Daxun 304 stainless steel plate and sheet China supplier
As China’s leading stainless steel plate supplier and exporter, Daxun provides stainless steel plates to the world.
- Grade: AISI 304/S30400
- Fabricación: chapa laminada en frío, chapa laminada en caliente, chapa forjada
- Estándar: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Tipo: chapa fina laminada en frío, chapa gruesa laminada en caliente
- Superficie: 2B, NO.1, NO.4, HL, BA, 8K, etc.
- Longitud: 2438mm3048mm6000mm se puede personalizar
- Origin: TISCO, Baosteel, Posco, Tsingshan, Delong
Líder mundial en servicios de fabricación de chapa de acero inoxidable
304 is one of the most popular grades of stainless steel because of its high strength, excellent corrosion resistance, and excellent formability. This grade has a low carbon content and excellent ductility. It can be cold worked by roll forming, deep drawing, and bending. This grade is suitable for forming complex shapes. You will see this grade in the oil and gas industry and the food service industry.Our 304 series is a standout product available in thicknesses from 0.4mm to 120mm.
Daxun is your trusted stainless steel sheet supplier.By choosing our 304stainless steel plates, you are investing in a material that guarantees long life, reliability and superior performance. Don’t compromise on quality – choose our stainless steel solutions and experience the difference they can make in your projects. Contact us today for more details or to order your required specifications and quantities.
Datos
- Parámetro
- Ingredients and properties
- Propiedades mecánicas
- PROPIEDADES FÍSICAS
| Stainless Plate and sheet Type | Plate, Sheet, Strip, Coils, Foils, Flats, Clad Plate, Plain Sheet, Rolling Sheet, Rolling Plate, Flat Shim, Flat Sheet, Shim Sheet, Rolls, Blank (Circle), sheared, annealed, soft annealed, descaled, tread plate, Checker Plate |
| Estándar | ASTM A240 / ASME SA240 ASTM/ASME A240/480,JIS 4305,DIN EN 10088-2JIS, AISI, ASTM, GB, DIN, EN, etc |
| Stainless Steel Plate and sheet Length | 1000mm-13000mm or as required |
| 304 Stainless Plate Width | 1000mm-1219mm-1500mm-1800mm-2000mm-2500mm or as required |
| UNS 304 Plate Thickness | 0.3 to 120mm or as required |
| ASTM A240 Stainless Steel 304 Plate Process | Hot/ Cold Rolled/forging |
| UNS 304 Plate surface | No.1, No. 2D, No. 2B, BA, No.3, No.4, No.6, No.7, 2B, 2D, BA NO(8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled ASTM A240Stainless Steel 304 Plate, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc. |
| Stainless 304 Sheet ASTM | ASTM A240 |
| Stainless 304 Sheet AMS | ASTM 240 |
| Tolerances of width and thickness | ASTM-ASME-GB-EN-DIN-JIS |
| 304 Stainless Plate standards and approvals | EN ISO 18286 EN 10051 EN 10088-1 ISO 15510 EN ISO 9445 ASTM A 480 ASTM A 959 ASME IID |
| 304 Plate & Sheet Sizes | 1000 x 2000 mm, 1220 x 2440 mm, 1500 x 3000 mm, 2000 x 2000 mm, 2000 x 4000 mm,1500*6000,Cold rolled 304 Stainless Plate 0.5-6.4 mm,Hot rolled 304 Stainless Plate 3.0–60.0 mm |
| UNS 304 Plate Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard ASTM A240Stainless Steel 304 Sheet suppliers |
| Cutting | To provide a comprehensive service, we use a variety of cutting methods, including:Laser Plate Cutting,Plasma Plate Cutting,Oxy-propane Flame Cutting |
| Plasma profiles | As per customer’s drawings |
| Value added services for 304 Stainless Plate | Laser cutting, Waterjet cutting, Plasma cutting, Bending and mechanical processing, edge preparation, welding, sawing and shearing. |
| Manufacturer | POSCO, Aperam, ATI, ThyssenKrupp, Baosteel, TISCO, ArcelorMittal, VDM, Nippon Metal, Outokumpu, Tsingshan, Delong. |
| China 304 Stainless Plate Manufacturer | ASTM A240Stainless Steel 304 Plate: material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width;304 Stainless Sheet: material under 3/16″ [5.00 mm] in thickness and 24″ [600 mm] and over in width;Steel Stainless 304 Clad plate: Steel Stainless 304 Clad plate is a composite steel plate made by bonding 304 Stainless 304 Plate, etc.ASTM A240Stainless Steel 304 Strip: cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width. |
