Daxun 304 stainless steel plate and sheet China supplier
As China’s leading stainless steel plate supplier and exporter, Daxun provides stainless steel plates to the world.
- Grade: AISI 304/S30400
- Fabrication : tôles laminées à froid, tôles laminées à chaud, tôles forgées
- Norme : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Type : tôles minces laminées à froid, tôles épaisses laminées à chaud
- Surface : 2B, NO.1, NO.4, HL, BA, 8K, etc.
- Longueur : 2438mm3048mm6000mm peut être personnalisé
- Origin: TISCO, Baosteel, Posco, Tsingshan, Delong
Leader mondial des services de fabrication de tôles en acier inoxydable
304 is one of the most popular grades of stainless steel because of its high strength, excellent corrosion resistance, and excellent formability. This grade has a low carbon content and excellent ductility. It can be cold worked by roll forming, deep drawing, and bending. This grade is suitable for forming complex shapes. You will see this grade in the oil and gas industry and the food service industry.Our 304 series is a standout product available in thicknesses from 0.4mm to 20mm. Available in 2B and 2D finishes, these stainless steel products offer excellent corrosion resistance, strength and a wide range of surface finish options to suit different project requirements.
Daxun is your trusted stainless steel sheet supplier.By choosing our 304stainless steel plates, you are investing in a material that guarantees long life, reliability and superior performance. Don’t compromise on quality – choose our stainless steel solutions and experience the difference they can make in your projects. Contact us today for more details or to order your required specifications and quantities.
Données
- Paramètres
- Ingredients and properties
- Propriétés mécaniques
- PROPRIÉTÉS PHYSIQUES
| Stainless Plate and sheet Type | Plate, Sheet, Strip, Coils, Foils, Flats, Clad Plate, Plain Sheet, Rolling Sheet, Rolling Plate, Flat Shim, Flat Sheet, Shim Sheet, Rolls, Blank (Circle), sheared, annealed, soft annealed, descaled, tread plate, Checker Plate |
| Standard | ASTM A240 / ASME SA240 ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2JIS, AISI, ASTM, GB, DIN, EN, etc |
| Stainless Steel Plate and sheet Length | 1000mm-13000mm or as required |
| 304 Stainless Plate Width | 1000mm-1219mm-1500mm-1800mm-2000mm-2500mm or as required |
| UNS 304 Plate Thickness | 0.3 to 120mm or as required |
| ASTM A240 Stainless Steel 304 Plate Process | Hot/ Cold Rolled/forging |
| UNS 304 Plate surface | No.1, No. 2D, No. 2B, BA, No.3, No.4, No.6, No.7, 2B, 2D, BA NO(8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled ASTM A240Stainless Steel 304 Plate, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc. |
| Stainless 304 Sheet ASTM | ASTM A240 |
| Stainless 304 Sheet AMS | AMS 240 |
| Tolerances of width and thickness | ASTM-ASME-GB-EN-DIN-JIS |
| 304 Stainless Plate standards and approvals | EN ISO 18286 EN 10051 EN 10088-1 ISO 15510 EN ISO 9445 ASTM A 480 ASTM A 959 ASME IID |
| 304 Plate & Sheet Sizes | 1000 x 2000 mm, 1220 x 2440 mm, 1500 x 3000 mm, 2000 x 2000 mm, 2000 x 4000 mm,1500*6000,Cold rolled 304 Stainless Plate 0.5-6.4 mm,Hot rolled 304 Stainless Plate 3.0–60.0 mm |
| UNS 304 Plate Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard ASTM A240Stainless Steel 304 Sheet suppliers |
| Cutting | To provide a comprehensive service, we use a variety of cutting methods, including:Laser Plate Cutting,Plasma Plate Cutting,Oxy-propane Flame Cutting |
| Profils plasmatiques | As per customer’s drawings |
| Value added services for 304 Stainless Plate | Laser cutting, Waterjet cutting, Plasma cutting, Bending and mechanical processing, edge preparation, welding, sawing and shearing. |
| Fabricant | POSCO, Aperam, ATI, ThyssenKrupp, Baosteel, TISCO, ArcelorMittal, VDM, Nippon Metal, Outokumpu, Tsingshan, Delong. |
| China 304 Stainless Plate Manufacturer | ASTM A240Stainless Steel 304 Plate: material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width;304 Stainless Sheet: material under 3/16″ [5.00 mm] in thickness and 24″ [600 mm] and over in width;Steel Stainless 304 Clad plate: Steel Stainless 304 Clad plate is a composite steel plate made by bonding 304 Stainless 304 Plate, etc.ASTM A240Stainless Steel 304 Strip: cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width. |
