- 티타늄 튜브 등급: 티타늄 튜브Grade 23 – UNS R56401
- 티타늄 튜브 유형 : 이음매없는 Ti 튜브, Ti 용접 튜브, 단조 Ti 튜브
- Titanium tube density The density of grade 23 titanium is 4.43 g/cm3
- Standards:ASTM B338/ASME SB338、ASTM B337/ASME SB337、ASTM B861/ASME SB861、ASTM B862/ASME SB862、AMS4911、AMS4928
----다순은 중국에서 티타늄 튜브를 생산하여 고객의 다양하고 -- 까다로운 요구를 충족합니다!.
Provide High Quality Grade 23 Titanium Pipe to Customers Around The World
Grade 23 titanium tubing, also known as Ti-6Al-4V ELI, is a high-strength, lightweight alloy composed of titanium with 6% aluminum and 4% vanadium in an extra-low interstitial (ELI) form.It is an improved alloy based on the classic Ti-6Al-4V (grade 5) by further reducing the content of interstitial elements such as oxygen, iron, and nitrogen (such as oxygen content ≤ 0.13%).Its extra-low interstitial (ELI) composition significantly enhances fracture toughness and fatigue resistance compared to standard titanium alloys, allowing it to perform reliably under cyclic loading conditions. The alloy maintains its impressive strength-to-weight ratio even at cryogenic temperatures, unlike many metals that become brittle in extreme cold. Additionally, Grade 23 exhibits superior corrosion resistance in both acidic and chloride environments, outperforming many stainless steels and other titanium grades in aggressive chemical settings.
Where is Grade 23 titanium pipe used?
Grade 23 titanium tubing has unique applications in cutting-edge medical devices, particularly orthopedic implants such as spinal fusion cages and joint replacement components, which require lifelong biocompatibility and fatigue resistance. It is particularly well-suited for dental implant systems, where osseointegration (a direct structural connection between bone and implant) is crucial to the long-term success of the system. In aerospace, it is the material of choice for hydraulic and fuel lines in commercial and military aircraft, which must balance weight reduction with extreme pressure requirements. The material’s properties also make it an ideal choice for high-performance bicycle frames used by professional cyclists, where its vibration-absorbing properties and fatigue resistance provide a competitive advantage.
Key Notes:
ELI (Extra Low Interstitial): Grade 23 has stricter limits on oxygen, nitrogen, hydrogen, and carbon compared to standard Grade 5 (Ti-6Al-4V) to enhance ductility and biocompatibility.
Primary alloying elements: Aluminum (Al) and vanadium (V) contribute to strength and phase stability.
Impurity control: Low iron, carbon, nitrogen, and hydrogen ensure superior corrosion resistance and fatigue performance.
Key performance:
High strength + high toughness: tensile strength can reach 895-930 MPa (annealed state), elongation ≥10%, better than ordinary Grade 5, suitable for scenes with dynamic loads.
Excellent corrosion resistance: acid resistance (such as hydrochloric acid, sulfuric acid), alkali resistance, seawater resistance, outstanding performance in medical implants and chemical equipment.
Biocompatibility: non-magnetic, non-toxic, excellent compatibility with human tissue, is the preferred material for orthopedic implants.
Processability: can be formed by forging, rolling, machining, welding performance is better than ordinary titanium alloy.
데이터
- 매개변수
- 기계적 특성
- 물리적 속성
| 요소 | Ti | Al | V | O | Fe | C | N | H | Other elements |
| 구성 범위(% 무게) | >89% | 5.50 – 6.75% | 3.50 – 4.50% | ≤ 0.13% | ≤ 0.25% | ≤ 0.08% | ≤ 0.05% | ≤ 0.0125% | ≤ 0.4% |
| 속성 | 가치 |
|---|---|
| 궁극의 인장 강도 | 860-950 MPa |
| 수율 강도 | 825-860 MPa |
| 신장 | 10-15% |
| Fatigue Strength | ~500 MPa (at 10⁷ cycles) |
| Fracture Toughness | 70-90 MPa√m |
| 경도 | 320-350 HV |
| 탄성 계수 | 90-110 GPa |
| 속성 | 가치 |
|---|---|
| 밀도 | 4.43g/cm³ |
| 녹는점 | 1660-1680°C |
| 열 전도성 | 7.2 W/m·K |
| 열팽창 계수 | 8.6 × 10⁻⁶ /°C |
| 전기 저항 | 1.78 μΩ-m |
| 비열 용량 | 560 J/kg·K |
프로젝트의 성공을 위해 Daxun을 선택하세요.

