  • Titanium bar grade: Grade 5-Ti6Al 4V- UNS R56400-3.7165-TC4
  • Titanium bar types: rolled bars, drawn bars, forged titanium bars
  • Titanium bar density The density of grade 5 titanium is 4.51 g/cm3
  • Main standards: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
  • High strength, high temperature resistance, corrosion resistance, light
  • weight, excellent comprehensive performance.

————Daxun produces titanium rods in China to meet the diverse and ——требовательные потребности клиентов!

The global leader in commercially pure titanium rod manufacturing services

Daxun, specializing in the production of alloy titanium rods for extreme environments—Ti6AL-4V titanium alloy rods.

Grade 5 titanium alloy rod (titanium aluminum vanadium alloy) is the most commonly used α-β titanium alloy, accounting for 50% of the total titanium alloy usage worldwide. One of the most notable features of grade 5 titanium alloy is that it is fully heat treatable and can be used at temperatures up to 400°C. It has low density (4.43 kg/dm), excellent corrosion resistance, and high mechanical strength. Grade 5 titanium alloy has high tensile strength at ambient temperature and good creep resistance at temperatures up to 300°C. It also has strong crack resistance and fatigue resistance. The age-hardening ability of 6AL-4V titanium alloy rod makes it an excellent choice for a wide range of applications, including fasteners and components in harsh environments. Its high machinability and weldability make it suitable for a wide range of industrial applications.

Даксун is your trusted titanium alloy rod production company. Daxun produces all grades of titanium alloys, including commercially pure titanium series CP, titanium alloy series, titanium nickel alloy, etc. They have reliable performance and provide high performance for your critical applications. In various industries and applications, you can rely on Daxun titanium alloy rods for high strength, high temperature and corrosive environments. For decades, Daxun Metals has been committed to producing highly engineered titanium alloy solutions to meet the most severe challenges.

