stainless steel coils
- Daxun has 30,000 tons of stainless steel coils in stock
- Cold-rolled stainless steel coils and hot-rolled stainless steel coils
- Surface processing services for stainless steel coils are available
- De grandes quantités de stocks ponctuels peuvent être expédiées rapidement.
Stainless Steel Coil Products
| Largeur | 3,5mm~1500mm |
| Épaisseur | 0,02mm~6mm |
| Standard | AISI, JIS, SUS, GB, ASTM A240 et AMS |
| Densité | Approx. 7.7–8.0 g/cm³ depending on grade |
| Finitions de surface | Brossé, poli, gaufré, BA, 2B, 2BA, 8K, NO.4, HL, SB, NO.1, 2H |
| Notes | 201, 202, 301, 304, 304L, 316, 316L, 316Ti, 321, 317l, et 430, 2205, 904l, 2507, 309s, 410s, 303, 309S, 310S, 347, 904L, 410, 414, 416, 416, 420, 431, 440A, 440B, 440C, S31803, S32101, S32205, S32304, S32750, 429, 430, 433, 434, 435, 436, 439, etc. |
Daxun offers a full range of stainless steel alloys in the form of stainless steel coils, known for their reliability, durability, and high performance. We provide a wide selection of grades, from austenitic to ferritic series, suitable for both industrial and construction applications. Our austenitic series includes grades like 201, 304, 304L, 321, 316, 316L, and more, available in various surface finishes such as 2B, BA, No.4, 8K, SB, and HL.
Pour les clients à la recherche de propriétés et d'applications uniques, notre série de ferrites comprend le 430, la ferrite ultra-pure 443 et le 436L/439/444/441. Les aciers duplex comprennent les aciers S31808/S32205/S32750/S32760. Ces produits répondent aux exigences d'épaisseur de 0,4 mm à 3,0 mm et sont disponibles dans une variété d'options de finition de surface, y compris 2B, BA, NO.4, 8K, SB, HL, et plus encore.
Stainless steel coil grades and characteristics
Each stainless steel coil material has its own different usage scenarios.
Stainless steel coil surface
Si la surface dont vous avez besoin n'est pas disponible ici, veuillez contacter Daxun.
Les rouleaux d'acier inoxydable peuvent être transformés en surfaces brossées pour l'ensemble du rouleau.
Les rouleaux d'acier inoxydable peuvent être transformés en surfaces miroir sur toute la longueur du rouleau.
Stainless steel coils can be made into bright annealed surfaces in full rolls
The original color of Daxun’s stainless steel coils is cold-rolled 2B surface
Daxun’s No.1 finish is generally used for hot-rolled stainless steel coil after pickling.
Nous pouvons effectuer un placage coloré en surface selon la carte de couleurs que vous nous fournissez.
Nous pouvons effectuer un placage coloré en surface selon la carte de couleurs que vous nous fournissez.
Nous pouvons effectuer un placage coloré en surface selon la carte de couleurs que vous nous fournissez.
Commonly used thicknesses of stainless steel coils
We offer stainless steel coils in a wide range of thicknesses, suitable for all types of applications. Our products can be processed to the width you need, using advanced slitting and flying shear equipment.
Performance of Stainless steel coil
La composition chimique protège contre la rouille, ce qui le rend idéal pour les appareils et les environnements exigeants.
Facile à utiliser et très durable, il réduit les coûts d'entretien.
Stainless steel coils are known for their durability, low maintenance, and versatility.
Facile à façonner, il est parfait pour les grandes utilisations industrielles et les petites applications détaillées.
Vaste stock de matériel de choix
Daxun keeps stainless steel coil in stock across common grades and sizes, so most orders ship in 3–7 days without waiting on a new production run. Raw material is sourced from established mills including TISCO, ZPSS, Baosteel, JISCO, ATI, VDM, ArcelorMittal, and Outokumpu, giving consistent quality across every batch.
Stainless Steel Grades (300 and 200 series)
Stainless steel grades are classified by composition, properties, and application, which is what determines the right material for your project. Austenitic grades (e.g., 304, 316, 321) are non-magnetic, easily welded and formed, with the best corrosion resistance and ductility of the common grades — the default choice for food equipment, architectural finishes, and general corrosion-resistant applications. Duplex grades (e.g., 2205, 2507) combine austenitic and ferritic properties for higher strength and stronger resistance to stress corrosion cracking than standard austenitic grades — specified for chemical processing, oil and gas, and marine environments where standard grades fall short.
Grades d'acier inoxydable (série 400)
Ferritic grades (e.g., 409, 430, 439) offer good corrosion resistance and higher cost-effectiveness than austenitic grades, at the trade-off of lower ductility — magnetic, with lower carbon content for better resistance to stress corrosion cracking, commonly specified for automotive exhaust systems, industrial equipment, and kitchenware. Martensitic grades (e.g., 410, 420, 440) are heat-treatable to a range of hardness and strength levels, making them the choice for cutlery, surgical instruments, and turbine blades — but with lower corrosion resistance than austenitic or ferritic grades, a trade-off worth confirming against your application before specifying.
Stainless Steel Coil Finishing Options
- Brossé Finition : Les bobines d'acier inoxydable peuvent être traitées pour obtenir un aspect brossé, idéal à des fins décoratives.
- Finition miroir : Obtenir une surface hautement réfléchissante et polie sur l'ensemble du rouleau.
