Daxun 304 stainless steel plate and sheet China supplier
As China’s leading stainless steel plate supplier and exporter, Daxun provides stainless steel plates to the world.
- Grade: AISI 304/S30400
- Производство: холоднокатаный лист, горячекатаный лист, кованый лист
- Стандарты: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Тип: холоднокатаный тонкий лист, горячекатаный толстый лист
- Поверхность: 2B, NO.1, NO.4, HL, BA, 8K и т.д.
- Длина: 2438мм3048мм6000мм может быть настроен
- Происхождение: TISCO, Baosteel, Posco, Tsingshan, Delong
Мировой лидер в области производства листов из нержавеющей стали
304 is one of the most popular grades of stainless steel because of its high strength, excellent corrosion resistance, and excellent formability. This grade has a low carbon content and excellent ductility. It can be cold worked by roll forming, deep drawing, and bending. This grade is suitable for forming complex shapes. You will see this grade in the oil and gas industry and the food service industry.Our 304 series is a standout product available in thicknesses from 0.4mm to 120mm.
Daxun is your trusted stainless steel sheet supplier.By choosing our 304stainless steel plates, you are investing in a material that guarantees long life, reliability and superior performance. Don’t compromise on quality – choose our stainless steel solutions and experience the difference they can make in your projects. Contact us today for more details or to order your required specifications and quantities.
Данные
- Параметр
- Состав и свойства
- Механические свойства
- ФИЗИЧЕСКИЕ СВОЙСТВА
| Stainless Plate and sheet Type | Plate, Sheet, Strip, Coils, Foils, Flats, Clad Plate, Plain Sheet, Rolling Sheet, Rolling Plate, Flat Shim, Flat Sheet, Shim Sheet, Rolls, Blank (Circle), sheared, annealed, soft annealed, descaled, tread plate, Checker Plate |
| Стандарт | ASTM A240 / ASME SA240 ASTM/ASME A240/480,JIS 4305,DIN EN 10088-2JIS, AISI, ASTM, GB, DIN, EN, etc |
| Stainless Steel Plate and sheet Length | 1000mm-13000mm or as required |
| 304 Stainless Plate Width | 1000mm-1219mm-1500mm-1800mm-2000mm-2500mm or as required |
| UNS 304 Plate Thickness | 0.3 to 120mm or as required |
| ASTM A240 Stainless Steel 304 Plate Process | Hot/ Cold Rolled/forging |
| UNS 304 Plate surface | No.1, No. 2D, No. 2B, BA, No.3, No.4, No.6, No.7, 2B, 2D, BA NO(8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled ASTM A240Stainless Steel 304 Plate, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc. |
| Stainless 304 Sheet ASTM | ASTM A240 |
| Stainless 304 Sheet AMS | ASTM 240 |
| Tolerances of width and thickness | ASTM-ASME-GB-EN-DIN-JIS |
| 304 Stainless Plate standards and approvals | EN ISO 18286 EN 10051 EN 10088-1 ISO 15510 EN ISO 9445 ASTM A 480 ASTM A 959 ASME IID |
| 304 Plate & Sheet Sizes | 1000 x 2000 mm, 1220 x 2440 mm, 1500 x 3000 mm, 2000 x 2000 mm, 2000 x 4000 mm,1500*6000,Cold rolled 304 Stainless Plate 0.5-6.4 mm,Hot rolled 304 Stainless Plate 3.0–60.0 mm |
| UNS 304 Plate Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard ASTM A240Stainless Steel 304 Sheet suppliers |
| Cutting | To provide a comprehensive service, we use a variety of cutting methods, including:Laser Plate Cutting,Plasma Plate Cutting,Oxy-propane Flame Cutting |
| Plasma profiles | As per customer’s drawings |
| Value added services for 304 Stainless Plate | Laser cutting, Waterjet cutting, Plasma cutting, Bending and mechanical processing, edge preparation, welding, sawing and shearing. |
| Производитель | POSCO, Aperam, ATI, ThyssenKrupp, Baosteel, TISCO, ArcelorMittal, VDM, Nippon Metal, Outokumpu, Tsingshan, Delong. |
| China 304 Stainless Plate Manufacturer | ASTM A240Stainless Steel 304 Plate: material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width;304 Stainless Sheet: material under 3/16″ [5.00 mm] in thickness and 24″ [600 mm] and over in width;Steel Stainless 304 Clad plate: Steel Stainless 304 Clad plate is a composite steel plate made by bonding 304 Stainless 304 Plate, etc.ASTM A240Stainless Steel 304 Strip: cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width. |
