x
Envoyez votre demande dès aujourd'hui
Devis rapide

Daxun 321 and 321H stainless steel PIPE and TUBE China supplier

As China’s leading Stainless Steel pipe and tube supplier and exporter, Daxun provides stainless steel PIPEs to the world.
  • Grade: AISI 321/321H-S32100
  • Manufacturing: hot-rolled, cold-drawn, forged, welded
  • Normes : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Type: both seamless and welded pipes
  • Diameter: from small diameter to large diameter pipes
  • Thickness: thin-walled pipes and thick-walled pipes
  • Surface: pickled, polished, bright annealed
  • Length: 3000mm, 6000mm, 9000mm, etc.

Global leader in stainless steel pipe and tube fabrication services

ASTM A312 / A358 Stainless Steel 321 Pipe Supplier; 321 / 321H Stainless Steel Seamless Pipe, Contact us for ASME SA312 321 Stainless Steel Pipe.

Type 321 stainless steel is an austenitic steel. It shares many of the same properties as Type 304, but with increased titanium and carbon content. Type 321 provides metal fabricators with superior corrosion and oxidation resistance, as well as exceptional toughness even at cryogenic temperatures. It is very resistant to oxidation and corrosion. Titanium in 321 stainless steel provides various attractive properties: Prevents harmful carbide precipitation in the heat affected zone (HAZ) of the weld. Offers partial protection against intergranular corrosion. Reduces embrittlement in high-risk areas of the weld. 321H stainless steel is commonly used in applications where parts are heated to carbide precipitation temperatures (800°F-1500°F) and exposed to corrosive atmospheres. 321 stainless steel is identical to 304 stainless steel, however it contains more nickel and is stabilised with titanium. Titanium preferentially interacts with the carbon in the steel, preventing the formation of chromium carbides at the grain boundaries. This maintains corrosion resistance qualities by minimising chromium consumption near the grain borders during exposure to critical temperatures. This grade hardens well with cold working. It is easily weldable and rarely requires post-weld annealing to maintain its outstanding performance in a variety of corrosive conditions.

321 Stainless Steel Seamless Pipe, 321 Stainless Steel ERW Pipe, 321 Stainless Steel EFW Pipe, 321 Stainless Steel Welded Pipes and Tubes (ASTM A213 / A312 / A269 / A358)

Daxun Alloys is a prominent producer, supplier, stockist, and exporter of high-quality stainless steel products such as Stainless Steel 321/321H Steel Pipes. The pipes we offer are manufactured in accordance with national and international raw material quality standards. The industry provides a vast selection of pipes with varied standards, sizes, and specifications. The pipes are easily available in customised specifications based on the needs of the consumers. As a result, purchasers can select items in a variety of sizes, wall thickness, length, diameters, and other specifications to meet their specific requirements. The products are sold to both international and domestic buyers at market-leading pricing. We provide a variety of mechanical tests to test and assure our products. To supply our valued clients with high satisfaction, we conduct flare tests, hardness testing, micro and macro tests, chemical tests, and so on.