Читать далее

Данные

Specification Details
Материал Titanium rod and bar Grade 5 (UNS R56400)
Стандарт ASTM B348, ASTM SB348, AMS 4921, AMS 4902
Dimensions EN, ASTM, JIS, ASME, BS, AISI , GB,GJB,DIN
Diameter Range 0.125″ – 14″ (3.175mm – 355.6mm), custom
Length Range Up to 240″ (6096mm), custom
Finish Cold (bright) drawn, centreless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centreless Ground & Black
Отделка поверхности Cold drawn, Centerless Ground, Polished, Or Rough Turned, Black, NO.4 Finish, BA Finish, Matt Finish, etc.
Condition Hardened & tempered, annealed
Толерантность Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm)
Form Titanium square bars, titanium ingots, titanium round bars, rectangular titanium bars, triangular titanium bars, forged titanium bars, titanium hexagonal bars, etc.
Физические свойства Density: 0.163 lb/in³ (4.51 g/cm³), Melting Point: 3,020°F (1,660°C), Elongation: 20-30%, Modulus of Elasticity: 16.5 x 10⁶ psi (114 GPa)
Химический состав Titanium (min): 99.2%, Oxygen (max): 0.25%, Carbon (max): 0.08%, Iron (max): 0.30%, Nitrogen (max): 0.03%, Hydrogen (max): 0.015%
Chemical Composition:
Symbol Элемент Min % Max %
Al Aluminum 5.50% 6.75%
V Vanadium 3.50% 4.50%
Fe Iron 0.30%
O Oxygen 0.20%
C Углерод 0.08%
N Азот 0.05%
H Hydrogen 0.01%
Y Yttrium 0.01%
Other, each 0.10%
Other, total 0.40%
Ti Титан Remainder
Физические свойства Metric English Comments
Плотность 4.43 g/cc 0.16 lb/in³
Механические свойства
Hardness, Brinell 334 334  Estimated from Rockwell C.
Hardness, Knoop 363 363  Estimated from Rockwell C.
Hardness, Rockwell C 36 36
Hardness, Vickers 349 349  Estimated from Rockwell C.
Tensile strength min. 895MPa 129810 psi
Yield strength min. 828MPa 120090 psi
Elongation at Break min.10 % 10 %
Reduction of Area min.25 % 25 %
Modulus of Elasticity 113.8 GPa 16500 ksi
Compressive Yield Strength 970 MPa 141000 psi
Notched Tensile Strength 1450 MPa 210000 psi  Kt (stress concentration factor) = 6.7
Ultimate Bearing Strength 1860 MPa 270000 psi  e/D = 2
Bearing Yield Strength 1480 MPa 215000 psi  e/D = 2
Poisson’s Ratio 0.342 0.342
Charpy Impact 17 J 12.5 ft-lb  V-notch
Fatigue Strength 240 MPa 34800 psi  at 1E+7 cycles. Kt (stress concentration factor) = 3.3
Fatigue Strength 510 MPa 74000 psi  Unnotched 10,000,000 Cycles
Fracture Toughness 75 MPa-m½ 68.3 ksi-in½
Shear Modulus 44 GPa 6380 ksi
Shear Strength 550 MPa 79800 psi  Ultimate shear strength
Electrical Properties
Электрическое сопротивление 0.000178 ohm-cm 0.000178 ohm-cm
Магнитная проницаемость 1.00005 1.00005  at 1.6kA/m
Magnetic Susceptibility 3.30E-06 3.30E-06  cgs/g
Thermal Properties
CTE, linear 20°C 8.6 µm/m-°C 4.78 µin/in-°F  20-100ºC
CTE, linear 250°C 9.2 µm/m-°C 5.11 µin/in-°F  Average over the range 20-315ºC
CTE, linear 500°C 9.7 µm/m-°C 5.39 µin/in-°F  Average over the range 20-650ºC
Specific Heat Capacity 0.5263 J/g-°C 0.126 BTU/lb-°F
Теплопроводность 6.7 W/m-K 46.5 BTU-in/hr-ft²-°F
Температура плавления 1604 – 1660 °C 2920 – 3020 °F
Solidus 1604 °C 2920 °F
Liquidus 1660 °C 3020 °F
Beta Transus 980 °C 1800 °F
Beta Transus (F ± 25) 1830
Coefficient of Thermal Expansion (10-6in./in./F) 32-212 5
32-600 5.3
32-1000 5.6
32-1200 5.9
32-1500 6.1
Density (lbs./cu. in.) 0.16
Melting Point, Approx (F) 3200
Electrical Resistivity at Room Temp. (Microhms cm) 171
Modulus Elasticity – Tension (106 psi) 16.5
Modulus Elasticity – Torsion (106 psi) 6.1
Теплопроводность 3.9 at Room Temperature
(Btu/hr/sq. ft./F/ft.)
Specific Heat (Btu/lb./F) at Room Temp. 0.135
Свариваемость Fair
Annealing Temp. (F) Полный 1300 – 1525°/15 Min. – 2 Hrs,; Air Cool
Stress Relief 900 – 1200°/1 -4 Hrs.; Air Cool
Forging* Temp. (F) Blocking 1750 – 1800°
Finishing 1650 – 1750°
Typical Application Compressor blades, discs, aircraft components, pressure vessels, rocket engine cases;
the most versatile titanium alloy.
ASTM B348 Gr5 Titanium Round Bar ASTM B348 GR 5 Cold Rolled Rods
Titanium Alloy Grade 5 Bright Bars ASTM B348 Gr 5 Titanium Polish Bars
B348 Grade 5 Titanium Forged Round Bars Titanium Alloy ASTM B348 Grade 5 Spring Steel Bars
Grade 5 Ti Alloy Hexagon Bars Titanium Alloy Werkstoff Nr. 3.7165 Square Bars
Titanium Alloy UNS R56400 Rods B348 Grade 5 Titanium Alloy Hex Bars
Ti Alloy GR5 Cold Drawn & Polished Square Bars Titanium Alloy Grade5 Hollow Bars
ASTM B348 Grade 5 Titanium Threaded Bars Titanium ASTM B348 Grade 5 Flat Bars
Top Quality B348 Grade 5 Titanium Cold Drawn Bars AS ASTM B348 Gr 5 Black Bars

Выберите Daxun, чтобы помочь вашему проекту взлететь.

