x
Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat

Daxun is a professional supplier of duplex 2205 stainless steel coils

Sebagai pemasok dan eksportir kumparan baja tahan karat terkemuka di Tiongkok, Daxun memasok kumparan baja tahan karat ke seluruh dunia.
  • Coil grade: S32205-S31803
  • High resistance to stress corrosion cracking, fatigue, and erosion
  • Higher heat conductivity and lower thermal expansion compared to austenitic steels
  • Outstanding and uniform resistance to pitting and crevice corrosion
  • Good sulfide stress corrosion cracking resistance
  • Useful up to 600°F

Global leader in stainless coil sheet fabrication services

Daxun manufactures stainless steel coils Alloy 2205 in a range of forms and sizes, and our Alloy 2205, like all of our products, complies with a number of industry standards set by organizations like as ASTM, ASME, ISO, UNS, and EN. Type 2205 is a duplex (austenitic/ferritic) stainless steel with better performance and corrosion resistance than 304 and 316 stainless steels. The alloy’s dispersed austenitic/ferritic microstructure, along with alloying additives, offers resistance to stress corrosion cracking, pitting, and chlorine-induced crevice corrosion. Alloy 2205 has acceptable oxidation resistance up to 980°C, but it is only appropriate for certain applications because the material becomes brittle when subjected to temperatures ranging from 300°C to 1000°C for extended durations. Type 2205 stainless steel strip, coil, and coil can be used in a wide range of applications.

Dah Hsun is an ISO 9001:2008 certified firm that is a major supplier and exporter of ASTM A240 Stainless Steel Coils. Stainless steel coils can be cut to your requirements and include a full set of mill test results. Custom lengths and widths are available up to 2000mm. Exporting is our specialty! We can obtain several hard-to-find grades and/or non-standard sizes to satisfy our customers’ specific needs. We have vast experience processing steel coil goods and can divide all stainless steel coils to the desired sizes. Introducing our extensive line of Dah Hsun Stainless Steel goods – the pinnacle of dependability, durability, and performance. We are glad to provide a wide selection of grades and varieties to fulfill the diverse needs of industrial and architectural applications.

Our stainless steel coil goods, which range from the Austenitic series to the Ferritic series and other special categories, are well-known for their high performance and extensive requirements. The austenitic series includes 304/304L/304J1, 321 and 316/316L/317L/316Ti/310/309, which can fulfill varied thickness requirements and give a variety of surface treatments, including 2B, BA, NO.4, 8K, SB, HL, NO.1, and so on.

Our ferrite line, which includes 430, ultra-pure ferrite 443, and 436L/439/444/441, caters to customers looking for unique qualities and applications. These materials can accommodate thicknesses ranging from 0.4mm to 3.0mm and offer a variety of surface treatment options such as 2B, BA, NO.4, 8K, SB, HL, and so on.

By selecting our stainless steel coils, you are investing in a material that ensures long service life, great reliability, and exceptional performance. Don’t compromise on quality; choose our stainless steel solutions and see the impact they can make in your project. Contact Daxun today for additional information or to place an order for the stainless steel coil specs and quantities that you require.

