x
Envoyez votre demande dès aujourd'hui
Devis rapide

Angle en acier inoxydable

  • Daxun is the world’s leading stainless steel angle steel and
  • Stainless Steel Angle Iron Suppliers and Manufacturers.
  • We produce high quality stainless steel angle steel.

Daxun is a stockist and manufacturer of stainless steel angle steel

  • China stainless steel angle steel supplier.
  • Daxun has 10,000 tons of stainless steel angle steel in stock
  • Daxun can provide angle steel surface processing services
  • Type: equal angle steel and unequal angle steel

Introduction to Daxun stainless steel angle steel

Product Parameters:   Stainless Steel Angle bar
Taille 20×20×3;25×25×3、25×25×4;30×30×3、30×30×4、30×30×5、30×30×6;40×40×3、40×40×4、40×40×5、40×40×6;50×50×4、50×50×5、50×50×6;60×60×5、60×60×6;65×65×5、65×65×6、65×65×7、65×65×8;70×70×6、70×70×7、
70×70×8;75×75×6、75×75×7、75×75×8、75×75×9;80×80×8、80×80×9、80×80×10;100×100×8、100×100×9、100×100×10、100×100×12  *Sizes from 100×100 to 150×150 can be customized.
Surface Décapage 8K, NO.1, NO.4, hairline, etc.
longueur 6000mm ou sur mesure
Grade 304 201 304L 310S 316L 321 904L 2205 2507 S32750 S32760 etc.
Normes ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227
Caractéristiques Anti-corrosion (le degré dépend des alliages contenus), résistance à la chaleur, bonnes propriétés de travail à froid et à chaud, bonne ténacité, bonnes performances globales et application étendue.

Daxun offers stainless steel angle steel in different sizes, material grades, profiles, finishes and other specifications. We can also produce custom stainless steel angles based on your specific needs or applications.

Lire la suite

Stainless Steel Angle Steel Grade

Each type of stainless steel angle steel has its own different usage scenarios.

Cliquez sur l'image pour obtenir plus d'informations sur ce produit

310S stainless steel angle

Cliquez sur l'image pour obtenir plus d'informations sur ce produit

321 stainless steel angle
2205 stainless steel angle

Cliquez sur l'image pour obtenir plus d'informations sur ce produit

12 produits trouvés.

Performance of stainless steel angle steel

Résistance à la corrosion

The chemical composition on stainless steel angle bars protects them from rust. Their corrosion resistance is enhanced by the necessary polished finish, making them ideal for architectural use.

Faible coût

Since stainless steel angles have a low melting point, no special tools are required. They are also durable and long-lasting materials, allowing industries to save on work and maintenance costs.

Métal précieux

The smarter option material SS angles have far lesser drawbacks than other alloys. They provide excellent value, cost-effectiveness, and durability. SS is an easy-to-clean metal material.

Aptitude au travail

Stainless steel angle material is an excellent choice for a variety of applications such as manufacturing. They are simple to use and ideal for large-scale industrial and complex uses.

Vaste stock de matériel de choix

Daxun dispose de stocks d'acier inoxydable pour les qualités et les tailles courantes afin de répondre rapidement à la demande de ses clients : TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc.

Common areas of stainless steel angle steel

  • Stainless steel angle bars are hot-rolled and pickled, making them versatile for use in a wide range of construction and engineering projects. They are commonly used in structures like house beams, bridges, power transmission towers, and shipyards.

Peut être transformé à la largeur souhaitée

1. Prix et qualité compétitifs de notre propre usine
2. Approuvé par ISO9001, CE, SGS chaque année
3. Meilleur service avec une réponse dans les 24 heures
4. Paiement flexible par T/T, L/C, paypal, etc.
5. Capacité de production régulière
6. Livraison rapide et emballage standard pour l'exportation
7. OEM/ODM

Informations techniques

Rolls,Of,Steel,Sheet
Méthode d'emballage

Chez Daxun, nous choisissons différents emballages pour différents produits en acier inoxydable, notamment : papier kraft, boîtes en bois, sacs tissés, palettes en bois, sur la base des normes industrielles les plus strictes afin de garantir que les marchandises arrivent entre vos mains en bon état.

Certification de l'essai des matériaux

Tous nos matériaux en acier inoxydable sont certifiés par différentes normes industrielles telles que ISO9001:2008, ISO14001:2014, AAA Certification, CQGC Certifications, etc. Notre société est également certifiée par le système de gestion de la qualité ISO9001:2015.

