x
Envoyez votre demande dès aujourd'hui
Devis rapide

Daxun is an experienced galvanized plate manufacturer

As a leading galvanized steel plate supplier and exporter in China, Daxun supplies galvanized steel plates to the world.
  • Manufacturing: hot-dip galvanized plate, electro-galvanized plate, galvalume plate
  • Normes : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Thickness: 0.2mm-5.0mm
  • Width: 600mm-1000mm-1200mm-1500mm etc.
  • Length: 1000mm-2000mm-2438mm-3048mm-6000mm etc.
  • Origin: Baosteel, Shagang, Angang, Shandong Steel, Shougang etc.

A global leader in galvanized steel plate fabrication services

Galvanized steel plates are among the most widely used materials across a wide range of industries. Composed primarily of steel coated with a protective layer of zinc, these plates are produced through hot-dip or electro-galvanizing processes to meet customers’ specific requirements for corrosion resistance and durability.

Available in various coating thicknesses and surface finishes, these plates are supplied in standard sizes or custom cut sizes to specific design profiles. High-grade galvanized steel plates are integral components in numerous applications, including roofing systems, automotive body parts, HVAC ductwork, agricultural equipment, electrical enclosures, fencing, outdoor signage, and a wide range of construction components.

Daxun offers a comprehensive range of galvanized steel plates and sheets, available in a variety of lengths, widths, thicknesses and coating weights to suit varying project specifications. Our inventory includes products that meet ASTM, EN and JIS standards, ensuring precise dimensions and consistent zinc coating (in grams per square meter) to meet stringent industry requirements.

The thickness of the zinc coating and the quality of the steel substrate are key factors in determining whether a steel plate is suitable for a specific application, affecting aspects such as corrosion resistance, formability, and weldability. Daxun offers a wide range of options to ensure that customers can select the right material to achieve optimal performance and service life in their respective products.

Données

Category Grades/Specifications
AISI DX51D, DX52D, DX53D, S280GD, S350GD
ASTM/ASME (Structural Grades) A653, A792, A875, A924
ASTM/ASME (Pressure Vessel Grades) A653 (CS Type B, SS Grade 33, 40, 50, 80)
CSA G40.21 (Structural Grades) G90, G115, G140, G165, G185
ABRASIVE RESISTANT GRADES Galvannealed (A40, A60, G30, G60, G90)
SHIPBUILDING AND OFFSHORE GRADES ABS, Lloyds, DNV, A653 (with marine coating), API 2H Grade 50 (galvanized)
EURONORM EN10025 (Available by special request) EN 10346 DX51DZ, DX53DZ, S220GDZ, S250GDZ, S280GDZ, S320GDZ, S350GDZ
MILITARY GRADES MIL-G-16474, MIL-G-16474 Type I, II, III
Épaisseur 0.012″ to 0.25″
Master Width 24″ to 72″
China America Japon Allemagne England France ISO
GB ASTM JIS DIN, DINEN BS, BSEN NF, NFEN ISO 630
Q195 Cr.B SS330; SPHC; SPHD S185 040; A10; S185 S185
Q215A Cr.C; Cr.58 SS330; SPHC
Q235A Cr.D SS440; SM400A E235B
Q235B Cr.D SS440; SM400A S235JR; S235JRG1; S235JRG2 S235JR; S235JRG1; S235JRG2 S235JR; S235JRG1; S235JRG2 E235B
Q255A SS440; SM400A
Q275 SS490 E275A

 

Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

galvanized plate
Contacter Daxun maintenant

Stock Galvanized Plate Types

Hot-Dip Galvanized Steel Plate
Electro-Galvanized Steel Plate
Galvannealed Steel Plate
Galvalume Steel Plate
Zinc-Aluminum-Magnesium Coated Steel Plate

Contacter Daxun maintenant

Usinage avancé

As one of the largest processors and distributors of galvanized plate products in China, we offer a large supply of high-quality, competitively priced products through our network of metal service centers. We leverage our industry expertise, extensive experience and investment in innovative technologies to provide an unparalleled supply of galvanized plate.

galvanized plate
galvanized plate
Contacter Daxun maintenant

Advantages of Buying Galvanized Plates in China

High quality and innovation:
Cost effectiveness:
Diverse product range and customization:
Government support and policy stability:
Combined with these factors, China becomes a strong sourcing source for galvanized plates, offering a balance of quality, price and reliability.

