Daxun is a 316/316L stainless steel coil China supplier
As a leading stainless steel coil supplier and exporter in China, Daxun supplies stainless steel coils to all over the world.
- Coil grade: S31600-S31603
- Coil features: corrosion resistant, acid and alkali resistant,
- Coil thickness: 0.4 mm to 12.00 mm
- Coil width: 1000 mm, 1250 mm, 1500 mm and 2000 mm.
- Coil surface: 2B, BA, matte, polished, 8k mirror.
If necessary, stainless steel coils will come with a protective film to protect the metal surface from unnecessary damage.
Global leader in stainless steel Coil fabrication services
Shop Daxun’s extensive range of SS 316L Stainless Steel Coil, AISI 316 Coil, SUS 316L Coil, 2B Surface Treatment 316 Stainless Steel Coil, BA Surface Treatment 316L Stainless Steel Coil, 2b Surface Treatment 316L Grade Stainless Steel Coil, ASTM A240 316 BA Stainless Steel Coil, Astm 316 Stainless Steel Coil, SS 316L Cold Rolled Stainless Steel Coil, SS 316 Coil Manufacturers.Daxun is well-known as a manufacturer, trader, and supplier of 316/316L Stainless Steel Coils. The Steel Coils we offer are precisely constructed and meet international quality requirements. Daxun is an ISO 9001:2008 certified firm that is a major supplier and exporter of ASTM A240 316 /316L stainless steel coils. 316/316L Stainless Steel Coils can be cut to your requirements and include a complete set of Mill Test Reports. Custom lengths and widths are available up to 2000 mm. Exporting is our specialty! We can source several hard-to-find grades and/or non-standard sizes to meet our clients’ specific requirements. With our extensive experience in processing Steel Coil goods, we can cut all ASTM SS 316 Steel Coils to the needed sizes.
Type 316/316L is a chromium-nickel austenitic stainless steel that contains molybdenum. The inclusion of molybdenum improves the corrosion resistance of 316/316L in halide conditions and reducing acids like sulfuric and phosphoric acids. Type 316L can be dual certified as 316 if the composition meets the lower carbon limit of 316L and the slightly higher strength level of 316. Type 316L should be used for welding applications because the low carbon version eliminates chromium carbide precipitation and improves corrosion resistance in the welded condition.
Type 316/316L is resistant to both air corrosion and moderately oxidizing conditions. In addition, it is resistant to marine atmospheric corrosion and has high intergranular corrosion resistance when welded. Type 316/316L provides high strength and toughness at cryogenic temperatures. Type 316/316L is nonmagnetic when annealed, however it can become somewhat magnetic after extreme cold working. Type 316L stainless steel is an ultra-low carbon variant of Type 316 that reduces hazardous carbide deposition in the heat-affected zone during welding.
Datos
- Parámetro
- Elemento
- Propiedades mecánicas
- PROPIEDADES FÍSICAS
- All equivalent
- 304 coil stock
| SS 316 / 316L Stainless Steel Coil Specification | ASTM A240 / ASME SA240 |
| SS 316 / 316L Stainless Steel Coil Manufacturing Process | Hot Rolled (HR) / Cold Rolled (CR) |
| SS 316 / 316L Stainless Steel Coil Grades | 202 / SS 316 / 316L / SS 316 / 316LL / SS 316 / 316LH / 309S / 310S / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L etc. |
