Daxun is an experienced carbon steel plate manufacturer
As a leading carbon steel plate supplier and exporter in China, Daxun supplies carbon steel plates to the world.
- Fabrication : tôles laminées à froid, tôles laminées à chaud, tôles forgées
- Normes : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Thickness: 0.8mm-60mm
- Width: 1000mm-1200mm-1500mm-2000mm-2500mm etc.
- Length: 2438mm-3048mm-6000mm-8000mm etc.
- Origin: Baosteel, Shagang, Angang, Shandong Steel, Shougang etc.
A global leader in carbon steel plate fabrication services
Carbon steel plates are among the most widely used materials across a wide range of industries. Composed primarily of iron and carbon, these alloys are produced by rolling carbon steel ingots or continuously cast slabs to meet customers’ specific requirements for size or chemical composition.
Available in the “as rolled” or heat treated state, these plates are supplied in standard sizes or custom cut sizes to specific design profiles. High-grade carbon steel plates are integral components in numerous applications, including steel frame buildings, storage tanks, welded structures, freight containers, chimneys, bridges, heat exchangers, pipelines, cranes and a wide range of industrial machinery parts.
Daxun offers a comprehensive range of carbon steel plates and sheets, available in a variety of lengths, widths, thicknesses and diameters to suit varying project specifications. Our inventory includes products that meet ASTM standards, ensuring precise dimensions and weights (in kilograms) to meet stringent industry requirements.
The weight and thickness of a carbon steel plate are key factors in determining its suitability for a particular application, affecting aspects such as structural integrity and load-bearing capacity. By offering a wide range of options, Daxun ensures that customers are able to select the right material to achieve optimal performance in their respective projects.
Données
- Paramètres
- Common Structural Steel Plate Grades Chart
| AISI | AISI 1020, 1045, 4130, 4140 |
| ASTM/ASME (Structural Grades) | A36, A572, A588 (CorTen), A656 , A709-36, (36W, 36WT, 36WF), A709-50, A709-HPS70W, A514 (grades B, S, F, H, Q), 100XF, A871 |
| ASTM/ASME (Pressure Vessel Grades) | A285-C, A387, A455, A516(N), A517, A612(N) |
| CSA G40.21 (Structural Grades) | 38W-38WT/260W-260WT, 44W-44WT/300W-300WT, 50W-50WT/350W-350WT, 50A-50AT/350A-350AT, 60W-60WT/400W-400WT |
| ABRASIVE RESISTANT GRADES | AR200, AR235, AR400F, AR450F, AR500 |
| SHIPBUILDING AND OFFSHORE GRADES | ABS, Lloyds, DNV, A131, API 2H Grade 50 |
| EURONORM EN10025 (Available by special request) | S235, S275, S355, S420, S460, S500, S690 |
| MILITARY GRADES | MIL-A-12560, MIL-A-46100, MIL-DTL-46177C |
| Épaisseur | 3/16″ to 8″ |
| Master Width | 72″ to 154″ |
| China | America | Japon | Allemagne | England | France | ISO |
| GB | ASTM | JIS | DIN, DINEN | BS, BSEN | NF, NFEN | ISO 630 |
| Q195 | Cr.B | SS330; SPHC; SPHD | S185 | 040;A10;S185 | S185 | |
| Q215A | Cr.C; Cr.58 | SS330; SPHC | ||||
| Q235A | Cr.D | SS440; SM400A | E235B | |||
| Q235B | Cr.D | SS440; SM400A | S235JR; S235JRG1; S235JRG2 | S235JR; S235JRG1; S235JRG2 | S235JR; S235JRG1; S235JRG2 | E235B |
| Q255A | SS440; SM400A | |||||
| Q275 | SS490 | E275A |
Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

Stock Carbon Steel Plate Types
Low carbon steel plate
Medium carbon steel plate
High carbon steel plate
Structural steel plate
Wear-resistant steel plate
Pressure vessel plate
Armor and ship plate
Usinage avancé
As one of the largest processors and distributors of carbon plate products in China, we offer a large supply of high-quality, competitively priced products through our network of metal service centers. We leverage our industry expertise, extensive experience and investment in innovative technologies to provide an unparalleled supply of carbon steel plate.


Advantages of Buying Carbon Steel Plates in China
High quality and innovation:
Cost effectiveness:
Diverse product range and customization:
Government support and policy stability:
Combined with these factors, China becomes a strong sourcing source for carbon steel plates, offering a balance of quality, price and reliability.
Please contact DAXUN experts when deciding on steel grade
Here are the international grades for carbon steel plates: ASTM Standards: A36, A283 (Grade A, B, C, D), A572 (Grade 42, 50, 55, 60, 65), A516 (Grade 55, 60, 65, 70), A1011 (CS Type A, B, C), A1008 (CS Type A, B, C); EN Standards: S235JR, S275JR, S355JR, S355J2, S460NL; JIS Standards: SS330, SS400, SS490, SPHC, SPHD, SPHE; GB/T Standards: Q195, Q235, Q275, Q345; Other International Grades: DIN 17100 (St37-2, St52-3), ISO 630 (Fe360A, Fe430B).