Let your brand improve rapidly

Cold rolled sheet tolerances

Taille Rang de tolérance
Groupe 1 Groupe 2 Groupe 3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
Hot rolled plate tolerance
Taille Rang de tolérance
Groupe 1 Groupe 2 Groupe 3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
Grade Type Épaisseur Surface
Austénitique 304/304H/304L/304J1 0,25-150 mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0,4-80 mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0.3-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
Ferrite 430 0,4-3,0 mm 2B/BA/NO.4/8K/SB/HL
Ferrite ultra pure 443 0,4-2,0 mm 2B
436L/439/444/441 0,5-3,0 mm 2B、2D
409L 0,4-2,5 mm 2B、2D
Grade Type Épaisseur Original
Acier résistant à la chaleur 309S 0,5-40 mm CHN
310S 0,5-40 mm CHN
Acier duplex 2101 1,5-50 mm CHN
2304 3.0-50mm CHN
2205 0,5-60 mm CHN
2507 1.0-60mm SWE / JPN / CHN
Acier super austénitique N08904 0,6-50 mm SWE / JPN / CHN
S31254 0,5-50 mm SWE / JPN / CHN
N08926 0,5-50 mm SWE / JPN / CHN
N08367 0,5-50 mm SWE / JPN / CHN
Alliage base nickel N08031 1.0-50mm US / JPN / GER
N08810/N08800 0,8-50 mm US / JPN / CHN
N08028 1.0-20mm US / GER / JPN
N08020 1.0-20mm US / GER / JPN
N08825 0,8-40 mm US / GER / SWE / JPN / CHN
N10276 0,5-50 mm US / GER / JPN
N06022 1.0-50mm US / GER / JPN
N06625 0,8-20 mm US / GER / CHN
N04400 1.0-20mm US / GER / JPN
N06600 1.0-50mm US / GER / JPN / CHN
N02201 0,5-20 mm US / JPN
Titane TA1/Gr1 0,5-50 mm JPN / CHN
TA2/Gr2 0,5-50 mm JPN / CHN
Matériel de soudage ERNiCrMo-13 1.2、2.4mm GER
ERNiCrMo-3 2,4 mm GER
ERNiCrMo-4 2,4 mm ÉTATS-UNIS

Daxun is a trustworthy steel plate manufacturer

As a galvanized plate manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all galvanized plates are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the galvanized plates have less defects.

Q1: What is the typical zinc coating thickness on your galvanized steel plates?

A1: Our galvanized steel plates typically feature a zinc coating thickness ranging from 60g/m² to 275g/m², depending on the specific product grade and customer requirements. This ensures excellent corrosion resistance for various applications.

Q2: How does galvanized steel compare to stainless steel in terms of corrosion resistance?

A2: While stainless steel generally offers superior corrosion resistance, galvanized steel provides excellent protection at a more economical price point. The zinc coating acts as a sacrificial layer, protecting the underlying steel from rust and extending its service life significantly.

Q3: Can you cut galvanized steel plates to custom sizes?

A3: Yes, we offer precision cutting services for galvanized steel plates according to your specifications. We can cut plates to dimensions ranging from 1000mm-2000mm in width and 2000mm-6000mm in length, with thickness options from 0.3mm-3.0mm.

Q4: What is the typical lead time for bulk orders of galvanized steel plates?

A4: For standard products, our typical lead time is 7-15 days depending on order quantity. For custom specifications or large volume orders, please allow 15-30 days for production and delivery.

Q5: Do your galvanized steel plates come with quality certifications?

A5:Yes, all our galvanized steel plates come with comprehensive quality certifications including ISO 9001, SGS, and BV certifications. We also provide mill test certificates to verify the chemical composition and mechanical properties of each batch.

Q6: What are the main applications for your galvanized steel plates?

A6: Our galvanized steel plates are widely used in construction, automotive manufacturing, appliance production, HVAC systems, and various industrial applications where corrosion resistance is essential.

Q7: How should galvanized steel plates be stored to maintain their quality?

A7: Galvanized steel plates should be stored in a dry, well-ventilated area away from direct contact with moisture. They should be kept off the ground using wooden pallets and covered with waterproof material if stored outdoors for extended periods.

Q8: Do you offer different grades of galvanized steel plates?

A8: Yes, we supply various grades including DX51D, DX52D, DX53D, S280GD, S350GD, and other structural grades to meet different strength and formability requirements for your specific applications.

Q9: What is the maximum size of galvanized steel plates you can supply?

A9:We can supply galvanized steel plates in widths up to 2000mm and lengths up to 6000mm, with thickness options ranging from 0.3mm to 3.0mm. Custom sizes can be arranged based on your specific project requirements.

Envoyez votre demande dès aujourd'hui
Devis rapide