Daxun is a stockist and manufacturer of stainless steel angle steel
- China stainless steel angle steel supplier.
- Daxun has 10,000 tons of stainless steel angle steel in stock
- Daxun can provide angle steel surface processing services
- Type: equal angle steel and unequal angle steel
Introduction to Daxun stainless steel angle steel
| Product Parameters: Stainless Steel Angle bar | |
| Ukuran | 20×20×3;25×25×3、25×25×4;30×30×3、30×30×4、30×30×5、30×30×6;40×40×3、40×40×4、40×40×5、40×40×6;50×50×4、50×50×5、50×50×6;60×60×5、60×60×6;65×65×5、65×65×6、65×65×7、65×65×8;70×70×6、70×70×7、 |
| 70×70×8;75×75×6、75×75×7、75×75×8、75×75×9;80×80×8、80×80×9、80×80×10;100×100×8、100×100×9、100×100×10、100×100×12 *Sizes from 100×100 to 150×150 can be customized. | |
| Permukaan | Pickling 8K, NO.1, NO.4,hairline, etc |
| length | 6000mm or Customized |
| Kelas | 304 201 304L 310S 316L 321 904L 2205 2507 S32750 S32760 etc |
| Standards | ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227 |
| Fitur | Anti-corrosion (the degree is susceptible to the alloys contained), heat-resistance, good cold and hot working properties, good toughness, good comprehensive performances and wide application. |
Daxun offers stainless steel angle steel in different sizes, material grades, profiles, finishes and other specifications. We can also produce custom stainless steel angles based on your specific needs or applications.
Stainless Steel Angle Steel Grade
Each type of stainless steel angle steel has its own different usage scenarios.
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Performance of stainless steel angle steel
The chemical composition on stainless steel angle bars protects them from rust. Their corrosion resistance is enhanced by the necessary polished finish, making them ideal for architectural use.
Since stainless steel angles have a low melting point, no special tools are required. They are also durable and long-lasting materials, allowing industries to save on work and maintenance costs.
The smarter option material SS angles have far lesser drawbacks than other alloys. They provide excellent value, cost-effectiveness, and durability. SS is an easy-to-clean metal material.
Stainless steel angle material is an excellent choice for a variety of applications such as manufacturing. They are simple to use and ideal for large-scale industrial and complex uses.
Huge Stock Choiceable Material
With choiceable material from the very start comes our high quality stainless steel products.Daxun have stainless steel inventories for common grades and common sizes to ensure fast response to our customers’ demand.Mill Origin: TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc.


Common areas of stainless steel angle steel
- Stainless steel angle bars are hot-rolled and pickled, making them versatile for use in a wide range of construction and engineering projects. They are commonly used in structures like house beams, bridges, power transmission towers, and shipyards.
Can be processed to the width you need
1. Competitive price and quality from our own factory
2. Approved by ISO9001, CE, SGS every year
3. Best service with 24 hour`s reply
4. Flexible payment with T/T,L/C , paypal, etc
5. Smooth production ability
6. Quick delivery and standard exporting package
7. OEM/ODM

Technical Information
At Daxun, we choose different packaging for different stainless steel products, including: kraft paper, wooden boxes, woven bags, wooden pallets, based on the highest industry standards to ensure that the goods arrive in your hands in good condition.
All our stainless steel materials are certified by different industry standards such as ISO9001:2008, ISO14001:2014, AAA Certification, CQGC Certifications, and more. Our company also have certifications from ISO9001:2015 quality management system.
At Daxun, we have testing laboratory and equipment to ensure that our stainless steel materials are in actual weight and good quality before shipment. Our strict quality control team also performs strict and 100% inspection on all production stages.
Our support and services are not only limited from the beginning of our transactions. Even if you have received your orders, Daxun will continue to provide excellent after-sales services. We will continue providing assistance and warranty to your orders.
Application cases of stainless steel angle in different industries
Stainless steel angles are widely used in the construction field and can be used for exterior wall supports, interior decoration, roofing materials, building structures, etc. Stainless steel is corrosion-resistant and has high strength, which can meet the design requirements of different buildings.
Stainless steel has the advantages of corrosion resistance, no rust, no discoloration, easy removal of attached food, and good high and low temperature mechanical properties. Widely used in food machinery, such as sanitary systems, fluid pipe tanks, food storage tanks, heat exchangers, vacuum containers, etc.
