x
Envoyez votre demande dès aujourd'hui
Devis rapide

Daxun 347-347H UNS S34700 stainless steel PIPE and TUBE China supplier

As a leading stainless steel supplier and exporter in China, Daxun supplies stainless steel barsRod (Round Bar)to all over the world.
  • Grade : AISI 17-4PH-SUS630
  • Fabrication : laminage à chaud, étirage à froid, forgeage
  • Norme : ASTM, ASME, GB, DIN, JIS, ISO
  • Haute résistance
  • Dureté élevée
  • Résistance à l'usure
  • Traitement thermique

Global leader in stainless steel pipe and tube fabrication services

Global Leader in Stainless Steel Rod and Round Bar Fabrication

Daxun is a trusted global supplier and exporter of SS 17-4PH/630 round bars and rods. We produce high-quality products in a range of surface finishes, end treatments, dimensions, shapes, and sizes to suit your exact requirements.

Why Choose SS 17-4PH?

SS 17-4PH is a martensitic stainless steel that undergoes precipitation hardening for superior mechanical properties. Its alloying elements—nickel, copper, and chromium—contribute to excellent strength, corrosion resistance, and durability. Widely adopted in the aerospace industry, this alloy is ideal for fasteners and other structural components thanks to its refined microstructure, which is developed through a controlled remelting process.

Optimized Properties Through Heat Treatment

UNS S17400, the designation for 17-4PH, responds well to heat treatment and aging. These processes enhance its toughness and ductility, making it suitable for demanding applications. Compared to many high-nickel, non-ferrous alloys, 17-4PH provides a more cost-effective solution without sacrificing performance.

A Versatile Choice for Many Industries

Stainless steel 17-4PH round bars are popular in manufacturing and engineering due to their corrosion resistance, high strength, and ease of production. The “PH” stands for precipitation hardening, a treatment method that further improves the material’s mechanical properties. With its balanced combination of features and value, 17-4PH is an excellent choice for a wide range of industrial projects.

ur network of service centers stock stainless steel bar products for fast, ready supply of bar in common sizes and alloys.We also produce custom-sized stainless steel rods and can arrange inventory schedules for quick turnaround in a timely manner if quantities are below factory minimums.Daxun Alloys stocks stainless steel round bars with diameters ranging from 1/16″ to 26″. Round bars are available in nearly every grade of stainless steel, including 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205, and Alloy 20. Heat treated stainless steel round bars are offered in 17-4PH, H900 temper (on request), H1025, H1150, Double H1150, and H1150M. Other heat-treated tempers can be manufactured upon request. We stock the following 400 series stainless steels: 410, 430, and 416. We also carry 303, 304, and 316/L precision and bearing quality stainless steel round bars. The majority of our inventory consists of our unique machined bar grades: stainless steel round bars that are melted to consistent standards to increase machinability and lower total cost per component. Our stainless steel bar processing machinery allows Daxun Alloys to produce to our customers’ exact specifications.

It performs reliably in high temperature service conditions between 600°F and 800°F.

