Daxun is an experienced Ti 6Al 4V-Grade 5 Titanium Tube manufacturer

En tant que principal fournisseur de tubes en titane et en alliage de titane en Chine, Daxun fournit des tubes en titane de haute performance au monde entier.
  • Titanium tube Grade:Grade 5 -Ti6Al 4V- UNS R56400-3.7165-TC4
  • Ti tube types:Seamless titanium tube, drawn tube, forged titanium tube
  • Titanium tube density The density of grade 5 titanium is 4.51 g/cm3
  • Main standards: ASTM  ASME GB GJB EN JIS DIN ISO ATP BS  etc.
  • High strength, high temperature resistance, corrosion resistance, lightweight

----Daxun produit des tubes en titane en Chine pour répondre aux besoins divers et -- exigeants des clients!.

A global leader in commercially pure titanium tube fabrication services

Daxun Alloy, as a leading titanium alloy tube manufacturer and supplier in China, provides high-quality Grade 5 titanium pipes to the world and has been well received by many projects.

Ti 6Al-4V (Grade 5 Titanium) is the most widely used of all titanium alloy tubes, accounting for more than 50% of the total titanium usage. It is usually used in the annealed state and has an operating temperature of up to 400°C (750°F). Ti 6Al/4V is welded with matching or ELI filler wire. Ti 6Al/4V has significantly higher strength than commercial pure titanium tubes, while having better stiffness and thermal properties (excluding thermal conductivity), and the thermal conductivity of Grade 5 titanium tube is about 60% lower than CP titanium. Among its many advantages, it can be heat treated. Thus, more ideal strength and performance are obtained. The advantages of using Grade 5 titanium seamless tubes include not only strong formability and low density, but also excellent corrosion resistance.

This grade is a perfect combination of strength, corrosion resistance, weldability and machinability. Therefore, it is widely used, such as in military aircraft or aviation industry, rocket parts, precision-guided components, armor parts, ship equipment, military vacuum equipment and other parts. The close version of 6-4, 6-4ELI, is also used in surgical implants. Typically, it is used in applications up to 400°C to improve ductility and toughness in cold working conditions. It also has excellent specific strength. It is usually provided in the annealed state and is easy to heat treat to increase strength for a variety of applications. As a general-purpose titanium alloy, Ti 6Al-4V titanium seamless tube has a wide range of ideal properties at temperatures around -210°C – 400°C. Grade 5 titanium alloy tube is the most commercialized of all titanium alloys. It combines high strength and toughness. Grade 5 titanium alloy tube has good welding and processing characteristics.

Titanium Alloy Grade 5 Seamless Pipe, Titanium Gr 5 High Pressure Pipe, ASTM B338 Titanium Alloy Gr 5 Seamless Pipe, Titanium Gr 5 Thick Wall Pipe. China Titanium Grade 5 ERW Pipe Supplier. Titanium Alloy Gr 5 Pipe, Titanium Gr 5 Electropolished Pipe, Anti-corrosion Titanium Pipe, Titanium Tube, ASTM B338 Titanium Grade 5 Welded Pipe, ASTM B861 / ASME SB861 Titanium Grade 5 Seamless Pipe China Titanium Gr-5 Seamless Pipe Manufacturer. Ti-6al-4v Pipe Dealer, ASTM B338 Titanium Grade 5 Pipe, Titanium Gr 5 Bright Annealed Pipe, Ti-6al-4v Pipe, Gr 5 Pipe, Titanium Gr 5 Pipe, Titanium WERKSTOFF NR 3.7165 Pipe

 

Are you looking to purchase titanium tubes for your project or order a range of titanium tubes? Daxun produces a wide range of titanium tubes including Grade 1 (3.7025), Grade 2 (3.7035), Grade 3 (3.7055), Grade 5 (3.7165), Grade 7 (3.7235), Grade 9 (3.7195) and Grade 12 (3.7105).

Buy titanium tubes at Daxun Alloys.
We offer a wide range of sizes starting from 1.0 mm in diameter with multiple variations, available directly from stock or custom made to your specifications through our network. We have wrought titanium tubes, seamless titanium tubes and longitudinally welded titanium tubes immediately available from stock for a wide range of applications.

We offer heat exchanger tubing in standard specifications such as ASTM B 338, ASME SB 338, DIN 17866 and VD TÜV welded titanium tubes or seamless titanium tubes. When it comes to titanium tubes, we have a large supply of titanium welded tubes and titanium seamless tubes in China in standard sizes up to 100 mm thick. We will supply welded titanium tubes for larger pipe sizes. The most common specifications used in the industry are ASTM B 861, ASFM B 862, NACE and NORSOK and VD TÜV Tube 230/2, depending on the specifications of the plant designer.

Titanium tube surface treatment options include bright annealing, pickling and grinding. Material parameters vary depending on the application and product requirements. The corrosion and mechanical properties of titanium alloy tubes vary. We are happy to assist you in evaluating your needs. If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee price and quantity for a specified period.

