Daxun is an excellent manufacturer of grade 23 (Ti-6Al-4V ELI)titanium rods and bars.
중국 최고의 티타늄 및 티타늄 합금 막대 공급업체인 Daxun은 전 세계에 고성능 티타늄 막대를 공급하고 있습니다.
- Titanium bar grade: Grade 23-Ti6Al 4V ELI- USN R56401
- 티타늄 바 유형: 압연 바, 인발 바, 단조 티타늄 바
- Titanium bar density The density of grade 23 titanium is 4.43 g/cm3
- 주요 표준: ASTM ASME GB GJB EN JIS DIN ISO ATP BS 등.
- 고강도, 고온 저항성, 내식성, 가벼움
- 무게, 뛰어난 종합 성능.
————Daxun은 중국에서 티타늄 막대를 생산하여 다양하고 ——고객의 까다로운 요구 사항!
상업용 순수 티타늄 막대 제조 서비스 분야의 글로벌 리더
Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 23 titanium alloy rods.
Grade 23 titanium bar, also known as Ti-6Al-4V ELI, is a high-performance alloy known for its excellent strength-to-weight ratio, corrosion resistance, and biocompatibility. It is widely used in aerospace, medical, and high-tech industries due to its ability to withstand extreme conditions while remaining lightweight. Compared to other titanium grades, Grade 23 offers enhanced ductility and fracture toughness, making it ideal for critical applications such as aircraft components, surgical implants, and advanced engineering parts.
Daxun 는 신뢰할 수 있는 티타늄 합금 막대 생산 회사입니다. Daxun은 상업적으로 순수한 티타늄 시리즈 CP, 티타늄 합금 시리즈, 티타늄 니켈 합금 등을 포함한 모든 등급의 티타늄 합금을 생산합니다. 안정적인 성능을 갖추고 있으며 중요한 애플리케이션에 고성능을 제공합니다. 다양한 산업 및 응용 분야에서 고강도, 고온 및 부식성 환경에서 Daxun 티타늄 합금 막대를 사용할 수 있습니다. 수십 년 동안 Daxun Metals는 가장 심각한 문제를 해결하기 위해 고도로 설계된 티타늄 합금 솔루션을 생산하기 위해 노력해 왔습니다.
데이터
- 매개변수
- 성분
- 기계적 특성
- 물리적 속성
| 사양 | 세부 정보 |
|---|---|
| 재료 | Titanium rod and bar Grade 23 (UNS R56400) |
| 표준 | ASTM B348, ASTM SB348, AMS 4921, AMS 4902 |
| 치수 | EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN |
| 직경 범위 | 0.125인치 - 14인치(3.175mm - 355.6mm), 커스텀 |
| 길이 범위 | 최대 240인치(6096mm), 맞춤형 |
| 완료 | 냉간(브라이트) 인발, 센터리스 연마, 열간 압연, 매끄러운 턴, 박리, 슬릿 압연 가장자리, 열간 압연 어닐링, 거친 턴, 브라이트, 광택, 연마, 센터리스 연마 및 블랙 |
| 표면 마감 | 냉간 인발, 센터리스 그라운드, 광택 또는 러프 턴, 블랙, NO.4 마감, BA 마감, 무광 마감 등. |
| 조건 | 경화 및 템퍼링, 어닐링 처리 |
| 허용 오차 | 직경 허용 오차: +/- 0.005″(0.127mm), 길이 허용 오차: +/- 0.125″(3.175mm) |
| 양식 | 티타늄 사각형 바, 티타늄 잉곳, 티타늄 원형 바, 직사각형 티타늄 바, 삼각형 티타늄 바, 단조 티타늄 바, 티타늄 육각 바 등이 있습니다. |
