What is Hastelloy

Hastelloy refers to a type of nickel-based alloy with excellent corrosion resistance. This type of alloy is composed of elements such as nickel, molybdenum, and chromium. It may also contain elements such as iron, tungsten, and copper to give the alloy specific properties. Hastelloy is a series of alloys developed by Haynes International, Inc. in the United States. They are mainly used in chemical, petrochemical, marine and other harsh corrosive environments.

The characteristics of Hastelloy include:

  • Corrosion resistance: It has good corrosion resistance in oxidizing, reducing and mixed corrosive media.
  • Heat resistance: It can maintain its mechanical properties and corrosion resistance at high temperatures.
  • Strength and toughness: It has good mechanical strength and good toughness.

Common Hastelloy Alloy Grades & Chemical Compositions

Common Hastelloy grades include:

  • Hastelloy B-3 (UNS N10675): has excellent corrosion resistance in reducing environments, especially in hydrochloric acid, and has better weldability and thermal stability than B-2 alloy.
  • Hastelloy C-276 (UNS N10276): a widely used grade with excellent resistance to pitting, crevice corrosion and stress corrosion cracking, suitable for a variety of corrosive environments.
  • Hastelloy C-22 (UNS N06022): provides better pitting and crevice corrosion resistance than C-276, suitable for more demanding corrosive environments.
  • Hastelloy C-4 (UNS N06455): the main feature is resistance to hot concentrated sulfuric acid corrosion, suitable for chemical and petrochemical industries.
  • Hastelloy C-2000: combines the advantages of C-276 and C-22, providing excellent resistance to pitting, crevice corrosion and stress corrosion cracking.
  • Hastelloy G-30 (UNS N06030): Especially suitable for resistance to sulfuric acid corrosion, including high concentrations of hot sulfuric acid.
  • Hastelloy G-35 (UNS N06035): Similar to G-30, it is also an alloy for resistance to sulfuric acid corrosion, but has a different alloy composition to suit specific applications.
  • Hastelloy X (UNS N06002): It has excellent high-temperature strength and oxidation resistance and is suitable for high-temperature applications such as gas turbines.

These grades are the more common ones in Hastelloy alloys. They play an important role in different industrial applications, especially where corrosion resistance is required.

Major Constituent Elements Hastelloy Grades
B3 C-276 C-22 C-4 C-2000 G30 G35 X
Ni 65% max 55-59% 58% 60% 59% 37% 43-48% 47.5-52%
Mo 27-32% 15-17% 13% 16% 15-17% 4-6% 18-22% 8-10%
Fe 1-3% 4-7% 3% 3% 3% 13-17% 1.50% 17-20%
Cr 1-3% 14.5-16.5% 20% 18% 22-24% 28.5-31.5% 17-21% 20.5-23%
W 3% max 3-4.5% 4% 3% max 0.8% max 1.5-4% 10% Tr.
Co 3% max 2.5% max 2.5% max 2% max 2% 5% max 5% 0.5-2.5%

 

Hastelloy B3

Commonly used Hastelloy grades and products

Hastelloy B3 Pipe
Hastelloy B3 Boru
Hastelloy B3 Coil
Hastelloy B3 Coil
Hastelloy B3 Bar
Hastelloy B3 Bar
4 Ürün Bulundu.

Hastelloy C-276

Hastelloy C-276 Plate
Hastelloy C-276 Plaka
Hastelloy C-276 Pipe
Hastelloy C-276 Boru
Hastelloy C-276 Coil
Hastelloy C-276 Coil
Hastelloy C-276 Bar
Hastelloy C-276 Bar
4 Ürün Bulundu.

Hastelloy C-22

Hastelloy Plate
Hastelloy C-22 Plaka
Hastelloy C-22 Pipe
Hastelloy C-22 Boru
Hastelloy C-22 Coil
Hastelloy C-22 Coil
Hastelloy C-22 Bar
Hastelloy C-22 Bar
4 Ürün Bulundu.

Hastelloy C-4

Hastelloy Plate
Hastelloy C-4 Plaka
Hastelloy C-4 Pipe
Hastelloy C-4 Boru
Hastelloy C-4 Coil
Hastelloy C-4 Coil
Hastelloy C-4 Bar
Hastelloy C-4 Bar
4 Ürün Bulundu.

Hastelloy C-2000

Hastelloy C-2000 plate
Hastelloy C-2000 Plate
Hastelloy C-2000 pipe
Hastelloy C-2000 Pipe
Hastelloy C-2000 Coil
Hastelloy C-2000 Coil
Hastelloy C-2000 bar
Hastelloy C-2000 Bar
4 Ürün Bulundu.

Hastelloy G30

Hastelloy G30 Plate
Hastelloy G30 Plaka
lnconel pipe
Hastelloy G30 Boru
Hastelloy G30 coil
Hastelloy G30 Coil
Hastelloy G30 bar
Hastelloy G30 Bar
4 Ürün Bulundu.

Hastelloy G35

Hastelloy G35 plate
Hastelloy G35 Plaka
titanium pipe
Hastelloy G35 Boru
lnconel coil
Hastelloy G35 Coil
Hastelloy G35 bar
Hastelloy G35 Bar
4 Ürün Bulundu.

Hastelloy X

lnconel plate
Hastelloy X Plaka
Hastelloy X Pipe
Hastelloy X coil
Hastelloy X Coil
Hastelloy X bar
Hastelloy X Bar
4 Ürün Bulundu.
Elinizde hiç stok var mı?

Evet, eksiksiz teknik özelliklere ve envantere sahibiz ve ihtiyaçlarınızı hızlı bir şekilde karşılayabiliriz.

Özelleştirilebilir mi?

Evet, özelleştirilebilir. Bizimle iletişime geçebilir ve özelleştirilmiş özellikleri ve miktarı bize gönderebilirsiniz.

Malları nasıl gönderiyorsunuz?

Taşıma yöntemlerimiz genellikle deniz taşımacılığı, kara taşımacılığı ve deniz taşımacılığını içerir. Size hızlı ve güvenli bir şekilde ulaşın.

Fiyatınız ne kadar?

Üretimimiz yüksek olduğu için maliyet çok daha düşük olacaktır, bu nedenle fiyat düşüktür.

Biraz örnek alabilir miyim?

Kaliteyi kontrol etmeniz için paslanmaz çelik sac örnekleri sağlayabiliriz. Numune ücretsizdir ve siz sadece navlunu ödersiniz.

Kaliteniz nasıl?

Ürün kalitesine büyük önem veriyoruz ve çeşitli kalite sistem testlerinden geçtik.

Sorgunuzu Bugün Gönderin
Hızlı Alıntı