고급 프로덕션
We offer a comprehensive selection of Grade 23 titanium tubing solutions, including both welded and seamless options to meet diverse industrial requirements. Our inventory features precision-engineered tubes manufactured to the highest quality standards, ensuring optimal performance in demanding applications. Whether you need welded tubes for cost-effective solutions or seamless tubes for superior pressure capabilities, our Grade 23 titanium products deliver exceptional strength-to-weight ratios, outstanding corrosion resistance, and biocompatibility for aerospace, medical, marine, and chemical processing industries.
테스트 보고서
We provide comprehensive documentation and certification reports for all our Grade 23 titanium tubing, ensuring complete transparency and compliance with industry standards. Our documentation package includes material test reports (MTRs), chemical analysis certificates, mechanical property verification, and non-destructive testing results. Each batch of our Grade 23 titanium tubes comes with full traceability records, detailing the manufacturing process, heat treatment information, and quality assurance protocols.


품질, 배송, 검사
Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 23 Titanium Welded Pipe and Grade 23 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.
- 배송 시간은 엄격하게 계약에 따릅니다.
- 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
- 고객 테스트를 위한 무료 샘플 지원
- 현장 또는 비디오 공장 검사 지원
기술 지원
추가 기술 지원이 필요한 경우 금속 전문가와 지식이 풍부한 직원이 기꺼이 도와드릴 것입니다. 또한 Daxun은 다중 금속 및 플라스틱 재고 업계 최초로 인증된 테스트 실험실을 보유하고 있습니다. 이는 품질에 대한 변함없는 헌신과 풀서비스 공급업체로서의 철학을 보여주는 것이라고 생각합니다.

Daxun Grade 23 Titanium TUBE Let your brand improve rapidly
- 갤러리
Grade 23 titanium tube form (4)
관련 제품 (5)
Grade 23 titanium pipe (Ti-6Al-4V ELI) is an extra low interstitial version of the popular Grade 5 titanium alloy. It contains reduced levels of oxygen, iron, and other interstitial elements, which results in improved fracture toughness, better fatigue resistance, and enhanced biocompatibility while maintaining high strength-to-weight ratio.
Grade 23 titanium tubes offer excellent biocompatibility, reducing the risk of adverse reactions when implanted in the human body. They have a modulus of elasticity closer to bone than many other metals, which helps reduce stress shielding. Additionally, their superior fatigue resistance ensures long-term performance in load-bearing medical applications.
Grade 23 titanium tubes exhibit outstanding corrosion resistance in most environments, including seawater, chlorides, and acidic conditions. The protective oxide layer that forms on the surface provides exceptional resistance to pitting and crevice corrosion, making them suitable for marine and chemical processing applications.
We offer Grade 23 titanium tubes in a comprehensive range of sizes, with outer diameters from 6mm to 120mm and wall thicknesses from 0.5mm to 10mm. We can also provide custom dimensions and special tolerances to meet specific project requirements.
Yes, we can supply Grade 23 titanium tubes with various surface treatments including anodizing, passivation, polishing, and coating options. These treatments can enhance specific properties such as wear resistance, friction characteristics, or aesthetic appearance depending on your application needs.
All our Grade 23 titanium tubes undergo rigorous quality control including ultrasonic testing, eddy current inspection, and dimensional verification. We provide full material traceability and complete documentation including chemical analysis, mechanical properties, and non-destructive testing reports with every order.
티타늄의 등급에 따라 비용이 약간 증가하지만, 총 비용은 주로 필요한 티타늄의 모양과 형태에 따라 결정됩니다.
DAXUN에서는 튜브, 튜브, 코일 및 바를 포함한 다양한 티타늄 제품을 제공합니다. 필요한 각 품목의 길이, 너비 및 수량은 결제 시 지불하는 금액에 영향을 미칩니다.
안타깝게도 프로젝트와 티타늄의 용도에 대해 잘 알지 못하면 온라인에서 가격을 책정하기 어렵습니다.
다행히도 저희 전문가 팀이 언제나 티타늄 관련 문의에 대해 도움을 드리고 조언해 드립니다. daxunalloy@gmail.com 으로 이메일을 보내주시면 몇 가지 조언과 정확한 견적을 알려드리겠습니다.
필요한 티타늄의 등급, 모양 및 수량에 대해 가능한 한 많은 정보를 포함하여 요구 사항을 더 잘 파악할 수 있도록 하세요.
“문의하기” 페이지의 양식을 작성하거나 영업 관리자(+86 13382898899)에게 전화하시면 최대한 빨리 연락드리겠습니다. WhatsApp은 온라인 상태이며 이메일(Daxunalloy@gmail.com)은 6시간 이내에 확인합니다. 모든 문의나 메시지는 신속하게 답변해 드립니다. 또한 매주 고객과 시장 정보를 공유합니다.
We can provide titanium tube samples for you to check the quality. Sample is free and you just pay the freight.
체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.