x
Envíe su consulta hoy mismo
Presupuesto rápido
  • Hastelloy plate
  • Hastelloy plate
  • Hastelloy plate
  • Hastelloy plate
  • Hastelloy plate
  • Hastelloy plate
  • Hastelloy plate
  • Hastelloy plate
  • Hastelloy plate
  • Hastelloy plate

Hastelloy G35 Plate - Daxun Alloy - The Best Alloy Supplier

Daxun Alloy supplies high quality Hastelloy G35 Plates to the world.
  • Grade : Hastelloy G35
  • Certification : SGS,ISO,CE
  • Finish : Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
  • Surface finish : Bright, Dull, Hair Line(HL), others
  • Thickness : 0.5mm to 50 mm Thk
  • Width : 500-2000mm
  • Length : 2m, 2.44m, 3m, or as required
  • Delivery Time : 7-15 days
  • MOQ : ≥50kg

Characteristics & Properties of Hastelloy G35

Hastelloy G35 plate is a high-performance corrosion-resistant alloy plate based on nickel, designed for extreme chemical environments. Its core components include chromium (28-33%), molybdenum (4.0-8.0%) and copper (1.0-2.4%), which give it excellent acid resistance, especially strong tolerance to sulfuric acid, phosphoric acid and chloride-containing media, and can effectively resist pitting, crevice corrosion and stress corrosion cracking. At the same time, the alloy can remain stable in high temperature environments and is suitable for key equipment in chemical production such as sulfuric acid and phosphoric acid, such as reactors, heat exchangers and evaporators, especially for the concentration process of “wet” phosphoric acid.

This plate has excellent processing performance and reliable mechanical strength, supports hot processing, cold processing and various welding methods, and has a thickness range of 0.5-50mm. It is widely used in chemical, energy, marine engineering and other fields. Hastelloy G35 plates have shown long-term stability in the black liquor recovery system of pulp and paper, seawater desalination equipment, and highly corrosive environments in pharmaceutical and food processing. Its flexible specifications and reliable performance make it an ideal choice to replace traditional stainless steel and nickel-based alloys, significantly improving equipment life and safety, especially under harsh working conditions.

Características

Excellent corrosion resistance:
– Acid media: Excellent resistance to strong acids such as sulfuric acid, sulfates, phosphoric acid, hydrochloric acid, and hydrofluoric acid. It can effectively resist corrosion in the production and processing environment of sulfuric acid and phosphoric acid, such as in the chemical industry for production and processing equipment (reactors, heat exchangers, pipelines and pumps, etc.) of sulfuric acid and phosphoric acid. When processing “wet-process” phosphoric acid, it performs far better than other metal materials and can play a good role in resisting localized corrosion under the evaporator deposits of concentrated “wet-process” phosphoric acid.

– Oxidizing and reducing media: The high chromium content makes it extremely resistant to other oxidizing acids (such as nitric acid) and mixtures containing nitric acid; the considerable molybdenum content makes it moderately resistant to reducing acids. In addition, it can also resist localized corrosion and chloride ion stress corrosion cracking in chloride-containing media. Unlike other nickel-chromium-molybdenum alloys, it has strong resistance to “caustic dealloying” in hot sodium hydroxide.

Good high-temperature performance: It has excellent high-temperature stability and can maintain good strength and toughness in high-temperature environments, ensuring the normal operation of equipment under high-temperature conditions. However, the specific data of its high temperature performance (such as quantitative indicators such as high temperature strength and oxidation resistance) are less and less uniform in different materials. It is only known that it has certain performance at high temperature, but lacks specific numerical support such as tensile strength and yield strength.

Good processing performance: It has good hot processing, cold processing and welding performance. The hot processing temperature range is usually 1050-1200℃. The heating rate should be moderate to avoid excessive thermal stress. After hot processing, it needs to be properly cooled to ensure the structure and performance of the alloy; during cold processing, due to the high strength, a large processing force is required. Multiple cold processing and intermediate annealing processes can be used to reduce the difficulty of processing and improve the quality; welding can be carried out by tungsten inert gas shielded welding (TIG), melt inert gas shielded welding (MIG) and other methods. Before welding, the weldment should be strictly cleaned, the heat input should be controlled during welding, and heat treatment may be required after welding to eliminate welding stress.