Lire la suite

Données

WERKSTOFF NR.1.4541 SS 321 Specification Stainless Steel 321, ASTM A312 TP 321 SS
DIN 1.4541 SS 321 Pipe 321 Stainless Steel Pipe
SS 321 Seamless Pipe Size 4 to 630mm W. T.: 0.5 to 50mm
321L Stainless Steel Welded Pipe Size 5.0 mm – 1219.2 mm
SS UNS S32103 EFW Pipe size 5.0 mm – 1219.2 mm
ASTM A312 Stainless Steel Pipe Swg & Bwg 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg.
SA312 TP321 Pipe Schedule SCH5, SCH10, SCH10S, SCH20, SCH30, SCH40, SCH40S, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
DIN 1.4541 SS 321 Swg & Bwg 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg.
321l Stainless Steel Tube wall thickness 0.020″ –0.220″, (special wall thicknesses available)
321 Steel Length Single Random, Double Random, Standard & Cut length Pipe & Tube
ASTM A312 TP 321 Stainless Steel Finish Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF
UNS S32100 Form Round, Hydraulic, ‘U’ bent or Hollow,LSAW, Boiler, Straight Pipe, Clad Pipe, Rectangular, Square Pipe Etc
Stainless Steel 321 Type Welded, Seamless, ERW, EFW, Fabricated Pipe, ‘U’ bent or Hollow, Hydraulic, LSAW, Boiler, Straight Tube, Tube Coil, Round, Rectangular, Square Tube etc
321 Steel End Plain End, Beveled End, Treaded Pipe
SS 321 Marking All 321l Stainless Steel Pipe are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.)
ASTM A 358 SS 321 Application Oil Pipe & Tube, Gas Pipe & Tube, Fluid Pipe & Tube, Boiler Pipe & Tube, Heat exchanger Tube
ASTM A312 TP 321 SS Value Added Service Draw & Expansion as per required Size & Length, Polish (Electro & Commercial) Annealed & Pickled Bending, Machining Etc.
ASTM A 312 SS 321 Specialize in Alloy 321 Large Diameter Pipe
WERKSTOFF NR.1.4541 SS 321 Capillary Tube
SS TP321 Heat Exchanger &
TP321 SS Condenser Tube
SS TP321 Test Certificate Manufacturer Test Certificate
Laboratory Test Certificate from Govt. Approved Lab.
Under Third Party Inspection
Manufacturers of 321 Stainless Steel Pipe Baosteel Stainless Steel
Taigang Stainless Steel
Qingshan Stainless Steel
ATI of the United States
Nippon Steel
Posco of South Korea
Marking All 321 Stainless Steel tubes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.)
321/321H stainless steel tubing Testing & Inspection Visual inspection • Surface roughness measurement • Helium-leak testing • Scanning Electron Microscopy (SEM) • Auger Electron Microscopy (AES) • Election Spectroscopy for Chemical Analysis (ESCA or XPS) • Particle testing • Moisture testing
We can also cut, thread, and groove 321l Stainless Steel Pipe to meet your specifications. Pipe Dimension ANSI/ ASME B36.10, B36.19, B2.1
Composition 321/321H Pipe and Tubing
Grade 321 321H
Désignation UNS S32100 S32109
Carbone (C) Max. 0.08 0.04–0.10
Manganèse (Mn) Max. 2 2
Phosphore (P) Max. 0.04 0.04
Soufre (S) Max. 0.03 0.03
Silicium (Si) Max. 0.75 0.75
Chrome (Cr) 17.0–20.0 17.0–20.0
Nickel (Ni) 9.0–12.0 9.0–12.0
Molybdène (Mo)
Azote (N) 0.1 Max. 0.1 Max.
Fer (Fe) Bal. Bal.
Autres éléments Ti=5(C) to 0.70% Ti=4(C) to 0.60%
Physical Properties of 321/321H Alloys in the Annealed Condition at -20°F to +100°F
Résistance à la traction Limite d'élasticité
Alliage Désignation UNS Spec. psi MPa ksi psi MPa ksi Elongation in 2 inches (min.) % Grain Size Req. Maximum Harndess Modulus of Elasticity (x106 psi) Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) Thermal Conductivity (BTU-in/ft2-h-°F)
321 S32100 75,000 515 30,000 205 35 29 9.2
321H S32109 75,000 515 30,000 205 35 7 or coarser 29 9.2