Stainless steel has good strength, toughness and corrosion resistance and is widely used in aircraft structural parts. For example, the wing structure, fuselage supports, seats and other components are all made of stainless steel.
Stainless steel angles are also used in the manufacture and maintenance of oil refining equipment, and the brackets used in the petrochemical industry are all made of stainless steel angles.
Main application parts: wing skin, wing stringers, upper and lower edge strips of wing spar, web, fuselage stringers, seat rails, keel beam, side frames, fuselage skin, lower fuselage wall panels, Main floor stringers, etc.
Stainless steel angle steel is widely used in the shipbuilding industry. The stainless steel angle supplied by Daxun are used in the shipbuilding and petroleum industries. They have high strength, good toughness, and are resistant to seawater corrosion, fatigue, and wear.
SS316L is the primary austenitic stainless steel grade used in offshore installations, where it enhances strength at high temperatures and protects structures from severe acidic environments.There are also duplex stainless steels, which offer an excellent combination of mechanical properties and resistance to stress corrosion cracking, making them ideal for offshore applications. UNS S32205 steel is the most commonly used duplex stainless steel grade for offshore installations.
The main application of stainless steel angle steel in electricity is the support of power station equipment. The excellent corrosion resistance and high strength of stainless steel make it the preferred material for power generation components.
Mechanical Information
- Stock
- Toleransi
- Status Pengiriman
| Size Range | |||||||
| Hot-rolled equal-leg angle bar | |||||||
| Designation | Mass | Designation | Mass | Designation | Mass | Designation | Mass |
| 20x20x3 | 0.88 | 70x70x5 | 5.37 | 120x120x8 | 14.7 | 180x180x16 | 43.5 |
| 25x25x3 | 1.12 | 70x70x6 | 6.38 | 120x120x9 | 16.5 | 180x180x17 | 46 |
| 25x25x4 | 1.45 | 70x70x7 | 7.38 | 120x120x10 | 18.2 | 180x180x18 | 48.6 |
| 25x25x5 | 1.78 | 70x70x8 | 8.37 | 120x120x11 | 19.9 | 180x180x19 | 51.1 |
| 30x30x3 | 1.36 | 70x70x9 | 9.32 | 120x120x12 | 21.6 | 180x180x20 | 53.7 |
| 30x30x4 | 1.78 | 70x70x10 | 10.3 | 120x120x13 | 23.3 | 200x200x13 | 39.8 |
| 30x30x5 | 2.18 | 75x75x4 | 4.65 | 120x120x14 | 25 | 200x200x14 | 42.7 |
| 35x35x3 | 1.6 | 75x75x5 | 5.76 | 120x120x15 | 26.6 | 200x200x15 | 45.6 |
| 35x35x3.5 | 1.85 | 75x75x6 | 6.85 | 120x120x16 | 28.3 | 200x200x16 | 48.5 |
| 35x35x4 | 2.09 | 75x75x7 | 7.93 | 130x130x8 | 16 | 200x200x17 | 51.4 |
| 35x35x5 | 2.57 | 75x75x8 | 8.99 | 130x130x9 | 17.9 | 200x200x18 | 54.3 |
| 38x38x4.5 | 2.56 | 75x75x9 | 10 | 130x130x10 | 19.8 | 200x200x19 | 57.1 |
| 38x38x6 | 3.33 | 75x75x10 | 11.1 | 130x130x11 | 21.7 | 200x200x20 | 59.9 |
| 40x40x3 | 1.84 | 76x76x5 | 5.84 | 130x130x12 | 23.6 | 200x200x21 | 62.8 |