Baca Lebih Lanjut

Data

2205/S32205 Stainless Steel Coil Specification ASTM A240 / ASME SA240
2205/S32205 Stainless Steel Coil Manufacturing Process Hot Rolled (HR) / Cold Rolled (CR)
2205/S32205 Stainless Steel Coil Grades 201 / 304 / 304L/ 2205/S32205 / 309S / 420 / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L etc.
UNS No. –  UNS S2205/S32205, UNS S31008, UNS S31600, UNS S31603, UNS S31603, UNS S31600, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904
EN No.  1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539
2205/S32205 Stainless Steel Coil Thickness 0.6 MM TO 16 MM THICKNESS
2205/S32205 Stainless Steel Coil Width 1250 MM / 1500 MM / 2000 MM / 04 Feet / 05 Feet and Custom Cut Width as Per Requirement
2205/S32205 Stainless Steel Coil Length 2400 MM / 2420 MM / 6000 MM / 08 Feet / 10 Feet / Coil Cut and Custom Cut Length as Per Requirement
2205/S32205 Stainless Steel Coil Surface Finish 2B, 2D, BA, MATT, MATT PVC, No.4, No.5, SB, HR, No.8, Mirror, Hairline, Brush, Textured, Oil base wet Polished, Both sides Polished available.
2205/S32205 Stainless Steel Coil Coating PVC coating Normal / Laser, Film: 100 micrometer, Color: black/white.
2205/S32205 Stainless Steel Coil Other Testing NACE MR0175, Ultrasoung TEST, IGC TEST, Intergranular Corrrosion Test as per ASTM A262 Practice E, Charpy Impact Test, Macro, Grain Size, Hardness, etc.
2205/S32205 Stainless Steel CoilValue Added Services Gas Cutting / CNC Plasma Cutting / Profiling / Rolling / Bending / Sheet Metal Fabrication / Drill / Punch / Machining / Sand Blasting / Shot Blasting / Heat Treatment
2205/S32205 Stainless Steel Coil Packaging Loose / Carrate / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps
2205/S32205 Stainless Steel Coil Shipment & Transportation By Road – Truck / Train Partial Load, Full Load, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes
2205/S32205 Stainless Steel Coil Material Test Certificate Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of Indian Standards BIS Approved ETC
Produsen POSCO, Aperam, Jindal Stainless, DKC Korea, Thyssenkrup, Baosteel, TISCO, Arcelor Mittal, VDM, Nippon Metal, Outokumpu, Qingshan, Delong.
Pelabuhan Pengiriman Pelabuhan Shanghai / Ningbo / Tianjin / Qindao
2205/S32205S31803 化学成分 ASTM A240:
C Mn P S Si Cr Ni Mo N Fe
MIN – – – – – 22 4.5 3 0.14 BAL
MAX 0.03 2 0.03 0.02 1 23 6.5 3.5 0.2 –
Typical Mechanical Properties
Kondisi Tensile Strength Min (UTS) 0.2% YS Min Elongation% in 2” Min (50.8 mm) Hardness Rockwell
Anil 120-150 ksi (825-1035 MPa) 95-125 ksi (655-860 MPa) 25% 30 HRC
Sifat Fisik
At 70°F  At 20°C
Kepadatan 0.284 lb./in³ 7.86 g/cm³
Modulus of Elasticity (E) 29.0 x 10³ksi 200 GPa
Coefficient of Expansion 11.1 x 10⁻⁶microinches/in.-°F(70-2000°F) 14.0 μm/m-°C (0-300°C)
Tahanan Listrik 33.5 μ ohm.in  85.1 μ ohm.cm
Konduktivitas Termal 104 Btu-in./ft.²hr.-°F 15.0 W/m-K
Kelas CHINA UNS Old British Euronorm Swedish SS Japanese JIS
No BS En No Nama
2205 022Cr23Ni5Mo3N S31803 / S32205 318S13 – 1.4462 X2CrNiMoN22-5-3 2377 SUS 329J3L
