Grade 9 Ti-3Al-2.5V Titanium Alloy Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:Grade 9 - UNS R56320
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of grade 9 titanium is 4.48 g/cm3
  • Standards:ASTM B381、AMS 4920、ASTM B265

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

Grade 9 Titanium Alloy Pipe Manufacturer - Daxun Alloy

Provide High Quality Grade 9 Titanium Pipe to Customers Around The World
Grade 9 titanium pipe is a versatile alpha-beta alloy (Ti-3Al-2.5V), offering an optimal balance between pure titanium’s formability and Grade 5’s strength. It features moderate strength, exceptional weldability, and outstanding corrosion resistance in diverse environments. Its density (4.48 g/cm³) is approximately 60% that of steel, yet it delivers strength comparable to some steels, making it ideal for weight-sensitive applications. The alloy excels in durability across harsh conditions, including seawater, chemical processing, and extreme temperatures, while maintaining excellent fracture toughness and fatigue resistance.

Where is Grade 9 titanium pipe used?
In aerospace, it’s used for hydraulic and fuel lines, ducting systems, and airframe components—reducing weight without sacrificing structural integrity. Chemical processing plants rely on it for heat exchangers, reactor tubing, and piping systems handling corrosive acids, alkalis, and chlorides due to its inertness. Marine and offshore industries use it for seawater cooling systems, desalination plants, and subsea equipment, leveraging its unparalleled seawater corrosion resistance. Oil and gas operations employ it in downhole tubing, risers, and Christmas tree components for high-pressure sour gas environments. Additionally, sports equipment manufacturers utilize it for high-performance bicycle frames, golf shafts, and racing components, where its strength-to-weight ratio and fatigue resistance are critical. It also serves in power generation (condenser tubing) and industrial heat transfer systems, combining longevity with thermal efficiency.

Key Performance:

Strength-Ductility Balance:

  • Tensile Strength: 620 MPa (annealed state) – Lower than Grade 23 but 30% stronger than pure titanium (Grade 1-4).
  • Elongation: ≥15% – Superior ductility vs. Grade 5 (≥10%), enabling complex forming and high fatigue resistance.
  • Density: 4.48 g/cm³ – 60% lighter than steel, ideal for weight-sensitive applications.

Corrosion Resistance:

  • Resists pitting/crevice corrosion in seawater, chlorides, and acidic/alkaline environments (e.g., HCl, H₂SO₄).
  • Outperforms stainless steel in marine/chemical processing, with no galvanic corrosion risk.

Weldability & Processability:

  • Welding: Exceptional compatibility with TIG, laser, and electron-beam welding – minimal post-weld cracking risk.
  • Forming: Cold-workable into tubes, sheets, and complex shapes; machinability comparable to Grade 5.
  • Heat Treatment: Stress-relieved at 480–650°C to optimize mechanical properties.

Application Advantages:

  • Aerospace: Hydraulic tubing, ducting – weight reduction without sacrificing fatigue life.
  • Marine: Heat exchangers, desalination plants – seawater immunity extends service life.
  • Chemical: Reactors, piping systems – handles sour gas (H₂S) and strong acids.
  • Industrial: High-pressure cylinders, sports equipment (bike frames, golf shafts) – lightweight durability.
Seguir leyendo

Datos

Elemento Composition Range (wt.%)
Ti Balance (>90%)
Al 2.50–3.50%
V 2.00–3.00%
Fe ≤0.25%
O ≤0.13%
C ≤0.08%
N ≤0.03%
H ≤0.015%
Otros ≤0.4% (single element)

Key Characteristics

  • Relación resistencia/peso: Higher than pure titanium (Grades 1–4) but lower than Ti-6Al-4V (Grade 5).
  • Resistencia a la corrosión: Excellent in marine, chemical, and chloride environments.
  • Biocompatibilidad: Non-toxic and MRI-compatible, but less commonly used in implants than Grade 23.
  • Formability: Superior to Grade 5; suitable for complex forming, welding, and machining.