Poids réel et bonne qualité

Chez Daxun, nous disposons d'un laboratoire et d'un équipement de test pour garantir que nos matériaux en acier inoxydable sont de poids réel et de bonne qualité avant l'expédition. Notre équipe de contrôle de la qualité effectue également des inspections strictes et 100% à tous les stades de la production.

Excellents services après-vente

Notre soutien et nos services ne se limitent pas au début de nos transactions. Même si vous avez reçu vos commandes, Daxun continuera à fournir d'excellents services après-vente. Nous continuerons à fournir une assistance et une garantie pour vos commandes.

Application cases of stainless steel angle in different industries

Décoration des bâtiments

Stainless steel angles are widely used in the construction field and can be used for exterior wall supports, interior decoration, roofing materials, building structures, etc. Stainless steel is corrosion-resistant and has high strength, which can meet the design requirements of different buildings.

Équipements mécaniques

L'acier inoxydable présente les avantages suivants : résistance à la corrosion, absence de rouille, absence de décoloration, élimination facile des aliments attachés, bonnes propriétés mécaniques à haute et basse température. Il est largement utilisé dans les machines alimentaires, telles que les systèmes sanitaires, les réservoirs de fluides, les réservoirs de stockage des aliments, les échangeurs de chaleur, les récipients sous vide, etc.

Aérospatiale

L'acier inoxydable présente une bonne solidité, une bonne ténacité et une bonne résistance à la corrosion, et il est largement utilisé dans les pièces structurelles des avions. Par exemple, la structure des ailes, les supports du fuselage, les sièges et d'autres composants sont tous fabriqués en acier inoxydable.

Pétrochimie

Stainless steel angles are also used in the manufacture and maintenance of oil refining equipment, and the brackets used in the petrochemical industry are all made of stainless steel angles.

armure militaire

Principales applications : revêtement d'aile, longerons d'aile, bandes de bord supérieur et inférieur du longeron d'aile, âme, longerons de fuselage, rails de siège, poutre de quille, cadres latéraux, revêtement de fuselage, panneaux de la paroi inférieure du fuselage, longerons du plancher principal, etc.

Champ de navires

Stainless steel angle steel is widely used in the shipbuilding industry. The stainless steel angle supplied by Daxun are used in the shipbuilding and petroleum industries. They have high strength, good toughness, and are resistant to seawater corrosion, fatigue, and wear.

Génie maritime

SS316L est la principale nuance d'acier inoxydable austénitique utilisée dans les installations offshore, où elle améliore la résistance à des températures élevées et protège les structures contre les environnements acides sévères. L'acier UNS S32205 est la nuance d'acier inoxydable duplex la plus couramment utilisée pour les installations offshore.

Champ de puissance électrique

The main application of stainless steel angle steel in electricity is the support of power station equipment. The excellent corrosion resistance and high strength of stainless steel make it the preferred material for power generation components.

about-feature3
Let us be your trustworthy stainless steel angle supplier

Our stainless steel angle are fully certified and traceable. We provide the highest quality stainless steel angle for leading industries such as building decoration, industrial equipment, chemical energy, shipbuilding, and petrochemicals.