Lire la suite

Données

Stainless Steel 347 Tube Standards ASTM A213, ASTM A249, ASTM A269, ASME SA213, ASME SA249, ASME SA269, EN 10216-5 TC1 / TC2, PED 97/23/EC, AD 2000, NACE MR0175/ISO 15156
347 SEAMLESS Stainless Steel Aerospace Tubing AMS 5557, AMS 5897 (Canceled & non-current specs include MIL-T-8808, MIL-T-8973)
347 WELDED & DRAWN Stainless Steel Aerospace Tubing AMS 5556, AMS 5575 (Canceled & non-current specs include MIL-T-6737, MIL-T-8606, MIL-T-8808)
Stainless Steel 347 Seamless Tube Size 1.2 mm OD To 630 mm OD
Stainless Steel 347 Welded Tube Size 1.2 mm OD To 1219 mm OD
Swg & Bwg 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg.
Stainless Steel 347 tubing wall thickness 0.020″ –0.220″, (special wall thicknesses available)
SS 347 tube Length Single Random, Double Random, Standard & Cut length
347 Stainless Steel Tube Finish Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF
Stainless Steel 347 tube Form Round, Coil, Square, Rectangular, Boiler, Hydraulic, Straight or ‘U’ bent Tubes, Hollow, LSAW Tubes Etc.
Stainless Steel 347 Tube Type Seamless, ERW, EFW, Welded, Fabricated
Electropolished (EP) Electropolished for Ultra High Purity Systems
Non-Electropolished (BA) Bright Annealed or (AP) Annealed & Pickled for High-Purity, (CFOS) Cleaned for Oxygen Grade Service or Corrosive Systems
I.D. Surface Finish Options 5, 7 & 10 µin. Ra
JIS 8A to 250A
Tolérances In accordance with: ASTM: A269 & A632, JIS: G 3459
347 stainless steel tubing End Plain End, Beveled End, Treaded, Ends are suitable for orbital welding
Marking All 347 Stainless Steel tubes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.)
347 stainless steel tubing Application Oil Tube, Gas Tube, Fluid Tube, Boiler and Heatexchanger
Value Added Service Draw & Expansion as per required Size & Length, Polish (Electro & Commercial) Annealed & Pickled Bending, Machining Etc.
Specialize in Stainless Steel 347 Capillary Tube & Other Odd Size
Stainless Steel 347 Heat Exchanger & Condenser Tubes
Stainless Steel 347 Hydraulic tubing with OD up to 50.8 mm (2.0 in.) are delivered in bright annealed condition
Stainless Steel 347 hydraulic tube with OD larger than 50.8 mm are supplied in the annealed and pickled condition, Or in polished condition
Marking & Traceability Each Stainless Steel 347 Tubing is traceable to its producing mill and heat by an identification number etched within 24″ (610mm) of one end.
347 stainless steel tubing Test Certificate Manufacturer Test Certificate according to EN 10204 3.1 B
Laboratory Test Certificate from Govt. Approved Lab.
Under Third Party Inspection
347 stainless steel tubing Testing & Inspection Visual inspection • Surface roughness measurement • Helium-leak testing • Scanning Electron Microscopy (SEM) • Auger Electron Microscopy (AES) • Election Spectroscopy for Chemical Analysis (ESCA or XPS) • Particle testing • Moisture testing
We can also cut, thread, and groove Stainless Steel 347 Tubes to meet your specifications
Composition of 347/347H Pipe and Tubing
Grade 347 347H
Désignation UNS S34700 S34709
Carbone (C) Max. 0.08 0.04–0.10
Manganèse (Mn) Max. 2 2
Phosphore (P) Max. 0.04 0.04
Soufre (S) Max. 0.03 0.03
Silicium (Si) Max. 0.75 0.75
Chrome (Cr) 17.0–20.0 17.0–20.0
Nickel (Ni) 9.0–13.0 9.0–13.0
Molybdène (Mo)
Azote (N)
Fer (Fe) Bal. Bal.
Autres éléments Cb+Ta=10xC-1.0 Cb+Ta=8xC-1.0
Physical Properties of 347/347H Alloys in the Annealed Condition at -20°F to +100°F
Résistance à la traction Limite d'élasticité
Alliage Désignation UNS Spec. psi MPa ksi psi MPa ksi Elongation in 2 inches (min.) % Grain Size Req. Maximum Harndess Modulus of Elasticity (x106 psi) Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) Thermal Conductivity (BTU-in/ft2-h-°F)
347 S34700 75,000 515 30,000 205 35 29 9.2
347H S34709 75,000 515 30,000 205 35 7 or coarser 29 9.2
Grade Density (kg/m3) Elastic Modulus (GPa) Mean Coefficient of Thermal Expansion (m/m/0C) Thermal Conductivity (W/m.K) Specific Heat 0-1000C (J/kg.K) Electrical Resistivity (n.m)
0-1000C 0-3150C 0-5380C at 1000C at 5000C
347 8000 193 15.9 16.2 17 14.2 18.7 500 740
347H 8000 193 15.9 16.2 17 14.2 18.7 500 740
Grade CHINA UNS No Old British Euronorm Swedish SS Japanese JIS
BS En No Nom
347 0Cr18Ni11Nb S34700 X6CrNiNb18-10 1.455
347H 07Cr18Ni11Nb S34709 1.4961
Stainless Steel ASTM A213 TP347H/347 Condenser Tube Stainless Steel 347H/347 Welded Pipe
ASTM A269 TP347H/347 straight tube 347H/347 Stainless Steel Welded Tube
ASTM A249 TP347H/347 Mirror Tube Jis 347H/347 Stainless Steel Tubing
JIS SUS347H/347 Seamless Tubes Din 1.4550 Stainless Steel Tube