| UNS No. – UNS SSS 316 / 316L00, UNS SSS 316 / 316L03, UNS S31008, UNS S31620, UNS S31603, UNS S31603, UNS S31635, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904 | |
| EN No. – 1.4301, 1.4307, 1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539 | |
| SS 316 / 316L Stainless Steel Coil Thickness | 0.6 MM TO 80 MM THICKNESS |
| SS 316 / 316L Stainless Steel Coil Width | 1250 MM / 1500 MM / 2000 MM / 04 Feet / 05 Feet and Custom Cut Width as Per Requirement |
| SS 316 / 316L Stainless Steel Coil Length | 2400 MM / 2420 MM / 6000 MM / 08 Feet / 10 Feet / Coil Cut and Custom Cut Length as Per Requirement |
| SS 316 / 316L Stainless Steel Coil Surface Finish | 2B, 2D, BA, MATT, MATT PVC, No.4, No.5, SB, HR, No.8, Mirror, Hairline, Brush, Textured, Oil base wet Polished, Both sides Polished available. |
| SS 316 / 316L Stainless Steel Coil Coating | PVC coating Normal / Laser, Film: 100 micrometer, Color: black/white. |
| SS 316 / 316L Stainless Steel Coil Other Testing | NACE MR0175, Ultrasoung TEST, IGC TEST, Intergranular Corrrosion Test as per ASTM A262 Practice E, Charpy Impact Test, Macro, Grain Size, Hardness, etc. |
| SS 316 / 316L Stainless Steel CoilValue Added Services | Gas Cutting / CNC Plasma Cutting / Profiling / Rolling / Bending / coil Metal Fabrication / Drill / Punch / Machining / Sand Blasting / Shot Blasting / Heat Treatment |
| SS 316 / 316L Stainless Steel Coil Packaging | Loose / Carrate / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps |
| SS 316 / 316L Stainless Steel Coil Shipment & Transportation | By Road – Truck / Train Partial Load, Full Load, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes |
| SS 316 / 316L Stainless Steel Coil Material Test Certificate | Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of Indian Standards BIS Approved ETC |
| Manufacturer | POSCO, Aperam, Jindal Stainless, DKC Korea, Thyssenkrup, Baosteel, TISCO,Arcelor Mittal, VDM,Nippon Metal, Outokumpu,Qingshan,Delong. |
| Shipping Port | Shanghai/Ningbo port/Tianjin/Qindao |
| CHEMICAL COMPOSITION: ASTM A240, A666 | ||
| Elemento | Type 316 | Type 316L |
| Carbono | 0.08 max. | 0.030 max. |
| Manganese | 2.00 max. | 2.00 max. |
| Sulfur | 0.030 max. | 0.030 max. |
| Phosphorus | 0.045 max. | 0.045 max. |
| Silicon | 0.75 max. | 0.75 max. |
| Chromium | 16.0 – 18.0 | 16.0 – 18.0 |
| Nickel | 10.00 – 14.00 | 10.00 – 14.00 |
| Molybdenum | 2.00 – 3.00 | 2.00 – 3.00 |
| Nitrógeno | 0.10 max. | 0.10 max. |
| Tipo | Yield Strength 0.2% offset (KSI) | Tensile Strength (KSI) | % Elongation (2″ Gauge length) |
| 316 | 30 min. | 75 min. | 40 min. |
| 316L | 25 min. | 70 min. | 40 min. |
| Density (lb./ in^2) @ RT | 0.29 | |
| Modulus of Elasticity in Tension (psi x 10^6) | 28 | |
| Specific Heat (BTU/o F/lb.) | 32 to 212 oF | 0.12 |
| Thermal Conductivity (BTU/hr/ft^2/ft) | 212oF | 9.4 |
| 932oF | 12.4 | |
| Mean Coefficient of Thermal Expansion (in. x 10^-6 per o F) | 32 to 212oF | 8.9 |
| 32 to 600oF | 9 | |
| 32 to 1,000oF | 9.7 | |
| 32 to 1,200oF | 10.3 | |
| Electrical Resistivity (micro ohms – cm) | at 70oF | 29.4 |
| Melting Point Range (oF) | 2500 – 2550 |
| Grado | UNS No | Old British | Euronorm | Swedish SS | Japanese JIS | ||
| BS | En | No | Nombre | ||||
| 316l | S31603 | 316S11 | - | 1.4404 | X2CrNiMo17-12-2 | 2348 | SUS 316L |