- Recuit brillant Finition : Rouleaux complets d'acier inoxydable recuit brillant pour un aspect propre et brillant.
- 2B Surface : Laminés à froid avec une finition lisse originale.
- Finitions colorées : Les options comprennent des surfaces brossées dorées, miroir noir et or rose, personnalisables en fonction de vos besoins.
Contrôle de la qualité et fabrication
Quality control covers every stage of coil production. Raw material is inspected against specification before entering production. In-process inspection monitors dimensions, surface finish, and mechanical properties as the coil is formed. Finished coil is verified against specified mechanical properties, chemical composition, and corrosion resistance requirements, with ultrasonic and eddy current testing used to detect internal or surface defects without damaging the material.


Fabrication techniques for stainless steel coils include
Cold rolling brings the coil to the specified thickness and surface finish at room temperature, improving strength and surface quality in the process. Heat treatment adjusts hardness and corrosion resistance as needed for the application, extending the material’s service life. Cutting to final size and shape uses shearing, sawing, or laser cutting, depending on the tolerance the specification calls for.
Peut être transformé à la largeur souhaitée
- Nous disposons de machines à refendre et de cisailles volantes pour mieux vous servir.
- Largeur 9.0mm-2000mm, nous pouvons le faire.
- ASTM A240、ASTM A480、JIS G4303、BS 1449、DIN17441、G4305
Stainless steel coil processing and customization
Daxun offers stainless steel coil processing including BA, 2B, and No.4 finishes with PVC/PE protective film. Coils can be re-coiled into smaller weights on request, with inner diameter (ID) from 150mm to 510mm and outer diameter (OD) from 300mm to 1200mm.
Informations techniques
At Daxun, we use strong and secure packaging to protect our stainless steel coils. Packaging options include kraft paper, wooden boxes, woven bags, and wooden pallets. Our goal is to ensure your order arrives in perfect condition, ready for use.
Daxun’s quality management system is certified to ISO 9001:2015. Every shipment includes a mill test certificate, and material is traceable from source to delivery.
Daxun maintains an in-house testing laboratory to verify that every shipment meets the specified weight and quality standard before delivery. Our quality control team performs 100% inspection at every production stage.
Our support doesn’t end when your order ships. Daxun continues to provide after-sales assistance and warranty support for every order.
Application cases of stainless steel coils in different industries
Stainless steel coil is widely used in construction, including exterior wall cladding, interior decoration, roofing, and structural applications. Its corrosion resistance and mechanical strength suit both long-term exposed applications and structural use.
Corrosion resistance and a smooth, easy-to-clean surface make stainless steel coil well suited to food processing equipment — including storage tanks, sanitation systems, and fluid pipe tanks.
Stainless steel coil offers strength, toughness, and corrosion resistance suited to demanding structural applications.
Our corrosion resistant steel coils are perfect for shipbuilding, thanks to their high strength, toughness, and resistance to seawater corrosion and fatigue. Grades like SS316L are used for marine applications due to their excellent resistance in harsh environments.
Informations techniques
- Stock
- Tolérances et surface
| Épaisseur (mm) | Largeur (mm) | Longueur (mm) | Commentaire |
| 0.5 | 1000/1219/1500 | C | AAA |
| 0.8 | 1000/1219/1500 | C | AAA |
| 1.0 | 1000/1219/1500 | C | AAA |
| 1.5 | 1000/1219/1500 | C | AAA |
| 2.5 | 1000/1219/1500 | C | AAA |
| 3.0 | 1000/1219/1500 | C | AAA |
| 5.0 | 1500/1800/2000 | C | AAA |
| 6.0 | 1500/1800/2000 | C | AAA |
| 8.0 | 1500/1800/2000 | C | AAA |
| 10.0 | 1500/1800/2000 | C | AAA |
| 12.0+ | 1500/1800/2000 | C | AAA |
| Tolérances | |||||
| Rang de tolérance | |||||
| Taille | Groupe 1 | Groupe 2 | Groupe 3 | État de livraison | État de surface |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 | Laminés à froid | 2B 2D BA Ligne de démarcation des cheveux N° 3 N°4 6K 8K |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 | ||
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 | ||
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 | ||
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 | ||
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 | ||
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 | ||
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 | ||
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 | ||
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 | ||
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 | ||
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 | ||
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 | État de livraison | N°1 N° 3 N°4 6K 8K Mariné |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 | ||
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 | ||
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 | ||
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 | ||
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 | ||
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 | ||
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 | ||
| Remarque : 1. Si vous avez besoin d'un autre pays de livraison que ceux mentionnés ci-dessus, veuillez nous le confirmer. 2. En cas de demande ou de commande, veuillez nous faire part de toute exigence supplémentaire non indiquée ici. |
|||||
Pourquoi choisir Daxun ?
Large Inventory: 30,000 tons in stock across common grades and sizes.
Quality Assurance: ISO 9001:2015-certified, with mill test certificate on
every shipment.
Custom Solutions: A range of finishes, custom sizes, and free samples to
match your specification.
After-Sales Service: Ongoing support and warranty coverage after delivery.
Yes — we maintain stock across common specifications and can typically ship quickly from inventory.
Absolument. Nous proposons des adaptations pour répondre à vos besoins spécifiques.
Nous utilisons des moyens de transport maritimes et terrestres pour garantir que vos produits arrivent rapidement et en toute sécurité.
Yes — free samples are available for common grades and finishes. Send us
your specification and we’ll confirm sample availability and shipping.