•  Tisco Stainless Steel 2205 coil •  2205 Stainless Steel B. Q. Profile coil
•  SS 2205 Perforated coil •  Best selling 4’x8′ mirror finished ss 2205 coil
•  Stainless Steel 2205 UNS S31635 coil •  Decorative hairline inox cold rolled ss 2205 coil
•  A 240 Chequered 2205 coil •  Hair Line Finish SS 2205 coil
•  Aperam Stainless Steel 2205 coil •  Laser cutting ss 2205 coil
•  Stainless Steel 2205 coil •  Tisco Supplier 3mm Thickness Stainless Steel 2205 coil
•  A 240 2205 coil •  Decorative Stainless Steel 2205 coil
•  SS 2205 Embossed coil •  Scotch Brite SS 2205 coil
•  Outokumpu SS 2205 coil •  Baosteel Stainless Steel 2205 coil
•  SA 240 2205 stainless steel coil •  Stainless Steel Cladding 2205 coil
• Bright Hammered Pattern Decorative SS 2205 coil •  Black SS 2205 coil 4mm Thick
• Stainless Steel 2205 coil •  Bright-pickled Stainless Steel 2205 coil
•  SS DIN 1.4571 coil •  Cold rolled, heat treated 2205 coil
•  ThyssenKrupp Stainless Steel 2205 coil •  3mm Cold Rolled AISI SS 2205 coil
•  ASTM A240 Stainless Steel 2205 coil •  Mill Supply SS 2205 coil
•  Surface Polishing SS 2205 coil •  Grade Prime SS 2205 coil
•  2205 Stainless Steel HR coil •  Carpenter Custom 450 Stainless Steel 2205 coil
• 2205 Stainless Steel Chequered coil •  Cut to Size Stainless Steel 2205 coil
• 2205 Stainless Steel Golden Laser Pattern coil •  Non Magnetic Polishing Stainless Steel 2205 coil
• Super thin-Mirror surface BA ss 2205 coil •  ASME SA240 2205 coil
• Super Austenitic SS 2205 coil •  2205 Stainless Steel Blank coil
• ASTM A240 2205 coil •  2205 Stainless Steel Perforated coil
• JMSS cold rolled ss 2205 coil •  Embossed ss 2205 coil
• Cold Rolled No.1 Finish SS 2205 coil •  Cheap cold rolled ss 2205 coil with best price
• SEW 400 Stainless Steel 2205 coil •  Brush finish ss 2205 coil price list
• Hot Rolled Stainless Steel 2205 coil • SS URANUS B6 2205 coil
• Sales Promotion SS 2205 coil •  2B SUS SS 2205 coil
•  Cr Stainless Steel 2205 coil •  Food Grade Stainless Steel 2205 coil
•  SS 2205 Mill Test Certificate coil •  No. 4 PVC Coated SS 2205 coil
•  ASTM A240 2205 coil •  SS 2205 coil Blasted Tin-Gold Rose
•  Cold rolled, bright annealed 2205 coil •  2mm ASTM SS 2205 coil
•  Ground Stainless Steel 2205 coil •  Stainless Steel Corrugated 2205 coil
•  Hot Selling AISI SS 2205 coil •  ASTM B625 2205 coil
•  SS 2205 Rose Golden coil •  Brushed or dull polished Stainless Steel 2205 coil
• Surface coated Stainless Steel 2205 coil •  Cold rolled, heat treated, pickled 2205 coil
•  Satin finish Stainless Steel 2205 coil •  10K Mirror Finish Surface SS 2205 coil
•  AISI stainless steel 2205 armor coil •  Gold Etched SS 2205 coil
• Satin finish Stainless Steel 2205 coil •  18 Gauge SS 2205 coil
•  Mirror Finish SS 2205 coil •  Patterned Stainless Steel 2205 coil
•  SS 2205 coil Gold Brush Finish •  #4 Finish Stainless Steel 2205 coil
• 2205 Stainless Steel CR coil •  Patterned Stainless Steel 2205 coil
•  2205 Stainless Steel 2B coil •  Passenger Elevator Cabin SS 2205 coil