| • Tisco Stainless Steel 316l coil | • Best selling 4’x8′ mirror finished ss 316l coil |
| • SS 316l Perforated coil | • Decorative hairline inox cold rolled ss 316l coil |
| • Stainless Steel 316l UNS S31635 coil | • Hair Line Finish SS 316l coil |
| • A 240 Chequered 316l coil | • Laser cutting ss 316l coil |
| • Aperam Stainless Steel 316l coil | • Tisco Supplier 3mm Thickness Stainless Steel 316l coil |
| • Stainless Steel 316l coil | • Decorative Stainless Steel 316l coil |
| • A 240 316l coil | • Scotch Brite SS 316l coil |
| • SS 316l Embossed coil | • Baosteel Stainless Steel 316l coil |
| • Outokumpu SS 316l coil | • Stainless Steel Cladding 316l coil |
| • SA 240 316l stainless steel coil | • Black SS 316l coil 4mm Thick |
| • Bright Hammered Pattern Decorative SS 316l coil | • Bright-pickled Stainless Steel 316l coil |
| • Jindal Stainless Steel 316l coil | • Cold rolled, heat treated 316l coil |
| • SS DIN 1.4404 coil | • 3mm Cold Rolled AISI SS 316l coil |
| • ThyssenKrupp Stainless Steel 316l coil | • Mill Supply SS 316l coil |
| • ASTM A240 Stainless Steel 316l coil | • Grade Prime SS 316l coil |
| • Surface Polishing SS 316l coil | • Carpenter Custom 450 Stainless Steel 316l coil |
| • 316l Stainless Steel HR coil | • Cut to Size Stainless Steel 316l coil |
| • 316l Stainless Steel Chequered coil | • Non Magnetic Polishing Stainless Steel 316l coil |
| • 316l Stainless Steel Golden Laser Pattern coil | • ASME SA240 316l coil |
| • Super thin-Mirror surface BA ss 316l coil | • Grade 316l Stainless Steel Finish coil |
| • Super Austenitic SS 316l coil | • 316l Stainless Steel Blank coil |
| • ASTM A240 316l coil | • 316l Stainless Steel Perforated coil |
| • JMSS cold rolled ss 316l coil | • Embossed ss 316l coil |
| • Cold Rolled No.1 Finish SS 316l coil | • Cheap cold rolled ss 316l coil with best price |
| • SEW 400 Stainless Steel 316l coil | • Brush finish ss 316l coil price list |
| • Hot Rolled Stainless Steel 316l coil | • SS URANUS B6 316l coil |
| • Sales Promotion SS 316l coil | • 2B SUS SS 316l coil |
| • Cr Stainless Steel 316l coil | • Food Grade Stainless Steel 316l coil |
| • SS 316l Mill Test Certificate coil | • No. 4 PVC Coated SS 316l coil |
| • ASTM A240 316l coil | • SS 316l coil Blasted Tin-Gold Rose |
| • Cold rolled, bright annealed 316l coil | • 2mm ASTM SS 316l coil |
| • Ground Stainless Steel 316l coil | • Stainless Steel Corrugated 316l coil |
| • Hot Selling AISI SS 316l coil | • ASTM B625 316l coil |
| • SS 316l Rose Golden coil | • Brushed or dull polished Stainless Steel 316l coil |
| • Surface coated Stainless Steel 316l coil | • Cold rolled, heat treated, pickled 316l coil |
| • Satin finish Stainless Steel 316l coil | • 10K Mirror Finish Surface SS 316l coil |
| • AISI stainless steel 316l armor coil | • Gold Etched SS 316l coil |
| • Satin finish Stainless Steel 316l coil | • 18 Gauge SS 316l coil |
| • Mirror Finish SS 316l coil | • Patterned Stainless Steel 316l coil |
| • SS 316l coil Gold Brush Finish | • #4 Finish Stainless Steel 316l coil |
| • 316l Stainless Steel CR coil | • Patterned Stainless Steel 316l coil |
| • 316l Stainless Steel 2B coil | • Passenger Elevator Cabin SS 316l coil |
| • 316l Stainless Steel B. Q. Profile coil | • Dimensional Stainless Steel Grade 316l coil |
Elija Daxun y haga que sus clientes queden satisfechos.