| 물리적 속성 | Density: 0.163 lb/in³ (4.51 g/cm³), Melting Point: 3,020°F (1,660°C), Elongation: 20-30%, Modulus of Elasticity: 16.5 x 10⁶ psi (114 GPa) |
| 화학 성분 | Titanium (min): 99.2%, Oxygen (max): 0.25%, Carbon (max): 0.08%, Iron (max): 0.30%, Nitrogen (max): 0.03%, Hydrogen (max): 0.015% |
| 요소 | Minimum (%) | Maximum (%) |
|---|---|---|
| 티타늄(Ti) | 99.2 | - |
| 알루미늄(Al) | 5.5 | 6.75 |
| 바나듐(V) | 3.5 | 4.5 |
| 산소(O) | - | 0.25 |
| 탄소 © | - | 0.08 |
| 철(Fe) | - | 0.30 |
| 질소(N) | - | 0.03 |
| 수소(H) | - | 0.015 |
| 속성 | 가치 |
|---|---|
| 인장 강도 | 130,000–170,000 psi (900–1,170 MPa) |
| Yield Strength (0.2% Offset) | 115,000–150,000 psi (800–1,035 MPa) |
| 신장 | 20-30% |
| 경도(브리넬) | 300–360 HB |
| 탄성 계수 | 16.5 × 10⁶ psi (114 GPa) |
| 속성 | 가치 |
|---|---|
| 밀도 | 0.163 lb/in³ (4.51 g/cm³) |
| 녹는점 | 3,020°F (1,660°C) |
| 열 전도성 | 13.4 W/m·K (at 25°C) |
| 열팽창 계수 | 8.6 µm/m·°C (20–100°C) |
| 전기 저항 | 4.1 × 10⁻⁷ Ω·m |
프로젝트의 성공을 위해 Daxun을 선택하세요.
DAXUN® Grade 23 Titanium Rod Features
DAXUN® Ti Grade 5는 티타늄 합금 바(6al-4v)가 특징입니다:
- 열간 성형성 및 용접성이 우수합니다;
- 인장 강도는 1000MPa에 달할 수 있습니다;
- 고온에서의 치수 작업
- 바닷물이나 바닷물에 민감하지 않습니다;
- 다양한 부식성 매체의 영향을 받지 않습니다;
- 강도가 높고 인성이 우수합니다;
- 균열 시작 및 균열 전파를 방지합니다.
닥순 공장 장점
Daxun의 “성과 우수 관리” 개념은 “PDCA + 린” 관리 모델을 장려합니다. 회사의 명함에는 “Daxun = 신뢰할 수 있는 품질”이라고 적혀 있습니다. Daxun은 ERP 시스템을 사용하여 각 티타늄 막대의 품종, 사양 및 원산지를 완벽하게 추적하고 업계 위조 방지를 옹호하고 장려합니다. Daxun은 가공 및 사용자 정의 기술에 의존하며 고정밀 및 고품질은 업계 벤치 마크이며 서비스 측면에서 제품 수명주기 관리를 촉진하고 판매 전에 전문적인 재료 선택 및 처리 솔루션을 제공하고 판매 중에 엄격하게 모니터링하며 판매 후 걱정없는 서비스 보증을 제공합니다.
Grade 23 Titanium Rod Production Method
Daxun은 고성능의 고품질 티타늄 바를 생산하며 고객의 계약에 따라 제조할 수도 있습니다:
- 티타늄 잉곳은 열처리 및 가공, 침수 초음파 테스트, 기계적 특성 테스트, 거시적 및 미세 구조 검사 및 기타 공정을 거쳐야 합니다. 생산 공정: 열간 압연 티타늄 바 - 고효율, 안정적인 성능, 단조 티타늄 바 - 유연한 크기, 다중 화재 단조, 티타늄 바의 포괄적인 성능 향상, 냉간 인발 티타늄 바 - 일반적으로 소형 고정밀 티타늄 바; 위의 티타늄 바는 모두 밝은 표면으로 전달됩니다.
Grade 23 Rods Applications and Standards
Grade 23 Titanium Rods are widely used in the following industries under extreme corrosive conditions:
- 항공우주, 조선, 석유 및 가스 산업, 해양 엔지니어링, 화학 플랜트, 산업 기계, 전력 산업, 제지 및 펄프 산업, 식품 가공 산업, 정유소, 군수 산업, 제약 및 식품 가공 장비 등.
