Daxun is a 316/316L stainless steel channel supplier in China
As a leading stainless steel channel steel supplier and exporter in China, Daxun supplies stainless steel channel steel to all over the world.
- Brand: S31600 (316) – S31603 (316L)
- Delivery status: hot rolling, laser fusion, press bending
- Surface treatment: pickling, bright, polished, mirror, hairline
- Standards: ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227
- With full traceability and original factory test reports.
- building structure, architectural structure, engineering structure
Introduction to Austenitic Stainless Steel
Austenitic stainless steel is a type of stainless steel alloy that contains a high percentage of chromium and nickel. Known for its excellent corrosion resistance, high ductility and good formability, austenitic stainless steel is used in a wide range of industries. Its unique combination of properties makes it ideal for applications in the construction, automotive and food processing industries. This type of stainless steel stands out for its ability to withstand harsh environments while maintaining its structural integrity and aesthetics.
Veri
- Parametre
- Element
- Mekanik Özellikler
- FİZİKSEL ÖZELLİKLER
- Tüm eşdeğerler
| standard | ASTM、EN、DIN、JIS、ASME、BS、GB等, |
| aspect | C5-C30 |
| alloy | 201、310、304、304L、316、316L |
| type | U-slot, C-slot, |
| length | 1.0-12.0 m |
| thickness | 3mm to 25mm |
| Customization options | Evet |
| tolerance | ± ¼”, ± 1/16” |
| Bitirmek | Grinding machine, brush, mirror, polishing |
| Chemical composition: ASTM A240, A666 | ||
| element | Tip 316 | Tip 316L |
| carbon | Max. 0.08. | Max. 0.030. |
| manganese | 2.00 maks. | 2.00 maks. |
| sulfur | Max. 0.030. | Max. 0.030. |
| phosphorus | Max. 0.045. | Max. 0.045. |
| silicon | Max 0.75. | Max 0.75. |
| chromium | 16.0 - 18.0 | 16.0 - 18.0 |
| nickel | 10.00 - 14.00 | 10.00 - 14.00 |
| molybdenum | 2.00 - 3.00 | 2.00 - 3.00 |
| nitrogen | Max 0.10. | Max 0.10. |
| type | Yield Strength 0.2% Deviation (KSI) | Tensile Strength(KSI) | % Elongation (2″ Gauge Length) |
| 316 | 30 mins | 75 minutes | 40 mins |
| 316L | 25 mins | 70 minutes | 40 mins |
| Density (psi) @ RT | 0.29 | |
| Tensile modulus (psi x 10^6) | XXVIII | |
| Specific heat (BTU/o F/lb.) | 32 to 212 degrees Fahrenheit | 0.12 |
| Thermal Conductivity (BTU/hour/square foot/foot) | 212 degrees Fahrenheit | 9.4 |
| 932 degrees Fahrenheit | 12.4 | |
| Average Coefficient of Thermal Expansion (inches x 10^-6 per oF) | 32 ila 212oF | 8.9 |
| 32 ila 600oF | 9 | |
| 32 ila 1,000oF | 9.7 | |
| 32 ila 1,200oF | 10.3 | |
| Resistivity (microohm-cm) | At 70oF | 29.4 |
| Melting Point Range (°F) | 2500 - 2550 |
| grade | Çin | UNS Numarası | Old England | European Standards | İsveç SS | Japan JIS | ||
| Bachelor’s degree | kindness | Hayır | İsim | |||||
| 316 | 06Cr17Ni12Mo2 | S31600 | 304S11 | 58E | 1.4401 | X5CrNiMo17-12-2 | 2347 | Stainless Steel 316 |
Daxun'u seçin ve müşterilerinizi memnun edin.

Composition and Properties
Austenitic stainless steels typically contain 16-18% chromium, 10-14% nickel and 2-3% molybdenum. The addition of molybdenum significantly improves the corrosion resistance of the alloy, especially in chloride-rich environments. This composition not only provides excellent corrosion resistance, but also outstanding mechanical properties such as high tensile strength, good ductility and excellent weldability. These properties make austenitic stainless steels a versatile material suitable for a variety of demanding applications.
Corrosion Resistance and Heat Resistance
Austenitic stainless steel is known for its excellent corrosion resistance, especially in acidic and chloride environments. This makes it ideal for applications that require high strength and maximum corrosion resistance. In addition, it is resistant to stress corrosion cracking, further increasing its durability in harsh conditions. Austenitic stainless steel also has good heat resistance and can withstand temperatures up to approximately 870°C. This combination of properties ensures that it performs reliably in both high temperature and corrosive environments.