Lire la suite

Données

Ti-6Al-4V Grade 5 Titanium pipe & Tubes Specification ASTM B338 / ASTM B861 / ASTM B862 / ASME SB338 / ASME SB861 / ASME SB862
Grade 5 Titanium pipe & Tubes Grades Commercially pure titanium Grade 5-Ti-6Al4V- TC4- USN 56400
Grade 5 Titanium pipe & Tubes Type ot Rolled / Cold Drawn / Welded / ERW
Grade 5 Titanium pipe & Tubes Outer Diameter Size Titanium seamless pipe – φ1.0mm to φ508.3mm
Titanium welded pipe – φ6.0mm to φ1219mm
Grade 5 Titanium pipe & Tubes Wall Thickness 1.0mm—50mm (customizable wall thickness)
Grade 5 Titanium pipe & Tubes Length 5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size.
Titanium pipe Form Ti-6Al-4V ‘ Hollow, U’ bent, LSAW, Hydraulic, Straight Tube, Boiler, Round, Tube Coil, Square, Rectangular Etc
Marking  TC4 1.37165 All Titanium Tubes Tubing are marked as follows: Grade, Standard, Thickness, OD, Heat No., Length (Or according to the customer’s request.)
Uses of Titanium Alloy Tubes Gas pipes, oil pipes, heat exchanger tubes, boiler tubes, fluid pipes, titanium exhaust pipes.
Grade 5 Titanium pipe & Tubes Pipe Ends Plain Ends / Beveled Ends
Grade 5 Titanium pipe & Tubes Delivery Conditions As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered
Grade 5 Titanium pipe & Tubes Coating Electropolish, Mechanical Polish, Satin Finish, Passivated
Grade 5 Titanium pipe & Tubes Other Testing ardness Test, Hydrostatic Test, Eddy Current test, Eddy Current, Tensile Test, Flattening, Flare Test, Annealed, Hydrostatic Test, Tempered, Stress Relieved etc.
Grade 5 Titanium pipe & Tubes Dimension All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME
Grade 5 Titanium pipe & Tubes Value Added Services Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment
Grade 5 Titanium pipe & Tubes Packaging Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector
Grade 5 Titanium pipe & Tubes Shipment & Transportation By Road – Truck / Train, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes
Grade 5 Titanium pipe & Tubes Material Test Certificate Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS ETC
Chemical Composition:
Symbol Élément Min % Max %
Al Aluminum 5.50% 6.75%
V Vanadium 3.50% 4.50%
Fe Iron 0.30%
O Oxygen 0.20%
C Carbone 0.08%
N Azote 0.05%
H Hydrogen 0.01%
Y Yttrium 0.01%
Other, each 0.10%
Other, total 0.40%
Ti Titane Remainder
Propriétés physiques Metric English Comments
Densité 4.43 g/cc 0.16 lb/in³
Propriétés mécaniques
Hardness, Brinell 334 334  Estimated from Rockwell C.
Dureté, Knoop 363 363  Estimated from Rockwell C.
Hardness, Rockwell C 36 36
Dureté, Vickers 349 349  Estimated from Rockwell C.
Tensile strength min. 895MPa 129810 psi
Limite d'élasticité min. 828MPa 120090 psi
Allongement à la rupture min.10 % 10 %
Réduction de la surface min.25 % 25 %
Module d'élasticité 113.8 GPa 16500 ksi
Compressive Yield Strength 970 MPa 141000 psi
Notched Tensile Strength 1450 MPa 210000 psi  Kt (stress concentration factor) = 6.7
Ultimate Bearing Strength 1860 MPa 270000 psi  e/D = 2
Bearing Yield Strength 1480 MPa 215000 psi  e/D = 2
Rapport de Poisson 0.342 0.342
Charpy Impact 17 J 12.5 ft-lb  V-notch
Résistance à la fatigue 240 MPa 34800 psi  at 1E+7 cycles. Kt (stress concentration factor) = 3.3
Résistance à la fatigue 510 MPa 74000 psi  Unnotched 10,000,000 Cycles
Résistance à la rupture 75 MPa-m½ 68.3 ksi-in½
Module de cisaillement 44 GPa 6380 ksi
Résistance au cisaillement 550 MPa 79800 psi  Ultimate shear strength
Electrical Properties
Résistivité électrique 0.000178 ohm-cm 0.000178 ohm-cm
Perméabilité magnétique 1.00005 1.00005  at 1.6kA/m
Magnetic Susceptibility 3.30E-06 3.30E-06  cgs/g
Propriétés thermiques
CTE, linear 20°C 8.6 µm/m-°C 4.78 µin/in-°F  20-100ºC
CTE, linear 250°C 9.2 µm/m-°C 5.11 µin/in-°F  Average over the range 20-315ºC
CTE, linear 500°C 9.7 µm/m-°C 5.39 µin/in-°F  Average over the range 20-650ºC
Capacité thermique spécifique 0.5263 J/g-°C 0.126 BTU/lb-°F
Conductivité thermique 6.7 W/m-K 46.5 BTU-in/hr-ft²-°F
Point de fusion 1604 – 1660 °C 2920 – 3020 °F
Solidus 1604 °C 2920 °F
Liquidus 1660 °C 3020 °F
Beta Transus 980 °C 1800 °F
Beta Transus (F ± 25) 1830
Coefficient of Thermal Expansion (10-6in./in./F) 32-212 5
32-600 5.3
32-1000 5.6
32-1200 5.9