- 사양 AMS 4928, AMS 4967, AMS 4965, AMS 6931, ASTM B 348
- 표준 ASTM, ASME, EN, JIS, DIN, GB, GJB, API
품질, 배송, 검사
Daxun은 여러 가지 품질 보증 테스트를 수행하며, 이러한 테스트에는 면적 인장, 화학 분석, 재료 양성 식별 - PMI 테스트, 마이크로 및 매크로 테스트, 입계 부식 (IGC) 테스트, 초음파 결함 감지 테스트, 피팅 및 저항 테스트, 경도 테스트, 재료 양성 식별, 팽창 테스트 등과 같은 기계적 테스트가 포함됩니다. 이러한 모든 테스트를 통해 2등급 티타늄 로드 및 2등급 티타늄 라운드 바 소재가 필요한 용도에 적합한지 확인합니다. 생산 과정에서 제품의 직경, 두께 및 표면을 측정합니다.
- 배송 시간은 엄격하게 계약에 따릅니다.
- 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
- 고객 테스트를 위한 무료 샘플 지원
- 현장 또는 비디오 공장 검사 지원
패키징
상품이 다양한 경로를 거쳐 최종 목적지에 도착하는 국제화물에서 포장은 중요한 역할을 하기 때문에 대순합금은 포장에 각별한 주의를 기울이고 있으며 최고의 품질을 보장합니다. 제품에 따라 다양한 방법으로 상품을 포장합니다. 다음과 같은 다양한 방법으로 제품을 포장합니다:
- 상자 및 상자
- 수축 포장
- 목재 팔레트
- 나무 상자
기술 지원
추가 기술 지원이 필요한 경우 금속 전문가와 지식이 풍부한 직원이 기꺼이 도와드릴 것입니다. 또한 Daxun은 다중 금속 및 플라스틱 재고 업계 최초로 인증된 테스트 실험실을 보유하고 있습니다. 이는 품질에 대한 변함없는 헌신과 풀서비스 공급업체로서의 철학을 보여주는 것이라고 생각합니다.
Daxun Grade 23 Titanium Rods help your brand improve quickly
- Tolerances for Grade 23 Titanium Round Bars (BS EN ISO 286-2)
| 공칭 크기 | h5 | h6 | h7 | h8 | h9 | H10 | H11 | h12 |
|---|---|---|---|---|---|---|---|---|
| 직경 mm | ||||||||
| ~ ~ 3 | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| 3~6세 이상 | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| 6~10개 이상 | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| 10세 이상 18세 미만 | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| 18세 이상 30세 미만 | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| 30~50세 이상 | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| 50~80% 이상 | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| 80 이상 120 미만 | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| 120~180개 이상 | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| 180 이상 250 미만 | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
Types of Ti-6AL-4V Grade 23 Titanium Rods (3)
티타늄 로드
관련 제품 (8)
Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 23 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.
사양
AMS 4928 - 봉재, 단조품 및 단조 스톡(어닐링)
AMS 4965 – Bars, Forgings (Solution treated and aged)
AMS 4967 – Bars, Forgings (Annealed, Heat Treatable)
열 치료
When high hardness, tensile strength, and fatigue strength are required, annealing can be performed at 1,700-1,900°F (927 – 1,038°C).
DAXUN 6-4™ Grade 23 alloy can be heat treated in a variety of ways:
- Anneal: 1,275 – 1,400°F (691 – 760°C), ½ to 2 hours, air or furnace cool
- Stress Relief Anneal: 1,000 – 1,200°F (538 – 649°C), 1 to 8 hours, air or furnace cool
- Solution Heat Treat: 1,675 – 1,750°F (913 – 954°C), 1 hour, water quench
- Aging: 975 – 1,025°F (524 – 552°C), 4 to 8 hours – air cool
In the solution treated and aged condition, rapid quenching of small sections yields optimum properties. Larger section sizes and/or delayed quenching may result in less than optimum properties.