Grade Density (kg/m3) Elastic Modulus (GPa) Mean Coefficient of Thermal Expansion (m/m/0C) Thermal Conductivity (W/m.K) Specific Heat 0-1000C (J/kg.K) Electrical Resistivity (n.m)
0-1000C 0-3150C 0-5380C at 1000C at 5000C
321/321H 8027 193 16.6 17.2 18.6 16.1 22.2 500 720
Grade UNS No Old British Euronorm Swedish SS Japanese JIS
BS En No Nom
321 S32100 321S31 58B, 58C 1.4541 X6CrNiTi18-10 2337 SUS 321
321H S32109 321S51 - 1.4878 X10CrNiTi18-10 - SUS 321H
ASTM A312 / A213 / A249 TP 321 Stainless Steel Pipes & Tubes ASTM A249 321 Stainless Steel Square Seamless Pipes
ASTM A358 TP 321 Stainless Steel EFW Pipes ASME TP 321 Stainless Steel Electric Fusion Welding Pipes
Stainless Steel 321 Workstoff Nr. 1.4541 Pipes & Tubes TP 321 SS EFW Tubing
ASTM A312 SS 321 Round Pipes Stainless Steel JIS SUS 321 Cold Rolled Coiled Tubing
SS 321 Polished Pipes ASTM A249 321 Stainless Steel Tubing
321 Stainless Steel Pipes and Tubes SS 321 Austenitic Stainless Steel Pipes & Tubes
ASTM A312 TP 321 SS Seamless Pipes TP 321 Stainless Steel LSAW Pipes
SS DIN 1.4541 Rectangular Welded Pipes ASTM A213 Stainless Steel TP 321 Capillary Tube
TP 321 SS ERW Pipes Stainless Steel 321 U Shaped Tubing
TP321 Stainless Steel EFW Tubing TP 321 Stainless Steel Hydraulic Tubes
ASTM A213 SS TP321 Pipes A213 SS 321 Electric Resistance Welding Pipes
Stainless Steel 321 Black Round Tubes Stainless Steel ASTM A213 TP 321 Welded Tubing
ASTM A213 SS Seamless Tubing AISI Stainless Steel ASTM A249 321 Seamless Tubing
Stainless Steel 321 Welded Tubes SS ASME SA 269 TP 321 Welded Tubes
ASTM A312 TP 321 Stainless Steel Welded Pipes TP 321 Stainless Steel Instrumentation Tubes
SS UNS S32100 Square Pipes Stainless Steel 321 Pipe
TP 321 Stainless Steel Pipes & Tubing SS JIS SUS 321 Pipes
Stainless Steel TP 321 Seamless Pipes ASTM A358 TP 321 Stainless Steel EFW Pipes
ASTM A213 TP 321 Stainless Steel Seamless Tubes SS 321 Hexagonal Pipe
Stainless Steel TP 321 Seamless Tubing Austenitic Stainless Steel 321H Pipes
ASTM A213 Stainless Steel Welded Pipes SS UNS S32109 Welded 321 Pipe
A249 SS TP 321 Welded Tubes ASTM A312 TP 321 Stainless Steel Seamless Pipes
ASTM A312 321 Stainless Steel ERW Pipes 321 SS Hallow Pipe
A312 SS 321 Rectangular Seamless Pipes SS TP321 Seamless Pipe
ASTM A213 321 Stainless Steel Rectangular Tubes Stainless Steel 321 Seamless Pipe
TP 321 Stainless Steel ERW Tubes ASTM A249 TP 321 Stainless Steel Welded Tubes
Stainless Steel UNS S32100 Pipes & Tubes Stainless Steel 321 Welded Pipes
UNS S32100 Stainless Steel Coiled Seamless Tubing ASTM A312 TP 321 Stainless Steel Seamless Pipes
Stainless Steel TP 321 Heat Ex-changer Tubes SS 321 Hallow Pipe
ASTM A312 TP 321 Stainless Steel Pipes & tubes TP321 SS Welded Pipe
Stainless Steel DIN 1.4541 Round Tubing Stainless Steel 321 Round Pipe
Stainless Steel ASTM A213 TP 321 Welded Pipe AISI Stainless Steel ASTM A249 321 Seamless Pipe
SS ASME SA 269 TP 321 Welded Pipe TP 321 Stainless Steel Instrumentation Pipe
Stainless Steel 321 Pipe SS JIS SUS 321 Pipe
ASTM A358 TP 321 Stainless Steel EFW Pipe SS 321 Hexagonal Pipe
Austenitic Stainless Steel 321H Pipe SS UNS S32109 Welded 321 Pipe
ASTM A312 TP 321 Stainless Steel Seamless Pipe 321 SS Hallow Pipe
SS TP321 Seamless Pipe Stainless Steel 321 Seamless Pipe
ASTM A249 TP 321 Stainless Steel Welded Pipe Stainless Steel 321 Welded Pipe
ASTM A312 TP 321 Stainless Steel Seamless Pipe SS 321 Hallow Pipe
TP321 SS Welded Pipe Stainless Steel 321 Round Pipe
AISI Type 321 Stainless Steel Pipe 321 Stainless Steel Pipe

Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

Contacter Daxun maintenant

Réponse rapide

  • Bonne formabilité et soudabilité
  • Works at temperatures up to 900°C
  • Resistant to acids, alkalis and low temperatures
  • Responds well to cold work hardening
  • Good welding characteristics
  • Excellent corrosion resistance
  • High creep and stress rupture propertiesGrade: AISI 321/321H-S32100
    Manufacturing: hot-rolled, cold-drawn, forged, welded
    Normes : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
    Type: both seamless and welded pipes
    Diameter: from small diameter to large diameter pipes
    Thickness: thin-walled pipes and thick-walled pipes
    Surface: pickled, polished, bright annealed
    Length: 3000mm, 6000mm, 9000mm, etc.Grade: AISI 321/321H-S32100
    Manufacturing: hot-rolled, cold-drawn, forged, welded
    Normes : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
    Type: both seamless and welded pipes
    Diameter: from small diameter to large diameter pipes
    Thickness: thin-walled pipes and thick-walled pipes
    Surface: pickled, polished, bright annealed
    Length: 3000mm, 6000mm, 9000mm, etc.
  • Tube en acier inoxydable 321
Contacter Daxun maintenant

321 Stainless Steel pipe Daxun Advantages

  • Variety: From small to large diameter stainless steel pipe, we offer a wide range of sizes and grades, including 304L, 316L, 317L ,321,310,347,2205and more.
  • Flexibility: Whether you need seamless or welded steel pipe, our stainless steel pipe lengths are designed to meet your specific project requirements.
    Quality
  • Standards: Our stainless steel pipes meet stringent standards such as ISO9001, ABS, NSF/ANSI Standard 61, and NACE MR0175 to ensure reliability and performance.
  • Custom Orders: Looking for special size stainless steel pipes? We offer a variety of stainless steel pipe custom options at competitive prices and convenient online ordering.
Contacter Daxun maintenant

321 Stainless Steel pipe packaging

  1. Woven bag bale cargo (hexagonal)
  2. Special crates for U-bend pipes, (steel/wood) divided
  3. Each bale is wrapped in plastic to protect against wind and rain.
  4. SS 321 seamless pipes are protected by plastic covers.
  5. Plastic strips are used to secure the bale.
  6. Export-specific fumigation-free wooden crate packaging.
  7. Laminated packing slip attached to the bale or crate.
  8. Customized packaging as per customer needs.
Contacter Daxun maintenant

321 Stainless Steel pipe Ordering Information

321 stainless steel pipe The purchase order shall include quantity, PSL grade, type or class, API5L reference, outside diameter, wall thickness, length and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Pipe is solution bright annealed.

Contacter Daxun maintenant

Qualité, livraison, inspection

  • Daxun effectue également plusieurs tests d'assurance qualité. Ces tests comprennent le test d'aplatissement, le test de piqûre et de résistance, le test mécanique, le test de dureté, l'identification positive du matériau, le test d'expansion, etc. Tous ces tests garantissent que le matériau est adapté à l'application requise.
  • Au cours du processus de production, nous mesurons le diamètre, l'épaisseur et la surface du produit. Notre délai de livraison standard est de 7 à 15 jours, sauf pour certains produits de taille spéciale, pour lesquels le délai de livraison peut atteindre 20 jours.
    Nos délais de livraison sont strictement conformes au contrat.
  • Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
  • Fournir des échantillons gratuits aux clients pour qu'ils les testent
  • Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Contacter Daxun maintenant

Support technique

Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.

321/321H Stainless Steel pipe and tube Features

Haute résistance
Résistance à la corrosion
Résistance à la chaleur
Résistance aux basses températures
Protection de l'environnement
Performance de soudage