Pilih Daxun dan buat pelanggan Anda puas.

Hubungi Daxun sekarang

Quick response 2205 Stainless Steel coil

Kami menyediakan pengiriman produk baja tahan karat yang tepat waktu dan cepat untuk pelanggan dengan kebutuhan mendesak. Di balik kecepatan tersebut adalah dukungan sistem dari aliran informasi hingga logistik dan aliran modal. Misalnya, dalam hal aliran informasi, data pesanan Daxun didorong ke sistem logistik secara real time, dan data tersebut terhubung dengan mulus; dalam hal logistik, pusat pemrosesan dekat dengan jalan raya dan sungai dan laut, dengan penjadwalan yang wajar, respons yang cepat, hubungan penyimpanan dan transportasi, dan pemuatan yang efisien, memastikan bahwa tugas diselesaikan sesuai jadwal. bahan baja tahan karat Daxun memiliki kualitas yang dapat diandalkan, dan varietas, spesifikasi, serta bobot pengirimannya sangat sesuai dengan standar.

Hubungi Daxun sekarang

Keunggulan Daxun

Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel achieves full traceability of each steel coi from the ERP system, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strict monitoring during sales, and provides worry-free service guarantees after sales.

Hubungi Daxun sekarang

Stainless steel coil packaging

Daxun Alloy memastikan kualitas kemasan terbaik karena memainkan peran penting dalam pengiriman internasional di mana barang melewati berbagai saluran untuk mencapai tujuan akhir, jadi kami memberikan perhatian khusus pada pengemasan. Kami mengemas barang-barang kami dengan berbagai cara tergantung pada produknya. Kami mengemas produk kami dengan berbagai cara seperti:
- Kotak dan peti
- Kecilkan bungkus
- Palet kayu
- Kotak kayu

Hubungi Daxun sekarang

Kualitas, pengiriman, inspeksi

  • Daxun juga melakukan beberapa tes jaminan kualitas. Pengujian ini meliputi uji perataan, uji lubang dan ketahanan, uji mekanis, uji kekerasan, identifikasi positif material, uji ekspansi, dll. Semua pengujian ini memastikan bahwa bahan tersebut cocok untuk aplikasi yang dibutuhkan.
  • Selama proses produksi, kami mengukur diameter, ketebalan, dan permukaan produk. Waktu pengiriman standar kami adalah 7-15 hari, kecuali untuk beberapa produk ukuran khusus, waktu pengiriman kami akan bertambah menjadi 20 hari.
    Waktu pengiriman kami benar-benar sesuai dengan kontrak.
  • Mendukung agen pihak ketiga pelanggan untuk pergi ke pabrik untuk pemeriksaan
  • Mendukung sampel gratis kepada pelanggan untuk pengujian
  • Mendukung inspeksi pabrik di tempat atau video
Hubungi Daxun sekarang

Informasi Pemesanan

Pesanan pembelian harus mencakup jumlah, kelas, jenis atau kategori, referensi API5L, ketebalan, lebar, panjang, dan lampiran yang berlaku atau persyaratan tambahan yang terkait dengan komposisi kimia, sifat mekanik, perlakuan panas, pengujian tambahan, proses pembuatan, pelapisan permukaan, atau hasil akhir. Hubungi Daxun sekarang, kami akan membalas email Anda sesegera mungkin.

Hubungi Daxun sekarang

Dukungan Teknis

Jika Anda memerlukan bantuan teknis tambahan, ahli metalurgi dan staf kami yang berpengetahuan luas akan dengan senang hati membantu. Selain itu, Daxun memiliki laboratorium pengujian bersertifikat-yang pertama dalam industri inventaris multi-logam dan plastik. Ini, menurut pendapat kami, menunjukkan dedikasi kami yang tak tergoyahkan terhadap kualitas dan filosofi kami sebagai pemasok layanan penuh.

2205 Stainless Steel Coil Features

Kekuatan tinggi
Ketahanan korosi
Tahan panas
Tahan suhu rendah
Perlindungan lingkungan
Kinerja pengelasan