 Aplicaciones típicas

  • Aeroespacial: Hydraulic tubing, aircraft fittings, fasteners.
  • Marine: Heat exchangers, seawater components, propeller shafts.
  • Medical: Surgical instruments, non-implantable devices.
  • Industrial: Chemical processing equipment, pressure vessels.

 

Propiedad Value (Imperial) Value (Metric)
Densidad 0.160 lb/in³ 4.43 g/cm³
Punto de fusión 3,000–3,050°F 1,650–1,680°C
Conductividad térmica 6.5 Btu/(hr·ft·°F) 11.2 W/(m·K)
Coefficient of Thermal Expansion 5.3 × 10⁻⁶/°F 9.5 × 10⁻⁶/K
Resistividad eléctrica 120 µΩ·cm 120 nΩ·m

Elija Daxun para que su proyecto despegue.

Póngase en contacto con Daxun

Advanced Production:Titanium seamless pipe

Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.

Póngase en contacto con Daxun

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

Póngase en contacto con Daxun

Informes de las pruebas

Our Grade 9 titanium tubing comes with an extensive range of certification and testing documentation tailored to meet your specific project requirements. We supply detailed material traceability records, comprehensive chemical composition analysis, and mechanical property certifications that demonstrate the exceptional performance characteristics of our titanium products. Each tube shipment includes quality assurance documentation covering dimensional verification, surface inspection reports, and welding procedure specifications when applicable.

Póngase en contacto con Daxun

Applications and standards

Titanium Grade 9 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
Póngase en contacto con Daxun

Calidad, entrega, inspección

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 9 Titanium Welded Pipe and Grade 9 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • Nuestro plazo de entrega se ajusta estrictamente a lo estipulado en el contrato.
  • Apoyar a las agencias externas del cliente para que vayan a la fábrica a inspeccionar
  • Muestras gratuitas para las pruebas de los clientes
  • Apoyo a la inspección in situ o por vídeo en fábrica
Póngase en contacto con Daxun

Embalaje

Daxun Alloy garantiza la mejor calidad de embalaje, ya que desempeña un papel importante en el transporte internacional de mercancías, donde las mercancías pasan por varios canales para llegar al destino final, por lo que prestamos especial atención al embalaje. Embalamos nuestras mercancías de muchas maneras dependiendo del producto. Embalamos nuestros productos de muchas maneras, tales como:
- Cajas y cajones
- Retráctil
- Palés de madera
- Cajas de madera

Póngase en contacto con Daxun

Asistencia técnica

Si necesita asistencia técnica adicional, nuestro metalúrgico residente y nuestro personal experto estarán encantados de ayudarle. Además, Daxun cuenta con un laboratorio de pruebas certificado, una primicia en la industria de inventarios multimetal y plástico. Esto, en nuestra opinión, demuestra nuestra inquebrantable dedicación a la calidad y nuestra filosofía como proveedor de servicios completos.

Daxun Grade 9 Titanium TUBE Let your brand improve rapidly

Grade 9 titanium tube form (4)

  • Titanium seamless tubes are made by piercing and drawing solid titanium bars, and the hollow part of the tube is made by piercing or hot extrusion. Titanium seamless tubes are ideal for very large diameter to wall thickness ratios and have very good external dimensional tolerances.

  • Titanium welded pipe is a tubular product made of strip titanium that is roll formed and fusion welded along the longitudinal seam. The welding process used by Daxun Alloy does not use any filler metal during the welding process.

  • Titanium square tubes are drawn from round tubes or round tube billets and can be formed into right angles or rounded corners. They can also be cold extruded, which is efficient and low cost. The only disadvantage is that the tolerance will gradually increase.

  • Tubular products are welded and then re-drawn to final size. Welding and drawing is ideal for producing thick walled, large diameter tubes that cannot be welded directly to size but still offer cost savings over seamless tubes. All Daxun welded and drawn tubes are bright annealed.

Proyectos y productos recientes

Grade 9 Titanium pipe and tube
Grade 9 Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
How does Grade 9 titanium compare to Grade 5 in terms of performance?