Quick response 316 Stainless Steel coil
We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.Daxun’s stainless steel materials are of reliable quality, and their varieties, specifications and delivery weights strictly comply with the standards.
Daxun Advantages
Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel achieves full traceability of each steel coil from the ERP system, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strict monitoring during sales, and provides worry-free service guarantees after sales.


Stainless steel coil packaging
Daxun Alloy garantiza la mejor calidad de embalaje, ya que desempeña un papel importante en el transporte internacional de mercancías, donde las mercancías pasan por varios canales para llegar al destino final, por lo que prestamos especial atención al embalaje. Embalamos nuestras mercancías de muchas maneras dependiendo del producto. Embalamos nuestros productos de muchas maneras, tales como:
- Cajas y cajones
- Retráctil
- Palés de madera
- Cajas de madera
Calidad, entrega, inspección
- Daxun también lleva a cabo varias pruebas de garantía de calidad. Estas pruebas incluyen la prueba de aplanamiento, la prueba de picaduras y resistencia, la prueba mecánica, la prueba de dureza, la identificación positiva del material, la prueba de expansión, etc. Todas estas pruebas garantizan que el material es adecuado para la aplicación requerida.
- Durante el proceso de producción, medimos el diámetro, el grosor y la superficie del producto. Nuestro plazo de entrega estándar es de 7-15 días, excepto para algunos productos de tamaño especial, nuestro plazo de entrega aumentará a 20 días.
Nuestro plazo de entrega se ajusta estrictamente a lo estipulado en el contrato. - Apoyar a las agencias externas del cliente para que vayan a la fábrica a inspeccionar
- Ofrecer muestras gratuitas a los clientes para que las prueben
- Apoyo a la inspección in situ o por vídeo en fábrica

316 Stainless Steel coil Ordering Information
Las órdenes de compra deben incluir cantidad, grado, tipo o categoría, referencia API5L, espesor, anchura, longitud y cualquier anexo aplicable o requisito adicional relacionado con la composición química, propiedades mecánicas, tratamiento térmico, pruebas adicionales, proceso de fabricación, recubrimiento superficial o acabado final. Póngase en contacto con Daxun ahora, responderemos a su correo electrónico lo antes posible.
Asistencia técnica
Si necesita asistencia técnica adicional, nuestro metalúrgico residente y nuestro personal experto estarán encantados de ayudarle. Además, Daxun cuenta con un laboratorio de pruebas certificado, una primicia en la industria de inventarios multimetal y plástico. Esto, en nuestra opinión, demuestra nuestra inquebrantable dedicación a la calidad y nuestra filosofía como proveedor de servicios completos.
SS 316/316L Stainless Steel Coil Features
Daxun Alloy Let your brand improve rapidly
- Galería
- Product Series
- Main Equipment
| Grado | Tipo | Espesor | Superficie |
| Austenítico | 304/304H/304L/304J1 | 0,25-150 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0,3-80 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferrita | 430 | 0,4-3,0 mm | 2B/BA/NO.4/8K/SB/HL |
| Ferrita ultrapura | 443 | 0,4-2,0 mm | 2B |
| 436L/439/444/441 | 0,5-3,0 mm | 2B、2D | |
| 409L | 0,4-2,5 mm | 2B、2D | |
| Acero súper austenítico | N08904 | 0,6-50 mm | SWE / JPN / CHN |
| S31254 | 0,5-50 mm | SWE / JPN / CHN | |
| N08926 | 0,5-50 mm | SWE / JPN / CHN | |
| N08367 | 0,5-50 mm | SWE / JPN / CHN | |
| Aleación a base de níquel | N08031 | 1,0-50 mm | US / JPN / GER |
| N08810/N08800 | 0,8-50 mm | US / JPN / CHN | |
| N08028 | 1,0-20 mm | US / GER / JPN | |
| N08020 | 1,0-20 mm | US / GER / JPN | |