Application field

Chemical industry: Applicable to the production and processing equipment of sulfuric acid and phosphoric acid, such as reactors, heat exchangers, pipelines and pumps. It is also widely used in various corrosion-resistant equipment in chemical production, such as reactors, evaporators, etc.
Pulp and paper industry: can be used in black liquor recovery systems to withstand high temperature and highly corrosive environments.
Marine engineering: used for seawater desalination equipment and offshore platform structures to resist seawater corrosion.
Energy industry: in the fields of nuclear power and thermal power, used to manufacture corrosion-resistant high-temperature components; in the oil and gas industry, used for drilling and production facilities to resist hydrogen sulfide and other corrosive gases.
Food processing industry: suitable for equipment that handles acidic or alkaline foods, such as evaporators and heat exchangers.
Pharmaceutical industry: used to manufacture corrosion-resistant pharmaceutical equipment and containers.

Seguir leyendo

Hastelloy G35 Parameters

Ni Cr Co W Mo Fe
Resto 28% – 33% ≤1.0% ≤4.0% 4.0% – 8.0% 1.3% – 2.0%
Cu C Si Mn P S
1.0% – 2.4% ≤0.05% ≤0.6% ≤1.5% ≤0.035% ≤0.02%
Propiedad Densidad Punto de fusión Conductividad térmica Capacidad calorífica específica Coefficient of Thermal Expansion Elastic Modulus
Valor 8.22 – 8.72 g/cm³ 1325 – 1361°C 10 – 23 W/(m·K) 400 – 600 J/(kg·K) 13.9×10⁻⁶/°C (20 – 100°C) 177 GPa
Propiedad Resistencia a la tracción Yield Strength Elongation (A5%) Hardness
Valor σb ≥ 524 N/mm² σ0.2 ≥ 200 N/mm² δ ≥ 62% HB ≤ 350

Elija Daxun y haga que sus clientes queden satisfechos.

Póngase en contacto con Daxun

Entrega rápida

Daxun provides customers with timely and fast delivery of Hsatelloy G35 plate products. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to ports and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

Póngase en contacto con Daxun

Advanced machining

Daxun’s typical service of “more, faster, better and cheaper” for Hastelloy G35 plate materials starts with Daxun’s alloy varieties, specifications and spot inventory. It has strategic resource support from many large steel mills at home and abroad to ensure a stable supply chain and meet customers’ personalized needs for specific materials. It can be called the “Wal-Mart” of the stainless steel industry. With more than 20 years of experience, it has established the brand image of “Look for Daxun for stainless steel plates” in the Chinese market.

Póngase en contacto con Daxun

Hastelloy G35 plate packaging

Daxun Alloy ensures the best quality of hastelloy plate packaging, because packaging plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Cajas y cajones
• Kraft paper + wooden pallets
- Retráctil
• Fumigation-free wooden pallets
• Fumigation-free wooden boxes

Póngase en contacto con Daxun

Hastelloy G35 Plate Surface Treatment

1D: La superficie es mate con forma de partícula discontinua.
2D: Blanco con un tono plateado.
2B: Gris plateado con mejor brillo y planitud que la superficie 2D.
Ba: Superficie cercana al espejo con excelente brillo y reflectividad.
No.3: Buen brillo y superficie rugosa.
No.4: La superficie tiene líneas finas y buen brillo.
HL: Gris plateado con pelo dorado.
8K: Superficie de espejo.

Póngase en contacto con Daxun

Hastelloy G35 Sheet Processing:

  • Etching processing
  • Welding processing
  • Bending processing
  • Embossing processing
  • Sandblasting processing
  • Polishing processing
  • Punching processing
  • Stamping processing
  • Cutting processing

Daxun is a trustworthy metal manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all metal plates are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the metal plates have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

About Daxun Metal Products

Daxun metal plates are in high demand, have good quality, and are honest and trustworthy.

  • Daxun International has been in international business for over ten years. In 2022, its export revenue surpassed $100 million, and its export volume was among the top Chinese stainless steel processing enterprises. To serve abroad markets, we have built three export service facilities in China and collaborated with engineering organisations, steel mills, and international trade companies. We continue to enhance our service capabilities, establishing three export service bases in China, and collaborating with engineering firms, steel mills, and international trading firms to grow into new markets.
  • Daxun has long-standing relationships with dozens of well-known steel mills throughout the world, supplying 30,000 tonnes of standard stainless steel plates and 20,000 tonnes of metals such as duplex steel, nickel-based alloys, and heat-resistant steel. Daxun’s stainless steel materials are of consistent quality and never counterfeited. The kinds, specifications, and delivery weights strictly adhere to the standards.
  • Daxun has several stainless steel plate processing equipment, a professional physical and chemical testing centre, and “cutting, grinding, forming, beveling, welding, heat treatment, machining, and spraying” production lines. Services are provided in approximately 30 industries, including vehicles, home appliances, lifts, new energy, vacuum semiconductors, food and beverage/biofermentation, petrochemicals, and energy equipment. Collaborate with steel mills, research institutes, and other organisations to offer comprehensive services ranging from project design and material development to processing and manufacturing process optimisation.

