Duplex 2205/S31803 Stainless Steel Plate CE Certified Supplier
As China’s leading stainless steel plate supplier and exporter, Daxun provides 2205 stainless steel plates to the world.
- Grade: UNS 2205-S31803
- Features: high strength and reliability
- Производство: холоднокатаный лист, горячекатаный лист, кованый лист
- Стандарты: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Тип: холоднокатаный тонкий лист, горячекатаный толстый лист
- Поверхность: 2B, NO.1, NO.4, HL, BA, 8K и т.д.
- Длина: 2438мм3048мм6000мм может быть настроен
- Origin: TISCO, Baosteel, Posco, Tsingshan, Delong, ATI
Duplex 2205 stainless steel plate for extreme environments
Daxun offers a large stock of 2205 Duplex Stainless Steel Plates in sizes from 1/16 inch (1.0mm) to 6 inches (152.4mm) thick. The yield strength of this material is about twice as high as that of regular austenitic stainless steels, which means designers can use less material and save on costs compared to using 316L or 317L stainless steel.
2205 Duplex Stainless Steel is made up of 22% chromium, 3% molybdenum, and 5-6% nickel. It is strong and has great resistance to problems like stress corrosion cracking, crevice corrosion, pitting, erosion, and general corrosion, even in tough environments, thanks to its superior corrosion resistance. This type of stainless steel is popular because it combines the best properties of both ferritic and austenitic steels.
Grade 2205 standards have improved over the years, making it a reliable and versatile material. It has great resistance to corrosion, including in seawater, can be welded using common methods, and is highly resistant to heat. If you need more details or pricing, contact Daxun.
Технические данные
- Параметр
- Chemical Compositions
- Механические свойства
- ФИЗИЧЕСКИЕ СВОЙСТВА
- Стандарт
| Standard Industry Specifications | ASME SA 240, ASTM A 240, UNS S32205, W.NR. 1.4462,. |
| Материал | Duplex 2205 Sheet &Plate |
| Specification | ASTM A240 / ASME SA240 |
| Standard Sizes | 1000 x 2000 mm, 1220 x 2440 mm, 1500 x 3000 mm, 2000 x 2000 mm, 2000 x 4000 mm |
| Tolerances of Width and thickness | EN 10151 Duplex 2205 strip for springs |
| Ширина | 10-2500mm |
| SA-240 Duplex 2205 Plate & Sheet Thickness | 0.1mm to 100 mm Thk |
| SA 240 Type 2205 Plate & Sheet Length | 2m, 2.44m, 3m, or as required |
| SA 240 GR 2205 Plate & Sheet Finish | 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated), Cold rolled sheet (CR), Hot rolled plate (HR), No.1 finish hot rolled 2205 Duplex Plate, 2B, 1D, BA, No.4, 8K, hairline, satin, brush, mirror etc. |
| SA 240 TP 2205 Plate & Sheet Hardness | Quarter Hard, Half Hard,Spring Hard, Soft, Hard, Duplex 2205 Sheet suppliers |
| Stock available in form of | Shim Sheet, Rolls, Strip, Flats, Clad Plate, Plain Sheet, Plate, Sheet, Coils, Foils, Rolling Sheet, Rolling Plate, Flat Shim, Flat Sheet, Blank (Circle), soft annealed, sheared, annealed, tread plate,descaled, Checker Plate |
| Profiling | To provide a full profiling service in China we use numerous profiling methods including: |
| Plasma profiles | As per customer’s drawings |
| Value added services for Duplex 2205 Sheet & Plate | Plasma cutting, Waterjet cutting, Bending and mechanical processing, Laser cutting, welding, edge preparation, sawing and shearing. |
| Value added services for Duplex 2205 Coil | Slitting |
| Cut-to-length | |
| Why choose Daxun? | The third party inspection is accepted. |
| Mill Test Certificate is supplied with shipment. | |
| Free sample is available. (Yes, we could offer the sample for free charge but do not pay the cost of freight.) | |
| Minimum Nitrogen content and Ferrite Count Test | |
| Tested to ASTM A923 Method “C” or ASTM G48 Method “A”. | |