| N08825 | 0,8-40 mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0,5-50 mm | US / GER / JPN | |
| N06022 | 1,0-50 mm | US / GER / JPN | |
| N06625 | 0,8-20 mm | US / GER / CHN | |
| N04400 | 1,0-20 mm | US / GER / JPN | |
| N06600 | 1,0-50 mm | US / GER / JPN / CHN | |
| N02201 | 0,5-20 mm | US / JPN | |
| Titanio | TA1/Gr1 | 0,5-50 mm | JPN / CHN |
| TA2/Gr2 | 0,5-50 mm | JPN / CHN | |
| Material de soldadura | ERNiCrMo-13 | 1.2、2.4mm | GER |
| ERNiCrMo-3 | 2,4 mm | GER | |
| ERNiCrMo-4 | 2,4 mm | US |
| Subsidiary | Main Equipments | Qty | Annual Capacity |
| Daxun Stainless steel co.(JiangSu) | Slitting Machine | 1 | Decorative Sheet:60,000 tons |
| Cutting Machine | 1 | ||
| No.4 And Hairline Sheet To Sheet Polishing Machine | 1 | ||
| No.4/Hairline Coil To Coil Polishing Machines | 1 | ||
| 8K/Super Mirror Sheet To Sheet Polishing Machines | 2 | ||
| 8K/Super Mirror Coil To Coil Polishing Machines | 3 | ||
| PVD Color Coating Machines | 4 | ||
| Liquid Chemical Coating Machines | 2 | ||
| Anti Finger Printing Machines | 2 | ||
| Auto Pick and Place machines | 16 | ||
| coil Washing Machine | 1 | ||
| Daxun Stainless steel co.(Shanghai) | Cold Rolling Machine | 3 | 2B Coils:100,000 tons |
| Annealing & Pickling Line | 2 | Decorative Sheet;30,000 tons | |
| Slitting Machine | 1 | ||
| Cut to Length Machine | 1 | ||
| No.4/HL Polishing Machine(Sheet to Sheet) | 3 | ||
| 8K Polishing Machine(Sheet to Sheet) | 13 | ||
| PVD Titanium Coating Machine | 4 | ||
| Liquid Chemical Coating Machines | 1 | ||
| Daxun Stainless steel co.(Shandong) | Cold Rolling Machine | 3 | 2B & BA Coil:220,000 tons |
| Annealing & Pickling Line(2B & BA) | 2 | Decorative Sheet:60,000 tons | |
| Tension Levering & Skin Pass | 1 | ||
| Slitting Machine | 1 | ||
| Cut to Length Machine | 1 | ||
| No.4/HL Polishing Machine(Sheet to Sheet) | 1 | ||
| 8K Polishing Machine(Sheet to Sheet) | 11 | ||
| Automatic Copper Coating Machine | 1 | ||
| Digital Printing Machine | 1 | ||
| PVD Titanium Coating Machine | 3 | ||
| Liquid Chemical Coating Machines | 1 | ||
| Anti-finger Machine | 1 | ||
| Daxun Stainless steel co.(Sichuan) | Slitting Machine | 1 | 2B & BA Coil:180,000 tons |
| Cutting Machine | 1 | Decorative Sheet:50,000 tons | |
| No.4 And Hairline Sheet To Sheet Polishing Machine | 1 | ||
| No.4/Hairline Coil To Coil Polishing Machines | 1 | ||
| 8K/Super Mirror Sheet To Sheet Polishing Machines | 1 | ||
| 8K/Super Mirror Coil To Coil Polishing Machines | 1 | ||
| PVD Color Coating Machines | 1 | ||
| Liquid Chemical Coating Machines | 1 | ||
| Anti Finger Printing Machines | 1 |
SS 316/316L Surface Types of Stainless Steel Coils (6)
Información disponible para consulta y descarga
Daxun is a trustworthy stainless steel coil manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel coils have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
Proyectos y productos recientes
Productos relacionados (10)
Leading stainless steel coil Suppliers in China
Daxun has been engaged in international business for more than ten years. In 2023, its export revenue exceeded US$100 million, and its export volume ranked among the top Chinese stainless steel manufacturers. Daxun continues to improve its service skills. In order to serve the global market, we have established three export service facilities in China and cooperated with engineering enterprises, steel mills and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relationships with dozens of well-known steel mills around the world. Its inventory includes 50,000 tons of conventional stainless steel coils and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of consistent quality. Types, specifications and delivery weights strictly comply with standards.