Daxun Alloy Biarkan merek Anda meningkat dengan cepat

Kelas Jenis Ketebalan Permukaan
Austenitik 304/304H/304L/304J1 0,25-150mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0,4-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0,3-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
Ferit 430 0.4-3.0mm 2B/BA/NO.4/8K/SB/HL
Ferit Ultra Murni 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B 、 2D
409L 0,4-2,5 mm 2B 、 2D
Baja Austenitik Super N08904 0,6-50mm SWE / JPN / CHN
S31254 0,5-50mm SWE / JPN / CHN
N08926 0,5-50mm SWE / JPN / CHN
N08367 0,5-50mm SWE / JPN / CHN
Paduan Dasar Nikel N08031 1.0-50mm AS / JPN / GER
N08810 / N08800 0,8-50mm AS / JPN / CHN
N08028 1.0-20mm AS / JERMAN / JPN
N08020 1.0-20mm AS / JERMAN / JPN
N08825 0,8-40mm US / GER / SWE / JPN / CHN
N10276 0,5-50mm AS / JERMAN / JPN
N06022 1.0-50mm AS / JERMAN / JPN
N06625 0,8-20mm AS / GER / CHN
N04400 1.0-20mm AS / JERMAN / JPN
N06600 1.0-50mm US / GER / JPN / CHN
N02201 0,5-20mm AS / JPN
Titanium TA1/Gr1 0,5-50mm JPN / CHN
TA2/Gr2 0,5-50mm JPN / CHN
Bahan Pengelasan ERNiCrMo-13 1.2 、 2.4mm GER
ERNiCrMo-3 2.4mm GER
ERNiCrMo-4 2.4mm AS
Entitas Anak Peralatan Utama Jumlah Kapasitas Tahunan
Perusahaan baja tahan karat Daxun (JiangSu) Mesin Penggorok 1 Lembar Dekoratif: 60.000 ton
Mesin Pemotong 1
No.4 Dan Mesin Pemoles Lembar Ke Lembar Rambut 1
No.4 / Mesin Pemoles Coil To Coil 1
8K / Super Mirror Sheet To Sheet Polishing Machines 2
8K / Super Mirror Coil Untuk Mesin Poles Coil 3
Mesin Pelapis Warna PVD 4
Mesin Pelapis Kimia Cair 2
Mesin Cetak Anti Jari 2
Mesin Pilih dan Tempatkan Otomatis 16
coil Washing Machine 1
Perusahaan baja tahan karat Daxun (Shanghai) Mesin Penggulung Dingin 3 Kumparan 2B: 100.000 ton
Garis Anil & Pengawetan 2 Lembaran Dekoratif; 30.000 ton
Mesin Penggorok 1
Mesin Potong Memanjang 1
Mesin Poles No.4 / HL (Lembar ke Lembar) 3
Mesin Pemoles 8K (Lembar ke Lembar) 13
Mesin Pelapis Titanium PVD 4
Mesin Pelapis Kimia Cair 1
Perusahaan baja tahan karat Daxun (Shandong) Mesin Penggulung Dingin 3 Kumparan 2B & BA: 220.000 ton
Jalur Anil & Pengawetan (2B & BA) 2 Lembar Dekoratif: 60.000 ton
Pengungkit Ketegangan & Skin Pass 1
Mesin Penggorok 1
Mesin Potong Memanjang 1
Mesin Poles No.4 / HL (Lembar ke Lembar) 1
Mesin Pemoles 8K (Lembar ke Lembar) 11
Mesin Pelapis Tembaga Otomatis 1
Mesin Cetak Digital 1
Mesin Pelapis Titanium PVD 3
Mesin Pelapis Kimia Cair 1
Mesin Anti Jari 1
Perusahaan baja tahan karat Daxun (Sichuan) Mesin Penggorok 1 Kumparan 2B & BA: 180.000 ton
Mesin Pemotong 1 Lembar Dekoratif: 50.000 ton
No.4 Dan Mesin Pemoles Lembar Ke Lembar Rambut 1
No.4 / Mesin Pemoles Coil To Coil 1
8K / Super Mirror Sheet To Sheet Polishing Machines 1
8K / Super Mirror Coil Untuk Mesin Poles Coil 1
Mesin Pelapis Warna PVD 1
Mesin Pelapis Kimia Cair 1
Mesin Cetak Anti Jari 1

Informasi yang tersedia untuk referensi dan diunduh

Daxun adalah produsen kumparan baja tahan karat yang dapat dipercaya

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel coils have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

Proyek dan produk hot case terbaru

2205 kumparan baja tahan karat
koil baja tahan karat tanpa sambungan
Kumparan baja tahan karat
Furnitur Dapur dan Kamar Mandi
2205 kumparan baja tahan karat
Kumparan Baja Tahan Karat yang Dipoles
Kumparan baja tahan karat BA
Dekorasi mobil
Kumparan baja tahan karat
Pintu dan Jendela
Kumparan baja tahan karat
Energi Kimia
2205 stainless coil
Tenaga nuklir
Kumparan presisi baja tahan karat
Mesin Presisi
Stainless steel coil 2205
Wadah Kimia
Pengantar Rinci

Pemasok kumparan baja tahan karat terkemuka di Cina

Daxun telah terlibat dalam bisnis internasional selama lebih dari sepuluh tahun. Pada tahun 2023, pendapatan ekspornya melebihi US $ $100 juta, dan volume ekspornya berada di antara produsen baja nirkarat teratas di Tiongkok. Daxun terus meningkatkan keterampilan layanannya. Untuk melayani pasar global, kami telah mendirikan tiga fasilitas layanan ekspor di China dan bekerja sama dengan perusahaan teknik, pabrik baja, dan perusahaan perdagangan internasional. Daxun menyediakan layanan rantai baja tahan karat dan telah menjalin hubungan kerja sama jangka panjang dengan puluhan pabrik baja terkenal di seluruh dunia. Persediaannya mencakup 50.000 ton gulungan baja tahan karat konvensional dan 20.000 ton baja dupleks, paduan berbasis nikel, baja tahan panas, dan logam lainnya. Bahan baja tahan karat Daxun memiliki kualitas yang konsisten. Jenis, spesifikasi, dan bobot pengiriman secara ketat mematuhi standar.