| Specialized in | ASTM A240 Type Duplex 2205 Clad plate: ASTM A240 Type Duplex 2205 Clad plate is a composite steel plate made by bonding ASTM A240 Type Duplex 2205 plate, etc. |
| ASTM A240 Type Duplex 2205 Sheet: material under 3/16″ [5.00 mm] in thickness and 24″ [600 mm] and over in width; | |
| ASTM A240 Type Duplex 2205 Strip: cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width. | |
| ASTM A240 Type Duplex 2205 Plate: material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width; | |
| Delivery time | Generally it is 7-10 days if the Duplex 2205 Sheet & Plate are in stock. or it is 15-20 days if the Duplex 2205 Plate & Sheet are not in stock, it depends to quantity. |
| Chemical Element | % Present |
| Углерод (C) | 0.0 – 0.03 |
| Хром (Cr) | 22.0–23.0 |
| Марганец (Mn) | 0.0 – 2.00 |
| Кремний (Si) | 0.0 – 1.00 |
| Фосфор (P) | 0.0 – 0.03 |
| Sulphur (S) | 0.0 – 0.02 |
| Никель (Ni) | 4.50 – 6.50 |
| Азот (N) | 0.14–0.20 |
| Молибден (Mo) | 3.00–3.50 |
| Железо (Fe) | Баланс |
| ASTM A 240 | ASTM A 240 | Typical |
| Yield Strength 0.2%, ksi | 65 min. | 74 |
| Tensile Strength, ksi | 90 min. | 105 |
| Elongation, % | 25 min. | 30 |
| Hardness RC | 32 max. | 19 |
| Temperature °F | 68 | 212 | 392 | 572 | |
| Плотность | lb/in3 | 0.278 | — | — | — |
| Modulus of Elasticity | psi x 106 | 27.6 | 26.1 | 25.4 | 24.9 |
| Linear Expansion (68°F-T) | 10-6/°F | — | 7.5 | 7.8 | 8.1 |
| Теплопроводность | Btu/h ft°F | 8.7 | 9.2 | 9.8 | 10.4 |
| Heat Capacity | Btu/lb ft°F | 0.112 | 0.119 | 0.127 | 0.134 |
| Электрическое сопротивление | Ωin x 10-6 | 33.5 | 35.4 | 37.4 | 39.4 |
| UNS S32205 | UNS S31803 | UNS S32750 |
| ASTM A240 | ASTM A240 | ASTM A240 |
| ASTM A480 | ASTM A480 | ASTM A480 |
| ASME SA240 | ASME SA240 | ASME SA240 |
| AMS 5523 | AMS 5523 | AMS 5523 |
Выберите Daxun и сделайте своих клиентов довольными.

Duplex 2205 Stainless Steel sheet and plate
Duplex SS 2205 is a very useful type of stainless steel that combines two structures: ferritic and austenitic. It has 22% chromium, 3% molybdenum, and 5-6% nickel, which makes it strong and highly resistant to different kinds of corrosion, like pitting, crevice, and stress corrosion. It can handle tough conditions and is often used in harsh environments.
Packaging details for Duplex SS 2205 include the use of durable materials to ensure the product’s integrity during shipment, specific shipping marks for easy identification, and timely delivery schedules.
2205 plate features
- Increased corrosion resistance against crevice, pitting and stress corrosion cracking
- In terms of energy absorption: high resistance to erosion and abrasion over a wide temperature range
- Unique strength, surpassing that value of other chromium-nickel stainless
- Combined properties of ferritic and austenitic steels, which by their very nature have high mechanical strength and excellent toughness
- Excellent impact strength properties
- Higher formability compared to other chromium-nickel steels
- Excellent weldability, also possible on larger cross sections
- Can be used in temperatures up to 300°C

Stainless Steel 2205 Applications
- Chemical processing, transport and storage – pressure vessels, tanks, piping, and heat exchangers
- Oil and gas exploration and processing equipment – piping, tubing, and heat exchangers
- Marine and other high chloride environments
- Effluent scrubbing systems
- Pulp and paper industry – digesters, bleaching equipment, and stock-handling systems
- Cargo tanks for ships and trucks
- Food processing equipment
- Biofuels plants
Качество, доставка, проверка
- Daxun строго контролирует качество продукции. Перед размещением заказа мы вышлем вам гарантию на продукцию, а если вам нужны образцы для тестирования, мы также можем выслать образцы бесплатно.