| 40x40x4 | 2.42 | 76x76x6.5 | 7.49 | 130x130x13 | 25.4 | 200x200x22 | 65.6 |
| 40x40x5 | 2.97 | 76x76x8 | 9.11 | 130x130x14 | 27.2 | 200x200x23 | 68.3 |
| 40x40x6 | 3.52 | 76x76x9.5 | 10.7 | 130x130x15 | 29 | 200x200x24 | 71.1 |
| 45x45x3 | 2.09 | 80x80x5 | 6.17 | 130x130x16 | 30.8 | 200x200x25 | 73.9 |
| 45x45x4 | 2.74 | 80x80x6 | 7.34 | 140x140x9 | 19.3 | 200x200x26 | 76.6 |
| 45x45x4.5 | 3.06 | 80x80x7 | 8.49 | 140x140x10 | 21.4 | 200x200x27 | 79.3 |
| 45x45x5 | 3.38 | 80x80x8 | 9.63 | 140x140x11 | 23.4 | 200x200x28 | 82 |
| 45x45x6 | 4 | 80x80x9 | 10.8 | 140x140x12 | 25.4 | 250x250x17 | 64.4 |
| 45x45x7 | 4.6 | 80x80x10 | 11.9 | 140x140x13 | 27.5 | 250x250x18 | 68.1 |
| 50x50x3 | 2.33 | 90x90x5 | 6.97 | 140x140x14 | 29.4 | 250x250x19 | 71.7 |
| 50x50x4 | 3.06 | 90x90x6 | 8.3 | 140x140x15 | 31.4 | 250x250x20 | 75.3 |
| 50x50x5 | 3.77 | 90x90x7 | 9.61 | 140x140x16 | 33.3 | 250x250x21 | 78.9 |
| 50x50x6 | 4.47 | 90x90x8 | 10.9 | 140x140x18 | 37.2 | 250x250x22 | 82.5 |
| 50x50x7 | 5.15 | 90x90x9 | 12.2 | 150x150x10 | 23 | 250x250x23 | 86.1 |
| 50x50x8 | 5.82 | 90x90x10 | 13.4 | 150x150x11 | 25.2 | 250x250x24 | 89.7 |
| 50x50x9 | 6.47 | 90x90x11 | 14.7 | 150x150x12 | 27.3 | 250x250x25 | 93.2 |
| 55x55x4 | 3.38 | 90x90x16 | 20.7 | 150x150x13 | 29.5 | 250x250x26 | 96.7 |
| 55x55x5 | 4.18 | 100x100x6 | 9.26 | 150x150x14 | 31.6 | 250x250x27 | 101 |
| 55x55x6 | 4.95 | 100x100x7 | 10.7 | 150x150x15 | 33.8 | 250x250x28 | 104 |
| 60x60x4 | 3.7 | 100x100x8 | 12.2 | 150x150x16 | 35.9 | 250x250x29 | 107 |
| 60x60x5 | 4.57 | 100x100x9 | 13.6 | 150x150x17 | 38 | 250x250x30 | 111 |
| 60x60x6 | 5.42 | 100x100x10 | 15 | 150x150x18 | 40.1 | 250x250x31 | 114 |
| 60x60x7 | 6.26 | 100x100x11 | 16.4 | 150x150x19 | 42.1 | 250x250x32 | 118 |
| 60x60x8 | 7.09 | 100x100x12 | 17.8 | 150x150x20 | 44.2 | 250x250x33 | 121 |
| 60x60x10 | 8.69 | 100x100x13 | 19.2 | 160x160x12 | 29.3 | 250x250x34 | 124 |
| 63x63x5 | 4.82 | 100x100x14 | 20.6 | 160x160x13 | 31.6 | 250x250x35 | 128 |
| 63x63x6 | 5.72 | 100x100x15 | 21.9 | 160x160x14 | 33.9 | 300x300x25 | 112 |
| 63x63x6.5 | 6.17 | 100x100x16 | 23.2 | 160x160x15 | 36.2 | 300x300x26 | 116 |
| 65x65x4 | 4.02 | 110x110x6 | 10.2 | 160x160x16 | 38.4 | 300x300x27 | 121 |
| 65x65x5 | 4.97 | 110x110x7 | 11.8 | 160x160x17 | 40.7 | 300x300x28 | 125 |
| 65x65x6 | 5.91 | 110x110x8 | 13.4 | 160x160x18 | 42.9 | 300x300x29 | 129 |
| 65x65x7 | 6.83 | 110x110x9 | 15 | 160x160x19 | 45.1 | 300x300x30 | 133 |
| 65x65x8 | 7.73 | 110x110x10 | 16.6 | 160x160x20 | 47.3 | 300x300x31 | 138 |
| 65x65x9 | 8.62 | 110x110x11 | 18.2 | 180x180x13 | 35.7 | 300x300x32 | 142 |
| 65x65x10 | 9.49 | 110x110x12 | 19.7 | 180x180x14 | 38.3 | 300x300x33 | 146 |
| 65x65x11 | 10.3 | 120x120x7 | 12.9 | 180x180x15 | 40.9 | ||
| Hot-rolled unequal-leg angle bar | |||||||
| Designation | Mass | Designation | Mass | Designation | Mass | Designation | Mass |