| 304 Plate Origin | CHINA |
| Packing of 304 plate | Bundles with waterproof cloth outside or plywood box |
| Test | UT, SGS testing, TUV etc |
| Why buy 304 Sheet from DAXUN? | Free quote、Free sample、EN 10204 3.1、Mill Test Certificate is supplied with shipment、 TestGrade: AISI 304/S30400 Fabricación: chapa laminada en frío, chapa laminada en caliente, chapa forjada Estándar: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS Tipo: chapa fina laminada en frío, chapa gruesa laminada en caliente Superficie: 2B, NO.1, NO.4, HL, BA, 8K, etc. Length: 2438mm/3048mm/6000mm can be customized Origin: TISCO, Baosteel, Posco, Tsingshan, Delong |
| Estándar | Werkstoff Nr. | UNS | JIS | BS | GOST | AFNOR | EN | CN |
| SS 304 | 1.4301 | S30400 | SUS 304 | 304S31 | 08Х18Н10 | Z7CN18‐09 | X5CrNi18-10 | 06Cr19Ni10 |
| Grado | C | Mn | Si | P | S | Cr | Ni | N |
| 304 | ≤0.08% | ≤2.0% | ≤ 0.75% | ≤0.045% | ≤0.030% | 18%-20% | 8.0%-10.5% | ≤0.10% |
| Tipo | Yield Strength 0.2% offset (KSI) | Tensile Strength (KSI) | % Elongation(2″ Gauge length) |
| 304 Ann | 30 min. | 75 min. | 40 min. |
| 304 ¼ Hard | 75 min. | 125 min. | 12 min. |
| 304 ½ Hard | 110 min. | 150 min. | 7 min. |
| 304L Ann | 25 min. | 70 min. | 40 min. |
| 304L ¼ Hard | 75 min. | 125 min. | 12 min. |
| 304L ½ Hard | 110 min. | 150 min. | 6 min. |
| 304 & 304L | ||
| Density (lb./ in^2) @ RT | 0.29 | |
| Modulus of Elasticity in Tension (psi x 10^6) | 28 | |
| Specific Heat (BTU/o F/lb.) | 32 to 212 oF | 0.12 |
| Thermal Conductivity (BTU/hr/ft^2/ft) | 212oF | 9.4 |
| 932oF | 12.4 | |
| Mean Coefficient of Thermal Expansion (in. x 10^-6 per o F) | 32 to 212oF | 9.2 |
| 32 to 600oF | 9.9 | |
| 32 to 1,000oF | 10.2 | |
| 32 to 1,200oF | 10.4 | |
| Electrical Resistivity (micro ohms – cm) | at 70oF | 72 |
| Melting Point Range (oF) | 2550 to 2650 | |
| Oxidation Resistance – Continuous Service(oF) | 1,650 | |
| Oxidation Resistance – Intermittent Service(oF) | 1,500 |
Elija Daxun y haga que sus clientes queden satisfechos.

Entrega rápida
Daxun provides customers with timely and fast delivery of stainless steel plate products. Behind the speed is the system support from production capacity, information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Quick response
Daxun saves customers time, materials and stress, and ultimately saves them costs. With its professional advantages, Daxun can provide the most cost-optimized material recommendations based on customer needs, and can also reduce costs for customers through continuous processing, nesting processing, etc.

Advanced machining
Our advanced nesting processing method improves material utilization and cutting utilization. At the same time, Daxun can also achieve continuous cost reduction and efficiency improvement by promoting lean improvement activities, and return the benefits to customers.
304 stainless steel plate packaging
Daxun Alloy ensures the best quality of 304 stainless steel sheet packaging, because packaging plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Cajas y cajones
• Kraft paper + wooden pallets
- Retráctil
• Fumigation-free wooden pallets
• Fumigation-free wooden boxes

304 Stainless Steel Sheet Processing:
- Etching processing
- Welding processing
- Bending processing
- Embossing processing
- Sandblasting processing
- Polishing processing
- Punching processing
- Stamping processing
SS 304 Plate Surface Treatment
1D: La superficie es mate con forma de partícula discontinua.
2D: Blanco con un tono plateado.
2B: Gris plateado con mejor brillo y planitud que la superficie 2D.
Ba: Superficie cercana al espejo con excelente brillo y reflectividad.
No.3: Buen brillo y superficie rugosa.
No.4: La superficie tiene líneas finas y buen brillo.
HL: Gris plateado con pelo dorado.
8K: Superficie de espejo.