- During the production process, we measure the diameter, thickness, and surface of the product. Our delivery time is strictly in accordance with the contract.
- Поддержка сторонних агентств клиентов для посещения завода для проверки
- Поддержка бесплатных образцов для клиентов для тестирования
- Поддержка инспекции на месте или видеоинспекции на заводе
- Identification labels are used to ensure quality control and accurate product tracking, adhering to standard specifications or customer’s instructions.

ПРОЦЕССИНГ
Machining Duplex 2205 is a bit more challenging compared to 300 series austenitic stainless steels. It requires higher cutting forces and tends to wear tools more quickly. Here are some guidelines for machining:
A) Use powerful, rigid machines with strong, stable mounting for both tools and the workpiece.
B) Minimize vibration by keeping the tool extension as short as possible.
C) Use the appropriate cutting tools and speeds to manage wear and maintain quality.
Информация для заказа
Duplex 2205 stainless steel plate The purchase order shall include quantity, diameter, finish, length and any applicable attachments or additional requirements relating to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish or end finish, and any customer’s requirement for customized packing solutions. Bars are solution bright annealed.
2205 plate stainless steel Features
Daxun Позволяет вашему бренду быстро улучшаться
- Галерея
- Толерантность
- Delivery state
- Другие серии продукции
| Допуск для листа 2B | |||
| Размер | Рейтинг толерантности | ||
| Группа 1 | Группа 2 | Группа 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Допуски для горячекатаного листа № 1 | |||
| Размер | Рейтинг толерантности | ||
| Группа 1 | Группа 2 | Группа 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Выбор государства доставки | Состояние поверхности |
| Холодная прокатка | 2B |
| 2D | |
| BA | |
| Линия роста волос | |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Примечание: | |
| 1. Если вам требуется другое состояние доставки, чем перечисленные выше, пожалуйста, подтвердите с нами. | |
| 2. В случае запроса или заказа, пожалуйста, сообщите нам о любых дополнительных требованиях, не указанных здесь. | |
| Состояние доставки | |
| Выбор государства доставки | Состояние поверхности |
| Горячекатаный | No.1 |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Маринованные | |
| Примечание: | |
| 1. Если вам требуется другое состояние доставки, чем перечисленные выше, пожалуйста, подтвердите с нами. | |
| 2. В случае запроса или заказа, пожалуйста, сообщите нам о любых дополнительных требованиях, не указанных здесь. | |
| Класс | Тип | Толщина | Поверхность |
| Аустенитные | 304/304H/304L/304J1 | 0,25-150 мм | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80 мм | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0,3-80 мм | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Феррит | 430 | 0,4-3,0 мм | 2B/BA/NO.4/8K/SB/HL |
| Сверхчистый феррит | 443 | 0,4-2,0 мм | 2B |
| 436L/439/444/441 | 0,5-3,0 мм | 2B、2D | |
| 409L | 0,4-2,5 мм | 2B、2D | |
| Класс | Тип | Толщина | Оригинал |
| Жаропрочная сталь | 309S | 0,5-40 мм | CHN |
| 310S | 0,5-40 мм | CHN | |
| Дуплексная сталь | 2101 | 1,5-50 мм | CHN |
| 2304 | 3.0-50 мм | CHN | |
| 2205 | 0,5-60 мм | CHN | |
| 2507 | 1.0-60 мм | ПОТ / ИСПАНИЯ / КИТАЙ | |
| Супер аустенитная сталь | N08904 | 0,6-50 мм | ПОТ / ИСПАНИЯ / КИТАЙ |
| S31254 | 0,5-50 мм | ПОТ / ИСПАНИЯ / КИТАЙ | |
| N08926 | 0,5-50 мм | ПОТ / ИСПАНИЯ / КИТАЙ | |
| N08367 | 0,5-50 мм | ПОТ / ИСПАНИЯ / КИТАЙ | |
| Сплав на основе никеля | N08031 | 1.0-50 мм | США / JPN / GER |
| N08810/N08800 | 0,8-50 мм | США / JPN / CHN | |
| N08028 | 1,0-20 мм | США / ГЕРМАНИЯ / ЯПОНИЯ | |
| N08020 | 1,0-20 мм | США / ГЕРМАНИЯ / ЯПОНИЯ | |
| N08825 | 0,8-40 мм | США / ГЕРМАНИЯ / ПОТ / ЯПОНИЯ / КИТАЙ | |