Stainless Steel SA312 TP347H/347 Welded Tubes Stainless Steel AISI 347H/347 Seamless Tube
ASTM A312 TP347H/347 Coiled Tubing Stainless Steel Inox 347H/347 Capillary Tubing
ASTM A312 gr TP 347H/347 Aerospace tubes ASTM A632 TP347H/347 Electric Fusion Welding Pipes
Stainless Steel 347H/347 Grade Pipe Type 347H/347 Stainless Steel Polished Pipes
ASTM A312 TP347H/347 Elliptical Tubes ASTM A213 SS TP 347H/347 Stainless Steel Rectangular Tube
347H/347 Stainless Steel Oval Tubing SS 347H/347 Needle Tube
Din 1.4550 Stainless Steel Welded Pipes ASTM A358 TP347H/347 Coil Tubing Heat Exchanger
SAE J405 Uns S347H/34700 Thin Wall Tubing 347H/347 Stainless Steel Metric Tubing
347H/347 Stainless Steel Seamless Square Tubing Large Diameter 347H/347 Stainless Steel Tube
SS 347H/347 Erw Pipe 347H/347 Stainless Steel Instrumentation Tubing
High-pressure 347H/347 Stainless Steel Water Pipe Stainless Steel 347H/347 Hexagonal Pipe
Din W.-Nr. 1.4550 Aisi 347H/347 Corrugated Tube Stainless Steel 347H/347 Round Tube
UNS S347H/34700 Seamless Pipes Stainless Steel 347H/347 Seamless Round Tubing
ASTM A358 TP347H/347 Polished Tubing 347H/347 Stainless Steel Ornamental Tube
Stainless Steel ASTM A312 TP347H/347 erw 347H/347 Stainless Steel Spiral Pipe
ASME SA213 TP347H/347 Perforated Tube Din 1.4550 Material Tube
Stainless Steel SA 688 TP347H/347 Finned Tube SA312 TP347H/347 Dom Tube
Din 1.4550 AISI 347H/347 Perforated Exhaust Tube Stainless Steel 347H/347 Hypodermic Tubing
Material 1.4550 Aisi 347H/347 Slotted Handrail Tube SA312 TP347H/347 Thin Wall Tube
SA213 TP 347H/347 Thick Wall Tube En 1.4550 / Aisi 347H/347 Hydraulic Tubing
Stainless Steel 347H/347 Ornamental Pipe Stainless Steel 347H/347 Fin Tube / Finned Tube
S347H/34700 Stainless Steel U Shaped Tube 347H/347 Stainless Steel Square Tube Mirror Finish
Din 1.4550 Material Seamless Tubing Stainless Steel WERKSTOFF NR. 1.4550 Coaxial Tube
347H/347 Stainless Steel Rectangular Pipe 347H/347 Stainless Steel Hypodermic Tubing for Medical Needle
1.4550 Instrument Tubing 347H/347 Stainless Steel Square Tubing
Ultra-High Purity Electropolished Stainless Steel 347H/347 Tube Thin Wall S347H/34700 Stainless Steel Pipe
347H/347 Stainless Steel ERW Pipes Corrugated 347H/347 Stainless Steel Tube (CSST) for Gas
Jis 347H/347 Stainless Steel Coil Tubing Stainless Steel 347H/347 Seamless Pipe
Schedule 10 Type 347H/347 Stainless Steel Pipe Schedule 40 Type 347H/347 Stainless Steel Pipe
SA 312 TP347H/347 Seamless Tubing Polished 347H/347 Stainless Steel Tubing
347H/347 Stainless Steel Threaded Pipe SAE 347H/347 Stainless Steel Rectangular Tube
Stainless Steel 347H/347 EFW Pipe SS 347H/347 Electropolish Pipe
Stainless Steel 347H/347 Pipe SS UNS S347H/34700 Heat exchager Pipe
DIN 1.4550 SS 347H/347 Pipe Stainless Steel WERKSTOFF NR. 1.4550 Pipe
Stainless Steel UNS S347H/34700 Welded Pipe ASTM A249 TP 347H/347 Stainless Steel High Pressure Pipe
ASTM A312 TP 347H/347 SS Seamless Pipe Stainless Steel WERKSTOFF NR.1.4550
347H/347 SS Electropolished Pipe SS UNS S347H/34700 Heat exchager Pipe
Stainless Steel 347H/347 Seamless Pipe 347H/347 SS Decorative Pipe
SS 347H/347 Pipe ASTM A249 TP 347H/347 Stainless Steel High Pressure Pipe
Stainless Steel 347H/347 Round Pipe SS 347H/347 Cold Rolled Coiled Tubing
Austenitic Stainless Steel 347H/347 Pipe SS 347H/347 Polish Pipe
ASTM A312 Stainless Steel Pipe Stainless Steel 347H/347 Instrumentation Pipe
WERKSTOFF NR. 1.4550 SS 347H/347 Pipe Stainless Steel 347H/347 Bright Annealed Pipe
347H/347 Stainless Steel Seamless Pipe TP347H/347 SS Welded Pipe
Stainless Steel 347H/347 Seamless Pipe Stainless Steel 347H/347 Seamless Pipe
Stainless Steel GOST 08Ch18N12B Pipe SS 347H/347 Santiary Pipe
WERKSTOFF NR.1.4449 SS 347H/347 Pipe Stainless Steel 347H/347 Pipe
SS 347H/347 Welded Pipe Stainless Steel 347H/347 Welded tubing
Stainless Steel 347H/347 Welded Pipe SS TP347H/347 Seamless Tubing
SS TP347H/347 Seamless Pipe 347H/347 Stainless Steel Seamless Pipe
347H/347 SS Hollow Pipe SCH40 347H/347 Stainless Steel pipe
TP347H/347 SS Welded Pipe 347H/347 Stainless Steel erw Pipe
ASTM A213 Stainless Steel Tubing 347H/347 Seamless Stainless Steel Pipe
Stainless Steel 347H/347 Electropolish Pipe 347H/347 Stainless Steel erw Pipe
347H/347 Stainless Steel Seamless Pipe SS 347H/347 Cold Rolled Coiled Tubing
Stainless Steel WERKSTOFF NR. 1.4550 Pipe ASTM A249 TP 347H/347 SS Seamless Pipe
TP 347H/347 SS ERW Pipe SS 347H/347 Pipe
Stainless Steel 347H/347 Pipe Stainless Steel UNS S347H/34700 Square Pipe
ASTM A312 TP347H/347 Stainless Steel Pipe SS DIN 1.4550 Rectangular Welded Pipe

Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

Quick Response - 17-4 Stainless Steel Rod

  • Higher creep stress and rupture performance
  • Excellent for high temperature service
  • Can be used in ASME boilers and pressure vessels
  • The material has better overall corrosion resistance
  • Excellent mechanical properties
  • High carbon version (347H) has good high temperature creep performance
  • Used for heavy welding equipment where annealing is not possible
  • Good oxidation resistance
  • Prevents harmful carbide precipitation in the heat affected zone (HAZ) of the weld area
  • Imparts substantial immunity to intergranular corrosion
  • Reduces embrittlement in the heat affected zone of the weld are

—347 Stainless Steel pipe and tube

Contacter Daxun maintenant

Avantages de Daxun

  • Variétés : Nous proposons une large gamme de tailles et de qualités, y compris les séries 300, 400, 600, etc.
  • Flexibilité : Que vous ayez besoin de barres laminées à chaud ou étirées à froid, nos longueurs de barres en acier inoxydable sont conçues pour répondre aux exigences spécifiques de votre projet.
  • Normes de qualité : Les tiges en acier inoxydable 17-4 répondent aux normes strictes ASTM, ISO9001, GB, NSF/ANSI pour garantir la fiabilité et la performance.
  • Commandes personnalisées : Vous recherchez des barres en acier inoxydable de dimensions spéciales ? Nous offrons une variété d'options de personnalisation de barres en acier inoxydable à des prix compétitifs et une commande en ligne pratique.
Contacter Daxun maintenant

Emballage en acier inoxydable 17-4

Nous prêtons attention à chaque processus pour garantir la qualité, l'emballage de l'acier rond 17-4 que nous adoptons habituellement consiste à emballer les barres rondes en acier inoxydable dans des sacs en plastique écologiques, puis à les placer dans des boîtes en bois sans fumigation ou des palettes en bois. Les emballages personnalisés, tels que les OEM, peuvent également être négociés. Nous fournissons pratiquement tout ce qu'il faut pour répondre à vos besoins en matière d'emballage des barres rondes. Nous attachons une grande importance à l'emballage. Les barres rondes sont emballées dans des boîtes en bois ondulé, et l'extérieur est enveloppé d'un emballage plastique et d'un film à bulles.