What is 316L stainless steel coil?
- 316L stainless steel coil is an austenitic stainless steel that has excellent corrosion resistance and strength. It shares mechanical qualities with 304L coil but is more resistant to pitting and crevice corrosion.
- It has a lower melting temperature than 304L coil, making it better suited to applications where the material is subjected to greater temperatures before being formed into a component, such as welding or brazing.
- 316L stainless steel coils can be made via rolling, drawing, or forging. It is utilized in a variety of applications, including marine, chemical, and food processing equipment.
What applications can 316L stainless steel coils be used in?
- 316L stainless steel coils are commonly utilized in construction, transportation, and other industries. It is a common type of stainless steel with excellent corrosion resistance to many hostile substances, particularly chloride ions.
- 316L stainless steel coils offer outstanding mechanical qualities and can withstand high temperatures. It is also ideal for welding, cutting, and bending.
- 316L stainless steel coils are widely used in a variety of sectors.
- Chemical production industries frequently employ 316L stainless steel tubes to convey corrosive chemicals. It has excellent corrosion resistance to acids, alkalis, and a variety of other chemical compounds.
- Construction industry: We frequently utilize 316L stainless steel pipes to convey water or sewage from one locati0n to another. The material is strong enough for long-term use.
- Food industry: We typically use 316L stainless steel pipes as boiling tubes because they can withstand high temperatures without deforming during the cooking process, whereas other materials are readily destroyed by heat.
Features of 316L Stainless Steel Coils
Resistencia a la corrosión
316L stainless steel coil has superior corrosion resistance than 304 stainless steel coil and is suitable for use in the pulp and paper industries. In addition, 316L stainless steel coil is resistant to saltwater erosion and the corrosive industrial climate.
Resistencia al calor
In intermittent applications below 1600 degrees, 316 stainless steel coil has excellent oxidation resistance.
316L stainless steel coil is more resistant to carbide precipitation than standard 316 grade stainless steel coils.
Resistencia a la corrosión
- 316 stainless steel is highly corrosion resistant in a variety of situations. It performs well in air circumstances, can withstand most settings, and is frequently employed in marine regions or areas with high industrial pollution. The best appearance is maintained when the design allows for even rain washing of the surface, or when dirt deposits are occasionally rinsed off the steel.
- Grade 316 has also provided great service in potable water. Pitting and crevice corrosion may occur in waters with higher chloride concentrations, with 2000 ppm recognized as the top limit. 316’s greater molybdenum concentration makes it substantially more corrosion resistant than 304.
- 316 stainless steel can be used with seawater as long as precautions are taken to prevent crevice corrosion from forming under sediments, precipitation, and biofouling, as well as in planned fissures.
- Grades 316 and 304 may experience stress corrosion cracking in chloride-containing solutions at temperatures over 60°C. Stress corrosion cracking should be considered for all corrosion services using corrosive liquids that may contain chlorine.
Toughness/Hardness
- Austenitic stainless steels are intrinsically robust, and 316 stainless steel is no exception, maintaining the ductile fracture mode and high absorbed energy in impact tests at cryogenic temperatures (-200°C).
- AS1210 specifies that grade 316 can be used in pressure vessels up to 800°C. The standard permits for higher design stresses in 316H at all temperatures.
High-temperature corrosion
- The commonly accepted maximum service temperatures for grade 316 (and grade 304) in air are 870°C for intermittent use and 925°C for continuous use.
- Cold Fabrication
Grade 316 is generally workable using typical coil metal working processes, with the limitation that it cannot be oxygen cut. Plasma cutting is commonplace. Grade 316 has exceptional deep drawing capabilities because to its strong austenite stability. - 316 is an easy austenitic stainless steel to forge at temperatures above 925°C.