경도
Typical hardness in the annealed condition is Rockwell C 30-34, and about Rockwell C 35-39 in the solution and aged condition.
단조성 / 성형성
Ti-6Al-4V ELI (Grade 23) alloy bar is forged at 1,750°F (954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 35% reduction is recommended for optimum properties.
Grade 23 alloy bar is difficult to form at room temperature, even in the annealed condition. Therefore, severe forming operations such as bending or stretching can be performed on annealed material at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000 – 1,200°F (538 – 649°C).
기계 가공성
Ti-6Al-4V ELI (Grade 23) alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids.
용접성
Grade 23 titanium rod is readily weldable in the annealed condition or in the solution and partially aged condition, with aging being accomplished during post weld heat treatment. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. Spot, seam, and flash welding may be performed without the aid of a protective atmosphere.
Special Considerations
Grade 23 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics.
크기 범위
Grade 23 Titanium Bar Dimensions
Ø 0.7 – 30 mm (drawn, ground)
Ø 16 – 400 mm (hot rolled, peeled)
Tolerances: h11–h5 (ISO 286-2)
Tighter or different tolerances available on request
Lengths up to 9,000 mm long, depending on diameter
For larger diameters, other bar lengths and tolerances can be agreed upon request
Availability Grade 23 Titanium Rods
처리 옵션에는 다음이 포함됩니다:
- Drawing, straightening
- Drawing, straightening, polishing
- Drawing, grinding, polishing
- 그리기, 곧게 펴기, 연마, 연마하기
- Drawing, annealing, straightening
- Drawing, annealing, polishing
- Drawing, annealing, grinding, polishing
- Drawing, annealing, straightening, grinding, polishing
We produce bars according to your requirements.
Excellent surface and straightness, perfect roundness and tightest diameter tolerances (according to ISO 286-2 up to h5). Available in straightened, ground, polished conditions.
톱질
- Band saws (up to Ø510 mm)
- Bench band saws (up to 6,000 x 3,000 x 400 mm)
- High-performance sawing machines for precise sawing
Titanium Bar End Machining
- Single or double sided
- Chamfer 90° (45°)
- Point 60° (30°)
- Flat end
- Centered
Delivery Form
- ASTM American Society for Testing and Materials Standards
- AMS American Aerospace Materials Standards
- NACE American Association of Corrosion Engineers International Standards
- ASME American Society of Mechanical Engineers Standards
- GB Chinese National Standards
- GJB Chinese National Military Standards
- ISO International Standards
- DIN German Standards
- EN European Standards
- API American Petroleum Institute Standards
Detection Method
Non-destructive testing > 100% testing
Testing methods:
- Eddy current testing / eddy current crack testing
- Defect-free surface (level 4)
- Flat bottom hole diameter 0.7 mm and 0.4 mm
- Blind area can be cut off according to fixed length > Test to the end of the bar
- Full diameter ultrasonic testing
Our Titanium Bar Material Services
As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.
We will be happy to provide you with a consultation and explain everything you need to know about obtaining Grade 23 titanium bar material, including which standards require greater attention for the components to be manufactured.
If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.
Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 23 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.
주문 정보
Purchase orders should include quantity, grade, type or category, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.
필요한 티타늄 합금의 등급은 각 등급마다 다른 이점이 있으므로 작업 중인 프로젝트에 따라 다릅니다.
모든 등급의 티타늄 합금은 매우 강하고 부식에 강하기 때문에 가장 혹독한 환경에서도 잘 작동합니다.
더 높은 등급의 티타늄 합금(5-12)은 특정 이점을 위해 설계된 합금입니다. 예를 들어, 12등급 티타늄 합금은 내열성이 뛰어나 쉘 및 튜브 열교환기, 유압 배관 및 화학 산업 장비에 적합합니다.
