Daxun is an excellent manufacturer of grade 23 (Ti-6Al-4V ELI)titanium rods and bars.
Como principal proveedor chino de barras de titanio y aleaciones de titanio, Daxun suministra barras de titanio de alto rendimiento a todo el mundo.
- Titanium bar grade: Grade 23-Ti6Al 4V ELI- USN R56401
- Tipos de barras de titanio: barras laminadas, barras estiradas, barras de titanio forjado
- Titanium bar density The density of grade 23 titanium is 4.43 g/cm3
- Principales normas: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
- Alta resistencia, resistencia a altas temperaturas, resistencia a la corrosión, ligereza
- peso, excelente rendimiento integral.
————Daxun produce barras de titanio en China para satisfacer las diversas y ——exigentes necesidades de los clientes!.
Líder mundial en servicios de fabricación de barras de titanio comercialmente puro
Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 23 titanium alloy rods.
Grade 23 titanium bar, also known as Ti-6Al-4V ELI, is a high-performance alloy known for its excellent strength-to-weight ratio, corrosion resistance, and biocompatibility. It is widely used in aerospace, medical, and high-tech industries due to its ability to withstand extreme conditions while remaining lightweight. Compared to other titanium grades, Grade 23 offers enhanced ductility and fracture toughness, making it ideal for critical applications such as aircraft components, surgical implants, and advanced engineering parts.
Daxun es su empresa de producción de barras de aleación de titanio de confianza. Daxun produce todos los grados de aleaciones de titanio, incluyendo titanio comercialmente puro serie CP, serie de aleación de titanio, aleación de titanio y níquel, etc. Tienen un rendimiento fiable y proporcionan un alto rendimiento para sus aplicaciones críticas. En diversas industrias y aplicaciones, puede confiar en las varillas de aleación de titanio Daxun para alta resistencia, alta temperatura y ambientes corrosivos. Durante décadas, Daxun Metals se ha comprometido a producir soluciones de aleación de titanio de alta ingeniería para hacer frente a los desafíos más severos.
Datos
- Parámetro
- Ingrediente
- Propiedades mecánicas
- Propiedades físicas
| Especificación | Detalles |
|---|---|
| Material | Titanium rod and bar Grade 23 (UNS R56400) |
| Estándar | ASTM B348, ASTM SB348, AMS 4921, AMS 4902 |
| Dimensiones | EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN |
| Diámetro | 0.125″ – 14″ (3.175mm – 355.6mm), custom |
| Longitud Alcance | Up to 240″ (6096mm), custom |
| Acabado | Cold (bright) drawn, centerless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centerless Ground & Black |
| Acabado superficial | Estirado en frío, rectificado sin centros, pulido o torneado en bruto, negro, acabado NO.4, acabado BA, acabado mate, etc. |
| Condición | Endurecido y templado, recocido |
| Tolerancia | Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm) |
| Formulario | Barras cuadradas de titanio, lingotes de titanio, barras redondas de titanio, barras rectangulares de titanio, barras triangulares de titanio, barras forjadas de titanio, barras hexagonales de titanio, etc. |
| Propiedades físicas | Densidad: 4,51 g/cm³ (0,163 lb/in³), Punto de fusión: 1.660°C (3.020°F), Alargamiento: 20-30%, Módulo de elasticidad: 114 GPa (16,5 x 10⁶ psi) |
| Composición química | Titanio (min): 99,2%, Oxígeno (máx): 0,25%, Carbono (máx): 0,08%, Hierro (máx): 0,30%, Nitrógeno (máx): 0,03%, Hidrógeno (máx): 0,015% |
| Elemento | Minimum (%) | Maximum (%) |
|---|---|---|
| Titanium (Ti) | 99.2 | - |
| Aluminum (Al) | 5.5 | 6.75 |
| Vanadium (V) | 3.5 | 4.5 |
| Oxygen (O) | - | 0.25 |
| Carbon © | - | 0.08 |
| Hierro (Fe) | - | 0.30 |
| Nitrogen (N) | - | 0.03 |
| Hydrogen (H) | - | 0.015 |
| Propiedad | Valor |
|---|---|
| Resistencia a la tracción | 130,000–170,000 psi (900–1,170 MPa) |
| Yield Strength (0.2% Offset) | 115,000–150,000 psi (800–1,035 MPa) |
| Elongation | 20–30% |
| Dureza (Brinell) | 300–360 HB |
| Módulo de elasticidad | 16.5 × 10⁶ psi (114 GPa) |
| Propiedad | Valor |
|---|---|
| Densidad | 0.163 lb/in³ (4.51 g/cm³) |
| Punto de fusión | 3,020°F (1,660°C) |
| Conductividad térmica | 13.4 W/m·K (at 25°C) |
| Coefficient of Thermal Expansion | 8.6 µm/m·°C (20–100°C) |
| Resistividad eléctrica | 4.1 × 10⁻⁷ Ω·m |
Elija Daxun para que su proyecto despegue.