| 304 Plate Origin | КИТАЙ |
| Packing of 304 plate | Bundles with waterproof cloth outside or plywood box |
| Test | UT, SGS testing, TUV etc |
| Why buy 304 Sheet from DAXUN? | Free quote、Free sample、EN 10204 3.1、Mill Test Certificate is supplied with shipment、 TestGrade: AISI 304/S30400 Производство: холоднокатаный лист, горячекатаный лист, кованый лист Стандарты: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS Тип: холоднокатаный тонкий лист, горячекатаный толстый лист Поверхность: 2B, NO.1, NO.4, HL, BA, 8K и т.д. Length: 2438mm/3048mm/6000mm can be customized Происхождение: TISCO, Baosteel, Posco, Tsingshan, Delong |
| Стандарт | Werkstoff Nr. | UNS | JIS | BS | ГОСТ | AFNOR | EN | CN |
| SS 304 | 1.4301 | S30400 | SUS 304 | 304S31 | 08Х18Н10 | Z7CN18‐09 | X5CrNi18-10 | 06Cr19Ni10 |
| Класс | C | Mn | Si | P | S | Cr | Ni | N |
| 304 | ≤0.08% | ≤2.0% | ≤ 0.75% | ≤0.045% | ≤0.030% | 18%-20% | 8.0%-10.5% | ≤0.10% |
| Тип | Предел текучести 0,2% смещение (KSI) | Прочность на разрыв (KSI) | % Elongation(2″ Gauge length) |
| 304 Ann | 30 min. | 75 мин. | 40 min. |
| 304 ¼ Hard | 75 мин. | 125 мин. | 12 min. |
| 304 ½ Hard | 110 мин. | 150 мин. | 7 min. |
| 304L Ann | 25 min. | 70 min. | 40 min. |
| 304L ¼ Hard | 75 мин. | 125 мин. | 12 min. |
| 304L ½ Hard | 110 мин. | 150 мин. | 6 min. |
| 304 & 304L | ||
| Плотность (фунт/дюйм^2) @ RT | 0.29 | |
| Модуль упругости при растяжении (psi x 10^6) | 28 | |
| Удельная теплота (BTU/Ф/фунт) | От 32 до 212 oF | 0.12 |
| Теплопроводность (BTU/hr/ft^2/ft) | 212oF | 9.4 |
| 932oF | 12.4 | |
| Средний коэффициент теплового расширения (в дюймах x 10^-6 на o F) | От 32 до 212oF | 9.2 |
| От 32 до 600oF | 9.9 | |
| От 32 до 1,000oF | 10.2 | |
| 32 to 1,200oF | 10.4 | |
| Электрическое сопротивление (микро Ом - см) | при 70oF | 72 |
| Диапазон температуры плавления (oF) | 2550 to 2650 | |
| Стойкость к окислению - непрерывная эксплуатация(oF) | 1,650 | |
| Стойкость к окислению - периодическая эксплуатация(oF) | 1,500 |
Выберите Daxun и сделайте своих клиентов довольными.

Быстрая доставка
Daxun provides customers with timely and fast delivery of stainless steel plate products. Behind the speed is the system support from production capacity, information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Быстрый ответ
Daxun saves customers time, materials and stress, and ultimately saves them costs. With its professional advantages, Daxun can provide the most cost-optimized material recommendations based on customer needs, and can also reduce costs for customers through continuous processing, nesting processing, etc.

Передовая обработка
Our advanced nesting processing method improves material utilization and cutting utilization. At the same time, Daxun can also achieve continuous cost reduction and efficiency improvement by promoting lean improvement activities, and return the benefits to customers.
304 stainless steel plate packaging
Daxun Alloy ensures the best quality of 304 stainless steel sheet packaging, because packaging plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Коробки и ящики
- Крафт-бумага + деревянные поддоны
- Термоусадочная пленка
- Деревянные поддоны без фумигации
- Деревянные ящики без фумигации

304 Stainless Steel Sheet Processing:
- Обработка травлением
- Сварочная обработка
- Обработка гибки
- Обработка тиснения
- Пескоструйная обработка
- Полировальная обработка
- Обработка перфорации
- Штамповочная обработка
SS 304 Plate Surface Treatment
1D: поверхность матовая с прерывистой формой частиц.
2D: Белый с серебристым оттенком.
2B: серебристо-серый цвет с лучшим блеском и плоскостностью по сравнению с 2D-поверхностью.
Ба: Близкая к зеркальной поверхность с превосходным блеском и отражающей способностью.
No.3: Хороший блеск и шероховатая поверхность.
No.4: Поверхность имеет тонкие линии и хороший блеск.
ХЛ: Серебристо-серые с золотом волосы.
8K: Зеркальная поверхность.