GENERAL PROPERTIES

Duplex 2205 is a two-phase, ferritic, austenitic stainless steel alloyed with 22% chromium, 3% molybdenum, and 5-6% nickel. It is the most commonly used duplex stainless steel grade, with a yield strength that is double that of normal austenitic grades. It also has exceptional fatigue strength and excellent resistance to stress corrosion cracking, crevice, pitting, erosion, and general corrosion in harsh conditions.

APPLICATIONS

  • Pemrosesan, pengangkutan, dan penyimpanan bahan kimia - bejana bertekanan, tangki, perpipaan, dan penukar panas
  • Peralatan eksplorasi dan pemrosesan minyak dan gas - perpipaan, pipa, dan penukar panas
  • Lingkungan laut dan lingkungan klorida tinggi lainnya
  • Sistem penggosokan limbah cair
  • Industri pulp dan kertas - digester, peralatan pemutihan, dan sistem penanganan stok
  • Tangki kargo untuk kapal dan truk
  • Peralatan pengolahan makanan
  • Pabrik bahan bakar nabati

STANDARDS

  • ASTM/ASME: A240 UNS S32205/S31803
  • EURONORM: 1.4462 X2CrNiMoN 22.5.3
  • AFNOR: Z3 CrNi 22.05 AZ
  • DIN: W.Nr 1.4462

CORROSION RESISTANCE

  • Due to its high chromium, molybdenum, and nitrogen content, Duplex 2205 demonstrates superior corrosion resistant properties to 316 and 316L in most environments
  • Chromium, molybdenum, and nitrogen content also provide high resistance to pitting and crevice corrosion, even in oxidizing and acidic solutions
  • Resistant to chloride stress corrosion cracking and temperatures of up to about 302°F (150°C)
  • The presence of ferrite provides for good performance of Duplex 2205 in caustic environments

HEAT RESISTANCE

  • Similar to other duplex stainless steels, Duplex 2205 has good oxidation resistance at high temperatures
  • Subject to embrittlement when exposed to temperatures above 572°F (300°C) even when exposed for short periods of time; Duplex 2205 is therefore not recommended for use above 572°F (300°C)

WELDING CHARACTERISTICS

  • Possesses good weldability
  • Should not generally be welded without filler metal as this may result in excessive ferrite

HEAT TREATMENT

  • Annealing temperature range is 1868 to 2012°F (1020 to 1100°C)
  • Cannot be hardened by heat treatment – but Duplex 2205 does work-harden
  • Special consideration is needed to compensate for a higher coefficient of thermal expansion to avoid warping and distortion

PROCESSING – HOT FORMING

  • Most Duplex 2205 producers recommend a maximum hot forming temperature between 2010 and 2100°F (1100 to 1150°C). If the shape of the work piece is not compact, the edges may be significantly cooler than the bulk, and there is risk of cracking in the cooler regions.

PROCESSING – COLD FORMING

  • Duplex 2205 has shown good formability in a variety of fabrications. The high strength of Duplex 2205 can pose problems. Even when the equipment has sufficient power, allowance must be made for higher spring-back caused by the grade’s high strength.

MACHINABILITY

Duplex 2205 is slightly more difficult to process than the 300 series austenitic stainless steels. Higher cutting forces are required, which results in faster tool wear. Some machining guidelines are as follows: A) Use powerful, rigid machines with extremely strong rigid mounting of tools and work piece, B) Minimise vibration by keeping the tool extension as short as possible, C) Use a nose radius on the tool, no longer than necessary, for carbides with a sharp edge while still providing adequate strength, and D) Design machining sequences to always provide for a depth of cut below the work hardened layer resulting from previous passes.

Features of 2205 stainless steel coils

  • Type 2205 is a duplex (austenitic/ferritic) stainless steel alloyed with chromium, molybdenum, and nitrogen, which improves performance and corrosion resistance when compared to 304 and 316 stainless steel. The alloy’s dispersed austenite/ferrite microstructure, together with the alloying additives, offers resistance to stress corrosion cracking, pitting, and chlorine-induced crevice corrosion. Alloy 2205 has acceptable oxidation resistance up to 980°C, but only for specified applications because the material can become brittle when subjected to temperatures ranging from 300°C to 1000°C over extended durations. Type 2205 stainless steel strip, coil, and sheet can be used for a wide range of applications.