32-1500 6.1
Density (lbs./cu. in.) 0.16
Melting Point, Approx (F) 3200
Electrical Resistivity at Room Temp. (Microhms cm) 171
Modulus Elasticity – Tension (106 psi) 16.5
Modulus Elasticity – Torsion (106 psi) 6.1
Conductivité thermique 3.9 at Room Temperature
(Btu/hr/sq. ft./F/ft.)
Specific Heat (Btu/lb./F) at Room Temp. 0.135
Soudabilité Fair
Annealing Temp. (F) Complet 1300 – 1525°/15 Min. – 2 Hrs,; Air Cool
Stress Relief 900 – 1200°/1 -4 Hrs.; Air Cool
Forging* Temp. (F) Blocking 1750 – 1800°
Finishing 1650 – 1750°
Typical Application Compressor blades, discs, aircraft components, pressure vessels, rocket engine cases;
the most versatile titanium alloy.
Titanium Grade 5 Pipes 4 inch Ti Alloy Grade 5 Seamless Pipes
Ti Alloy Grade 5 Pipes Titanium gr 5 Welded Pipes
Grade 5 Titanium Seamless Steel Pipes Titanium UNS R56400 Cold Drawn Welded Pipes
Ti Alloy Grade 5 Welded Pipes Grade 5 Pure Titanium Cold Drawn Pipes
Titanium gr 5 ERW Pipes Schedule 5S Grade 5 Titanium Seamless Pipe
Grade 5 Pure Titanium EFW Pipes Schedule 40 Titanium 3.7165 Pipes
Grade 5 Titanium Cold Drawn Seamless Pipes Titanium gr 5 Precision Pipes
Alloy Grade 5 Seamless Steel Precision Pipes High pressure ASTM B337 Titanium Grade 5 Pipes
Titanium 3.7165 Cold Drawn Seamless Pipes Titanium Alloy Grade 5 Electropolished Pipes
Ti Alloy Grade 5 Custom Pipes Titanium Grade 5 Cold Drawn Pipes
UNS R56400 Round Pipes Gr 5 Ti Exhaust Pipes
Gr 5 Titanium Rectangular Pipes Small diameter Titanium Alloy Grade 5 Pipes
Grade 5 Titanium Hexagonal Pipe Ti Alloy Grade 5 Pipe material
UNS R56400 Welded Pipe Grade 5 Titanium Hexagonal Pipe
Ti Alloy Grade 5 Welded Pipe Titanium Alloy Gr 5 Pipe
Titanium Gr 5 EFW Pipe Grade 5 Titanium Seamless Pipe
Alloy Grade 5 Bush Hex Pipe DIN 3.7165 Precision Steel Pipes
Grade 5 Pure Titanium Fabricated Pipe UNS R56400 Annealed pipe
Ti Grade 5 Beveled End Pipe Grade 5 Pure Titanium Rectangle Pipe
ASTM B337 Titanium Grade 5 Cold Drawn Pipe Cold Drawn Alloy Grade 5 Welded Pipe
Titanium Grade 5 Seamless Tubes Titanium Alloy Gr 5 Welded Tubes
Titanium Gr 5 High Pressure Tube Titanium UNS R56400 Welded Tube
ASTM B338 Titanium Alloy Gr 5 Seamless Tubing Ti. Alloy WERKSTOFF NR. 3.7165 Welded Tubes
Titanium Alloy Gr 5 Tubes ASTM B338 Gr.5 Titanium Welded Tubes
Titanium Gr 5 Santiary Tube Grade 5 Alloy Round Tube
Titanium Gr 5 Cold Rolled Coiled Tube Grade 5 Titanium Alloy Round Tubes
Gr 5 Titanium Welded Tubes Titanium Grade 5 Round Tube
Dealer of ASTM B338 Titanium Grade 5 Tube UNS R56400 Round Tubes
Titanium Gr 5 Decorative Tube Titanium Alloy Gr 5 Round Tube
Gr 5 Titanium Bright Annealed Tube ASME SB338 Gr 5 Titanium Round Tubes
Ti. Alloy Grade 2 ERW Tubes UNS R56400 Gr5 Ti Alloy Tubing
Titanium UNS R56400 Tubing Grade 5 Ti Tubing
Titanium NCF Gr 5 Tubes ASTM B558 Titanium Alloy Welded Tubes
Titanium Gr 5 Tubing WERKSTOFF NR. 3.7165 Gr5 Titanium Tubes
Titanium WERKSTOFF NR. 3.7165 Tubing Ti-6Al-4V Tube
Titanium Alloy Gr 5 Tubing Titanium Alloy Grade 5 Seamless Tubes
Titanium Gr 5 Electropolish Tube Titanium Alloy Grade 5 Round Tube
ASTM B338 Titanium Grade 5 Welded Tubing Titanium Grade 5 Elliptical and Oval Tubes
Grade 5 Titanium Alloy Seamless Tubing Titanium Grade 5 Rectangular Tube
Titanium Grade 5 Welded Tubes0 Titanium Grade 5 Sighting Tube
Gr 5 Titanium Heat Exchanger Tube Titanium Grade 5 Polish Tubes
ASTM B338 Titanium Gr 5 Tube Titanium Grade 5 Aerospace tubes
Gr 5 Titanium Tubing Titanium Grade 5 High Pressure Tube
Titanium Grade 5 Tube Titanium Alloy Grade 5 Coiled Tubing
Grade 5 Titanium Alloy Seamless Tubes Grade 5 Titanium Capillary Tubing
Titanium Grade 5 Welded Tube Titanium Alloy Grade 5 Seamless Tubing
Titanium Alloy Grade 5 Tubing Titanium Grade 5 Condenser Tubes
Grade 5 Ti. Alloy Tubing Titanium Grade 5 Aero engine tubes
Ti. Alloy Gr 5 Seamless Tubes Titanium Alloy Grade 5 Straight Tube boiler
Gr 5 Alloy Seamless Tube Titanium Grade 5 Furnace Tube
Titanium Alloy Gr.5 Seamless Tubes Grade 5 Titanium Seamless Tube
UNS R56400 Seamless Tube Grade 5 Titanium Tube
WERKSTOFF NR. 3.7165 Seamless Tubes Titanium Grade 5 Tubing
ASME SB338 Gr.5 Titanium Seamless Tube Grade 5 Alloy Welded Tube
Titanium Alloy Grade 5 Welded Tubes Titanium Grade 5 Seamless Tubes