Daxun Alloy Permettez à votre marque de s'améliorer rapidement

NPS Outside Diameter Épaisseur de la paroi Weight Weight
in mm in mm Sched kg/Mtr Lb/ft
1/2″ 0.84 21 0.109 2.769 40 STD 1.268 0.851
0.147 3.734 80 STD 1.621 1.088
3/4″ 1.05 27 0.113 2.87 40 STD 1.684 1.131
0.154 3.912 80 STD 2.195 1.474
1″ 1.315 33 0.133 3.378 40 STD 2.501 1.679
0.179 4.547 80 STD 3.325 2.172
1 1/4″ 1.66 42 0.14 3.556 40 STD 3.385 2.273
0.191 4.851 80 STD 4.464 2.997
1 1/2″ 1.9 48 0.145 3.683 40 STD 4.048 2.718
0.2 5.08 80 STD 5.409 3.361
2″ 2.375 60 0.154 3.912 40 STD 5.441 3.653
0.218 5.537 80 STD 7.48 5.022
2 1/2″ 2.875 73 0.203 5.516 40 STD 8.629 5.793
0.276 7.01 80 STD 11.411 7.661
3″ 3.5 89 0.216 5.486 40 STD 11.284 7.576
0.3 7.62 80 STD 15.272 10.253
4″ 4.5 114 0.237 6.02 16.073 10.79
0.337 8.56 22.318 14.983
6″ 6.625 168 0.188 4.775 19.252 12.924
0.203 5.516 20.739 13.923
0.219 5.563 22.318 14.983
0.25 6.35 25.354 17.021
0.28 7.112 40 STD 58.263 18.974
0.312 7.925 31.334 21.036
0.375 9.525 37.285 25.031
0.432 10.973 80 XHY 42.561 28.573
0.5 12.7 48.719 32.708
8″ 8.625 219 0.188 4.775 25.233 16.94
0.203 5.156 27.198 18.259
0.219 5.563 29.286 19.661
0.25 6.35 20 33.308 22.361
0.277 7.036 30 36.786 24.696
0.322 8.179 40 42.352 28.554
0.375 9.525 49.216 33.041
0.406 10.312 60 53.085 35.638
0.5 12.7 80 XHY 64.627 43.388
10″ 10.75 273 0.188 4.775 31.588 21.207
0.219 5.563 36.689 24.631
0.25 6.35 20 41.759 28.035
0.307 7.798 30 51.002 34.24
0.344 8.738 56.946 38.231
0.365 9.271 40 STD 63.301 40.483
0.438 11.125 71.852 48.238
0.5 12.7 60 XHY 81.53 54.735
0.594 15.088 80 95.969 64.429
12″ 12.75 324 0.188 4.775 37.57 25.222
0.219 5.563 43.657 29.309
0.25 6.35 49.713 33.375
0.281 7.137 55.739 37.42
0.312 7.925 61.735 41.445
0.375 9.525 73.824 49.562
0.406 10.312 79.727 53.525
0.5 12.7 97.438 65.415
0.562 14.275 108.966 73.154
14″ 14 356 0.188 4.775 41.308 27.732
0.219 5.563 48.012 32.233
0.25 6.35 20 54.685 36.713
0.281 7.137 61.327 41.172
0.312 7.925 67.939 45.611
0.375 9.525 STD 81.281 54.568
0.438 11.125 40 94.498 63.441
0.5 12.7 XHY 107.381 72.09
0.625 15.875 132.983 89.278
16” 16 406 0.188 4.775 47.29 21.748
0.219 5.563 54.98 36.91
0.25 6.35 10 62.639 42.053
0.281 7.137 70.268 47.174
0.312 7.925 20 77.866 52.275
0.344 8.738 85.677 57.519
0.375 9.525 30 93.213 62.578
STD
0.438 11.125 108.433 72.797
0.5 12.7 40 123.289 82.77
XHY
18″ 18 457 0.219 5.563 61.948 41.588
0.25 6.35 70.593 47.393
0.281 7.137 79.208 53.176
0.312 7.925 20 87.792 58.939
0.375 9.525 STD 105.144 70.588
0.438 11.125 30 122.369 82.152
0.5 12.7 XHY 139.198 93.45
0.562 14.275 40 155.904 104.666
0.625 15.875 172.754 115.978
20″ 20 508 0.25 6.35 78.547 52.733
0.282 7.163 88.458 59.386
0.312 7.925 97.719 65.604
0.375 9.525 20 STD 117.075 78.598
0.438 11.125 136.305 91.508
0.5 12.7 30 XHY 155.106 104.13
0.594 15.088 40 183.378 123.11
0.625 15.875 192.64 129.328
0.688 17.475 211.368 141.901
24″ 24 610 0.25 6.35 94.456 63.413
0.281 7.137 106.029 71.183
0.312 7.925 117.573 18.932
0.375 9.525 20 STD 140.938 64.618
0.438 11.125 164.176 110.219