Carbon steel plate characteristics
Let your brand improve rapidly
- TOLERANCE
- Autres séries de produits
Cold rolled sheet tolerances
| Taille | Rang de tolérance | ||
| Groupe 1 | Groupe 2 | Groupe 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Hot rolled plate tolerance | |||
| Taille | Rang de tolérance | ||
| Groupe 1 | Groupe 2 | Groupe 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Grade | Type | Épaisseur | Surface |
| Austénitique | 304/304H/304L/304J1 | 0,25-150 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0.3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferrite | 430 | 0,4-3,0 mm | 2B/BA/NO.4/8K/SB/HL |
| Ferrite ultra pure | 443 | 0,4-2,0 mm | 2B |
| 436L/439/444/441 | 0,5-3,0 mm | 2B、2D | |
| 409L | 0,4-2,5 mm | 2B、2D | |
| Grade | Type | Épaisseur | Original |
| Acier résistant à la chaleur | 309S | 0,5-40 mm | CHN |
| 310S | 0,5-40 mm | CHN | |
| Acier duplex | 2101 | 1,5-50 mm | CHN |
| 2304 | 3.0-50mm | CHN | |
| 2205 | 0,5-60 mm | CHN | |
| 2507 | 1.0-60mm | SWE / JPN / CHN | |
| Acier super austénitique | N08904 | 0,6-50 mm | SWE / JPN / CHN |
| S31254 | 0,5-50 mm | SWE / JPN / CHN | |
| N08926 | 0,5-50 mm | SWE / JPN / CHN | |
| N08367 | 0,5-50 mm | SWE / JPN / CHN | |
| Alliage base nickel | N08031 | 1.0-50mm | US / JPN / GER |
| N08810/N08800 | 0,8-50 mm | US / JPN / CHN | |
| N08028 | 1.0-20mm | US / GER / JPN | |
| N08020 | 1.0-20mm | US / GER / JPN | |
| N08825 | 0,8-40 mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0,5-50 mm | US / GER / JPN | |
| N06022 | 1.0-50mm | US / GER / JPN | |
| N06625 | 0,8-20 mm | US / GER / CHN | |
| N04400 | 1.0-20mm | US / GER / JPN | |
| N06600 | 1.0-50mm | US / GER / JPN / CHN | |
| N02201 | 0,5-20 mm | US / JPN | |
| Titane | TA1/Gr1 | 0,5-50 mm | JPN / CHN |
| TA2/Gr2 | 0,5-50 mm | JPN / CHN | |
| Matériel de soudage | ERNiCrMo-13 | 1.2、2.4mm | GER |
| ERNiCrMo-3 | 2,4 mm | GER | |
| ERNiCrMo-4 | 2,4 mm | ÉTATS-UNIS |
Informations disponibles pour référence et téléchargement
Daxun is a trustworthy steel plate manufacturer
As a carbon steel plate manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all carbon steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the carbon steel plates have less defects.
Produits apparentés (13)
A1: Carbon steel is a type of steel where the primary alloying element is carbon. It is commonly used in construction, automotive, and manufacturing industries due to its strength, durability, and versatility.
A2: Carbon steel plates are generally classified into three types based on carbon content: low carbon steel (0.05% – 0.25% carbon), medium carbon steel (0.25% – 0.60% carbon), and high carbon steel (0.60% – 1.00% carbon).
A3: Common grades include ASTM A36, ASTM A572, ASTM A516, S235JR, S275JR, S355JR, and JIS SS400, among others.
A4: Carbon steel plates are used in construction, shipbuilding, automotive manufacturing, machinery, pressure vessels, and structural components due to their strength and versatility.
A5: Low carbon steel has higher ductility and is easier to weld and form, while high carbon steel has greater hardness and strength but is less ductile and more prone to cracking during welding.
A6: Yes, carbon steel plates can be welded, though the specific welding process and techniques may vary depending on the carbon content and plate thickness.
A7: To prevent rusting, carbon steel plates should be properly coated with paint, oil, or other protective coatings. In some cases, galvanizing or applying corrosion-resistant alloys can also help protect the steel.
A8: The main advantages include high strength, durability, low cost, and ease of fabrication. Carbon steel plates are also widely available and can be heat-treated to meet various requirements.
A9: The main disadvantages include susceptibility to corrosion, especially in harsh environments, and lower resistance to wear compared to other materials like stainless steel.
A10: Selection depends on factors such as the intended application, required strength, welding capability, environmental conditions, and cost considerations. It is important to choose the grade that meets both mechanical and chemical property requirements for the specific use case.
If you need more details or have other questions, please contact Daxun’s sales team and experts, we will serve you quickly!