DAXUN® Grade 23 Titanium Rod Features
DAXUN® Ti Grado 5 es una barra de aleación de titanio (6al-4v) que se caracteriza por:
- Buena conformabilidad en caliente y soldabilidad;
- La resistencia a la tracción puede alcanzar 1000MPa;
- Trabajo dimensional a alta temperatura
- Insensible al agua de mar o al agua de mar;
- No se ve afectado por diversos medios corrosivos;
- Alta resistencia y buena tenacidad;
- Resistir el inicio y la propagación de grietas.
Ventajas de la fábrica de Daxun
El concepto de “Gestión de la Excelencia en el Rendimiento” de Daxun promueve el modelo de gestión “PDCA + Lean”. La tarjeta de visita de la empresa dice “Daxun = Calidad fiable”. Daxun utiliza el sistema ERP para lograr la trazabilidad completa de la variedad, especificación y origen de cada barra de titanio, y defiende y fomenta la lucha contra la falsificación en la industria. Daxun confía en la tecnología para el procesamiento y la personalización, y la alta precisión y la alta calidad son los puntos de referencia de la industria; en términos de servicio, promueve la gestión del ciclo de vida del producto, proporciona soluciones profesionales de selección de materiales y procesamiento antes de las ventas, supervisa estrictamente durante las ventas y proporciona garantías de servicio sin preocupaciones después de las ventas.
Grade 23 Titanium Rod Production Method
Daxun produce barras de titanio de alta calidad y alto rendimiento, y también puede fabricar según el acuerdo del cliente:
- Los lingotes de titanio deben someterse a tratamiento térmico y mecanizado, pruebas de ultrasonidos por inmersión, pruebas de propiedades mecánicas, inspección estructural macroscópica y microscópica y otros procesos. Proceso de producción: barras de titanio laminado en caliente - alta eficiencia, rendimiento estable, barras de titanio forjado - tamaño flexible, forja multi-fuego, mejorar el rendimiento integral de barras de titanio, barras de titanio estirado en frío - barras de titanio de alta precisión por lo general de pequeño tamaño; las barras de titanio anteriores se entregan con superficie brillante.
Grade 23 Rods Applications and Standards
Grade 23 Titanium Rods are widely used in the following industries under extreme corrosive conditions:
- Industria aeroespacial, construcción naval, industria del petróleo y el gas, ingeniería naval, plantas químicas, maquinaria industrial, industria energética, industria del papel y la pasta de papel, industria alimentaria, refinerías, industria militar, equipos farmacéuticos y de procesamiento de alimentos, etc.
- Especificaciones: AMS 4928,AMS 4967,AMS 4965 ,AMS 6931 ,ASTM B 348
- Normas: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
Calidad, entrega, inspección
Daxun realiza varias pruebas de aseguramiento de la calidad, estas pruebas incluyen pruebas mecánicas como la tracción de área, análisis químico, identificación positiva del material - prueba PMI, micro y macro pruebas, prueba de corrosión intergranular (IGC), prueba de detección de defectos por ultrasonidos, picaduras y prueba de resistencia, prueba de dureza, identificación positiva del material, prueba de expansión, etc. Todas estas pruebas garantizan que el material de la barra de titanio de grado 2 y la barra redonda de titanio de grado 2 es adecuado para la aplicación requerida. Durante el proceso de producción, medimos el diámetro, el grosor y la superficie del producto.
- Nuestro plazo de entrega se ajusta estrictamente a lo estipulado en el contrato.
- Apoyar a las agencias externas del cliente para que vayan a la fábrica a inspeccionar
- Muestras gratuitas para las pruebas de los clientes
- Apoyo a la inspección in situ o por vídeo en fábrica
Embalaje
Daxun Alloy garantiza la mejor calidad de embalaje, ya que desempeña un papel importante en el transporte internacional de mercancías, donde las mercancías pasan por varios canales para llegar al destino final, por lo que prestamos especial atención al embalaje. Embalamos nuestras mercancías de muchas maneras dependiendo del producto. Embalamos nuestros productos de muchas maneras, tales como:
- Cajas y cajones
- Retráctil
- Palés de madera
- Cajas de madera
Asistencia técnica
Si necesita asistencia técnica adicional, nuestro metalúrgico residente y nuestro personal experto estarán encantados de ayudarle. Además, Daxun cuenta con un laboratorio de pruebas certificado, una primicia en la industria de inventarios multimetal y plástico. Esto, en nuestra opinión, demuestra nuestra inquebrantable dedicación a la calidad y nuestra filosofía como proveedor de servicios completos.