| N10276 | 0,5-50 мм | США / ГЕРМАНИЯ / ЯПОНИЯ | |
| N06022 | 1.0-50 мм | США / ГЕРМАНИЯ / ЯПОНИЯ | |
| N06625 | 0,8-20 мм | США / ГЕР / ЧН | |
| N04400 | 1,0-20 мм | США / ГЕРМАНИЯ / ЯПОНИЯ | |
| N06600 | 1.0-50 мм | США / ГЕРМАНИЯ / ЯПОНИЯ / КИТАЙ | |
| N02201 | 0,5-20 мм | США / ЯПОНИЯ | |
| Титан | TA1/Gr1 | 0,5-50 мм | JPN / CHN |
| TA2/Gr2 | 0,5-50 мм | JPN / CHN | |
| Сварочный материал | ERNiCrMo-13 | 1.2、2.4 мм | GER |
| ERNiCrMo-3 | 2,4 мм | GER | |
| ERNiCrMo-4 | 2,4 мм | США |
The surface and shape of 2205 stainless steel plate (7)
Информация доступна для ознакомления и скачивания
Daxun является надежным производителем листов из нержавеющей стали
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also have strict quality control to ensure that the stainless steel plates have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
To maintain product quality during transit, we use anti-rust paper as a packaging material to prevent rust and damage.
Последние проекты и продукты для горячих случаев
Сопутствующие товары (13)
Duplex 2205 stainless steel is designed to offer great benefits for many industries and uses. Some key benefits of 2205 stainless steel are:
- High strength, allowing it to handle heavy loads
- Good resistance to fatigue, meaning it can endure repeated use without breaking
- Excellent resistance to corrosion, which helps it last longer
- Protection against issues like cracking, crevice corrosion, pitting, and general corrosion
Duplex 2205 is a type of stainless steel that is resistant to corrosion, making it great for use in very harsh environments. Some important properties of Duplex SS 2205 are:
- Grade 2205 Annealed
- Brinell Hardness: Maximum of 31 HRC
- Tensile Strength: At least 95 KSI
- Yield Strength: At least 65 KSI
- Elongation (in 2 inches): At least 25%
- Density: 0.283 lb/in³
Typical Uses
Duplex 2205 stainless steel is perfect for high-pressure and highly corrosive environments that need more protection than regular materials. Some common uses are:
- Chemical processing facilities
- Теплообменники
- Oil and gas processing equipment
- Pulp and paper mills
- Cargo tanks
- Food processing equipment
- Biofuel plants
- Marine environments
Our stainless steel sheets come in different finishes, like brushed, 2B smooth, and 8K mirror.
The front side of each sheet is covered with a protective film that can be peeled off after the sheet is made or installed. This film helps prevent scratches or marks. The back side of the sheet is unfinished.
2205 Grade Stainless Steel Sheet is the most commonly used type. It is easy to weld, shape, and has good resistance to corrosion.
We can provide stainless steel sheets in any size you need. To meet your needs, our sheets come in three finishes and a variety of sizes. We also offer free unlimited cutting to give you the exact size you want.
We can supply sheets between 0.3 and 30 mm in thickness, and sizes ranging from 50 x 50 mm to 2500 x 1250 mm. Our advanced cutting machine lets us cut precisely to your specifications without extra cost.
Easy Ordering
Ordering stainless steel sheets is simple. You can follow the instructions on our website to place an order online, or you can call us at +86 13382898899 or email daxunhejin@gmail.com for help. Our team is ready to assist with any questions.
We offer fast delivery, with typical delivery times of just one to two days.
Мы можем предоставить вам образцы листов из нержавеющей стали для проверки качества. Образец бесплатен, и вы просто оплачиваете перевозку.
Мы экспортировали продукцию в более чем 42 страны, такие как Канада, Чили, Кувейт, Германия, Южная Корея, Саудовская Аравия, Сингапур и др.
Наш MOQ составляет 1 тонну для листов из нержавеющей стали.
Пробные заказы могут быть доставлены в течение недели. Для обычных заказов требуется примерно две недели.