304 plate stainless steel Features
Let your brand improve rapidly
- Galería
- TOLERANCE
- DELIVERY STATE
- Otras series de productos
| Tolerancia para chapa 2B | |||
| Talla | Rango de tolerancia | ||
| Grupo 1 | Grupo 2 | Grupo 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Tolerancia de la chapa laminada en caliente n.º 1 | |||
| Talla | Rango de tolerancia | ||
| Grupo 1 | Grupo 2 | Grupo 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Elección del Estado de entrega | Estado de la superficie |
| Laminado en frío | 2B |
| 2D | |
| BA | |
| Línea del cabello | |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Nota: | |
| 1. Si necesita un estado de entrega diferente al indicado anteriormente, confírmelo con nosotros. | |
| 2. En caso de cualquier consulta o pedido, por favor, háganos saber cualquier requisito adicional no indicado aquí. | |
| Estado de entrega | |
| Elección del Estado de entrega | Estado de la superficie |
| Laminado en caliente | No.1 |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| En escabeche | |
| Nota: | |
| 1. Si necesita un estado de entrega diferente al indicado anteriormente, confírmelo con nosotros. | |
| 2. En caso de cualquier consulta o pedido, por favor, háganos saber cualquier requisito adicional no indicado aquí. | |
| Grado | Tipo | Espesor | Superficie |
| Austenítico | 304/304H/304L/304J1 | 0,25-150 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0,3-80 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferrita | 430 | 0,4-3,0 mm | 2B/BA/NO.4/8K/SB/HL |
| Ferrita ultrapura | 443 | 0,4-2,0 mm | 2B |
| 436L/439/444/441 | 0,5-3,0 mm | 2B、2D | |
| 409L | 0,4-2,5 mm | 2B、2D | |
| Grado | Tipo | Espesor | Original |
| Acero resistente al calor | 309S | 0,5-40 mm | CHN |
| 310S | 0,5-40 mm | CHN | |
| Acero dúplex | 2101 | 1,5-50 mm | CHN |
| 2304 | 3,0-50 mm | CHN | |
| 2205 | 0,5-60 mm | CHN | |
| 2507 | 1,0-60 mm | SWE / JPN / CHN | |
| Acero súper austenítico | N08904 | 0,6-50 mm | SWE / JPN / CHN |
| S31254 | 0,5-50 mm | SWE / JPN / CHN | |
| N08926 | 0,5-50 mm | SWE / JPN / CHN | |
| N08367 | 0,5-50 mm | SWE / JPN / CHN | |
| Aleación a base de níquel | N08031 | 1,0-50 mm | US / JPN / GER |
| N08810/N08800 | 0,8-50 mm | US / JPN / CHN | |
| N08028 | 1,0-20 mm | US / GER / JPN | |
| N08020 | 1,0-20 mm | US / GER / JPN | |
| N08825 | 0,8-40 mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0,5-50 mm | US / GER / JPN | |
| N06022 | 1,0-50 mm | US / GER / JPN | |
| N06625 | 0,8-20 mm | US / GER / CHN | |
| N04400 | 1,0-20 mm | US / GER / JPN | |
| N06600 | 1,0-50 mm | US / GER / JPN / CHN | |
| N02201 | 0,5-20 mm | US / JPN | |
| Titanio | TA1/Gr1 | 0,5-50 mm | JPN / CHN |
| TA2/Gr2 | 0,5-50 mm | JPN / CHN | |
| Material de soldadura | ERNiCrMo-13 | 1.2、2.4mm | GER |
| ERNiCrMo-3 | 2,4 mm | GER | |
| ERNiCrMo-4 | 2,4 mm | US |
The surface and shape of 304 stainless steel plate (6)
Información disponible para consulta y descarga
Daxun es un fabricante de placas de acero inoxidable de confianza
Como fabricante profesional, Daxun asegura que todos los productos que producimos son de alta calidad. Por lo tanto, nos aseguramos de que todas las placas de acero inoxidable estén certificadas por ISO9001, SGS, CE, OQC y más normas internacionales de calidad.También tenemos un estricto control de calidad para garantizar que las placas de acero inoxidable tengan menos defectos. En Daxun, puede estar seguro de que todos los productos son duraderos, de alta calidad y alto rendimiento.
Proyectos y productos recientes
Productos relacionados (13)
Podemos proporcionarle muestras de chapa de acero inoxidable para que compruebe la calidad. La muestra es gratuita y usted sólo paga el flete.
Hemos exportado a más de 42 países, como Canadá, Chile, Kuwait, Alemania, Corea del Sur, Arabia Saudí, Singapur, etc.
Nuestro MOQ es de 1 tonelada de chapa de acero inoxidable.
Los pedidos de prueba pueden entregarse en una semana. Los pedidos normales tardan unas dos semanas.