Mechanical Information

Gamme de tailles
Hot-rolled equal-leg angle bar
Désignation Masse Désignation Masse Désignation Masse Désignation Masse
20x20x3 0.88 70x70x5 5.37 120x120x8 14.7 180x180x16 43.5
25x25x3 1.12 70x70x6 6.38 120x120x9 16.5 180x180x17 46
25x25x4 1.45 70x70x7 7.38 120x120x10 18.2 180x180x18 48.6
25x25x5 1.78 70x70x8 8.37 120x120x11 19.9 180x180x19 51.1
30x30x3 1.36 70x70x9 9.32 120x120x12 21.6 180x180x20 53.7
30x30x4 1.78 70x70x10 10.3 120x120x13 23.3 200x200x13 39.8
30x30x5 2.18 75x75x4 4.65 120x120x14 25 200x200x14 42.7
35x35x3 1.6 75x75x5 5.76 120x120x15 26.6 200x200x15 45.6
35x35x3.5 1.85 75x75x6 6.85 120x120x16 28.3 200x200x16 48.5
35x35x4 2.09 75x75x7 7.93 130x130x8 16 200x200x17 51.4
35x35x5 2.57 75x75x8 8.99 130x130x9 17.9 200x200x18 54.3
38x38x4.5 2.56 75x75x9 10 130x130x10 19.8 200x200x19 57.1
38x38x6 3.33 75x75x10 11.1 130x130x11 21.7 200x200x20 59.9
40x40x3 1.84 76x76x5 5.84 130x130x12 23.6 200x200x21 62.8
40x40x4 2.42 76x76x6.5 7.49 130x130x13 25.4 200x200x22 65.6
40x40x5 2.97 76x76x8 9.11 130x130x14 27.2 200x200x23 68.3
40x40x6 3.52 76x76x9.5 10.7 130x130x15 29 200x200x24 71.1
45x45x3 2.09 80x80x5 6.17 130x130x16 30.8 200x200x25 73.9
45x45x4 2.74 80x80x6 7.34 140x140x9 19.3 200x200x26 76.6
45x45x4.5 3.06 80x80x7 8.49 140x140x10 21.4 200x200x27 79.3
45x45x5 3.38 80x80x8 9.63 140x140x11 23.4 200x200x28 82
45x45x6 4 80x80x9 10.8 140x140x12 25.4 250x250x17 64.4
45x45x7 4.6 80x80x10 11.9 140x140x13 27.5 250x250x18 68.1
50x50x3 2.33 90x90x5 6.97 140x140x14 29.4 250x250x19 71.7
50x50x4 3.06 90x90x6 8.3 140x140x15 31.4 250x250x20 75.3
50x50x5 3.77 90x90x7 9.61 140x140x16 33.3 250x250x21 78.9
50x50x6 4.47 90x90x8 10.9 140x140x18 37.2 250x250x22 82.5
50x50x7 5.15 90x90x9 12.2 150x150x10 23 250x250x23 86.1
50x50x8 5.82 90x90x10 13.4 150x150x11 25.2 250x250x24 89.7
50x50x9 6.47 90x90x11 14.7 150x150x12 27.3 250x250x25 93.2
55x55x4 3.38 90x90x16 20.7 150x150x13 29.5 250x250x26 96.7
55x55x5 4.18 100x100x6 9.26 150x150x14 31.6 250x250x27 101
55x55x6 4.95 100x100x7 10.7 150x150x15 33.8 250x250x28 104
60x60x4 3.7 100x100x8 12.2 150x150x16 35.9 250x250x29 107
60x60x5 4.57 100x100x9 13.6 150x150x17 38 250x250x30 111
60x60x6 5.42 100x100x10 15 150x150x18 40.1 250x250x31 114
60x60x7 6.26 100x100x11 16.4 150x150x19 42.1 250x250x32 118
60x60x8 7.09 100x100x12 17.8 150x150x20 44.2 250x250x33 121
60x60x10 8.69 100x100x13 19.2 160x160x12 29.3 250x250x34 124
63x63x5 4.82 100x100x14 20.6 160x160x13 31.6 250x250x35 128
63x63x6 5.72 100x100x15 21.9 160x160x14 33.9 300x300x25 112
63x63x6.5 6.17 100x100x16 23.2 160x160x15 36.2 300x300x26 116
65x65x4 4.02 110x110x6 10.2 160x160x16 38.4 300x300x27 121
65x65x5 4.97 110x110x7 11.8 160x160x17 40.7 300x300x28 125
65x65x6 5.91 110x110x8 13.4 160x160x18 42.9 300x300x29 129
65x65x7 6.83 110x110x9 15 160x160x19 45.1 300x300x30 133
65x65x8 7.73 110x110x10 16.6 160x160x20 47.3 300x300x31 138
65x65x9 8.62 110x110x11 18.2 180x180x13 35.7 300x300x32 142
65x65x10 9.49 110x110x12 19.7 180x180x14 38.3 300x300x33 146
65x65x11 10.3 120x120x7 12.9 180x180x15 40.9
Hot-rolled unequal-leg angle bar
Désignation Masse Désignation Masse Désignation Masse Désignation Masse
30x20x3 1.12 100x50x6 6.84 125x75x8 12.2 150x90x10 18.2
30x20x4 1.46 100x50x8 8.97 125x75x10 15 150x90x11 19.9
40x20x4 1.77 100x65x7 8.77 125x75x12 17.8 150x90x12 21.6
40x25x4 1.93 100x65x8 9.94 130x90x10 16.6 150x90x15 26.6
45x30x4 2.25 100x65x9 11.1 130x90x12 19.7 150x100x10 19
50x30x5 2.96 100x65x10 12.3 130x90x14 22.8 150x100x12 22.5
60x30x5 3.36 100x65x11 13.4 135x65x8 12.2 150x100x14 26.1
60x40x5 3.76 100x65x12 14.5 135x65x10 15 200x100x10 23
60x40x6 4.46 100x75x8 10.6 140x90x8 14 200x100x12 27.3
65x50x5 4.35 100x75x10 13 140x90x10 17.4 200x100x14 31.6
70x50x6 5.41 100x75x12 15.4 140x90x12 20.6 200x100x15 33.8
75x50x6 5.65 110x70x10 13.4 140x90x14 23.8 200x100x16 35.9
75x50x8 7.39 110x70x11 15.9 150x75x9 15.4 200x150x12 32
80x40x6 5.41 120x80x8 12.2 150x75x10 17 200x150x15 39.6
80x40x8 7.07 120x80x10 15 150x75x12 20.2
80x60x7 7.36 120x80x12 17.8 150x75x15 24.8
Tolérance
Side Width              Tolerance for Width Épaisseur
          3                  4               5                6                 7               8                9                10
Tolerance for Thickness
20 ±1.5 ±0.4
25 ±1.5 ±0.5 ±0.5
30 ±2.0 ±0.5 ±0.5 ±0.5 ±0.5
40 ±2.0 ±0.6 ±0.6 ±0.6 ±0.6
50 ±2.0 ±0.6 ±0.6 ±0.6
60 ±3.0 ±0.6 ±0.6
65 ±3.0 ±0.6 ±0.6 ±0.7 ±0.7
70 ±3.0 ±0.7 ±0.7 ±0.7
75 ±3.0 ±0.7 ±0.7 ±0.7 ±0.7
80 ±3.0 ±0.7 ±0.7 ±0.7 ±0.7
90 ±3.0 ±0.7 ±0.7 ±0.8
100 ±4.0 ±0.7 ±0.7 ±0.8
Choix de l'État de livraison État de surface
Laminés à chaud Mariné
Sablage
Poli
Remarque :
1. Si vous avez besoin d'un autre pays de livraison que ceux mentionnés ci-dessus, veuillez nous le confirmer.
2. En cas de demande ou de commande, veuillez nous faire part de toute exigence supplémentaire non indiquée ici.
  • “Thank you Daxun for the extremely durable, world-class quality stainless steel angle. I also appreciate the professional customization service. I am happy to work with you for my stainless steel angle needs. Looking forward to working with you next time!”

