x
Envoyez votre demande dès aujourd'hui
Devis rapide

Daxun is an excellent manufacturer of CP Grade 4 titanium rods and bars.

  • Titanium bar grade: UNS R50700
  • Types de barres de titane : barres laminées, barres étirées, barres de titane forgées
  • Principales normes : ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
  • High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.

The global leader in commercially titanium alloy rod manufacturing services

Daxun, specializing in the production of alloy titanium rods for extreme environments

CP Grade 4 titanium bar represents the highest strength variant within the commercially pure titanium family, combining exceptional mechanical properties with outstanding corrosion resistance. As an unalloyed titanium grade, it maintains the inherent biocompatibility and weldability of pure titanium while delivering significantly enhanced tensile strength, with minimum yield strength reaching 480 MPa and ultimate tensile strength exceeding 550 MPa. This unique combination makes CP Grade 4 titanium bars particularly valuable in applications demanding both structural integrity and environmental durability.

The chemical composition of CP Grade 4 titanium bar consists primarily of titanium with controlled amounts of oxygen (0.40% maximum), iron (0.50% maximum), carbon (0.08% maximum), and nitrogen (0.05% maximum). The elevated oxygen content compared to other CP grades directly contributes to its superior strength characteristics. These bars exhibit excellent ductility, allowing for various forming processes while maintaining their enhanced mechanical properties, making them suitable for cold working, machining, and fabrication into complex components.

Key Application Areas

  • Aérospatiale : Used for critical structural components, aircraft fasteners, and springs where high strength-to-weight ratio is essential.
  • Traitement chimique : Ideal for pump shafts, valve components, and heat exchanger parts exposed to aggressive media.
  • Génie maritime : Employed for hardware and components that require long-term durability in seawater.
  • Medical Implants: Utilized for surgical instruments and implant devices that demand both high strength and biocompatibility.

Manufacturing & Product Forms

  • Production Processes: Can be produced through hot rolling, forging, or extrusion, followed by annealing.
  • Available Forms: Supplied in various shapes, including round, square, hexagonal, and flat bars.
  • Custom Dimensions: Available in a wide range of sizes, with options for custom dimensions to meet specific project needs.
  • Machining: Can be effectively machined using appropriate tooling and cooling strategies, though it requires more robust parameters than lower titanium grades.
Spécifications Détails
Matériau CP Grade 4 Titanium Bar
Standard ASTM B348, ASTM F67, AMS 4921, ISO 5832-2
Dimensions EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN
Gamme de diamètres 0.125″ - 14″ (3.175mm - 355.6mm), sur mesure
Longueur Plage Jusqu'à 240″ (6096mm), sur mesure
Formulaire Round Bar, Square Bar, Hexagonal Bar
Finition de la surface Cold drawn, Centerless Ground, Polished, Rough Turned, Black, NO.4 Finish, BA Finish, Matt Finish
Condition Annealed, Hardened & tempered
Tolérance Tolérance sur le diamètre : +/- 0.005″ (0.127mm), tolérance sur la longueur : +/- 0.125″ (3.175mm)
Formulaire Titanium square bars, titanium ingots, titanium round bars, rectangular titanium bars, triangular titanium bars, forged titanium bars, titanium hexagonal bars

Données

Élément Minimum Maximum
Titane (Ti) 99.2 -
Oxygène (O) 0.35 0.40
Fer (Fe) - 0.50
Carbone © - 0.08
Azote (N) - 0.05
Hydrogène (H) - 0.015
Propriété Minimum Value Unit
Résistance ultime à la traction 550 MPa
Limite d'élasticité (décalage de 0,2%) 480 MPa
Élongation 15 %
Réduction de la surface 30 %
Brinell Hardness 320 HBW
Modulus of Rigidity 44 GPa

 

Propriété Valeur Unit
Densité 4.51 g/cm³
Point de fusion 1668 °C
Module d'élasticité 105 GPa
Conductivité thermique 16.4 W/m·K
Résistivité électrique 560 nΩ·m
Chaleur spécifique 0.52 J/g·K

Choisissez Daxun pour faire décoller votre projet.

Contacter Daxun maintenant

Avantages de l'usine de Daxun

Le concept de “gestion de l'excellence des performances” de Daxun promeut le modèle de gestion “PDCA + Lean”. La carte de visite de l'entreprise indique “Daxun = Qualité fiable”. Daxun utilise le système ERP pour assurer la traçabilité complète de la variété, de la spécification et de l'origine de chaque tige de titane, et préconise et encourage la lutte contre la contrefaçon dans l'industrie. Daxun s'appuie sur la technologie pour le traitement et la personnalisation, et la haute précision et la haute qualité sont les références de l'industrie ; en termes de service, elle promeut la gestion du cycle de vie des produits, fournit une sélection professionnelle des matériaux et des solutions de traitement avant les ventes, assure un suivi strict pendant les ventes et fournit des garanties de service sans souci après les ventes.