| 304 Plate Origin | CHINA |
| Packing of 304 plate | Bundles with waterproof cloth outside or plywood box |
| Test | UT, SGS testing, TUV etc |
| Why buy 304 Sheet from DAXUN? | Free quote、Free sample、EN 10204 3.1、Mill Test Certificate is supplied with shipment、NABL Approved Lab Reports、Any third party inspection is accepted、Tested to ASTM A923 Method “C” or ASTM G48 Method “A”.Minimum Nitrogen content and Ferrite Count TestGrade: AISI 304/S30400 Fabrication : tôles laminées à froid, tôles laminées à chaud, tôles forgées Norme : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS Type : tôles minces laminées à froid, tôles épaisses laminées à chaud Surface : 2B, NO.1, NO.4, HL, BA, 8K, etc. Longueur : 2438mm3048mm6000mm peut être personnalisé Origin: TISCO, Baosteel, Posco, Tsingshan, Delong |
| Standard | Werkstoff Nr. | UNS | JIS | BS | GOST | AFNOR | FR | CN |
| SS 304 | 1.4301 | S30400 | SUS 304 | 304S31 | 08Х18Н10 | Z7CN18-09 | X5CrNi18-10 | 06Cr19Ni10 |
| Grade | C | Mn | Si | P | S | Cr | Ni | N |
| 304 | ≤0.08% | ≤2.0% | ≤ 0.75% | ≤0.045% | ≤0.030% | 18%-20% | 8.0%-10.5% | ≤0.10% |
| Type | Limite d'élasticité 0.2% offset (KSI) | Résistance à la traction (KSI) | % Allongement (2″ Longueur de la jauge) |
| 304 Ann | 30 min. | 75 min. | 40 min. |
| 304 ¼ Dur | 75 min. | 125 min. | 12 min. |
| 304 ½ Dur | 110 min. | 150 min. | 7 min. |
| 304L Ann | 25 min. | 70 min. | 40 min. |
| 304L ¼ Dur | 75 min. | 125 min. | 12 min. |
| 304L ½ Dur | 110 min. | 150 min. | 6 min. |
| 304 & 304L | ||
| Densité (lb./ in^2) @ RT | 0.29 | |
| Module d'élasticité en traction (psi x 10^6) | 28 | |
| Chaleur spécifique (BTU/o F/lb.) | 32 à 212 oF | 0.12 |
| Conductivité thermique (BTU/hr/ft^2/ft) | 212oF | 9.4 |
| 932oF | 12.4 | |
| Coefficient moyen de dilatation thermique (po x 10^-6 par o F) | 32 à 212oF | 9.2 |
| 32 à 600oF | 9.9 | |
| 32 à 1 000oF | 10.2 | |
| 32 à 1 200oF | 10.4 | |
| Résistivité électrique (micro ohms - cm) | à 70oF | 72 |
| Gamme de points de fusion (oF) | 2550 à 2650 | |
| Résistance à l'oxydation - Service continu(oF) | 1,650 | |
| Résistance à l'oxydation - Service intermittent(oF) | 1,500 |
Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

Livraison rapide
Daxun provides customers with timely and fast delivery of stainless steel plate products. Behind the speed is the system support from production capacity, information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Réponse rapide
Daxun saves customers time, materials and stress, and ultimately saves them costs. With its professional advantages, Daxun can provide the most cost-optimized material recommendations based on customer needs, and can also reduce costs for customers through continuous processing, nesting processing, etc.

Usinage avancé
Our advanced nesting processing method improves material utilization and cutting utilization. At the same time, Daxun can also achieve continuous cost reduction and efficiency improvement by promoting lean improvement activities, and return the benefits to customers. In addition, Daiming also has a complete product traceability system and rapid handling of quality objections, which makes customers worry-free.
304 stainless steel plate packaging
Daxun Alloy ensures the best quality of 304 stainless steel sheet packaging, because packaging plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Boîtes et caisses
- Papier kraft + palettes en bois
- Emballage rétractable
- Palettes en bois sans fumigation
- Boîtes en bois sans fumigation

304 Stainless Steel Sheet Processing:
- Traitement de la gravure
- Traitement des soudures
- Traitement du pliage
- Traitement du gaufrage
- Traitement par sablage
- Traitement par polissage
- Traitement du poinçonnage
- Traitement de l'estampage
SS 304 Plate Surface Treatment
1D : la surface est mate et la forme des particules est discontinue.
2D : Blanc avec un ton argenté.
2B : gris argenté avec une meilleure brillance et planéité que la surface 2D.
Ba : Surface proche d'un miroir avec une brillance et une réflectivité excellentes.
No.3 : Bonne brillance et surface rugueuse.
No.4 : La surface présente des lignes fines et une bonne brillance.
HL : Gris argenté avec des cheveux dorés.
8K : Surface miroir.