Contacter Daxun maintenant

Qualité, livraison, inspection

  • Daxun effectue également plusieurs tests d'assurance qualité. Ces tests comprennent le test d'aplatissement, le test de piqûre et de résistance, le test mécanique, le test de dureté, l'identification positive du matériau, le test d'expansion, etc. Tous ces tests garantissent que le matériau est adapté à l'application requise.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days. Our delivery time is strictly in accordance with the contract.
  • Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
  • Fournir des échantillons gratuits aux clients pour qu'ils les testent
  • Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Contacter Daxun maintenant

Support technique

  • Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.

17-4 Stainless Steel Rod Ordering Information

Support technique

17-4 stainless steel rod The purchase order shall include quantity, PSL grade, type or category, API5L reference, diameter, finish, length and any applicable attachments or additional requirements relating to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish or end finish. Bars are solution bright annealed.

347-347H UNS S34700 Stainless Steel pipe and tube Features

Haute résistance
Résistance à la corrosion
Résistance à la chaleur
Résistance aux basses températures
Protection de l'environnement
Performance de soudage

Daxun Alloy Permettez à votre marque de s'améliorer rapidement

NPS Outside Diameter Épaisseur de la paroi Weight Weight
in mm in mm Sched kg/Mtr Lb/ft
1/2″ 0.84 21 0.109 2.769 40 STD 1.268 0.851
0.147 3.734 80 STD 1.621 1.088
3/4″ 1.05 27 0.113 2.87 40 STD 1.684 1.131
0.154 3.912 80 STD 2.195 1.474
1″ 1.315 33 0.133 3.378 40 STD 2.501 1.679
0.179 4.547 80 STD 3.325 2.172
1 1/4″ 1.66 42 0.14 3.556 40 STD 3.385 2.273
0.191 4.851 80 STD 4.464 2.997
1 1/2″ 1.9 48 0.145 3.683 40 STD 4.048 2.718
0.2 5.08 80 STD 5.409 3.361
2″ 2.375 60 0.154 3.912 40 STD 5.441 3.653
0.218 5.537 80 STD 7.48 5.022
2 1/2″ 2.875 73 0.203 5.516 40 STD 8.629 5.793
0.276 7.01 80 STD 11.411 7.661
3″ 3.5 89 0.216 5.486 40 STD 11.284 7.576
0.3 7.62 80 STD 15.272 10.253
4″ 4.5 114 0.237 6.02 16.073 10.79
0.337 8.56 22.318 14.983
6″ 6.625 168 0.188 4.775 19.252 12.924
0.203 5.516 20.739 13.923
0.219 5.563 22.318 14.983
0.25 6.35 25.354 17.021
0.28 7.112 40 STD 58.263 18.974
0.312 7.925 31.334 21.036
0.375 9.525 37.285 25.031
0.432 10.973 80 XHY 42.561 28.573
0.5 12.7 48.719 32.708
8″ 8.625 219 0.188 4.775 25.233 16.94
0.203 5.156 27.198 18.259
0.219 5.563 29.286 19.661
0.25 6.35 20 33.308 22.361
0.277 7.036 30 36.786 24.696
0.322 8.179 40 42.352 28.554
0.375 9.525 49.216 33.041
0.406 10.312 60 53.085 35.638
0.5 12.7 80 XHY 64.627 43.388
10″ 10.75 273 0.188 4.775 31.588 21.207
0.219 5.563 36.689 24.631
0.25 6.35 20 41.759 28.035
0.307 7.798 30 51.002 34.24
0.344 8.738 56.946 38.231
0.365 9.271 40 STD 63.301 40.483
0.438 11.125 71.852 48.238
0.5 12.7 60 XHY 81.53 54.735
0.594 15.088 80 95.969 64.429
12″ 12.75 324 0.188 4.775 37.57 25.222
0.219 5.563 43.657 29.309
0.25 6.35 49.713 33.375
0.281 7.137 55.739 37.42
0.312 7.925 61.735 41.445
0.375 9.525 73.824 49.562
0.406 10.312 79.727 53.525
0.5 12.7 97.438 65.415
0.562 14.275 108.966 73.154
14″ 14 356 0.188 4.775 41.308 27.732
0.219 5.563 48.012 32.233
0.25 6.35 20 54.685 36.713
0.281 7.137 61.327 41.172
0.312 7.925 67.939 45.611
0.375 9.525 STD 81.281 54.568
0.438 11.125 40 94.498 63.441
0.5 12.7 XHY 107.381 72.09
0.625 15.875 132.983 89.278
16” 16 406 0.188 4.775 47.29 21.748
0.219 5.563 54.98 36.91
0.25 6.35 10 62.639 42.053
0.281 7.137 70.268 47.174
0.312 7.925 20 77.866 52.275
0.344 8.738 85.677 57.519
0.375 9.525 30 93.213 62.578
STD
0.438 11.125 108.433 72.797
0.5 12.7 40 123.289 82.77
XHY
18″ 18 457 0.219 5.563 61.948 41.588
0.25 6.35 70.593 47.393
0.281 7.137 79.208 53.176
0.312 7.925 20 87.792 58.939
0.375 9.525 STD 105.144 70.588
0.438 11.125 30 122.369 82.152
0.5 12.7 XHY 139.198 93.45
0.562 14.275 40 155.904 104.666
0.625 15.875 172.754 115.978