Choisissez Daxun pour faire décoller votre projet.

Contacter Daxun maintenant

Production avancée : tube sans soudure en titane

  • Grade 5 steel seamless pipes are processed by hot turning or hot pressing, straightening, inner and outer diameter processing, and can be provided in heat treatment or non-heat treatment forms. / Hot rolled seamless pipe: outer diameter 1.0mm to 325mm, wall thickness 0.3mm to 50mm, length up to 12000mm. Cold rolled seamless pipe: cold processed pipes are heat treated, surface engraved, water pressure tested or ultrasonically tested according to the manufacturing standards of outer diameter 6mm to 102mm, wall thickness 0.5mm to 20mm, and length up to 9000mm.
    (The above is determined according to the specific situation of the manufacturer and the customer)
Contacter Daxun maintenant

Grade 5 Titanium Tube Features

Ti-6Al4V Grade 5 Titanium Alloy Tube is the most commercially available of all Titanium alloys. It combines high strength and toughness. Grade 5 Titanium alloy has good welding and processing characteristics:

  • High Strength Titanium Alloy
  • Heat Treatable
  • Good Ductility
  • Good Machinability
  • Good Weldability

We stock and sell Grade 5 Titanium Alloy Seamless Tubes, Forged Seamless Tubes, Welded Tubes, etc.

Contacter Daxun maintenant

Advanced Production: Forged Titanium Alloy Tube

Forged Titanium Seamless Tubes: Diameters range from 100mm to 1219mm, wall thickness ranges from 5mm to 100mm (depending on diameter), lengths up to 2000mm, made from Grade 5 Titanium. Forged Titanium alloy tubes undergo multiple forgings to achieve more uniform grains and metallographic structures, better performance and stability, and are finally heat treated. Before the finished products are packaged according to customer specifications, they undergo mechanical testing, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing. Manufacturing technology as well as inspection and testing equipment ensure that forged 6-4 titanium tubes meet ASTM and ASME specifications.

Contacter Daxun maintenant

Rapports d'essais

The test reports we provide include: Factory test certificate for Grade 5 Titanium Seamless Pipe and Ti-6al-4v Titanium Seamless Pipe, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, NABL Approved Laboratory Report, Destructive Test Report, Non-destructive Testing Report. (DaXun will provide according to customer requirements)

Contacter Daxun maintenant

Applications et normes

Grade 5 titanium tubes are widely used in the following industries under extreme corrosive conditions:

  • Chemical processing parts, military industry, aerospace, chemical energy, marine engineering, oil and gas industry, rockets and missiles, military armor, ships and vessels, industrial machinery, power industry, paper and pulp industry, pharmaceutical and food processing equipment, etc.
  • Spécifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
  • Standards: ASTM, GB, GJB, ASME and API
Contacter Daxun maintenant

Qualité, livraison, inspection

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 1 Titanium Welded Pipe and Grade 1 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • Nos délais de livraison sont strictement conformes au contrat.
  • Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
  • Prise en charge d'échantillons gratuits pour les essais des clients
  • Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Contacter Daxun maintenant

Emballage

Daxun Alloy ensures the best quality of titanium tube packaging, because it plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Boîtes et caisses
- Emballage rétractable
- Palettes en bois
- Boîtes en bois

Contacter Daxun maintenant

Support technique

Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.

Grade 5 Titanium TUBE Features

Haute résistance
Résistance à la corrosion
Résistance à la chaleur
Résistance aux basses températures
Protection de l'environnement
Léger