| 30x20x3 | 1.12 | 100x50x6 | 6.84 | 125x75x8 | 12.2 | 150x90x10 | 18.2 |
| 30x20x4 | 1.46 | 100x50x8 | 8.97 | 125x75x10 | 15 | 150x90x11 | 19.9 |
| 40x20x4 | 1.77 | 100x65x7 | 8.77 | 125x75x12 | 17.8 | 150x90x12 | 21.6 |
| 40x25x4 | 1.93 | 100x65x8 | 9.94 | 130x90x10 | 16.6 | 150x90x15 | 26.6 |
| 45x30x4 | 2.25 | 100x65x9 | 11.1 | 130x90x12 | 19.7 | 150x100x10 | 19 |
| 50x30x5 | 2.96 | 100x65x10 | 12.3 | 130x90x14 | 22.8 | 150x100x12 | 22.5 |
| 60x30x5 | 3.36 | 100x65x11 | 13.4 | 135x65x8 | 12.2 | 150x100x14 | 26.1 |
| 60x40x5 | 3.76 | 100x65x12 | 14.5 | 135x65x10 | 15 | 200x100x10 | 23 |
| 60x40x6 | 4.46 | 100x75x8 | 10.6 | 140x90x8 | 14 | 200x100x12 | 27.3 |
| 65x50x5 | 4.35 | 100x75x10 | 13 | 140x90x10 | 17.4 | 200x100x14 | 31.6 |
| 70x50x6 | 5.41 | 100x75x12 | 15.4 | 140x90x12 | 20.6 | 200x100x15 | 33.8 |
| 75x50x6 | 5.65 | 110x70x10 | 13.4 | 140x90x14 | 23.8 | 200x100x16 | 35.9 |
| 75x50x8 | 7.39 | 110x70x11 | 15.9 | 150x75x9 | 15.4 | 200x150x12 | 32 |
| 80x40x6 | 5.41 | 120x80x8 | 12.2 | 150x75x10 | 17 | 200x150x15 | 39.6 |
| 80x40x8 | 7.07 | 120x80x10 | 15 | 150x75x12 | 20.2 | ||
| 80x60x7 | 7.36 | 120x80x12 | 17.8 | 150x75x15 | 24.8 | ||
| Toleransi | |||||||||
| Side Width Tolerance for Width | Ketebalan | ||||||||
| 3 4 5 6 7 8 9 10 | |||||||||
| Tolerance for Thickness | |||||||||
| 20 | ±1.5 | ±0.4 | |||||||
| 25 | ±1.5 | ±0.5 | ±0.5 | ||||||
| 30 | ±2.0 | ±0.5 | ±0.5 | ±0.5 | ±0.5 | ||||
| 40 | ±2.0 | ±0.6 | ±0.6 | ±0.6 | ±0.6 | ||||
| 50 | ±2.0 | ±0.6 | ±0.6 | ±0.6 | |||||
| 60 | ±3.0 | ±0.6 | ±0.6 | ||||||
| 65 | ±3.0 | ±0.6 | ±0.6 | ±0.7 | ±0.7 | ||||
| 70 | ±3.0 | ±0.7 | ±0.7 | ±0.7 | |||||
| 75 | ±3.0 | ±0.7 | ±0.7 | ±0.7 | ±0.7 | ||||
| 80 | ±3.0 | ±0.7 | ±0.7 | ±0.7 | ±0.7 | ||||
| 90 | ±3.0 | ±0.7 | ±0.7 | ±0.8 | |||||
| 100 | ±4.0 | ±0.7 | ±0.7 | ±0.8 | |||||
| Pilihan Status Pengiriman | Kondisi Permukaan |
| Canai Panas | Acar |
| Sand Blasting | |
| Polished | |
| Catatan: | |
| 1. Jika Anda memerlukan status pengiriman yang berbeda dari yang tercantum di atas, mohon konfirmasi dengan kami. | |
| 2. Jika ada pertanyaan atau pesanan, mohon beritahukan kepada kami persyaratan tambahan yang tidak disebutkan di sini. | |
Related Product
Paduan Daxun
Regarding stainless steel angle, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.
Yes, we have complete specifications and inventory and can quickly meet your needs.
Yes, it can be customized. You can contact us and send us the customized specifications and quantity.
Our transportation methods generally include sea transportation, land transportation, and sea transportation. Reach you quickly and safely.
Because our output is high, the cost will be much lower, so the price is low.
We can provide stainless steel angle samples for you to check the quality. Sample is free and you just pay the freight.
We attach great importance to product quality and have passed various quality system tests.