20″ 20 508 0.25 6.35 78.547 52.733
0.282 7.163 88.458 59.386
0.312 7.925 97.719 65.604
0.375 9.525 20 STD 117.075 78.598
0.438 11.125 136.305 91.508
0.5 12.7 30 XHY 155.106 104.13
0.594 15.088 40 183.378 123.11
0.625 15.875 192.64 129.328
0.688 17.475 211.368 141.901
24″ 24 610 0.25 6.35 94.456 63.413
0.281 7.137 106.029 71.183
0.312 7.925 117.573 18.932
0.375 9.525 20 STD 140.938 64.618
0.438 11.125 164.176 110.219
0.5 12.7 XHY 186.923 125.49
0.625 15.875 232.41 156.028
0.688 17.475 40 255.148 171.293
0.75 19.05 277.401 186.233
30″ 30 762 0.25 6.35 118.318 79.433
0.281 7.137 132.851 89.189
0.312 7.925 10 147.353 98.925
0.375 9.525 STD 176.731 118.648
0.438 11.125 205.983 138.286
0.5 12.7 20 XHY 234.647 157.53
0.625 15.875 30 292.066 196.078
0.688 17.475 320.817 215.38
0.75 19.05 348.988 234.293
36″ 36 914 0.25 6.35 142.18 95.453
0.281 7.137 159.672 107.196
0.312 7.925 10 177.133 118.918
0.375 9.525 STD 215.525 142.678
0.438 11.125 247.79 166.353
0.5 12.7 20 XHY 282.372 198.57
0.625 15.875 351.723 236.128
0.688 17.475 386.487 259.467
0.75 19.05 420.576 282.353
42″ 42 1067 0.312 7.925 206.914 138.911
0.375 9.525 STD 248.319 166.708
0.5 12.7 XHY 33.097 221.61
0.75 19.05 492.163 330.413
48″ 48 1219 0.375 9.525 STD 284.112 190.738
0.438 11.125 331.404 222.487
0.5 12.7 XHY 377.822 253.65
0.75 19.05 563.75 378.473
0.875 22.225 655.969 440.383
ASTM A312 SS TP347 Seamless Pipe Pressure Rating
SS Pipe Pressure Rating (psig)
SS Pipe Size(inches) SS Pipe Schedule Temperature(F)
100 200 300 400 500 600 650 700 750
1″ 40 3048 2629 2362 2171 2019 1924 1867 1824 1810
80 4213 3634 3265 3002 2791 2659 2580 2528 2501
160 6140 5296 4759 4375 4068 3876 3761 3684 3646
1 1/2″ 40 2257 1947 1750 1608 1496 1425 1383 1354 1340
80 3182 2744 2466 2267 2108 2009 1949 1909 1889
160 4619 3984 3580 3291 3060 2916 2829 2772 2743
2″ 40 1902 1640 1474 1355 1260 1201 1165 1141 1129
80 2747 2369 2129 1957 1820 1734 1682 1648 1631
160 4499 3880 3486 3205 2980 2840 2755 2699 2671
3″ 40 1806 1558 1400 1287 1196 1140 1106 1084 1072
80 2553 2202 1979 1819 1691 1612 1564 1532 1516
160 3840 3312 2976 2736 2544 2424 2352 2304 2280
4″ 40 1531 1321 1187 1091 1014 967 938 919 909
80 2213 1909 1715 1577 1466 1397 1355 1328 1314
160 3601 3106 2791 2566 2386 2273 2206 2161 2138
5″ 40 1342 1158 1040 956 889 847 822 805 797
80 1981 1709 1535 1411 1312 1250 1213 1189 1176
160 3414 2945 2646 2433 2262 2155 2091 2049 2027
6 40 1219 1052 945 869 808 770 747 732 724
80 1913 1650 1483 1363 1267 1208 1172 1148 1136
160 3289 2836 2549 2343 2179 2076 2014 1973 1953
8″ 40 1073 926 832 765 711 678 657 644 637
80 1692 1459 1311 1205 1121 1068 1036 1015 1005
160 3175 2738 2460 2262 2103 2004 1944 1905 1885
10″ 40 974 840 755 694 645 615 596 584 578
80 1609 1388 1247 1147 1066 1016 986 966 56
160 3147 2714 2439 2242 2085 1986 1927 1880 1868
1 psi (lb/in2) = 6,894.8 Pa (N/m2) = 6.895×10-2 bar
Notes:
Maximum safe working pressure is calculated per ASME B 31.3-2012, paragraph 304.1.2 (formula 3a). Calculations assume maximum allowable O.D. and minimum allowable wall thickness (worst case scenario).
Material: TP 304L or TP 316L per ASTM A269 and A632.
Temperature Range = -20°F to +300°F, -28.8°C to 148.9°C
Les types Out diameter Tailles Longueur
NB Sizes (in stock) .0035” ~ 20” 1/8″, 1/4″, 3/8″, 1/2″, 5/8″, 3/4″, 1″, 1.25″, 1.5″, 2″, 2.5″, 3″, 4″, 5″, 6″etc Cut to length
Stainless Steel 347-347H UNS S34700 Seamless Tube (Custom Sizes) 6.35 mm OD To 508 mm OD As per requirement Cut to length
Stainless Steel 347-347H UNS S34700 Welded Tube (ERW Tube) (in Stock + Custom Sizes) 6.35 mm OD To 1219 mm OD As per requirement Cut to length
Finition de la surface Internal Surface(ID) Exterbal Surface(OD)
Roughness Average(RA) Roughness Average(RA)
μ inch μm μ inch μm
AP Annealed & Pickled Not defined Not defined 40 or Not defined 1.0 or Not defined
BA Beight Annealed 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
MP Mechanical Polish 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
EP Electro Polish 15,10,7,5 0.38,0.25,0.20;0.13 32 0.8