Daxun Grade 5 Titanium TUBE Let your brand improve rapidly

Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of pipe/tube Bar and Tube.
Norme relative aux produits/transformations Qualité/taille
Titanium pipe/tube, — ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Epaisseur :( 0.0197”-6”)Largeur maximale : 12 pieds,Longueur maximale : 50 pieds)
AMS-T-9046
Titanium and Titanium alloy pipe/tube
Titane commercialement pur (CP)
Désignation du code Limite d'élasticité
minimum, ksi 1 /
CP-1 70
CP-2 55
CP-3 40
CP-4 25
Alliages de titane alpha(A)
Désignation du code Composition
A-1 5A1-2,5Sn
A-2 5A1-2,5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0,8Mo
A-4 8A1-1Mo-1V
Alliages de titane alpha-bêta (AB)
Désignation du code Composition
AB-1 6A1-4V
AB-2 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2,5V
AB-6 8Mn
Alliages de titane bêta(B)
Désignation du code Composition
B-1 13V-11Cr-3A1
B-2 11,5Mo-6Zr-4,5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
Traitement :
Laminage à chaud Laminage à froid
Classes disponibles :
CP grade 1 Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP grade 2 Grade 6Al-4V ELI (anciennement grade 23)
7e année Grade 6Al-6V-2Sn (6-62)
19e année Grade 8Al-1Mo-1V (8-1-1)
Grade 5 (6Al-4V) 9e année (3Al-2,5V)
Grade 6 (5Al-2.5Sn) CP grade 3
Application
Industrie chimique Dessalement de l'eau de mer
Industrie pétrochimique Aérospatiale
Domaine de l'usinage, domaine de l'automobile Téléphone mobile Champ des composants.
urface Finish Internal Surface(ID) Exterbal Surface(OD)
Roughness Average(RA) Roughness Average(RA)
μ inch μm μ inch μm
BA Beight Annealed 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
EP Electro Polish 15,10,7,5 0.38,0.25,0.20;0.13 32 0.8
MP Mechanical Polish 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
AP Annealed & Pickled Not defined Not defined 40 or Not defined 1.0 or Not defined
Titanium Grade 5 Seamless Pipe Titanium DIN 3.7165 Seamless Pipe
Titanium UNS R56400 Seamless Pipe
Titanium Grade 5 Seamless Pipes
Titanium Alloy Gr.5 Seamless Pipe
ASTM B337 Titanium Grade 5 Seamless Pipe
ASME SB337 Ti Alloy Gr.5 Seamless Pipes
Titanium Grade 5 Welded Pipe Titanium DIN 3.7165 Welded Pipe
Titanium UNS R56400 Welded Pipe
Titanium Grade 5 Welded Pipes
Titanium Alloy Gr.5 Welded Pipe
ASTM B337 Titanium Grade 5 Welded Pipes
ASME SB337 Ti Alloy Gr.5 Welded Pipes
Titanium Grade 5 Round Pipe Titanium DIN 3.7165 Round Pipe
Titanium UNS R56400 Round Pipes
Titanium Grade 5 Round Pipes
Titanium Alloy Gr.5 Round Pipe
Titanium Grade 5 Round Pipe
Ti Alloy Gr.5 Round Pipes
Titanium Gr.5 Seamless Tubes Titanium DIN 3.7165 Seamless Tubes
Titanium UNS R56400 Seamless Tubes
Titanium Grade 5 Seamless Tubing
Titanium Alloy Gr.5 Seamless Tubes
ASTM B338 Titanium Gr.5 Seamless Tubing
ASME SB338 Ti Alloy Grade 5 Seamless Tubes
Titanium Grade 5 Welded Tubes Titanium DIN 3.7165 Welded Tubes
Titanium UNS R56400 Welded Tubes
Titanium Grade 5 Welded Tubing
Titanium Alloy Gr.5 Welded Tubes
ASTM B338 Titanium Grade 5 Welded Tubing
ASME SB338 Ti Alloy Gr.5 Welded Tubes
Titanium Grade 5 Round Tubes Titanium DIN 3.7165 Round Tubes
Titanium UNS R56400 Round Tubes
Titanium Grade 5 Round Tubing
Titanium Alloy Gr.5 Round Tubes
Titanium Grade 5 Round Tubing
Ti Alloy Gr.5 Round Tubes
Titanium Grade 5 Pipe Titanium DIN 3.7165 Pipe
Titanium UNS R56400 Pipes
Titanium Grade 5 Pipe
Titanium Alloy Gr.5 Pipes
Titanium Grade 5 Pipes
Ti Alloy Gr.5 Pipe
Titanium Grade 5 Tube Titanium DIN 3.7165 Tubes
Titanium UNS R56400 Tube
Titanium Grade 5 Tubing
Titanium Alloy Gr.5 Tubes
Titanium Grade 5 Tubes
Ti Alloy Gr.5 Tubes

 