Paketleme
Daxun Alloy, malların nihai varış noktasına ulaşmak için çeşitli kanallardan geçtiği uluslararası taşımacılıkta önemli bir rol oynadığı için en iyi ambalaj kalitesini sağlar, bu nedenle ambalajlamaya özel önem veririz. Ürünlerimizi ürüne bağlı olarak birçok şekilde paketliyoruz. Ürünlerimizi aşağıdaki gibi birçok şekilde paketliyoruz:
- Kutular ve kasalar
- Shrink ambalaj
- Ahşap paletler
- Ahşap kutular
Kalite, teslimat, denetim
- At Daxun, we carry out several quality checks to ensure product reliability. These checks include tests for flattening, corrosion resistance, mechanical properties, hardness, material verification, and expansion. Each test guarantees that our stainless steel meets the needs of your applications.During production, we monitor the diameter, thickness, and surface quality carefully. Our standard delivery time is between 7-15 days, with special sizes taking up to 20 days. All deliveries are made on time, strictly following the contract terms.
- Müşterinin üçüncü taraf acentelerinin denetim için fabrikaya gitmesine destek olun
- Test için müşterilere ücretsiz numune desteği
- Yerinde veya video fabrika denetimini destekleyin

Sipariş Bilgileri
To reach us, please fill out the form on the “Contact Us” page or call our sales manager at +86 13382898899. We will respond as soon as possible. You can also contact us through WhatsApp or email us at Daxunalloy@gmail.com, which is checked every 6 hours. We reply promptly to all messages. We also share market updates with our customers each week to keep them informed.
Teknik Destek
Herhangi bir ek teknik yardıma ihtiyacınız olursa, yerleşik metalürji uzmanımız ve bilgili personelimiz size yardımcı olmaktan memnuniyet duyacaktır. Ayrıca Daxun, çoklu metal ve plastik envanter endüstrisinde bir ilk olan sertifikalı bir test laboratuvarına sahiptir. Bu, bize göre, kaliteye olan sarsılmaz bağlılığımızı ve tam hizmet tedarikçisi olarak felsefemizi göstermektedir.

SS 316-316L Austenitic Stainless Steel Channel Features
Daxun Alloy Markanızın hızla gelişmesine izin verin
- Şartname Tablosu
- Galeri
| Channel steel cross-sectional dimensions, cross-sectional area and theoretical weight table | ||||||||
| model | size | Sectional area | Theoretical weight | |||||
| h | b | d | t | r | r 1 | |||
| (mm) | (cm2) | (kg/m) | ||||||
| 5 | 50 | 37 | 4.5 | 7 | 7 | 3.5 | 6.925 | 5.44 |
| 6.3 | 63 | 40 | 4.8 | 7.5 | 7.5 | 3.8 | 8.446 | 6.63 |
| 6.5 | 65 | 40 | 4.3 | 7.5 | 7.5 | 3.8 | 8.292 | 6.51 |
| 8 | 80 | 43 | 5 | 8 | 8 | 4 | 10.24 | 8.04 |
| 10 | 100 | 48 | 5.3 | 8.5 | 8.5 | 4.25 | 12.74 | 10 |
| 12 | 120 | 53 | 5.5 | 9 | 9 | 4.5 | 15.36 | 12.1 |
| 12.6 | 126 | 53 | 5.5 | 9 | 9 | 4.5 | 15.69 | 12.3 |
| 14a | 140 | 58 | 6 | 9.5 | 9.5 | 4.8 | 18.51 | 14.5 |
| 14b | 60 | 8 | 21.31 | 16.7 | ||||
| 16a | 160 | 63 | 6.5 | 10 | 10 | 5 | 21.95 | 17.2 |
| 16b | 65 | 8.5 | 25.15 | 19.8 | ||||
| 18a | 180 | 68 | 7 | 10.5 | 10.5 | 5.2 | 25.69 | 20.2 |
| 18b | 70 | 9 | 29.29 | 23 | ||||
| 20a | 200 | 73 | 7 | 11 | 11 | 5.5 | 28.83 | 22.6 |
| 20b | 75 | 9 | 32.83 | 25.8 | ||||
| 22a | 220 | 77 | 7 | 11.5 | 11.5 | 5.8 | 31.83 | 25 |
| 22b | 79 | 9 | 36.23 | 28.5 | ||||
| 24a | 240 | 78 | 7 | 12 | 12 | 6 | 34.21 | 26.9 |
| 24b | 80 | 9 | 39.01 | 30.6 | ||||
| 24c | 82 | 11 | 43.81 | 34.4 | ||||
| 25a | 250 | 78 | 7 | 12 | 12 | 6 | 34.91 | 27.4 |
| 25b | 80 | 9 | 39.91 | 31.3 | ||||
| 25c | 82 | 11 | 44.91 | 35.3 | ||||
| 27a | 270 | 82 | 7.5 | 12.5 | 12.5 | 6.2 | 39.27 | 30.8 |
| 27b | 84 | 9.5 | 44.67 | 35.1 | ||||
| 27c | 86 | 11.5 | 50.07 | 39.3 | ||||
| 28a | 280 | 82 | 7.5 | 12.5 | 12.5 | 6.2 | 40.02 | 31.4 |
| 28b | 84 | 9.5 | 45.62 | 35.8 | ||||
| 28c | 86 | 11.5 | 51.22 | 40.2 | ||||