    Témoignages de clients situés au Moyen-Orient
  • “Daxun has always been a trustworthy company when it comes to stainless steel angle. All the stainless steel angle I purchased are of very high quality. I ordered stainless steel angle at a very low price at Daxun. The staff was also happy to answer my questions .” Asked questions and was impressed with my needs! “

    Témoignages de clients situés en Europe et aux États-Unis
  • “We were very impressed with the quality and superiority of Daxun stainless steel angle. There are a variety of sizes available that fit our needs perfectly. Additionally, we really appreciate the affordable price and service.”

    Témoignages de clients situés en Russie

Daxun Alloy

Regarding stainless steel angle, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.

Avez-vous des stocks en réserve ?

Oui, nous disposons de spécifications et d'un inventaire complets et pouvons rapidement répondre à vos besoins.

Peut-il être personnalisé ?

Oui, il peut être personnalisé. Vous pouvez nous contacter et nous envoyer les spécifications et quantités personnalisées.

Comment expédiez-vous les marchandises ?

Nos méthodes de transport comprennent généralement le transport maritime, le transport terrestre et le transport maritime. Ils vous permettent d'arriver à destination rapidement et en toute sécurité.

Quel est votre prix ?

Parce que notre production est élevée, le coût sera beaucoup plus faible, donc le prix est bas.

Puis-je obtenir des échantillons ?

We can provide stainless steel angle samples for you to check the quality. Sample is free and you just pay the freight.

Quelle est votre qualité ?

Nous attachons une grande importance à la qualité de nos produits et avons passé plusieurs tests de qualité.

Envoyez votre demande dès aujourd'hui
Devis rapide