Daxun Alloy - Hastelloy B3 pipe made in China
As a leading supplier of Hastelloy B3 pipes in China, Daxun provides high-performance alloy tubes to the world.
- Hastelloy B3 types: Seamless tube, welded tube, forged tube
- Certification : ASTM,SGS,ISO,CE
- Délai de livraison : 7-15 jours
- Finition de la surface : Recuit, poli, etc.
- MOQ : ≥300kg
————Daxun produit des tubes en hastelloy en Chine pour répondre aux besoins divers et variés des consommateurs. ——les besoins exigeants des clients!
Characteristics & Properties of Hastelloy B3
Hastelloy B3 pipe (N10675) is a nickel-based high-temperature alloy composed of nickel, molybdenum, cobalt and other elements, with a nickel content of about 65%. Hastelloy B3 (N10675) nickel-based alloy material is a new material improved on the basis of Hastelloy B2, which improves the thermal stability of the material, thereby improving the corrosion resistance, and at the same time, improves the hot forming and cold forming properties.
Corrosion resistance: Hastelloy B3 has excellent corrosion resistance to hydrochloric acid at any temperature and concentration, and also has good corrosion resistance to non-oxidizing media such as sulfuric acid, acetic acid, formic acid, phosphoric acid, etc. Its thermal stability has been significantly improved compared to B2, and it has high resistance to pitting corrosion, stress corrosion cracking, knife corrosion, and corrosion in the heat-affected zone of welding.
Mechanical properties: The tensile strength of Hastelloy B3 is usually between 690 and 860 MPa, the yield strength is usually between 310 and 550 MPa, the elongation is generally between 40% and 50%, and the hardness is usually between 20 and 30 Rockwell hardness (HRC).
Forming processing characteristics: Hastelloy B3 has a high elongation, which creates favorable conditions for cold forming. However, since it is harder than austenitic stainless steel and has a more obvious tendency to work hardening, it requires greater pressure or step-by-step forming during cold forming. When the cold forming deformation rate is less than 10%, it will not affect the corrosion resistance of the workpiece, but the presence of residual stress may cause thermal cracks in the weld during welding.
Hastelloy B3 is widely used in the fields of chemical, petrochemical, energy manufacturing and pollution control, especially in industries such as H2SO4, HCl, H3PO4, CH3COOH, etc. It is used to manufacture key equipment such as reactors, heat exchangers, pipelines and valves. Due to its excellent hydrochloric acid corrosion resistance, these equipment can operate stably for a long time in a high concentration of hydrochloric acid environment.
Welding characteristics: Hastelloy B3 can be welded by all common welding methods, but GTAW welding method is recommended. ERNiMo-10 welding materials should be selected according to ASME ⅡSFA-5.14/SFA-5.14M standards. The groove and welding materials should be cleaned before welding, and small line energy should be used during welding to prevent excessive heat input.
Hastelloy B3 Parameters
- Composition chimique
- Propriétés physiques
- Propriétés mécaniques
| C≤ | Si≤ | Mn≤ | P≤ | S≤ | Cr≥ | Ni≥ | Mo≥ | Cu≤ |
| 0.01 | 0.1 | 3 | 0.03 | 0.01 | 1.00-3.00 | 65 | 27.0-32.0 | 0.2 |
| Nb/Ta≤ | Al≤ | Ti≤ | Fe≤ | Co≤ | V≤ | W≤ | Ni+Mo | Ta≤ |
| 0.2 | 0.5 | 0.2 | 1.00-3.00 | 3 | 0.2 | 3 | 94.0-98.0 | 0.2 |
| Densité | 9.22 – 9.24 g/cm³ |
| Melting point | 1370 – 1418°C |
| Thermal expansion coefficient | Approx. 0.6μm/m°C (20-100°C) |
| Conductivité thermique | Approx. 10 W/m·K |
| Tensile strength | 690 – 860 MPa |
| Limite d'élasticité | 310 – 550 MPa |
| Élongation | 40% – 50% |
| Dureté | 20 – 30 Rockwell hardness (HRC) |
Choisissez Daxun pour faire décoller votre projet.

Production avancée : tube en alliage d'Hastelloy
- Hastelloy B3 seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface treated. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities.
- Hot rolled tube/hot extruded Hastelloy B3 seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm.
- Cold rolled Hastelloy B3 seamless tube: Cold processed tubes are supplied after heat treatment, surface treatment, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm
Hastelloy B3 Pipe Features
Hastelloy B3 pipe is a nickel-based alloy pipe. Because it contains high nickel and molybdenum and other elements, it has resistance to a variety of strong acid corrosion and certain high temperature performance. It is made by a specific process and is widely used in pipeline transportation in chemical, marine, environmental protection and other environments with strong corrosive media.
- Excellent corrosion resistance
- High temperature stability
- Good processing performance
- High strength and toughness


Qualité, livraison, inspection
Daxun conducts a series of quality assurance tests on Hastelloy B3 pipes. These tests include flattening test, flaring test, ultrasonic flaw detection, crevice corrosion resistance test, mechanical property test, hardness test, material positive identification, and expansion test, etc. All these tests are designed to ensure that the Hastelloy B3 pipes meet the requirements of the intended applications. During the production process, we meticulously measure the outer diameter, wall thickness, and surface quality of the products. Our standard delivery time is 5 – 7 days, and for special sizes, it is 15 – 20 days.
- Nos délais de livraison sont strictement conformes au contrat.
- Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
- Prise en charge d'échantillons gratuits pour les essais des clients
- Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Emballage
Daxun Alloy garantit la meilleure qualité d'emballage, car celui-ci joue un rôle important dans le fret international, où les marchandises passent par différents canaux avant d'atteindre leur destination finale ; nous accordons donc une attention particulière à l'emballage. Nous emballons nos marchandises de différentes manières, en fonction du produit. Nous emballons nos produits de différentes manières, notamment :
- Boîtes et caisses
- Emballage rétractable
- Palettes en bois
- Boîtes en bois


Support technique
Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.
Daxun est un fabricant de tubes en acier inoxydable digne de confiance.
En tant que fabricant professionnel, Daxun s'assure que tous les produits qu'il fabrique sont de haute qualité. Par conséquent, nous veillons à ce que tous les tubes en titane soient certifiés ISO9001, SGS, CE, OQC et autres normes de qualité internationales. Nous effectuons également un contrôle de qualité strict afin de garantir que les tubes en acier inoxydable présentent moins de défauts. Chez Daxun, vous pouvez être assuré que tous les produits sont durables, de haute qualité et d'excellentes performances.
Produits apparentés (8)
Veuillez remplir le formulaire de la page “Contactez-nous” ou appeler notre responsable des ventes au “+86 13382898899”, nous vous contacterons dans les plus brefs délais. Notre WhatsApp est en ligne, et l'email (Daxunalloy@gmail.com) sera vérifié dans les 6 heures. Chaque demande ou message recevra une réponse rapide. En outre, nous partageons chaque semaine des informations sur le marché avec nos clients
Nous pouvons vous fournir des échantillons de tôles d'acier inoxydable pour vous permettre de vérifier la qualité. L'échantillon est gratuit et vous ne payez que les frais de transport.
Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.
La quantité minimale de commande pour nos produits en Hastelloy est de 300 kg.
Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.