| 30a | 300 | 85 | 7.5 | 13.5 | 13.5 | 6.8 | 43.89 | 34.5 |
| 30b | 87 | 9.5 | 49.89 | 39.2 | ||||
| 30c | 89 | 11.5 | 55.89 | 43.9 | ||||
| 32a | 320 | 88 | 8 | 14 | 14 | 7 | 48.5 | 38.1 |
| 32b | 90 | 10 | 54.9 | 43.1 | ||||
| 32c | 92 | 12 | 61.3 | 48.1 | ||||
| 36a | 360 | 96 | 9 | 16 | 16 | 8 | 60.89 | 47.8 |
| 36b | 98 | 11 | 68.09 | 53.5 | ||||
| 36c | 100 | 13 | 75.29 | 59.1 | ||||
| 40a | 400 | 100 | 10.5 | 18 | 18 | 9 | 75.04 | 58.9 |
| 40b | 102 | 12.5 | 83.04 | 65.2 | ||||
| 40c | 104 | 14.5 | 91.04 | 71.5 | ||||
SS 316 /316L Stainless Steel Channel Type (3)
Referans ve indirme için mevcut bilgiler
Daxun is a trustworthy stainless steel channel manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified to ISO9001, SGS, CE, OQC and more international quality standards. Stainless steel is an iron alloy known for its specific composition and unique properties, especially 316 stainless steel, which is classified as austenitic, non-magnetic and highly corrosion-resistant. We also conduct strict quality control to ensure that stainless steel channels have fewer defects. At Daxun, you can rest assured that all products are durable, high-quality and excellent in performance.
Güncel sıcak vaka projeleri ve ürünleri
Daxun has been engaged in international business for more than ten years. In 2023, the export volume exceeded 100 million US dollars, and the export volume ranked among the top Chinese stainless steel manufacturers. Daxun continuously improves its service skills. To serve the global market, it has established three export service facilities in China, cooperating with engineering companies, steel mills, and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relations with dozens of well-known steel mills around the world. The inventory includes 50,000 tons of conventional stainless steel and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of stable quality, and the varieties, specifications, and delivery weights strictly meet the standards.
Our stock of stainless steel channels includes hot rolled channels and laser fused channels, and we have the sizes and grades you need for immediate shipment. Grades include: 316 and 304. We also stock specialty products, non-standard sizes, and offer a quick turnaround finish service for commercial customers.
Whether you are looking for a large stock, or a smaller requirement from one of our domestic customers, we are here to help. Our friendly and experienced team can help you decide which size, grade and finish will suit you best. So for more information, help and advice please email: daxunalloy@gmail.com
- ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227
Corrosion resistance (depending on alloy content), heat resistance, good hot and cold working properties, toughness and excellent overall performance. Suitable for a wide range of applications. In addition, these materials are highly durable even in harsh environments, making them ideal for industrial use. They also have good weldability and formability, which makes them easier to form into different shapes and structures, providing flexibility for custom projects. Austenitic stainless steels such as 316 have lower thermal conductivity compared to ferritic steels, which affects their expansion and melting points, making them perform well in extreme temperature conditions.
- ASTM A276
- ASTM A484
- ASTM A479
- ASME SA479
-
ASTM A1069/A1069M/11
- ASTM A276
- ASTM A484
- ASTM A479/A479
Samples can be provided free of charge, but the freight is borne by the customer and will be refunded after cooperation.
Our minimum order quantity for stainless steel channels is 1 ton.
Trial orders can be shipped within a week, regular orders take about two weeks.