1~4등급은 순수 티타늄 합금으로, 배관 시스템과 튜빙에 용접 가능한 연성 소재가 필요한 경우 완벽한 선택입니다. 그보다 낮은 등급은 해양 및 산업 산업에서 사용됩니다.
프로젝트를 시작하면서 어떤 등급의 티타늄 합금이 가장 적합한지 잘 모르겠다면 지금 바로 문의하시면 기꺼이 도와드리겠습니다.
DAXUN에서는 1등급부터 12등급까지 다양한 티타늄 합금 등급을 제공합니다.
1~4등급은 순수 티타늄이고 그 이상 등급은 합금입니다.
합금 등급은 무게 대비 강도가 높기 때문에 인기가 높습니다.
가장 일반적으로 사용되는 티타늄 합금 등급은 5등급입니다. 티타늄 함량이 여전히 높지만 이 등급은 최대 600°F의 온도와 극한의 조건을 견딜 수 있기 때문에 가장 신뢰할 수 있는 등급 중 하나입니다.
항공우주 및 해양 산업과 같은 산업에서는 내마모성과 내식성 때문에 등급이 높을수록 선호합니다.
반대로 낮은 등급은 강도가 낮기 때문에 주로 용접에 사용됩니다.
다양한 등급의 티타늄 합금의 차이점에 대해 자세히 알아보려면 지금 바로 +86 13382898899으로 전화하여 전문가와 직접 상담하세요.
티타늄의 등급에 따라 비용이 약간 증가하지만, 총 비용은 주로 필요한 티타늄의 모양과 형태에 따라 결정됩니다.
DAXUN에서는 플레이트, 튜브, 코일 및 바를 포함한 다양한 티타늄 제품을 제공합니다. 필요한 각 품목의 길이, 너비 및 수량은 결제 시 지불하는 금액에 영향을 미칩니다.
안타깝게도 프로젝트와 티타늄의 용도에 대해 잘 알지 못하면 온라인에서 가격을 책정하기 어렵습니다.
다행히도 저희 전문가 팀이 언제나 티타늄 관련 문의에 대해 도움을 드리고 조언해 드립니다. daxunalloy@gmail.com 으로 이메일을 보내주시면 몇 가지 조언과 정확한 견적을 알려드리겠습니다.
필요한 티타늄의 등급, 모양 및 수량에 대해 가능한 한 많은 정보를 포함하여 요구 사항을 더 잘 파악할 수 있도록 하세요.
DAXUN의 팀은 경험이 풍부하고 지식이 풍부하며 친절합니다. 업계에서 다년간의 경험을 바탕으로 티타늄의 용도, 장점, 등급 등 티타늄에 대한 모든 것을 잘 알고 있습니다.
티타늄, 티타늄의 용도 및 산업 전반에 걸친 티타늄의 활용에 대한 정기적인 업데이트를 확인하려면 블로그를 확인하세요. 궁금한 점이 있을 때 언제든지 참고할 수 있도록 전문가들이 쉽게 따라할 수 있는 가이드를 작성했습니다.
여전히 문제가 있는 경우 언제든지 문의해 주세요. 기꺼이 도와드리겠습니다.
daxunalloy@gmail.com 으로 이메일을 보내주시면 빠른 답변을 받으실 수 있습니다. 적합한 솔루션을 추천할 수 있도록 질문에 가능한 한 자세한 내용을 포함해 주세요.
“문의하기” 페이지의 양식을 작성하거나 영업 관리자(+86 13382898899)에게 전화하시면 최대한 빨리 연락드리겠습니다. WhatsApp은 온라인 상태이며 이메일(Daxunalloy@gmail.com)은 6시간 이내에 확인합니다. 모든 문의나 메시지는 신속하게 답변해 드립니다. 또한 매주 고객과 시장 정보를 공유합니다.
품질을 확인할 수 있도록 티타늄 막대 샘플을 제공할 수 있습니다. 샘플은 무료이며 운임만 지불하면 됩니다.
캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.
티타늄 막대의 경우 MOQ는 300Kg입니다.
체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.