Contacter Daxun maintenant

CP Grade 4 Titanium Rod Production Method

Daxun produit des barres de titane de haute qualité et de haute performance, et peut également fabriquer selon l'accord du client :

  • Les lingots de titane doivent subir un traitement thermique et un usinage, des essais ultrasoniques par immersion, des essais de propriétés mécaniques, une inspection structurelle macroscopique et microscopique et d'autres processus. Processus de production : barres de titane laminées à chaud - haute efficacité, performances stables, barres de titane forgées - taille flexible, forgeage à feu multiple, amélioration des performances globales des barres de titane, barres de titane étirées à froid - généralement des barres de titane de haute précision de petite taille ; les barres de titane susmentionnées sont toutes livrées avec une surface brillante.
Contacter Daxun maintenant

Qualité, livraison, inspection

Daxun performs several quality assurance tests, these tests include mechanical tests like area tensile, chemical analysis, material positive identification – PMI test, micro and macro testing, intergranular corrosion (IGC) test, ultrasonic flaw detection test, pitting and resistance test, hardness test, material positive identification, expansion test etc. All these tests ensure that the CP Grade 4 Titanium Rod and CP Grade 4 Titanium Round Bar material is suitable for the required application. During the production process, we measure the diameter, thickness and surface of the product.

  • Nos délais de livraison sont strictement conformes au contrat.
  • Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
  • Prise en charge d'échantillons gratuits pour les essais des clients
  • Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Contacter Daxun maintenant

Emballage

Daxun Alloy garantit la meilleure qualité d'emballage, car celui-ci joue un rôle important dans le fret international, où les marchandises passent par différents canaux avant d'atteindre leur destination finale ; nous accordons donc une attention particulière à l'emballage. Nous emballons nos marchandises de différentes manières, en fonction du produit. Nous emballons nos produits de différentes manières, notamment :
- Boîtes et caisses
- Emballage rétractable
- Palettes en bois
- Boîtes en bois

Contacter Daxun maintenant

Support technique

Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.

Daxun CP Grade 4 Titanium Rods help your brand improve quickly

TAILLE NOMINALE
h5
h6
h7
h8
h9
H10
H11
h12
DIAMÈTRE mm
~ à 3 +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
plus de 3 à 6 ans +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
plus de 6 à 10 +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
plus de 10 ans à 18 ans +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
plus de 18 ans à 30 ans +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
plus de 30 à 50 +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
plus de 50 à 80 +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
plus de 80 à 120 +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
plus de 120 à 180 +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
plus de 180 à 250 +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

Projets et produits récents

Grade 7 Titanium rod and bar
Barres et tiges en titane
Barres et tiges en titane
Barres et tiges en titane
What makes CP Grade 4 titanium bar different from other commercially pure grades?

CP Grade 4 is the strongest of all the commercially pure titanium grades. Its key differentiator is its higher oxygen content, which gives it a minimum yield strength of 480 MPa, significantly higher than CP Grade 2 (275 MPa). This makes it the preferred choice when high strength and durability are critical, while still maintaining excellent corrosion resistance.

What are the most common applications for CP Grade 4 titanium bar?

Due to its high strength-to-weight ratio and biocompatibility, CP Grade 4 titanium bar is widely used in the aerospace industry for fasteners and springs, in chemical processing for pump and valve components, in marine engineering for durable hardware, and in the medical field for surgical instruments and implants that require superior structural integrity.

Is CP Grade 4 titanium bar difficult to machine or weld?

While it is more challenging to machine than lower grades due to its strength, it can be effectively machined with proper tooling and cooling. It is also readily weldable using standard methods like TIG welding, but it requires an inert gas shield (like argon) to protect the weld area from atmospheric contamination and prevent embrittlement.

Why should I choose CP Grade 4 titanium over stainless steel?

The primary advantage is its superior corrosion resistance, especially in chloride environments like seawater, where stainless steel is prone to pitting and stress corrosion cracking. CP Grade 4 also offers a much better strength-to-weight ratio. Although the initial cost is higher, its extended service life and reduced maintenance in harsh environments often result in a lower total cost of ownership.

Comment obtenir un devis OU comprendre les informations du marché le plus rapidement possible ?

Veuillez remplir le formulaire de la page “Contactez-nous” ou appeler notre responsable des ventes au “+86 13382898899”, nous vous contacterons dans les plus brefs délais. Notre WhatsApp est en ligne, et l'email (Daxunalloy@gmail.com) sera vérifié dans les 6 heures. Chaque demande ou message recevra une réponse rapide. En outre, nous partageons chaque semaine des informations sur le marché avec nos clients

Puis-je obtenir des échantillons ?

Nous pouvons vous fournir des échantillons de barres de titane pour que vous puissiez en vérifier la qualité. L'échantillon est gratuit et vous ne payez que les frais de transport.

Quels sont les pays que vous avez déjà exportés ?

Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.

Quel est le délai de livraison ?

Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.

Envoyez votre demande dès aujourd'hui
Devis rapide