While Grade 5 titanium offers higher strength, Grade 9 provides better formability, weldability, and corrosion resistance. Grade 9 is often preferred for tubing applications due to its excellent balance of properties and easier fabrication characteristics.

What sizes of Grade 9 titanium tubes do you supply?

We offer Grade 9 titanium tubes in a wide range of outside diameters from 6mm to 120mm, with wall thicknesses from 0.5mm to 10mm. We can supply both seamless and welded tubes, with lengths up to 6 meters or as specified by customer requirements.

Can you provide custom specifications for Grade 9 titanium tubes?

Yes, we can produce Grade 9 titanium tubes to your specific requirements including custom dimensions, special tolerances, unique tempers, and specific surface finishes. Please provide your technical specifications, and our engineering team will work with you to meet your exact needs.

How do you ensure the quality of your Grade 9 titanium tubes?

All our Grade 9 titanium tubes undergo comprehensive quality control including dimensional checks, surface inspection, and mechanical testing. We provide complete material traceability and full documentation including chemical analysis, mechanical properties, and conformity certificates with every shipment.

¿En qué se diferencian los grados superiores de titanio de los inferiores?

En DAXUN, ofrecemos una amplia gama de grados de aleación de titanio, desde el grado 1 hasta el grado 12.

Los grados 1-4 son titanio puro, mientras que los grados superiores son aleaciones.

Los grados de aleación son populares por su elevada relación resistencia-peso.

El grado de aleación de titanio más utilizado que encontramos es el grado 5. Aunque sigue teniendo un alto contenido en titanio, este grado es uno de los más fiables porque puede soportar temperaturas de hasta 600 °F y soportar condiciones extremas.

Las calidades superiores son las preferidas por industrias como la aeroespacial y la naval por su resistencia al desgaste y a la corrosión.

Por el contrario, las calidades inferiores se utilizan principalmente para soldar debido a su menor resistencia.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

¿Influye el grado de titanio en el coste?

Aunque el grado de titanio aumenta ligeramente el coste, el coste total viene determinado principalmente por la forma del titanio que necesite.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

Por desgracia, es difícil dar un precio en línea sin saber mucho sobre su proyecto y para qué se utilizará el titanio.

Afortunadamente, nuestro equipo de expertos está siempre a su disposición para ayudarle y asesorarle en sus necesidades de titanio. Enviando un correo electrónico a daxunalloy@gmail.com, podremos responderle con algunos consejos y un presupuesto preciso.

Asegúrese de incluir toda la información posible sobre el grado, la forma y la cantidad de titanio que necesita para conocer mejor sus necesidades.

¿Dónde puedo obtener más información sobre las calidades del titanio?

El equipo de DAXUN es experimentado, experto y amable. Con años de experiencia en el sector, lo saben todo sobre el titanio, incluidos sus usos, ventajas y calidades.

Si desea información actualizada sobre el titanio, sus usos y aplicaciones en distintos sectores, no deje de consultar nuestro blog. Nuestros expertos han escrito guías fáciles de seguir a las que siempre podrá recurrir cuando tenga preguntas.

Si sigues teniendo problemas, no dudes en ponerte en contacto con nosotros; estaremos encantados de ayudarte.

Si envía un correo electrónico a daxunalloy@gmail.com, recibirá una respuesta rápida. Asegúrate de incluir en tu pregunta todos los detalles posibles para que podamos recomendarte una solución adecuada.

¿Puedo obtener algunas muestras?

We can providetitanium tube for you to check the quality. Sample is free and you just pay the freight.

¿A qué países ha exportado ya?

Hemos exportado a más de 42 países, como Canadá, Chile, Kuwait, Alemania, Corea del Sur, Arabia Saudí, Singapur, etc.

¿Cuál es el plazo de entrega?

Los pedidos de prueba pueden entregarse en una semana. Los pedidos normales tardan unas dos semanas.

Envíe su consulta hoy mismo
Presupuesto rápido