Свяжитесь с Daxun прямо сейчас

DAXUN® Grade 5 Titanium Rod Features

DAXUN® Ti Grade 5 is a titanium alloy bar (6al-4v) featuring:

  • Good hot formability and weldability;
  • Tensile strength can reach 1000MPa;
  • Dimensional work at high temperature
  • Insensitive to seawater or seawater;
  • Not affected by various corrosive media;
  • High strength and good toughness;
  • Resist crack initiation and crack propagation.
Свяжитесь с Daxun прямо сейчас

Daxun Factory Advantages

Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

Свяжитесь с Daxun прямо сейчас

Grade 5 Titanium Rod Production Method

Daxun produces high-quality titanium bars with high performance, and can also manufacture according to customer’s agreement:

  • Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
Свяжитесь с Daxun прямо сейчас

Отчеты о тестировании

The test reports we provide include: Grade 2 Titanium Rod and Grade 2 Titanium Round Bar Factory Test Certificate, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, NABL Approved Laboratory Report, Destructive Test Report, Non-destructive Testing Report. (Daxun will provide according to customer requirements)

Свяжитесь с Daxun прямо сейчас

Grade 5 Rods Applications and Standards

Grade 5 Titanium Rods are widely used in the following industries under extreme corrosive conditions:

  • Aerospace, shipbuilding, oil and gas industry, marine engineering, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, military industry, pharmaceutical and food processing equipment, etc.
  • Specifications: AMS 4928,AMS 4967,AMS 4965 ,AMS 6931 ,ASTM B 348
  • Standards: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
Свяжитесь с Daxun прямо сейчас

Качество, доставка, проверка

Daxun performs several quality assurance tests, these tests include mechanical tests like area tensile, chemical analysis, material positive identification – PMI test, micro and macro testing, intergranular corrosion (IGC) test, ultrasonic flaw detection test, pitting and resistance test, hardness test, material positive identification, expansion test etc. All these tests ensure that the Grade 2 Titanium Rod and Grade 2 Titanium Round Bar material is suitable for the required application. During the production process, we measure the diameter, thickness and surface of the product.

  • Сроки доставки строго соответствуют договору.
  • Поддержка сторонних агентств клиентов для посещения завода для проверки
  • Поддержка бесплатных образцов для тестирования клиентов
  • Поддержка инспекции на месте или видеоинспекции на заводе
Свяжитесь с Daxun прямо сейчас

Упаковка

Daxun Alloy обеспечивает наилучшее качество упаковки, поскольку она играет важную роль в международных перевозках, где товары проходят через различные каналы, чтобы достичь конечного пункта назначения, поэтому мы уделяем особое внимание упаковке. Мы упаковываем наши товары различными способами в зависимости от продукта. Мы упаковываем наши товары различными способами, такими как:
- Коробки и ящики
- Термоусадочная пленка
- Деревянные поддоны
- Деревянные ящики

Свяжитесь с Daxun прямо сейчас

Техническая поддержка

Если вам потребуется дополнительная техническая помощь, наш постоянный металлург и компетентный персонал будут рады помочь. Кроме того, Daxun может похвастаться сертифицированной испытательной лабораторией - впервые в отрасли производства инвентаря из нескольких металлов и пластика. Это, по нашему мнению, демонстрирует нашу неизменную приверженность качеству и философию поставщика полного цикла.

You can trust it Daxun Alloy

Высокая прочность
Устойчивость к коррозии
Термостойкость
Устойчивость к низким температурам
Защита окружающей среды
Легкий