Maquinabilidad
- Grade 316 is generally straightforward to process, but more difficult than carbon steel. More power is needed to machine grade 316. Cutting speed should be reduced, feed rate increased, and tools and equipment heavier. The machinability of 316 is roughly 60% that of AISI B1112 resulphurized free cutting carbon steel. There is a free-machining variant of 316 available as a bar.
- Heat treatment involves annealing the solution at 1065-1120°C, followed by quick cooling to prevent chromium carbide precipitation. 316 cannot be toughened through heat treatment. Stress relief is rarely required due to 316’s strong ductility.
Soldabilidad
- Grade 316 stainless steel can be welded using most fusion procedures (GTAW / TIG, GMAW / MIG / MAG, MMAW / stick, SAW), with no need for preheat, postheat, or interpass temperature regulation. It is typically welded using filler metals of the same grade, 316 or 316L (or silicon-containing variants), which maintain corrosion resistance and strength. These grades are pre-qualified weld metals under AS1554.6:1994 for welding grade 316 to itself.
What are the commonly used surfaces of stainless steel coils?
The surface finish of 201 stainless steel coil might vary depending on the cold rolling processing methods used and the surface treatment used after rolling. Surface treatments for stainless steel coils include NO.1, 2B, 4, HL, 6, 8, BA, TR hard, heavy rolling bright 2H, polished bright, and other surface treatments:
- NO.1: The surface obtained after hot rolling, heat treatment and pickling of stainless steel strip. It is used to remove the black oxide scale formed by pickling or similar processes during hot rolling and heat treatment. It ranks first in surface treatment. The No. 1 surface is silvery white and matte. It is generally used in heat-resistant and corrosion-resistant industries that do not require high surface gloss, such as the alcohol industry, chemical industry, large containers, etc.
- 2B: Unlike the 2D surface, the 2B surface is smoothed by a light roller, and the surface is brighter. The surface roughness Ra value measured by the equipment ranges from 0.1 to 0.5μm, which is a typical value for most processing types. This stainless steel strip surface has the strongest adaptability and is suitable for industries such as chemical, papermaking, petroleum, medical, and a wide range of fields such as building curtain walls.
- TR hard surface: TR stainless steel is also called hard steel. Its characteristic steel grades include 304 and 301, which are used for items that require high strength and hardness, such as railway vehicles, conveyor belts, springs and washers. The idea is to use the work hardening characteristics of austenitic stainless steel to improve the strength and hardness of steel coils through cold working methods such as rolling. In order to replace the gentle flatness of the 2B base surface, the hard material is gently rolled by a few percent to tens of percent, and no annealing is performed after rolling. Therefore, the TR hard surface of the hard material is the rolled surface after the cold rolling process.
- Re-rolled bright 2H: After the rolling operation, the stainless steel strip will be bright annealed. A continuous annealing line can be used to quickly cool the strip. The stainless steel strip travels along the line at a speed of 60-80m/min. After this process, the surface finish will be 2H re-rolled bright.
- No. 4: The No. 4 surface has a good polishing effect and is brighter than No. 3. It can also be obtained by polishing the cold-rolled stainless steel coil with a 2D or 2B surface, and then polishing the processed surface with a sanding belt with a particle size of 150-180#. The tool measures the surface roughness (Ra) between 0.2 and 1.5μm. The No. 4 surface is widely used in restaurants and cooking equipment, medical equipment, architectural decoration, containers and other applications.
- HL: The HL surface is often called a hairline finish. The Japanese JIS standard specifies a continuous hairline abrasive surface obtained by polishing with a 150-240# abrasive belt. The restrictions under the Chinese GB3280 standard are unclear. HL surface finish is commonly used for architectural decoration, such as elevators, escalators, and exterior walls.
- No. 6: The No. 6 surface is further polished on the basis of No. 4 with a Tampico brush or a W63 grit abrasive material specified in the GB2477 standard. The surface has good metallic luster, softness, weak reflection, and no imaging. Due to its good performance, it is very suitable for curtain walls, tassel decoration, and cooking supplies.