The surface and shape of 347-347H UNS S34700 stainless steel tube (6)

Daxun est un fabricant fiable de barres en acier inoxydable.

En tant que fabricant professionnel, Daxun s'assure que tous les produits qu'il fabrique sont de haute qualité. Par conséquent, nous veillons à ce que toutes les tiges en acier inoxydable soient certifiées ISO9001, SGS, CE, OQC et autres normes de qualité internationales. Chez Daxun, vous pouvez être sûr que tous les produits sont durables, de haute qualité et de haute performance.

Projets et produits récents

347-347H UNS S34700 stainless steel pipe
tube en acier inoxydable sans soudure
347-347H UNS S34700 stainless steel pipe
tube en acier inoxydable de grand diamètre
Tube en acier inoxydable poli
347-347H UNS S34700 seamless pipe
BA stainless steel pipe
Tube en acier inoxydable
Stainless steel tube / pipe
347-347H UNS S34700 stainless pipe
Stainless steel precision tube
Puis-je obtenir des échantillons ?

Nous pouvons vous fournir des échantillons de tiges d'acier inoxydable 17-4 afin que vous puissiez en vérifier la qualité. L'échantillon est gratuit et vous ne payez que les frais de transport.

Quels sont les pays que vous avez déjà exportés ?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

Quel est votre MOQ ?

Notre MOQ est de 1 tonne pour les barres d'acier inoxydable 17-4.

Quel est le délai de livraison ?

Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.

Envoyez votre demande dès aujourd'hui
Devis rapide