Daxun Grade 5 Titanium Rods help your brand improve quickly

Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube.
Products/Processing Standard Grade/Size
Titanium Plate, rod, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Thickness:( 0.0197”-6”)Max Width: 12 feet,Max Length: 50 feet)
AMS-T-9046
Titanium and Titanium alloy rod, plate
Commercially pure titanium (CP)
Code designation Yield strength
minimum, ksi 1 /
CP-1 70
CP-2 55
CP-3 40
CP-4 25
Alpha titanium alloys(A)
Code designation Composition
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
Alpha-beta titanium alloys(AB)
Code designation Composition
AB-1 6A1-4V
AB-2 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
Beta titanium alloys(B)
Code designation Composition
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
Processing:
Горячая прокатка Холодная прокатка
Available Grades:
CP Класс 1 Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP Класс 2 Grade 6Al-4V ELI (Formerly Grade 23)
Grade 7 Grade 6Al-6V-2Sn (6-62)
Grade 19 Grade 8Al-1Mo-1V (8-1-1)
Grade 5 (6Al-4V) Grade 9 (3Al-2.5V)
Grade 6 (5Al-2.5Sn) CP 3 класс
Application
Химическая промышленность Desalination Of Sea Water
Petrochemical Industry Аэрокосмическая промышленность
Machining Field, Automobile Field Mobile Phone Component Field.
Titanium Grade 5 Bright Bar Titanium Grade 5 Bright Bar
Grade 5 Titanium Alloy Bright Bar
Titanium Gr 5 Bright Bar
UNS R56400 Titanium Bright Bar
WERKSTOFF NR. 3.7035 Bright Bar
ASTM B348 Gr 5 Titanium Bright Bar
Titanium Grade 5 Hex Bar Titanium Gr 5 Hex Bar
Grade 5 Titanium Hexagonal Bar
Gr 5 Titanium Alloy Hex Bar
UNS R56400 Titanium Hexagonal Bar
ASTM B348 Grade 5 Titanium Hex Bar
Titanium Alloy Grade 5 Square Bar Titanium Grade 5 Square Bar
Grade 5 Titanium Square Bars
Gr 5Titanium Alloy Square Bar
UNS R56400 Titanium Square Bar
WERKSTOFF NR. 3.7035 Square Bar
ASTM B348 Gr 5 Titanium Square Bars
Titanium Grade 5 Rectangular Bar Titanium Grade 5 Rectangular Bar
Ti. Alloy Gr2 Rectangular Bars
Gr 5 Titanium Alloy Rectangular Bar
UNS R56400 Titanium Rectangular Bars
WERKSTOFF NR. 3.7035 Rectangular Bar
ASTM B348 Gr 5 Titanium Rectangular Bar
Titanium Grade 5 Flat Bars Titanium Grade 5 Flat Bar
Gr 5Titanium Alloy Flat Bars
Titanium Gr 5Flat Bars
UNS R56400 Titanium Flat Bars
WERKSTOFF NR. 3.7035 Flat Bars
ASTM B348 Gr 5 Titanium Flat Bars
Titanium Grade 5 Polished Bar Titanium Grade 5 Polished Bar
Grade 5Titanium Polished Bars
Gr 5Titanium Alloy Polished Bar
UNS R56400 Titanium Polished Bars
WERKSTOFF NR. 3.7035 Polished Bar
ASTM B348 Gr 5 Titanium Polished Bar
Titanium Grade 5 Threaded Bar Titanium Gr 5 Threaded Bar
Grade 5Titanium Threaded Bars
Ti. Alloy Grade 5 Threaded Bar
UNS R56400 Titanium Threaded Bar
WERKSTOFF NR. 3.7035 Threaded Bar
ASTM B348 Gr 5 Titanium Threaded Bar
NOMINAL SIZE h5 h6 h7 h8 h9 H10 H11 h12
DIAMETER mm
~ to 3 +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
over 3 to 6 +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
over 6 to 10 +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
over 10 to 18 +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
over 18 to 30 +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
over 30 to 50 +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
over 50 to 80 +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
over 80 to 120 +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
over 120 to 180 +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
over 180 to 250 +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

Информация доступна для ознакомления и скачивания

Титановый стержень

Daxun is a reliable manufacturer of grade 5 titanium rods

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium bars are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the titanium rod have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

Последние проекты и продукты для горячих случаев

Ti6AL-4V Titanium Alloy Tube, Titanium Tube Grade 5/UNS R56400

Даксун has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 5 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.