304 plate stainless steel Features
Let your brand improve rapidly
- Галерея
- TOLERANCE
- DELIVERY STATE
- Другие серии продукции
| Допуск для листа 2B | |||
| Размер | Рейтинг толерантности | ||
| Группа 1 | Группа 2 | Группа 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Допуски для горячекатаного листа № 1 | |||
| Размер | Рейтинг толерантности | ||
| Группа 1 | Группа 2 | Группа 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Выбор государства доставки | Состояние поверхности |
| Холодная прокатка | 2B |
| 2D | |
| BA | |
| Линия роста волос | |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Примечание: | |
| 1. Если вам требуется другое состояние доставки, чем перечисленные выше, пожалуйста, подтвердите с нами. | |
| 2. В случае запроса или заказа, пожалуйста, сообщите нам о любых дополнительных требованиях, не указанных здесь. | |
| Состояние доставки | |
| Выбор государства доставки | Состояние поверхности |
| Горячекатаный | No.1 |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Маринованные | |
| Примечание: | |
| 1. Если вам требуется другое состояние доставки, чем перечисленные выше, пожалуйста, подтвердите с нами. | |
| 2. В случае запроса или заказа, пожалуйста, сообщите нам о любых дополнительных требованиях, не указанных здесь. | |
| Класс | Тип | Толщина | Поверхность |
| Аустенитные | 304/304H/304L/304J1 | 0,25-150 мм | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80 мм | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0,3-80 мм | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Феррит | 430 | 0,4-3,0 мм | 2B/BA/NO.4/8K/SB/HL |
| Сверхчистый феррит | 443 | 0,4-2,0 мм | 2B |
| 436L/439/444/441 | 0,5-3,0 мм | 2B、2D | |
| 409L | 0,4-2,5 мм | 2B、2D | |
| Класс | Тип | Толщина | Оригинал |
| Жаропрочная сталь | 309S | 0,5-40 мм | CHN |
| 310S | 0,5-40 мм | CHN | |
| Дуплексная сталь | 2101 | 1,5-50 мм | CHN |
| 2304 | 3.0-50 мм | CHN | |
| 2205 | 0,5-60 мм | CHN | |
| 2507 | 1.0-60 мм | ПОТ / ИСПАНИЯ / КИТАЙ | |
| Супер аустенитная сталь | N08904 | 0,6-50 мм | ПОТ / ИСПАНИЯ / КИТАЙ |
| S31254 | 0,5-50 мм | ПОТ / ИСПАНИЯ / КИТАЙ | |
| N08926 | 0,5-50 мм | ПОТ / ИСПАНИЯ / КИТАЙ | |
| N08367 | 0,5-50 мм | ПОТ / ИСПАНИЯ / КИТАЙ | |
| Сплав на основе никеля | N08031 | 1.0-50 мм | США / JPN / GER |
| N08810/N08800 | 0,8-50 мм | США / JPN / CHN | |
| N08028 | 1,0-20 мм | США / ГЕРМАНИЯ / ЯПОНИЯ | |
| N08020 | 1,0-20 мм | США / ГЕРМАНИЯ / ЯПОНИЯ | |
| N08825 | 0,8-40 мм | США / ГЕРМАНИЯ / ПОТ / ЯПОНИЯ / КИТАЙ | |
| N10276 | 0,5-50 мм | США / ГЕРМАНИЯ / ЯПОНИЯ | |
| N06022 | 1.0-50 мм | США / ГЕРМАНИЯ / ЯПОНИЯ | |
| N06625 | 0,8-20 мм | США / ГЕР / ЧН | |
| N04400 | 1,0-20 мм | США / ГЕРМАНИЯ / ЯПОНИЯ | |
| N06600 | 1.0-50 мм | США / ГЕРМАНИЯ / ЯПОНИЯ / КИТАЙ | |
| N02201 | 0,5-20 мм | США / ЯПОНИЯ | |
| Титан | TA1/Gr1 | 0,5-50 мм | JPN / CHN |
| TA2/Gr2 | 0,5-50 мм | JPN / CHN | |
| Сварочный материал | ERNiCrMo-13 | 1.2、2.4 мм | GER |
| ERNiCrMo-3 | 2,4 мм | GER | |
| ERNiCrMo-4 | 2,4 мм | США |
The surface and shape of 304 stainless steel plate (6)
Информация доступна для ознакомления и скачивания
Daxun является надежным производителем листов из нержавеющей стали
Как профессиональный производитель, Daxun гарантирует, что все продукты, которые мы производим, имеют высокое качество. Поэтому мы гарантируем, что все пластины из нержавеющей стали сертифицированы по ISO9001, SGS, CE, OQC и другим международным стандартам качества. Мы также осуществляем строгий контроль качества, чтобы гарантировать, что пластины из нержавеющей стали имеют меньше дефектов. В Daxun, будьте уверены, что все продукты являются долговечными, высококачественными и высокопроизводительными.
Последние проекты и продукты для горячих случаев
Сопутствующие товары (13)
Мы можем предоставить вам образцы листов из нержавеющей стали для проверки качества. Образец бесплатен, и вы просто оплачиваете перевозку.
Мы экспортировали продукцию в более чем 42 страны, такие как Канада, Чили, Кувейт, Германия, Южная Корея, Саудовская Аравия, Сингапур и др.
Наш MOQ составляет 1 тонну для листов из нержавеющей стали.
Пробные заказы могут быть доставлены в течение недели. Для обычных заказов требуется примерно две недели.