NPS Outside Diameter Épaisseur de la paroi Weight Weight
in mm in mm Sched kg/Mtr Lb/ft
1/2″ 0.84 21 0.109 2.769 40 STD 1.268 0.851
0.147 3.734 80 STD 1.621 1.088
3/4″ 1.05 27 0.113 2.87 40 STD 1.684 1.131
0.154 3.912 80 STD 2.195 1.474
1″ 1.315 33 0.133 3.378 40 STD 2.501 1.679
0.179 4.547 80 STD 3.325 2.172
1 1/4″ 1.66 42 0.14 3.556 40 STD 3.385 2.273
0.191 4.851 80 STD 4.464 2.997
1 1/2″ 1.9 48 0.145 3.683 40 STD 4.048 2.718
0.2 5.08 80 STD 5.409 3.361
2″ 2.375 60 0.154 3.912 40 STD 5.441 3.653
0.218 5.537 80 STD 7.48 5.022
2 1/2″ 2.875 73 0.203 5.516 40 STD 8.629 5.793
0.276 7.01 80 STD 11.411 7.661
3″ 3.5 89 0.216 5.486 40 STD 11.284 7.576
0.3 7.62 80 STD 15.272 10.253
4″ 4.5 114 0.237 6.02 16.073 10.79
0.337 8.56 22.318 14.983
6″ 6.625 168 0.188 4.775 19.252 12.924
0.203 5.516 20.739 13.923
0.219 5.563 22.318 14.983
0.25 6.35 25.354 17.021
0.28 7.112 40 STD 58.263 18.974
0.312 7.925 31.334 21.036
0.375 9.525 37.285 25.031
0.432 10.973 80 XHY 42.561 28.573
0.5 12.7 48.719 32.708
8″ 8.625 219 0.188 4.775 25.233 16.94
0.203 5.156 27.198 18.259
0.219 5.563 29.286 19.661
0.25 6.35 20 33.308 22.361
0.277 7.036 30 36.786 24.696
0.322 8.179 40 42.352 28.554
0.375 9.525 49.216 33.041
0.406 10.312 60 53.085 35.638
0.5 12.7 80 XHY 64.627 43.388
10″ 10.75 273 0.188 4.775 31.588 21.207
0.219 5.563 36.689 24.631
0.25 6.35 20 41.759 28.035
0.307 7.798 30 51.002 34.24
0.344 8.738 56.946 38.231
0.365 9.271 40 STD 63.301 40.483
0.438 11.125 71.852 48.238
0.5 12.7 60 XHY 81.53 54.735
0.594 15.088 80 95.969 64.429
12″ 12.75 324 0.188 4.775 37.57 25.222
0.219 5.563 43.657 29.309
0.25 6.35 49.713 33.375
0.281 7.137 55.739 37.42
0.312 7.925 61.735 41.445
0.375 9.525 73.824 49.562
0.406 10.312 79.727 53.525
0.5 12.7 97.438 65.415
0.562 14.275 108.966 73.154
14″ 14 356 0.188 4.775 41.308 27.732
0.219 5.563 48.012 32.233
0.25 6.35 20 54.685 36.713
0.281 7.137 61.327 41.172
0.312 7.925 67.939 45.611
0.375 9.525 STD 81.281 54.568
0.438 11.125 40 94.498 63.441
0.5 12.7 XHY 107.381 72.09
0.625 15.875 132.983 89.278
16” 16 406 0.188 4.775 47.29 21.748
0.219 5.563 54.98 36.91
0.25 6.35 10 62.639 42.053
0.281 7.137 70.268 47.174
0.312 7.925 20 77.866 52.275
0.344 8.738 85.677 57.519
0.375 9.525 30 93.213 62.578
STD
0.438 11.125 108.433 72.797
0.5 12.7 40 123.289 82.77
XHY
18″ 18 457 0.219 5.563 61.948 41.588
0.25 6.35 70.593 47.393
0.281 7.137 79.208 53.176
0.312 7.925 20 87.792 58.939
0.375 9.525 STD 105.144 70.588
0.438 11.125 30 122.369 82.152
0.5 12.7 XHY 139.198 93.45
0.562 14.275 40 155.904 104.666
0.625 15.875 172.754 115.978
20″ 20 508 0.25 6.35 78.547 52.733
0.282 7.163 88.458 59.386
0.312 7.925 97.719 65.604
0.375 9.525 20 STD 117.075 78.598
0.438 11.125 136.305 91.508
0.5 12.7 30 XHY 155.106 104.13
0.594 15.088 40 183.378 123.11
0.625 15.875 192.64 129.328
0.688 17.475 211.368 141.901
24″ 24 610 0.25 6.35 94.456 63.413
0.281 7.137 106.029 71.183
0.312 7.925 117.573 18.932
0.375 9.525 20 STD 140.938 64.618
0.438 11.125 164.176 110.219
0.5 12.7 XHY 186.923 125.49
0.625 15.875 232.41 156.028
0.688 17.475 40 255.148 171.293
0.75 19.05 277.401 186.233
30″ 30 762 0.25 6.35 118.318 79.433
0.281 7.137 132.851 89.189
0.312 7.925 10 147.353 98.925
0.375 9.525 STD 176.731 118.648
0.438 11.125 205.983 138.286
0.5 12.7 20 XHY 234.647 157.53
0.625 15.875 30 292.066 196.078
0.688 17.475 320.817 215.38
0.75 19.05 348.988 234.293
36″ 36 914 0.25 6.35 142.18 95.453
0.281 7.137 159.672 107.196
0.312 7.925 10 177.133 118.918
0.375 9.525 STD 215.525 142.678
0.438 11.125 247.79 166.353
0.5 12.7 20 XHY 282.372 198.57
0.625 15.875 351.723 236.128
0.688 17.475 386.487 259.467
0.75 19.05 420.576 282.353
42″ 42 1067 0.312 7.925 206.914 138.911
0.375 9.525 STD 248.319 166.708
0.5 12.7 XHY 33.097 221.61
0.75 19.05 492.163 330.413
48″ 48 1219 0.375 9.525 STD 284.112 190.738
0.438 11.125 331.404 222.487
0.5 12.7 XHY 377.822 253.65
0.75 19.05 563.75 378.473
0.875 22.225 655.969 440.383

Grade 2 titanium tube form (4)

  • Titanium seamless pipe is made by perforating and drawing solid titanium rod, and the hollow part of the pipe is made by perforation or hot extrusion process. Titanium seamless pipe is an ideal choice for very large diameter to wall thickness ratio and has very good external dimension tolerance.

  • Le tube soudé en titane est un produit tubulaire fabriqué à partir de bandes de titane formées par laminage et soudées par fusion le long du joint longitudinal. Le procédé de soudage utilisé par Daxun Alloy n'utilise pas de métal d'apport pendant le processus de soudage.