Metal materials “more, faster, better, and cheaper” customised services

  • First, it refers to Daxun’s metal plate kinds and specifications, as well as its spot inventories.Daxun has strategic resource assistance from many large steel mills at home and abroad, ensuring the stability of the metal plate supply chain and meeting clients’ individualised needs on specific materials.
  • Secondly, Daxun’s processing technology is diverse.
    processes, including metal plate cutting, grinding, cutting, forming, welding, and machining, to provide customers with “one-stop” service.

Daxun services a large number of consumers in a variety of sectors.

  • Daxun alloy company focuses on the key sectors of equipment manufacture. far, it has served over 30,000 customers, including over 10,000 active customers from more than 30 industries and a big number of major businesses. This demonstrates Daxun’s extensive service experience, as well as its widespread consumer recognition across industries.

Customers with urgent needs can rest assured that we will supply metal plate products on time and quickly.

  • Behind the speed is the support of the system, including information flow, logistics, and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, seamlessly connected; in terms of logistics, the processing center is close to ports, rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading to ensure that the task is completed on time.

We provide excellent quality and high-quality services.

  • Quality is belief, and integrity is a business card. Daxun pioneered the concept of “excellent performance management” and promoted the “PDCA+Lean” management model, making “Daxun = assured quality” the company’s business card. In terms of materials, Daxun Alloy has achieved full traceability of each steel plate from the ERP system, including varieties, specifications, and origins, and advocated and encouraged industry anti-counterfeiting.
  • Daxun Alloy relies on technology for processing, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, closely monitors during sales, and provides worry-free service guarantees after sales.

We save our customers time, materials and energy, and ultimately save them money.

Daxun’s professional advantages enable us to provide the most cost-effective material recommendations based on customer needs, and minimize costs for customers through methods such as continuous processing and nesting processing.

Our innovative nesting processing methods optimize material and cutting utilization.

At the same time, Daxun achieves continuous cost reduction and efficiency improvement by promoting lean improvement activities and passing the benefits to customers. Daxun also has a complete product traceability system and timely quality objection handling, which relieves customers’ concerns.

Leading Metal Sheet Suppliers in China

Contact the top suppliers in China for metal sheets (steel plates) in a variety of finishes. You need no other metal sheet supplier than Daxun Alloys, who offer free cutting services and delivery times as short as 5-7 days.

We can assist in providing metal sheets in any required size.

To meet your specific requirements, our metal sheets are available in three finishes and a variety of sizes. We can readily provide any custom size you may need with our free unlimited cutting service.

We are able to meet any size needs between 0.3 and 30 mm in thickness and between 50 x 50 mm and 2500 x 1250 mm in size. In addition, we provide free unlimited cutting with every order, using a state-of-the-art cutting machine to precisely meet your requirements.

Order metal Sheets by Phone or Online.

There has never been an easier way to get metal sheets. Simply refer to the simple and detailed instructions on our website. Alternatively, our sales staff will be happy to take your order or answer any questions when you call +86 13382898899 or email daxunhejin@gmail.com.

Our delivery time is only one to two days.

Characteristics:

This grade is more resistant to corrosion and pitting than 304 and offers higher strength at elevated temperatures. In addition, 316L is an extra low carbon variation that helps avoid carbide precipitation due to welding.

Important Safety Note:

The edges of the metal sheets we sell are not polished, ground or finished, so they may be sharp, just like the edges of any metal sheet. We remind users to use, install and handle these devices with care.

¿Puedo obtener algunas muestras?

We can provide metal sheet samples for you to check the quality. Sample is free and you just pay the freight.

¿A qué países ha exportado ya?

Hemos exportado a más de 42 países, como Canadá, Chile, Kuwait, Alemania, Corea del Sur, Arabia Saudí, Singapur, etc.

¿Cuál es su MOQ?

Our MOQ is 1 ton for metal sheet.

¿Cuál es el plazo de entrega?

Los pedidos de prueba pueden entregarse en una semana. Los pedidos normales tardan unas dos semanas.

Envíe su consulta hoy mismo
Presupuesto rápido