Apa saja permukaan kumparan baja tahan karat yang umum digunakan?

Permukaan akhir dari 201 kumparan baja tahan karat dapat bervariasi tergantung pada metode pemrosesan penggulungan dingin yang digunakan dan perawatan permukaan yang digunakan setelah penggulungan. Perawatan permukaan untuk kumparan baja tahan karat meliputi NO.1, 2B, 4, HL, 6, 8, BA, TR keras, penggulungan berat 2H cerah, dipoles cerah, dan perawatan permukaan lainnya:

  • NO.1: Permukaan yang diperoleh setelah pengerolan panas, perlakuan panas dan pengawetan strip baja tahan karat. Ini digunakan untuk menghilangkan kerak oksida hitam yang terbentuk oleh pengawetan atau proses serupa selama pengerolan panas dan perlakuan panas. Ini menempati urutan pertama dalam perawatan permukaan. Permukaan No. 1 berwarna putih keperakan dan matte. Umumnya digunakan dalam industri tahan panas dan tahan korosi yang tidak membutuhkan kilap permukaan yang tinggi, seperti industri alkohol, industri kimia, wadah besar, dll.
  • 2B: Tidak seperti permukaan 2D, permukaan 2B dihaluskan oleh roller ringan, dan permukaannya lebih cerah. Nilai Ra kekasaran permukaan yang diukur oleh peralatan berkisar antara 0,1 hingga 0,5μm, yang merupakan nilai tipikal untuk sebagian besar jenis pemrosesan. Permukaan strip baja tahan karat ini memiliki kemampuan beradaptasi terkuat dan cocok untuk industri seperti kimia, pembuatan kertas, perminyakan, medis, dan berbagai bidang seperti membangun dinding tirai.
  • Permukaan keras TR: Baja tahan karat TR juga disebut baja keras. Kelas baja yang khas meliputi 304 dan 301, yang digunakan untuk barang-barang yang membutuhkan kekuatan dan kekerasan tinggi, seperti kendaraan kereta api, ban berjalan, pegas, dan mesin cuci. Idenya adalah menggunakan karakteristik pengerasan kerja baja tahan karat austenitik untuk meningkatkan kekuatan dan kekerasan gulungan baja melalui metode pengerjaan dingin seperti pengerolan. Untuk mengganti kerataan lembut permukaan dasar 2B, bahan keras digulung dengan lembut beberapa persen hingga puluhan persen, dan tidak ada anil yang dilakukan setelah penggulungan. Oleh karena itu, permukaan keras TR dari bahan keras adalah permukaan yang digulung setelah proses penggulungan dingin.
  • Penggulungan ulang 2H yang cerah: Setelah operasi penggulungan, strip baja tahan karat akan dianil dengan cerah. Garis anil kontinu dapat digunakan untuk mendinginkan strip dengan cepat. Strip baja tahan karat bergerak di sepanjang garis dengan kecepatan 60-80m / menit. Setelah proses ini, permukaan akhir akan digulung kembali menjadi cerah 2H.
  • No. 4: Permukaan No. 4 memiliki efek pemolesan yang baik dan lebih cerah dari No. 3. Hal ini juga dapat diperoleh dengan memoles kumparan baja tahan karat canai dingin dengan permukaan 2D atau 2B, lalu memoles permukaan yang diproses dengan sabuk pengamplasan dengan ukuran partikel 150-180#. Alat ini mengukur kekasaran permukaan (Ra) antara 0,2 dan 1,5μm. Permukaan No. 4 banyak digunakan di restoran dan peralatan memasak, peralatan medis, dekorasi arsitektur, wadah dan aplikasi lainnya.
  • HL: Permukaan HL sering disebut sebagai hasil akhir garis rambut. Standar JIS Jepang menetapkan permukaan abrasif garis rambut kontinu yang diperoleh dengan memoles menggunakan sabuk abrasif 150-240#. Pembatasan di bawah standar GB3280 Cina tidak jelas. Permukaan akhir HL biasanya digunakan untuk dekorasi arsitektur, seperti lift, eskalator, dan dinding eksterior.
  • No. 6: Permukaan No. 6 dipoles lebih lanjut berdasarkan No. 4 dengan sikat Tampico atau bahan abrasif grit W63 yang ditentukan dalam standar GB2477. Permukaannya memiliki kilau logam yang bagus, kelembutan, pantulan yang lemah, dan tidak ada pencitraan. Karena kinerjanya yang bagus, ini sangat cocok untuk dinding gorden, dekorasi rumbai, dan perlengkapan memasak.
  • BA: BA adalah permukaan yang diberi perlakuan panas cerah setelah penggulungan dingin. Perlakuan panas terang adalah anil dalam atmosfer pelindung untuk memastikan bahwa permukaan tidak teroksidasi dan mempertahankan kilau permukaan canai dingin, dan kemudian dipoles dengan roller halus presisi tinggi untuk meningkatkan kecerahan permukaan. Instrumen mengevaluasi kekasaran permukaan menjadi 0,05-0,1μm, yang menunjukkan bahwa permukaannya dekat dengan permukaan cermin. Permukaan BA dapat digunakan dalam berbagai aplikasi, termasuk peralatan makanan, peralatan rumah tangga, peralatan medis, suku cadang otomotif, dan dekorasi.
  • No. 8: Permukaan cermin, reflektifitas maksimum, tidak ada partikel abrasif. Industri pengolahan dalam baja tahan karat juga mengacu pada papan 8K. Bahan BA sering digunakan sebagai bahan baku untuk pemrosesan cermin. Itu hanya perlu dipoles. Permukaannya indah setelah pemrosesan cermin dan sering digunakan pada pintu masuk gedung dan dekorasi interior.

