping systems and tubing.

When considerding titanium grades, the common physcial properties are heat treatment, fracture toughness, thermal conductivity, mechanical properties, tensile strength and yield strength. Also, we need to understand application to help you to archive your goal.

If you are starting a project and are unsure which grade is best for you, contact us now; we are more than happy to help you.

How are higher grades of titanium different from the lower grades?

Titanium Gerades as known as commercially pure titanium and titanium alloys grade level.

At DAXUN, we offer a wide range of titanium alloy grades from grade 1 to grade 29.

Grades 1-4 are pure titanium, while higher grades are alloys. Alloy grades are popular for their high strength-to-weight ratio.

The most commonly used titanium alloy grades is grade 5 (ti 6al 4v). From grade 5, it combines with different metals together, like aluminum and iron. These excellent combination extends the excellent weldability and high temperature creep strength.

항공우주 및 해양 산업과 같은 산업에서는 내마모성과 내식성 때문에 등급이 높을수록 선호합니다.

다양한 등급의 티타늄 합금의 차이점에 대해 자세히 알아보려면 지금 바로 +86 13382898899으로 전화하여 전문가와 직접 상담하세요.

티타늄 등급이 비용에 영향을 주나요?

티타늄의 등급에 따라 비용이 약간 증가하지만, 총 비용은 주로 필요한 티타늄의 모양과 형태에 따라 결정됩니다.

At DAXUN, we offer all sorts of titanium products, including plates, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

It is difficult to offer a price online without knowing much about your project and what the metal will be used for.

But don’t worry. Our team is always here to help with your titanium needs. By sending an email to us, we will be able to get back to you with some advice and an accurate quote. Make sure to include as much information as possible about your needs.

Where can I learn more about the grades of titanium?

DAXUN의 팀은 경험이 풍부하고 지식이 풍부하며 친절합니다. 업계에서 다년간의 경험을 바탕으로 티타늄의 용도, 장점, 등급 등 티타늄에 대한 모든 것을 잘 알고 있습니다.

For regular updates on titanium, its uses, and its applications across industries, be sure to check out our blog. Our experts have written easy-to-follow posts that you can always refer to.

By sending an email to daxunalloy@gmail.com, you’ll receive a quick response.

견적을 받거나 시장 정보를 최대한 빨리 파악하려면 어떻게 해야 하나요?

“문의하기” 페이지의 양식을 작성하거나 영업 관리자(+86 13382898899)에게 전화하시면 최대한 빨리 연락드리겠습니다. WhatsApp은 온라인 상태이며 이메일(Daxunalloy@gmail.com)는 6시간 이내에 확인됩니다. 모든 문의나 메시지는 신속하게 답변해 드립니다. 또한 매주 고객과 시장 정보를 공유합니다.

샘플을 받을 수 있나요?

We can provide Titanium sheet samples for you to check the quality. The sample is free and you just pay the freight. Contact us for more details and we are happy to make you a special offer.

MOQ는 얼마인가요?

MOQ is 1 ton for the Titanium sheet.

Overview of Titanium Alloys

Titanium alloys are a blend of titanium and other chemical elements, designed to offer exceptional tensile strength and toughness, even under extreme temperatures. These alloys are lightweight, exhibit extraordinary corrosion resistance, and can endure high temperatures, making them indispensable in various industries. From aerospace and aircraft to medical devices and jewelry, titanium alloys are integral to many high-stress applications.

Commercially pure titanium, known for its acceptable mechanical properties, is often used in orthopedic and dental implants. The most common titanium alloy, Ti 6Al 4V, includes small amounts of aluminum and vanadium (6% and 4% by weight, respectively). This combination allows for precipitation strengthening, enhancing the alloy’s mechanical properties. Whether in the form of alpha alloys, beta alloys, or alpha-beta alloys, titanium alloys continue to be a cornerstone in industries requiring materials that offer both strength and corrosion resistance.

빠른 견적