  • Les tubes carrés en titane sont étirés à partir de tubes ronds ou de billettes de tubes ronds et peuvent être formés en angles droits ou arrondis. Ils peuvent également être extrudés à froid, ce qui est efficace et peu coûteux. Le seul inconvénient est que la tolérance augmente progressivement.

  • Les produits tubulaires sont soudés puis ré-étirés à la taille finale. Le soudage et l'étirage sont idéaux pour produire des tubes à parois épaisses et de grand diamètre qui ne peuvent pas être soudés directement à la dimension voulue, mais qui permettent néanmoins de réaliser des économies par rapport aux tubes sans soudure. Tous les tubes soudés et étirés de Daxun sont recuits brillamment.

Informations disponibles pour référence et téléchargement

Daxun is a reliable manufacturer of grade 5 titanium tubes

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel plates have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

Projets et produits récents

Tubes et tuyaux en titane de grade 5
Tubes et tuyaux en titane de grade 5
6al 4v Titanium pipe and tube
Titanium pipe and tube 6al 4v
6al 4v Titanium pipe and tube
6al 4v Titanium pipe and tube
Titanium pipe and tube 6al 4v
Titanium pipe and tube 6al 4v
Titanium pipe and tube 6al 4v
Commercially Pure Titanium Tube Grade 5/UNS R56400/Ti-6AL-4V

Ti-6Al-4V- Grade 5 Titanium tube

  • Titanium Alloy-(UNS R56400)

INTRODUCTION

  • DAXUN Ti-6Al-4V, Grade 5 Alloy Tube (UNS R56400) is the most popular titanium alloy. It is a duplex alpha+beta titanium alloy that uses aluminium as an alpha stabiliser and vanadium as a beta stabiliser. This high-strength alloy can be employed at cryogenic temperatures of around 800°F (427°C). ATI Ti-6Al-4V, Grade 5 alloy is used in annealing, solution treatment, and ageing. Compressor blades, discs, and rings for jet engines; fuselage and space capsule components; pressure containers; rocket engine cases; helicopter rotor hubs; fasteners; and crucial forgings with a high strength-to-weight ratio.
  • The alloy is initially melted using vacuum arc (VAR), electron beam (EB) or plasma arc hearth melting (PAM). Remelting is achieved in one or two vacuum arc steps.

CARACTÉRISTIQUES TECHNIQUES

•ASTE B338 – Tubes Titanium tubes standard heat treatable
• AMS 4928 – Forgings and forging stock (annealed)
• AMS 4965 – Forgings (solution treated and aged)
• AMS 4967 – Forgings (annealed, heat treatable)

PROPRIÉTÉS PHYSIQUES

  • Melting Range: 2,800-3,000°F (1,538 – 1,649°C)
  • Density: 0.160 lbs/cu. in.; 4.47 gm/cc
  • Beta Transus Temperature: 1830°F (± 25°); 999°C (± 14°)

TRAITEMENT THERMIQUE

  • Annealing at 1,700-1,900°F (927 – 1,038°C) is done where high hardness, tensile and fatigue strength are desired.
  • DAXUN 6-4™, Grade 5 Alloy can be heat treated in several ways.
  • 1. Anneal: 1,275 -1,400°F; (691 – 760°C), ½ to 2 hours, air or furnace cool
  • 2. Stress Relief Anneal: 1,000 -1,200°F; (538 – 649°C), 1 to 8 hours, air or furnace cool
  • 3. Solution Heat Treatment: 1,675 -1,750°F; (913 – 954°C), 1 hour, water quench
  • 4. Aging Treatment: 975 -1,025°F; (524 – 552°C), 4 to 8 hours – air cool
  • The very best of properties In the solution treated and aged condition, small cross sections are obtained that are rapidly
    quenched. Larger sections sizes and/or a quench delay may cause properties to be lower than the optimum values.

DURETE

Typical hardness in the annealed condition is Rockwell C 30-34, and about Rockwell C 35-39 in the solution and aged condition.

FORGEABILITY/ FORMABILITY

  • DAXUN Ti-6Al-4V, Grade 5 alloy tubes are forged at 1,750°F (954°C), with an end forging temperature of 1,450°F (788°C). For optimal results, a reduction of at least 35% is recommended.
  • DAXUN Ti-6Al-4V, Grade 5 alloy is difficult to form at room temperature, even when annealed. As a result, harsh forming operations like bending or stretching can be conducted on annealed material at temperatures as high as 1,200°F (649°C) without altering its mechanical qualities. Creep forming can be used for hot sizing or forming at temperatures ranging from 1,000 to 1,200°F (538 to 649°C).

MACHINABILITY

  • DAXUN  Ti-6Al-4V, Grade 5 alloy can be machined using practices for austenitic stainless steels with slow speeds, heavy feeds, rigid
    tooling, and large amounts of non-chlorinated cutting fluid.

SOUDABILITÉ

  • DAXUN Ti-6Al-4V Grade 5 Alloy Titanium Tube is easily welded in the annealed or solution and partially aged form, with ageing.
  • done during the post-weld heat treatment. Precautions must be made to avoid contamination by oxygen, nitrogen, and hydrogen. Fusion welding can be performed in an inert gas-filled chamber or with an inert gas tail shield applied to the molten metal and nearby hot zone. Spot welding, seam welding, and flash welding can all be performed without the use of a protective environment.

SPECIAL PRECAUTIONS

  • DAXUN Ti-6Al-4V, Grade 5 alloy may be contaminated with hydrogen as a result of incorrect pickling, as well as the absorption of oxygen, nitrogen, and carbon during forging, heat treatment, brazing, and so on. This contamination may reduce ductility, compromising notch sensitivity and forming properties.
Quelle est la meilleure qualité de titane ?

La qualité de l'alliage de titane dont vous avez besoin dépend du projet sur lequel vous travaillez, car chaque qualité présente des avantages différents.

Toutes les qualités d'alliage de titane sont extrêmement solides et résistantes à la corrosion, ce qui signifie qu'elles continueront à fonctionner dans les conditions les plus difficiles.

Les grades supérieurs d'alliage de titane (5-12) sont des alliages conçus pour des avantages spécifiques. Par exemple, l'alliage de titane de grade 12 présente une excellente résistance à la chaleur, ce qui en fait un choix parfait pour les échangeurs de chaleur à calandre et à tube, les tuyauteries hydrauliques et les équipements de l'industrie chimique.

Les grades 1 à 4 sont des alliages de titane pur et constituent un choix idéal si vous avez besoin d'un matériau ductile et soudable pour les systèmes de tuyauterie et les tubes. Les grades inférieurs sont utilisés dans la marine et l'industrie.

Si vous démarrez un projet et que vous ne savez pas quelle qualité d'alliage de titane vous convient le mieux, contactez-nous dès aujourd'hui ; nous nous ferons un plaisir de vous aider.

En quoi les qualités supérieures de titane sont-elles différentes des qualités inférieures ?

Chez DAXUN, nous proposons une large gamme d'alliages de titane allant de la nuance 1 à la nuance 12.

Les grades 1 à 4 sont du titane pur, tandis que les grades supérieurs sont des alliages.

Les alliages sont appréciés pour leur rapport résistance/poids élevé.

La nuance d'alliage de titane la plus couramment utilisée est la nuance 5. Bien qu'elle soit encore riche en titane, cette nuance est l'une des plus fiables car elle peut résister à des températures allant jusqu'à 600°F et à des conditions extrêmes.

Les qualités supérieures sont privilégiées par les industries telles que l'aérospatiale et la marine pour leur résistance à l'usure et à la corrosion.

Inversement, les qualités inférieures sont principalement utilisées pour le soudage en raison de leur faible résistance.

Pour en savoir plus sur les différences entre les différents grades d'alliage de titane, appelez +86 13382898899 aujourd'hui pour parler directement à nos experts.

La qualité du titane a-t-elle une incidence sur le coût ?

Bien que la qualité du titane augmente légèrement le coût, le coût total est principalement déterminé par la forme du titane dont vous avez besoin.

DAXUN propose une large gamme de produits en titane, notamment des plaques, des tubes, des bobines et des barres. La longueur, la largeur et la quantité de chaque article dont vous avez besoin influencent le montant que vous payez à la caisse.

Malheureusement, il est difficile d'établir un prix en ligne sans en savoir plus sur votre projet et sur l'utilisation du titane.

Heureusement, notre équipe d'experts est toujours là pour vous aider et vous conseiller dans vos besoins en titane. En envoyant un e-mail à [email protected], nous pourrons vous donner des conseils et un devis précis.

Veillez à inclure autant d'informations que possible sur le grade, la forme et la quantité de titane dont vous avez besoin afin d'obtenir une meilleure compréhension de vos besoins.

Où puis-je en savoir plus sur les qualités de titane ?

L'équipe de DAXUN est expérimentée, compétente et sympathique. Forte de ses années d'expérience dans l'industrie, elle connaît parfaitement le titane, notamment ses utilisations, ses avantages et ses qualités.

Pour des mises à jour régulières sur le titane, ses utilisations et ses applications dans tous les secteurs, ne manquez pas de consulter notre blog. Nos experts ont rédigé des guides faciles à suivre auxquels vous pouvez toujours vous référer lorsque vous avez des questions.

Si vous rencontrez encore des difficultés, n'hésitez pas à nous contacter, nous nous ferons un plaisir de vous aider.

En envoyant un courriel à [email protected], vous recevrez une réponse rapide. Veillez à donner le plus de détails possible dans votre question afin que nous puissions vous recommander une solution adaptée.

Comment obtenir un devis OU comprendre les informations du marché le plus rapidement possible ?

Veuillez remplir le formulaire de la page “Contactez-nous” ou appeler notre responsable des ventes au “+86 13382898899”, nous vous contacterons dans les plus brefs délais. Notre WhatsApp est en ligne, et l'email ([email protected]) sera vérifié dans les 6 heures. Chaque demande ou message recevra une réponse rapide. En outre, nous partageons chaque semaine des informations sur le marché avec nos clients

Puis-je obtenir des échantillons ?

We can provide stainless steel pipe/tube samples for you to check the quality. Sample is free and you just pay the freight.

Quels sont les pays que vous avez déjà exportés ?

Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.

Quel est votre MOQ ?

Our MOQ is 1 ton for stainless steel pipe/tube

Quel est le délai de livraison ?

Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.

Envoyez votre demande dès aujourd'hui
Devis rapide