Daxun Grade 23 Titanium Rods help your brand improve quickly
- Tolerances for Grade 23 Titanium Round Bars (BS EN ISO 286-2)
| TAMAÑO NOMINAL | h5 | h6 | h7 | h8 | h9 | H10 | H11 | h12 |
|---|---|---|---|---|---|---|---|---|
| DIÁMETRO mm | ||||||||
| ~ a 3 | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| de 3 a 6 años | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| de 6 a 10 años | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| de 10 a 18 años | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| de 18 a 30 años | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| más de 30 a 50 | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| más de 50 a 80 | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| más de 80 a 120 | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| más de 120 a 180 | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| más de 180 a 250 | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
Types of Ti-6AL-4V Grade 23 Titanium Rods (3)
Varilla de titanio
Proyectos y productos recientes
Productos relacionados (8)
Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 23 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.
ESPECIFICACIONES
AMS 4928 – Bars, Forgings, and Forging Stock (Annealed)
AMS 4965 – Bars, Forgings (Solution treated and aged)
AMS 4967 – Bars, Forgings (Annealed, Heat Treatable)
TRATAMIENTO TÉRMICO
When high hardness, tensile strength, and fatigue strength are required, annealing can be performed at 1,700-1,900°F (927 – 1,038°C).
DAXUN 6-4™ Grade 23 alloy can be heat treated in a variety of ways:
- Anneal: 1,275 – 1,400°F (691 – 760°C), ½ to 2 hours, air or furnace cool
- Stress Relief Anneal: 1,000 – 1,200°F (538 – 649°C), 1 to 8 hours, air or furnace cool
- Solution Heat Treat: 1,675 – 1,750°F (913 – 954°C), 1 hour, water quench
- Aging: 975 – 1,025°F (524 – 552°C), 4 to 8 hours – air cool
En la condición de tratamiento en solución y envejecido, el enfriamiento rápido de secciones pequeñas produce propiedades óptimas. Las secciones de mayor tamaño y/o el enfriamiento retardado pueden dar lugar a propiedades inferiores a las óptimas.
DUREZA
Typical hardness in the annealed condition is Rockwell C 30-34, and about Rockwell C 35-39 in the solution and aged condition.
Forgeability / Formability
Ti-6Al-4V ELI (Grade 23) alloy bar is forged at 1,750°F (954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 35% reduction is recommended for optimum properties.
Grade 23 alloy bar is difficult to form at room temperature, even in the annealed condition. Therefore, severe forming operations such as bending or stretching can be performed on annealed material at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000 – 1,200°F (538 – 649°C).
Maquinabilidad
Ti-6Al-4V ELI (Grade 23) alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids.
Soldabilidad
Grade 23 titanium rod is readily weldable in the annealed condition or in the solution and partially aged condition, with aging being accomplished during post weld heat treatment. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. Spot, seam, and flash welding may be performed without the aid of a protective atmosphere.
Consideraciones especiales
Grade 23 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics.
Size Range
Grade 23 Titanium Bar Dimensions
Ø 0.7 – 30 mm (drawn, ground)
Ø 16 - 400 mm (laminado en caliente, pelado)
Tolerances: h11–h5 (ISO 286-2)
Tolerancias más estrictas o diferentes disponibles bajo pedido
Longitudes de hasta 9.000 mm, en función del diámetro
Para diámetros mayores, se pueden acordar otras longitudes de barra y tolerancias bajo pedido.
Availability Grade 23 Titanium Rods
Processing options include:
- Dibujo, enderezado
- Estirar, enderezar, pulir
- Trefilado, esmerilado, pulido
- Embutición, enderezado, esmerilado, pulido
- Trefilado, recocido, enderezado
- Trefilado, recocido, pulido
- Trefilado, recocido, esmerilado, pulido
- Trefilado, recocido, enderezado, rectificado, pulido
Fabricamos barras según sus necesidades.
Excelente superficie y rectitud, redondez perfecta y tolerancias de diámetro muy ajustadas (según ISO 286-2 hasta h5). Disponibles en estado enderezado, rectificado y pulido.
Serrar
- Sierras de cinta (hasta Ø510 mm)
- Sierras de cinta de banco (hasta 6.000 x 3.000 x 400 mm)
- Sierras de alto rendimiento para un aserrado preciso
Titanium Bar End Machining
- Una o dos caras
- Chaflán 90° (45°)
- Punto 60° (30°)
- Extremo plano
- Centrado
Delivery Form
- ASTM American Society for Testing and Materials Standards
- AMS American Aerospace Materials Standards
- NACE American Association of Corrosion Engineers International Standards
- ASME American Society of Mechanical Engineers Standards
- GB Chinese National Standards
- GJB Chinese National Military Standards
- ISO International Standards
- DIN German Standards
- EN European Standards
- API American Petroleum Institute Standards
Detection Method
Ensayos no destructivos > Ensayo 100%
Testing methods:
- Eddy current testing / eddy current crack testing
- Superficie sin defectos (nivel 4)
- Diámetro del orificio de fondo plano 0,7 mm y 0,4 mm
- Blind area can be cut off according to fixed length > Test to the end of the bar
- Pruebas ultrasónicas de diámetro completo
Nuestros servicios de material de barra de titanio
As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.