304 plate stainless steel Features
Let your brand improve rapidly
- Galerie
- TOLERANCE
- DELIVERY STATE
- Autres séries de produits
| Tolérance pour la tôle 2B | |||
| Taille | Rang de tolérance | ||
| Groupe 1 | Groupe 2 | Groupe 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Tolérance pour la tôle laminée à chaud n° 1 | |||
| Taille | Rang de tolérance | ||
| Groupe 1 | Groupe 2 | Groupe 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Choix de l'État de livraison | État de surface |
| Laminés à froid | 2B |
| 2D | |
| BA | |
| Ligne de démarcation des cheveux | |
| N° 3 | |
| N°4 | |
| 6K | |
| 8K | |
| Remarque : | |
| 1. Si vous avez besoin d'un autre pays de livraison que ceux mentionnés ci-dessus, veuillez nous le confirmer. | |
| 2. En cas de demande ou de commande, veuillez nous faire part de toute exigence supplémentaire non indiquée ici. | |
| État de livraison | |
| Choix de l'État de livraison | État de surface |
| Laminés à chaud | N°1 |
| N° 3 | |
| N°4 | |
| 6K | |
| 8K | |
| Mariné | |
| Remarque : | |
| 1. Si vous avez besoin d'un autre pays de livraison que ceux mentionnés ci-dessus, veuillez nous le confirmer. | |
| 2. En cas de demande ou de commande, veuillez nous faire part de toute exigence supplémentaire non indiquée ici. | |
| Grade | Type | Épaisseur | Surface |
| Austénitique | 304/304H/304L/304J1 | 0,25-150 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0.3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferrite | 430 | 0,4-3,0 mm | 2B/BA/NO.4/8K/SB/HL |
| Ferrite ultra pure | 443 | 0,4-2,0 mm | 2B |
| 436L/439/444/441 | 0,5-3,0 mm | 2B、2D | |
| 409L | 0,4-2,5 mm | 2B、2D | |
| Grade | Type | Épaisseur | Original |
| Acier résistant à la chaleur | 309S | 0,5-40 mm | CHN |
| 310S | 0,5-40 mm | CHN | |
| Acier duplex | 2101 | 1,5-50 mm | CHN |
| 2304 | 3.0-50mm | CHN | |
| 2205 | 0,5-60 mm | CHN | |
| 2507 | 1.0-60mm | SWE / JPN / CHN | |
| Acier super austénitique | N08904 | 0,6-50 mm | SWE / JPN / CHN |
| S31254 | 0,5-50 mm | SWE / JPN / CHN | |
| N08926 | 0,5-50 mm | SWE / JPN / CHN | |
| N08367 | 0,5-50 mm | SWE / JPN / CHN | |
| Alliage base nickel | N08031 | 1.0-50mm | US / JPN / GER |
| N08810/N08800 | 0,8-50 mm | US / JPN / CHN | |
| N08028 | 1.0-20mm | US / GER / JPN | |
| N08020 | 1.0-20mm | US / GER / JPN | |
| N08825 | 0,8-40 mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0,5-50 mm | US / GER / JPN | |
| N06022 | 1.0-50mm | US / GER / JPN | |
| N06625 | 0,8-20 mm | US / GER / CHN | |
| N04400 | 1.0-20mm | US / GER / JPN | |
| N06600 | 1.0-50mm | US / GER / JPN / CHN | |
| N02201 | 0,5-20 mm | US / JPN | |
| Titane | TA1/Gr1 | 0,5-50 mm | JPN / CHN |
| TA2/Gr2 | 0,5-50 mm | JPN / CHN | |
| Matériel de soudage | ERNiCrMo-13 | 1.2、2.4mm | GER |
| ERNiCrMo-3 | 2,4 mm | GER | |
| ERNiCrMo-4 | 2,4 mm | ÉTATS-UNIS |
The surface and shape of 304 stainless steel plate (6)
Informations disponibles pour référence et téléchargement
Daxun est un fabricant de plaques d'acier inoxydable digne de confiance.
En tant que fabricant professionnel, Daxun s'assure que tous les produits qu'il fabrique sont de haute qualité. Par conséquent, nous veillons à ce que toutes les plaques d'acier inoxydable soient certifiées ISO9001, SGS, CE, OQC et autres normes de qualité internationales. Chez Daxun, vous avez l'assurance que tous les produits sont durables, de haute qualité et très performants.
Projets et produits récents
Produits apparentés (13)
Nous pouvons vous fournir des échantillons de tôles d'acier inoxydable pour vous permettre de vérifier la qualité. L'échantillon est gratuit et vous ne payez que les frais de transport.
Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.
Notre MOQ est de 1 tonne pour les tôles d'acier inoxydable.
Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.