- BA: BA is a surface that is brightly heat treated after cold rolling. Bright heat treatment is annealing in a protective atmosphere to ensure that the surface is not oxidized and retain the gloss of the cold-rolled surface, and then it is polished with a high-precision smooth roller to improve the surface brightness. The instrument evaluates the surface roughness to be 0.05-0.1μm, indicating that the surface is close to a mirror surface. BA surfaces can be used in a variety of applications, including food utensils, household appliances, medical equipment, automotive parts, and decorations.
- No. 8: Mirror surface, maximum reflectivity, no abrasive particles. The stainless steel deep processing industry also refers to 8K board. BA material is often used as raw material for mirror processing. It only needs to be polished. The surface is beautiful after mirror processing and is often used in building entrances and interior decoration.
What is the standard sea packaging stainless steel coil?
- Standard export sea packaging:
Waterproof Paper Winding+PVC Film+Strap Banding+Wooden Pallet or Wooden Case; - Customized packaging as your request (Logo or other contents accepted to be printed on the packaging);
- Other special packaging will be designed as customer’s request;
Eye to wall and eye to sky are both available; - By International Express: DHL/UPS/FEDEX/EMS and our own express line;
- By air, sea or land;
- Shipping Port: Shanghai, Ningbo, Qingdao, Tianjin or as your request.
Why choose Daxun’s stainless steel coils?
Reliable Stainless Steel Coils and Sheets Inventory Guarantee
- Have you ever been in a situation where you required a significant quantity of stainless steel coils right away, only to discover that the supplier was running low on stock? This condition may impair your workflow and plans.
- Our Advantages: With us, this situation will be a thing of the past. Our inventory is always ample, guaranteeing that even the largest orders are fulfilled quickly and in accordance with your business schedule.
Custom Stainless Steel Material Processing
- You may have experienced a circumstance in which bespoke processing is required, but locating the correct supplier to match your exact requirements might be difficult.
- Our Advantages: We have great processing capabilities to satisfy any of your specific needs. Whether it is size, stainless steel surface treatment, or other unique requirements, we offer expert one-stop service.
Competitive Stainless Steel Prices
- When looking for a stainless steel coil provider, price is typically a major factor. You may have to make a compromise with your chosen supplier due to excessive costs.
- Our Advantages: We keep pricing low by implementing excellent cost control and improved sourcing methods. This implies that by choosing us, you will not only receive high-quality products but also outstanding value for money.
Various Specifications of Stainless Steel Coils in Stock
- Finding stainless steel coils with exact specifications might be a challenge. It is critical to select a supplier who understands and serves these specific needs.
- Our Advantages: Our portfolio demonstrates versatility, with a wide choice of materials, thicknesses, and widths. We take pleasure in our ability to satisfy your project’s exact specifications.
Precision Stainless Steel Shearing Service.
- Precision shearing is required for the usage of stainless steel coils, but not all vendors offer this precise service.
- Our Advantages: Our shearing service is both professional and efficient, delivering precise cuts that fit your exact demands.
Contact your stainless steel coil suppliers
- You can easily order stainless steel coils in any size and quantity online.
Alternatively, our friendly sales team will be happy to take your order. Simply call +86 13382898899 or email Daxunhejin@gmail and we will get back to you as soon as possible.
Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email (Daxunalloy@gmail.com) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week
Samples can be provided free of charge, but the freight is borne by the customer, and will be refunded after cooperation.
Hemos exportado a más de 42 países, como Canadá, Chile, Kuwait, Alemania, Corea del Sur, Arabia Saudí, Singapur, etc.
Our MOQ is 1 ton for stainless steel coil.
We have a complete organization from raw material purchasing to processing and shipment arranging. In the whole chain, the documentary people ad QC will look for and check it by precise requirements.The third party inspection is welcomed.
Los pedidos de prueba pueden entregarse en una semana. Los pedidos normales tardan unas dos semanas.