Apa kemasan laut standar dari 201 kumparan baja tahan karat?

  • Kemasan laut standar ekspor:
    Gulungan Kertas Tahan Air + Film PVC + Tali Pengikat + Pallet Kayu atau Kotak Kayu;
  • Kemasan yang disesuaikan dengan permintaan Anda (Logo atau konten lain dapat dicetak pada kemasan);
  • Kemasan khusus lainnya akan dirancang sesuai permintaan pelanggan;
    Mata ke dinding dan mata ke langit keduanya tersedia;
  • Dengan Ekspres Internasional: DHL/UPS/FEDEX/EMS dan jalur ekspres kami sendiri;
  • Melalui udara, laut atau darat;
  • Pelabuhan Pengiriman: Shanghai, Ningbo, Qingdao, Tianjin atau sebagai permintaan Anda.

Hubungi pemasok kumparan baja tahan karat Anda

  • Anda dapat dengan mudah memesan gulungan baja tahan karat dalam berbagai ukuran dan jumlah secara online.
    Atau, tim penjualan kami yang ramah akan dengan senang hati menerima pesanan Anda. Cukup hubungi +86 13382898899 atau email Daxunhejin@gmail dan kami akan menghubungi Anda sesegera mungkin.
Bagaimana cara mendapatkan penawaran atau memahami informasi pasar secepatnya?

Silakan isi formulir di halaman “Hubungi Kami”, atau hubungi manajer penjualan kami di “+86 13382898899”, kami akan menghubungi Anda sesegera mungkin. WhatsApp kami sedang online, dan email (Daxunalloy@gmail.com) akan diperiksa dalam waktu 6 jam. Setiap pertanyaan atau pesan akan segera ditanggapi. Selain itu, kami berbagi informasi pasar dengan pelanggan kami setiap minggu

Bisakah saya mendapatkan beberapa sampel?

Sampel dapat diberikan secara gratis, tetapi ongkos kirim ditanggung oleh pelanggan, dan akan dikembalikan setelah kerja sama.

Negara mana saja yang sudah Anda ekspor?

Kami telah mengekspor ke lebih dari 42 negara, seperti Kanada, Chili, Kuwait, Jerman, Korea Selatan, Arab Saudi, Singapura, dll.

Apa MOQ Anda?

MOQ kami adalah 1 ton untuk lembaran baja tahan karat.

Bagaimana Anda mengontrol kualitas?

Kami memiliki organisasi yang lengkap mulai dari pembelian bahan baku hingga pemrosesan dan pengaturan pengiriman. Di seluruh rantai, orang dokumenter iklan QC akan mencari dan memeriksanya dengan persyaratan yang tepat, inspeksi pihak ketiga disambut baik.

Berapa lama waktu pengiriman Anda?

Pesanan percobaan dapat dikirim dalam waktu satu minggu. Untuk pesanan reguler, kira-kira membutuhkan waktu dua minggu.

Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat