Daxun is an excellent manufacturer of grade 7 (Ti-0.15Pd) titanium rods and bars.
- Titanium bar grade: Grade 7-Ti / UNS R52400
- Types de barres de titane : barres laminées, barres étirées, barres de titane forgées
- Titanium bar density: The density of grade 7 titanium is 4.51 g/cm³
- Principales normes : ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
- High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.
Le leader mondial des services de fabrication de barres de titane commercialement pur
Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 7 titanium alloy rods.
Grade 7 titanium bar (Ti Grade 7 / UNS R52400) is a palladium-enhanced, commercially pure (CP) titanium alloy specifically engineered for supreme corrosion resistance in aggressive environments. It consists of titanium (≥99%) with a critical addition of 0.12–0.25% palladium (Pd), which fundamentally alters its electrochemical behavior. This palladium modification dramatically improves resistance to reducing acids (e.g., sulfuric, hydrochloric, phosphoric), chloride solutions (including seawater and brines), and crevice/pitting corrosion—scenarios where standard CP grades like Grade 2 would rapidly degrade. While retaining the inherent advantages of titanium—low density (~4.5 g/cm³), high strength-to-weight ratio, excellent weldability, and biocompatibility—Grade 7 exhibits superior performance at elevated temperatures (up to ~400°C/750°F) and in highly oxidizing or acidic conditions. Its passive oxide layer, stabilized by palladium, provides unparalleled protection against chemical attack, making it one of the most corrosion-resistant metallic materials available.
Where is Grade 7 titanium bar used?
Grade 7 titanium bar is extensively used in chemical processing for critical components like valve stems, pump shafts, fasteners, and instrumentation components handling acids, chlorides, or organic solvents. In marine and offshore engineering, it serves in seawater desalination equipment, heat exchanger components, and subsea fastening systems exposed to high-salinity environments. The alloy also excels in pollution control systems (e.g., scrubber components), pharmaceutical manufacturing equipment, and medical implants (e.g., surgical instruments and orthopedic devices) due to its inertness and longevity. Despite its higher initial cost—driven by palladium content—Grade 7 delivers exceptional lifecycle value by minimizing downtime, maintenance, and replacement costs in corrosive service. Its reliability in preventing catastrophic failures ensures safety and efficiency in applications ranging from nuclear waste containment to aerospace fluid systems, justifying its selection as a premium solution for the most demanding corrosion challenges.
Daxun est votre société de confiance pour la production de barres d'alliage de titane. Daxun produit toutes les catégories d'alliages de titane, y compris le titane commercialement pur de la série CP, la série d'alliages de titane, l'alliage de titane et de nickel, etc. Ils ont des performances fiables et fournissent des performances élevées pour vos applications critiques. Dans diverses industries et applications, vous pouvez compter sur les barres d'alliage de titane de Daxun pour une résistance élevée, des températures élevées et des environnements corrosifs. Depuis des décennies, Daxun Metals s'engage à produire des solutions d'alliage de titane de haute technicité pour répondre aux défis les plus sévères.
Données
- Paramètres
- Ingrédient
- Propriétés mécaniques
- Propriétés physiques
| Spécifications | Détails |
|---|---|
| Matériau | Titanium rod and bar Grade 7 (UNS R52400) |
| Standard | ASTM B348, ASTM SB348, AMS 4921, AMS 4902 |
| Dimensions | EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN |
| Gamme de diamètres | 0.125″ - 14″ (3.175mm - 355.6mm), sur mesure |
| Longueur Plage | Jusqu'à 240″ (6096mm), sur mesure |
| Finition | Etiré à froid (brillant), rectifié sans centre, laminé à chaud, tourné lisse, pelé, bord laminé fendu, recuit laminé à chaud, tourné brut, brillant, poli, rectifié, rectifié sans centre et noir. |
| Finition de la surface | Étiré à froid, rectifié sans centre, poli ou tourné brut, noir, finition NO.4, finition BA, finition mate, etc. |
| Condition | Trempé et revenu, recuit |
| Tolérance | Tolérance sur le diamètre : +/- 0.005″ (0.127mm), tolérance sur la longueur : +/- 0.125″ (3.175mm) |
| Formulaire | Barres carrées en titane, lingots de titane, barres rondes en titane, barres rectangulaires en titane, barres triangulaires en titane, barres forgées en titane, barres hexagonales en titane, etc. |
| Élément | Symbol | Gamme de composition (wt.%) |
|---|---|---|
| Titane | Ti | Balance (>99%) |
| Palladium | Pd | 0.12–0.25% |
| Iron | Fe | ≤0.30% |
| Oxygen | O | ≤0.25% |
| Carbone | C | ≤0.08% |
| Azote | N | ≤0.03% |
| Hydrogen | H | ≤0.015% |
| Autres éléments | Each | ≤0.40% (single element) |
| Propriété | Valeur (impériale) | Valeur (métrique) |
|---|---|---|
| Résistance à la traction | 50,000–65,000 psi | 345–450 MPa |
| Limite d'élasticité | 30,000–45,000 psi | 207–310 MPa |
| Élongation | 20-30% | 20-30% |
| Dureté (Brinell) | 120–160 HB | 120–160 HB |
| Module d'élasticité | 14.9–16.0 × 10⁶ psi | 103–110 GPa |
| Propriété | Valeur (impériale) | Valeur (métrique) |
|---|---|---|
| Densité | 0.163 lb/in³ | 4.51 g/cm³ |
| Point de fusion | 3,000-3,050°F | 1,650-1,680°C |
| Conductivité thermique | 9.5 Btu/(hr·ft·°F) | 16.4 W/(m·K) |
| Coefficient de dilatation thermique | 4.8 × 10⁻⁶/°F | 8.6 × 10⁻⁶/K |
| Résistivité électrique | 1.78 × 10⁻⁶ Ω·cm | 1.78 μΩ·m |
Choisissez Daxun pour faire décoller votre projet.
DAXUN® Grade 7 Titanium Rod Features
DAXUN® Ti Grade 5 est une barre en alliage de titane (6al-4v) :
- Bonne aptitude au formage à chaud et à la soudure ;
- La résistance à la traction peut atteindre 1000MPa ;
- Travail dimensionnel à haute température
- Insensible à l'eau de mer ou à l'eau de mer ;
- N'est pas affecté par divers milieux corrosifs ;
- Haute résistance et bonne ténacité ;
- Résister à l'apparition et à la propagation de fissures.
Avantages de l'usine de Daxun
Le concept de “gestion de l'excellence des performances” de Daxun promeut le modèle de gestion “PDCA + Lean”. La carte de visite de l'entreprise indique “Daxun = Qualité fiable”. Daxun utilise le système ERP pour assurer la traçabilité complète de la variété, de la spécification et de l'origine de chaque tige de titane, et préconise et encourage la lutte contre la contrefaçon dans l'industrie. Daxun s'appuie sur la technologie pour le traitement et la personnalisation, et la haute précision et la haute qualité sont les références de l'industrie ; en termes de service, elle promeut la gestion du cycle de vie des produits, fournit une sélection professionnelle des matériaux et des solutions de traitement avant les ventes, assure un suivi strict pendant les ventes et fournit des garanties de service sans souci après les ventes.
Grade 7 Titanium Rod Production Method
Daxun produit des barres de titane de haute qualité et de haute performance, et peut également fabriquer selon l'accord du client :
- Les lingots de titane doivent subir un traitement thermique et un usinage, des essais ultrasoniques par immersion, des essais de propriétés mécaniques, une inspection structurelle macroscopique et microscopique et d'autres processus. Processus de production : barres de titane laminées à chaud - haute efficacité, performances stables, barres de titane forgées - taille flexible, forgeage à feu multiple, amélioration des performances globales des barres de titane, barres de titane étirées à froid - généralement des barres de titane de haute précision de petite taille ; les barres de titane susmentionnées sont toutes livrées avec une surface brillante.
Rapports d'essais
Les rapports d'essai que nous fournissons comprennent : Certificat de test d'usine pour les barres rondes en titane de grade 2 et les barres rondes en titane de grade 2, EN 10204 3.1, rapport chimique, rapport mécanique, rapport de test PMI, rapport d'inspection visuelle, rapport d'inspection par une tierce partie, rapport de laboratoire approuvé par la NABL, rapport de test destructif, rapport de test non destructif. (Daxun fournira selon les exigences du client)
Grade 7 Rods Applications and Standards
Grade 7 Titanium Rods are widely used in the following industries under extreme corrosive conditions:
- Aérospatiale, construction navale, industrie pétrolière et gazière, génie maritime, usines chimiques, machines industrielles, industrie énergétique, industrie du papier et de la pâte à papier, industrie agroalimentaire, raffineries, industrie militaire, équipements pharmaceutiques et agroalimentaires, etc.
- Spécifications : AMS 4928,AMS 4967,AMS 4965 ,AMS 6931 ,ASTM B 348
- Normes : ASTM, ASME, EN, JIS, DIN, GB, GJB, API
Qualité, livraison, inspection
Daxun effectue plusieurs tests d'assurance qualité, notamment des tests mécaniques tels que la traction sur zone, l'analyse chimique, l'identification positive du matériau, le test PMI, les tests micro et macro, le test de corrosion intergranulaire (IGC), le test de détection des défauts par ultrasons, le test de résistance aux piqûres, le test de dureté, l'identification positive du matériau, le test de dilatation, etc. Tous ces tests garantissent que les barres en titane de grade 2 et les barres rondes en titane de grade 2 sont adaptées à l'application requise. Au cours du processus de production, nous mesurons le diamètre, l'épaisseur et la surface du produit.
- Nos délais de livraison sont strictement conformes au contrat.
- Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
- Prise en charge d'échantillons gratuits pour les essais des clients
- Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Emballage
Daxun Alloy garantit la meilleure qualité d'emballage, car celui-ci joue un rôle important dans le fret international, où les marchandises passent par différents canaux avant d'atteindre leur destination finale ; nous accordons donc une attention particulière à l'emballage. Nous emballons nos marchandises de différentes manières, en fonction du produit. Nous emballons nos produits de différentes manières, notamment :
- Boîtes et caisses
- Emballage rétractable
- Palettes en bois
- Boîtes en bois
Support technique
Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.
Daxun Grade 7 Titanium Rods help your brand improve quickly
- Tolerances for Grade 7 Titanium Round Bars (BS EN ISO 286-2)
| TAILLE NOMINALE | h5 | h6 | h7 | h8 | h9 | H10 | H11 | h12 |
|---|---|---|---|---|---|---|---|---|
| DIAMÈTRE mm | ||||||||
| ~ à 3 | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| plus de 3 à 6 ans | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| plus de 6 à 10 | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| plus de 10 ans à 18 ans | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| plus de 18 ans à 30 ans | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| plus de 30 à 50 | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| plus de 50 à 80 | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| plus de 80 à 120 | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| plus de 120 à 180 | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| plus de 180 à 250 | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
Types of Grade 7 Titanium Rods (3)
Tige en titane
Projets et produits récents
Produits apparentés (8)
Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 7 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.
CARACTÉRISTIQUES TECHNIQUES
ASTM B348 – Titanium and Titanium Alloy Bars and Billets
ASTM SB348 – Specification for Titanium and Titanium Alloy Bars and Billets
AMS 4921 – Titanium Alloy Bars, Wire, and Forgings
AMS 4902 – Titanium Alloy Bars and Billets
TRAITEMENT THERMIQUE
When enhanced corrosion resistance and mechanical properties are required, annealing can be performed at 1,200-1,400°F (649-760°C).
DAXUN Grade 7 alloy can be heat treated in a variety of ways:
- Anneal: 1,200-1,400°F (649-760°C), 1 to 2 hours, air cool
- Stress Relief Anneal: 900-1,100°F (482-593°C), 1 to 4 hours, air cool
DURETE
Typical hardness in the annealed condition is Rockwell B 70-80, providing excellent machinability while maintaining superior corrosion resistance.
Forgeabilité / Formabilité
Grade 7 titanium alloy bar is forged at 1,650-1,750°F (899-954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 30% reduction is recommended for optimum properties.
Grade 7 alloy bar exhibits good formability in the annealed condition. For severe forming operations such as bending or stretching, these can be performed at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000-1,200°F (538-649°C).
Usinabilité
Grade 7 titanium alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids. The palladium content does not significantly affect machinability compared to other CP titanium grades.
Soudabilité
Grade 7 titanium rod is readily weldable in the annealed condition. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. The palladium addition enhances weld integrity in corrosive environments.
Considérations particulières
Grade 7 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics. The palladium content provides additional protection against corrosion in contaminated conditions.
Gamme de tailles
Grade 7 Titanium Bar Dimensions
Ø 0,7 - 30 mm (étiré, rectifié)
Ø 16 - 400 mm (laminé à chaud, pelé)
Tolérances : h11-h5 (ISO 286-2)
Des tolérances plus étroites ou différentes sont disponibles sur demande
Longueurs jusqu'à 9 000 mm, en fonction du diamètre
Pour les diamètres plus importants, d'autres longueurs de barres et tolérances peuvent être convenues sur demande.
Availability Grade 7 Titanium Rods
Les options de traitement comprennent
- Dessin, redressement
- Dessiner, redresser, polir
- Dessin, meulage, polissage
- Étirage, redressement, meulage, polissage
- Etirage, recuit, redressage
- Étirage, recuit, polissage
- Etirage, recuit, meulage, polissage
- Etirage, recuit, redressage, meulage, polissage
Nous produisons des barres selon vos exigences.
Excellente surface et rectitude, rondeur parfaite et tolérances de diamètre les plus étroites (selon ISO 286-2 jusqu'à h5). Disponible en version redressée, rectifiée et polie.
Sciage
- Scies à ruban (jusqu'à Ø510 mm)
- Bench band saws (up to 6,000 x 3,000 x 400 mm)
- Des machines à scier performantes pour un sciage précis
Usinage des extrémités de barres en titane
- Simple ou double face
- Chanfrein 90° (45°)
- Point 60° (30°)
- Extrémité plate
- Centré
Formulaire de livraison
- ASTM Normes de l'American Society for Testing and Materials
- AMS Normes américaines sur les matériaux aérospatiaux
- NACE American Association of Corrosion Engineers Normes internationales
- ASME Normes de l'American Society of Mechanical Engineers
- GB Normes nationales chinoises
- GJB Normes militaires nationales chinoises
- ISO Normes internationales
- DIN Normes allemandes
- FR Normes européennes
- API Normes de l'American Petroleum Institute
Méthode de détection
Essais non destructifs > Essai 100%
Méthodes d'essai :
- Contrôle par courants de Foucault / contrôle des fissures par courants de Foucault
- Surface sans défaut (niveau 4)
- Diamètre des trous à fond plat : 0,7 mm et 0,4 mm
- La zone aveugle peut être coupée selon une longueur fixe > Test jusqu'à la fin de la barre
- Contrôle par ultrasons sur tout le diamètre
Nos services de matériaux pour barres de titane
En tant que centre de service expérimenté, nous pouvons adapter votre barre de titane à vos spécifications, travailler avec différents organismes de certification tels que TÜV Rheinland ou DNV d'approuver les spécifications et de lancer la modernisation des produits semi-finis en titane pour répondre aux applications appropriées.
Nous nous ferons un plaisir de vous conseiller et de vous expliquer tout ce que vous devez savoir sur l'obtention d'un permis de conduire. Grade 7 titanium bar material, including which standards require greater attention for the components to be manufactured.
Si vous avez un engagement d'approvisionnement à long terme, vous pouvez établir un accord-cadre avec Daxun. Nous garantissons les prix et les quantités pour une période déterminée.
Bénéficiez de notre vaste expérience sur le marché mondial. Nous aidons les entreprises du monde entier depuis 2003. Si vous avez besoin d'informations complémentaires sur Grade 7 Titanium Bar, Nos professionnels se feront un plaisir de vous aider. Nous nous réjouissons d'ores et déjà de votre appel.
Informations sur les commandes
Les bons de commande doivent mentionner la quantité, la qualité, le type ou la catégorie, la référence API5L, l'épaisseur, la largeur, la longueur et toutes les pièces jointes ou exigences supplémentaires relatives à la composition chimique, aux propriétés mécaniques, au traitement thermique, aux essais supplémentaires, au processus de fabrication, au revêtement de surface ou à la finition. Contact Daxun maintenant, nous répondrons à votre courriel dans les plus brefs délais.
La qualité de l'alliage de titane dont vous avez besoin dépend du projet sur lequel vous travaillez, car chaque qualité présente des avantages différents.
Toutes les qualités d'alliage de titane sont extrêmement solides et résistantes à la corrosion, ce qui signifie qu'elles continueront à fonctionner dans les conditions les plus difficiles.
Les grades supérieurs d'alliage de titane (5-12) sont des alliages conçus pour des avantages spécifiques. Par exemple, l'alliage de titane de grade 12 présente une excellente résistance à la chaleur, ce qui en fait un choix parfait pour les échangeurs de chaleur à calandre et à tube, les tuyauteries hydrauliques et les équipements de l'industrie chimique.
Les grades 1 à 4 sont des alliages de titane pur et constituent un choix idéal si vous avez besoin d'un matériau ductile et soudable pour les systèmes de tuyauterie et les tubes. Les grades inférieurs sont utilisés dans la marine et l'industrie.
Si vous démarrez un projet et que vous ne savez pas quelle qualité d'alliage de titane vous convient le mieux, contactez-nous dès aujourd'hui ; nous nous ferons un plaisir de vous aider.
Chez DAXUN, nous proposons une large gamme d'alliages de titane allant de la nuance 1 à la nuance 12.
Les grades 1 à 4 sont du titane pur, tandis que les grades supérieurs sont des alliages.
Les alliages sont appréciés pour leur rapport résistance/poids élevé.
La nuance d'alliage de titane la plus couramment utilisée est la nuance 5. Bien qu'elle soit encore riche en titane, cette nuance est l'une des plus fiables car elle peut résister à des températures allant jusqu'à 600°F et à des conditions extrêmes.
Les qualités supérieures sont privilégiées par les industries telles que l'aérospatiale et la marine pour leur résistance à l'usure et à la corrosion.
Inversement, les qualités inférieures sont principalement utilisées pour le soudage en raison de leur faible résistance.
Pour en savoir plus sur les différences entre les différents grades d'alliage de titane, appelez +86 13382898899 aujourd'hui pour parler directement à nos experts.
Bien que la qualité du titane augmente légèrement le coût, le coût total est principalement déterminé par la forme du titane dont vous avez besoin.
DAXUN propose une large gamme de produits en titane, notamment des plaques, des tubes, des bobines et des barres. La longueur, la largeur et la quantité de chaque article dont vous avez besoin influencent le montant que vous payez à la caisse.
Malheureusement, il est difficile d'établir un prix en ligne sans en savoir plus sur votre projet et sur l'utilisation du titane.
Heureusement, notre équipe d'experts est toujours là pour vous aider et vous conseiller dans vos besoins en titane. En envoyant un e-mail à [email protected], nous pourrons vous donner des conseils et un devis précis.
Veillez à inclure autant d'informations que possible sur le grade, la forme et la quantité de titane dont vous avez besoin afin d'obtenir une meilleure compréhension de vos besoins.
L'équipe de DAXUN est expérimentée, compétente et sympathique. Forte de ses années d'expérience dans l'industrie, elle connaît parfaitement le titane, notamment ses utilisations, ses avantages et ses qualités.
Pour des mises à jour régulières sur le titane, ses utilisations et ses applications dans tous les secteurs, ne manquez pas de consulter notre blog. Nos experts ont rédigé des guides faciles à suivre auxquels vous pouvez toujours vous référer lorsque vous avez des questions.
Si vous rencontrez encore des difficultés, n'hésitez pas à nous contacter, nous nous ferons un plaisir de vous aider.
En envoyant un courriel à [email protected], vous recevrez une réponse rapide. Veillez à donner le plus de détails possible dans votre question afin que nous puissions vous recommander une solution adaptée.
Veuillez remplir le formulaire de la page “Contactez-nous” ou appeler notre responsable des ventes au “+86 13382898899”, nous vous contacterons dans les plus brefs délais. Notre WhatsApp est en ligne, et l'email ([email protected]) sera vérifié dans les 6 heures. Chaque demande ou message recevra une réponse rapide. En outre, nous partageons chaque semaine des informations sur le marché avec nos clients
Nous pouvons vous fournir des échantillons de barres de titane pour que vous puissiez en vérifier la qualité. L'échantillon est gratuit et vous ne payez que les frais de transport.
Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.
Notre MOQ est de 300 kg pour les barres de titane.
Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.