ТЕХНИЧЕСКИЕ ХАРАКТЕРИСТИКИ

AMS 4928 – Bars, Forgings, and Forging Stock (Annealed)

AMS 4965 – Bars, Forgings (Solution treated and aged)

AMS 4967 – Bars, Forgings (Annealed, Heat Treatable)

HEAT TREATMENT

  • When high hardness, tensile strength, and fatigue strength are required, annealing can be performed at 1,700-1,900°F (927 – 1,038°C).
    DAXUN 6-4™ Grade 5 alloy can be heat treated in a variety of ways.
  • 1. Anneal: 1,275 -1,400°F; (691 – 760°C), ½ to 2 hours, air or furnace cool
  • 2. Stress Relief Anneal: 1,000 -1,200°F; (538 – 649°C), 1 to 8 hours, air or furnace cool
  • 3. Solution Heat Treat: 1,675 -1,750°F; (913 – 954°C), 1 hour, water quench
  • 4. Aging: 975 -1,025°F; (524 – 552°C), 4 to 8 hours – air cool

In the solution treated and aged condition, rapid quenching of small sections yields optimum properties. Larger section sizes and/or delayed quenching may result in less than optimum properties.

HARDNESS

Typical hardness in the annealed condition is Rockwell C 30-34, and about Rockwell C 35-39 in the solution and aged condition.

Forgeability/Formability

  • Ti-6Al-4V, Grade 5 alloy bar is forged at 1,750°F; (954°C) with a final forging temperature of 1,450°F; (788°C). A minimum of 35% reduction is recommended for optimum properties.
  • Ti-6Al-4V, Grade 5 alloy bar is difficult to form at room temperature, even in the annealed condition. Therefore, severe forming operations such as bending or stretching can be performed on annealed material at temperatures up to 1,200°F; (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000 – 1,200°F; (538 – 649°C).

Обрабатываемость

Ti-6Al-4V, Grade 5 alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids.

Свариваемость

Ti-6Al-4V, Grade 5 alloy rod is readily weldable in the annealed condition or in the solution and partially aged condition, with aging being accomplished during post weld heat treatment. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. Spot, seam, and flash welding may be performed without the aid of a protective atmosphere.

Special Considerations

Ti-6Al-4V, Grade 5 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics.

Size range

  • Grade 1 Titanium Bar Dimensions
  • Ø 0,7 – 30 mm (drawn, ground)
  • Ø 16 – 400 mm (hot rolled, peeled)
  • h11-h5 possible
  • Tighter or different tolerances available on request
  • Lengths up to 9,000 mm long, depending on diameter
  • For larger diameters, other bar lengths and tolerances can be agreed upon request

Availability Grade 5 Titanium rods

  • Drawing, straightening
  • Drawing, straightening, polishing
  • Drawing, grinding, polishing
  • Drawing, straightening, grinding, polishing
  • Drawing, annealing, straightening
  • Drawing, annealing, polishing
  • Drawing, annealing, grinding, polishing
  • Drawing, annealing, straightening, grinding, polishing

Processing

We produce bars according to your requirements.

Excellent surface and straightness, perfect roundness and tightest diameter tolerances (according to ISO 286-2 up to h5). Available in straightened, ground, polished conditions.

Sawing

Band saws (up to Ø510 mm)
Bench band saws (up to 6,000 x 3,000 x 400 mm)
High-performance sawing machines for precise sawing

Titanium Bar end machining

Single or double sided
Chamfer 90° (45°)
Point 60° (30°)
Flat end
Centered

Delivery form

ASTM American Society for Testing and Materials Standards
AMS American Aerospace Materials Standards
NACE American Association of Corrosion Engineers International Standards
ASME American Society of Mechanical Engineers Standards
GB Chinese National Standards
GJB Chinese National Military Standards
ISO International Standards
DIN German Standards
EN European Standards
API American Petroleum Institute Standards

Detection method

Non-destructive testing > 100% testing

Testing methods
Eddy current testing/eddy current crack testing
Defect-free surface (level 4)
Flat bottom hole diameter 0.7 mm and 0.4 mm
Blind area can be cut off according to fixed length >Test to the end of the bar
Full diameter ultrasonic testing

Our Titanium Bar Material Services

  • As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.
  • We will be happy to provide you with a consultation and explain everything you need to know about obtaining titanium bar material, including which standards require greater attention for the components to be manufactured.
  • If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.
  • Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 5 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.