We will be happy to provide you with a consultation and explain everything you need to know about obtaining Grade 23 titanium bar material, including which standards require greater attention for the components to be manufactured.
If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.
Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 23 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.
Información para pedidos
Purchase orders should include quantity, grade, type or category, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.
El grado de aleación de titanio que necesita depende del proyecto en el que esté trabajando, ya que cada grado tiene ventajas diferentes.
Todos los grados de aleación de titanio son extremadamente fuertes y resistentes a la corrosión, lo que significa que seguirán funcionando bien en las condiciones más duras.
Los grados superiores de aleación de titanio (5-12) son aleaciones diseñadas para prestaciones específicas. Por ejemplo, la aleación de titanio de grado 12 tiene una excelente resistencia al calor, por lo que es una opción perfecta para intercambiadores de calor de carcasa y tubos, tuberías hidráulicas y equipos de la industria química.
Los grados 1-4 son aleaciones de titanio puro y son la elección perfecta si necesita un material soldable y dúctil para sistemas de tuberías y conductos. Los grados inferiores se utilizan en la industria naval e industrial.
Si está iniciando un proyecto y no está seguro de qué grado de aleación de titanio es el más adecuado para usted, póngase en contacto con nosotros hoy mismo; estaremos encantados de ayudarle.
En DAXUN, ofrecemos una amplia gama de grados de aleación de titanio, desde el grado 1 hasta el grado 12.
Los grados 1-4 son titanio puro, mientras que los grados superiores son aleaciones.
Los grados de aleación son populares por su elevada relación resistencia-peso.
El grado de aleación de titanio más utilizado que encontramos es el grado 5. Aunque sigue teniendo un alto contenido en titanio, este grado es uno de los más fiables porque puede soportar temperaturas de hasta 600 °F y soportar condiciones extremas.
Las calidades superiores son las preferidas por industrias como la aeroespacial y la naval por su resistencia al desgaste y a la corrosión.
Por el contrario, las calidades inferiores se utilizan principalmente para soldar debido a su menor resistencia.
To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.
Aunque el grado de titanio aumenta ligeramente el coste, el coste total viene determinado principalmente por la forma del titanio que necesite.
En DAXUN ofrecemos una amplia gama de productos de titanio, como placas, tubos, bobinas y barras. La longitud, la anchura y la cantidad de cada artículo que necesite influirán en el importe que pague al realizar la compra.
Por desgracia, es difícil dar un precio en línea sin saber mucho sobre su proyecto y para qué se utilizará el titanio.
Afortunadamente, nuestro equipo de expertos está siempre a su disposición para ayudarle y asesorarle en sus necesidades de titanio. Enviando un correo electrónico a daxunalloy@gmail.com, podremos responderle con algunos consejos y un presupuesto preciso.
Asegúrese de incluir toda la información posible sobre el grado, la forma y la cantidad de titanio que necesita para conocer mejor sus necesidades.
El equipo de DAXUN es experimentado, experto y amable. Con años de experiencia en el sector, lo saben todo sobre el titanio, incluidos sus usos, ventajas y calidades.
Si desea información actualizada sobre el titanio, sus usos y aplicaciones en distintos sectores, no deje de consultar nuestro blog. Nuestros expertos han escrito guías fáciles de seguir a las que siempre podrá recurrir cuando tenga preguntas.
Si sigues teniendo problemas, no dudes en ponerte en contacto con nosotros; estaremos encantados de ayudarte.
Si envía un correo electrónico a daxunalloy@gmail.com, recibirá una respuesta rápida. Asegúrate de incluir en tu pregunta todos los detalles posibles para que podamos recomendarte una solución adecuada.
Rellene el formulario de la página “Contacto” o llame a nuestro responsable de ventas al “+86 13382898899”, nos pondremos en contacto con usted lo antes posible. Nuestro WhatsApp está en línea, y el correo electrónico (Daxunalloy@gmail.com) se comprobará en un plazo de 6 horas. Cada consulta o mensaje será respondido con prontitud. Además, compartimos información de mercado con nuestros clientes cada semana
Podemos proporcionarle muestras de barras de titanio para que compruebe la calidad. La muestra es gratis y usted sólo paga el flete.
Hemos exportado a más de 42 países, como Canadá, Chile, Kuwait, Alemania, Corea del Sur, Arabia Saudí, Singapur, etc.
Our MOQ is 300 Kg for titanium rod.
Los pedidos de prueba pueden entregarse en una semana. Los pedidos normales tardan unas dos semanas.