Информация для заказа

Заказы на поставку должны включать количество, сорт, тип или категорию, ссылку на API5L, толщину, ширину, длину, а также любые применимые приложения или дополнительные требования, связанные с химическим составом, механическими свойствами, термообработкой, дополнительными испытаниями, процессом производства, покрытием поверхности или конечной отделкой. Свяжитесь с Daxun сейчас, мы ответим на ваше письмо как можно скорее.

Which grade of titanium is the best?

The grade of titanium alloy you need depends on the project you are working on, as each grade has different benefits.

All grades of titanium alloy are extremely strong and corrosion resistant, which means they will continue to work well in the harshest conditions.

The higher grades of titanium alloy (5-12) are alloys designed for specific benefits. For example, grade 12 titanium alloy has excellent heat resistance, making it a perfect choice for shell and tube heat exchangers, hydraulic piping, and chemical industry equipment.

Grades 1-4 are pure titanium alloys, and they are a perfect choice if you need a weldable, ductile material for piping systems and tubing. You will find lower grades used in the marine and industrial industries.

If you are starting a project and are unsure which grade of titanium alloy is best for you, contact us today; we are more than happy to help you.

How are higher grades of titanium different to the lower grades?

At DAXUN, we offer a wide range of titanium alloy grades from grade 1 to grade 12.

Grades 1-4 are pure titanium, while higher grades are alloys.

Alloy grades are popular for their high strength-to-weight ratio.

The most commonly used titanium alloy grade we find is grade 5. While still high in titanium, this grade is one of the most reliable because it can withstand temperatures up to 600°F and withstand extreme conditions.

Higher grades are favored by industries such as aerospace and marine industries for their wear and corrosion resistance.

Conversely, lower grades are primarily used for welding due to their lower strength.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

Влияет ли марка титана на стоимость?

Хотя марка титана несколько повышает стоимость, общая стоимость в основном определяется формой и видом титана, который вам нужен.

At DAXUN, we offer a wide range of titanium products, including plates, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

К сожалению, сложно назвать цену в интернете, не зная подробностей вашего проекта и того, для чего будет использоваться титан.

К счастью, наша команда экспертов всегда готова помочь и проконсультировать вас по вопросам, связанным с титаном. Отправив письмо по адресу daxunalloy@gmail.com, мы сможем ответить вам советом и точным предложением.

Обязательно укажите как можно больше информации о сорте, форме и количестве титана, который вам требуется, чтобы лучше понять ваши потребности.

Where can I learn more about grades of titanium?

The team at DAXUN is experienced, knowledgeable, and friendly. With years of experience in the industry, they know all about titanium, including its uses, benefits, and grades.

For regular updates on titanium, its uses, and its applications across industries, be sure to check out our blog. Our experts have written easy-to-follow guides that you can always refer to when you have questions.

If you’re still having trouble, feel free to contact us; we’ll be happy to help.

By sending an email to daxunalloy@gmail.com, you’ll receive a quick response. Make sure to include as much detail as possible in your question so we can recommend a suitable solution.

Как получить котировку ИЛИ понять информацию о рынке как можно скорее?

Пожалуйста, заполните форму на странице “Контакты” или позвоните нашему менеджеру по продажам по телефону “+86 13382898899”, мы свяжемся с вами в кратчайшие сроки. Наш WhatsApp работает в режиме онлайн, а электронная почта (Daxunalloy@gmail.com) будет проверена в течение 6 часов. На каждый запрос или сообщение мы ответим незамедлительно. Кроме того, каждую неделю мы делимся с нашими клиентами информацией о рынке

Могу я получить несколько образцов?

We can provide titanium rod samples for you to check the quality. Sample is free and you just pay the freight.

В какие страны вы уже экспортировали свою продукцию?

Мы экспортировали продукцию в более чем 42 страны, такие как Канада, Чили, Кувейт, Германия, Южная Корея, Саудовская Аравия, Сингапур и др.

Какова ваша MOQ?

Our MOQ is 1 ton for titanium rod.

Как долго длится доставка?

Пробные заказы могут быть доставлены в течение недели. Для обычных заказов требуется примерно две недели.

Отправьте запрос сегодня
Быстрая цитата