0.5 12.7 XHY 186.923 125.49
0.625 15.875 232.41 156.028
0.688 17.475 40 255.148 171.293
0.75 19.05 277.401 186.233
30″ 30 762 0.25 6.35 118.318 79.433
0.281 7.137 132.851 89.189
0.312 7.925 10 147.353 98.925
0.375 9.525 STD 176.731 118.648
0.438 11.125 205.983 138.286
0.5 12.7 20 XHY 234.647 157.53
0.625 15.875 30 292.066 196.078
0.688 17.475 320.817 215.38
0.75 19.05 348.988 234.293
36″ 36 914 0.25 6.35 142.18 95.453
0.281 7.137 159.672 107.196
0.312 7.925 10 177.133 118.918
0.375 9.525 STD 215.525 142.678
0.438 11.125 247.79 166.353
0.5 12.7 20 XHY 282.372 198.57
0.625 15.875 351.723 236.128
0.688 17.475 386.487 259.467
0.75 19.05 420.576 282.353
42″ 42 1067 0.312 7.925 206.914 138.911
0.375 9.525 STD 248.319 166.708
0.5 12.7 XHY 33.097 221.61
0.75 19.05 492.163 330.413
48″ 48 1219 0.375 9.525 STD 284.112 190.738
0.438 11.125 331.404 222.487
0.5 12.7 XHY 377.822 253.65
0.75 19.05 563.75 378.473
0.875 22.225 655.969 440.383
PRESSURE RATING (PSIG)
SIZES SCHEDULE (SCH) OUTSIDE WALL TEMPERATURE (OF)
(INCHES) DIA. THICK. 100 200 300 400 500 600 650 700 750
(IN) (IN) ALLOWABLE STRESS (PSI)
16700 16700 16700 15500 14400 13500 13200 12900 12600
1″ 40 1.315 0.133 2205 2205 2205 2047 1902 1783 1743 1703 1664
80 1.315 0.179 3061 3061 3061 2841 2640 2475 2420 2365 2310
160 1.315 0.25 4493 4493 4493 4170 3874 3632 3552 3471 3390
1 1/2″ 40 1.9 0.145 1629 1629 1629 1512 1404 1317 1287 1258 1229
80 1.9 0.2 2303 2303 2303 2138 1986 1862 1821 1779 1738
160 1.9 0.281 3362 3362 3362 3120 2899 2717 2657 2597 2536
2″ 40 2.375 0.154 1371 1371 1371 1272 1182 1108 1083 1059 1034
80 2.375 0.218 1985 1985 1985 1843 1712 1605 1569 1534 1498
160 2.375 0.344 3283 3283 3283 3047 2831 2654 2595 2536 2477
3″ 40 3.5 0.216 1301 1301 1301 1208 1122 1052 1028 1005 982
80 3.5 0.3 1844 1844 1844 1712 1590 1491 1458 1425 1391
160 3.5 0.438 2787 2787 2787 2587 2403 2253 2203 2153 2103
4″ 40 4.5 0.237 1102 1102 1102 1023 950 891 871 851 831
80 4.5 0.337 1596 1596 1596 1482 1377 1291 1262 1233 1204
160 4.5 0.531 2611 2611 2611 2424 2552 2111 2064 2017 1970
5″ 40 5.563 0.258 965 965 965 896 832 780 763 746 728
80 5.563 0.375 1428 1428 1428 1325 1231 1154 1129 1103 1077
160 5.563 0.625 2474 2474 2474 2296 2133 2000 1955 1911 1866
6″ 40 6.625 0.28 877 877 877 814 756 709 693 677 661
80 6.625 0.432 1379 1379 1379 1280 1189 1115 1090 1065 1040
160 6.625 0.719 2382 2382 2382 2211 2054 1925 1883 1840 1797
8″ 40 8.625 0.322 771 771 771 716 665 623 610 596 582
80 8.625 0.5 1218 1218 1218 1131 1050 985 963 941 919
160 8.625 0.906 2298 2298 2298 2133 1982 1858 1817 1775 1734
10″ 40 10.75 0.365 699 699 699 649 603 565 553 540 528
80 10.75 0.594 1159 1159 1159 1075 999 937 916 895 874
160 10.75 1.125 2289 2289 2289 2124 1974 1850 1809 1768 1727
Les types Out diameter Tailles Longueur
NB Sizes (in stock) .0035” ~ 20” 1/8″, 1/4″, 3/8″, 1/2″, 5/8″, 3/4″, 1″, 1.25″, 1.5″, 2″, 2.5″, 3″, 4″, 5″, 6″etc Cut to length
Stainless Steel 321/321H Seamless Tube (Custom Sizes) 6.35 mm OD To 508 mm OD As per requirement Cut to length
Stainless Steel 321/321H Welded Tube (ERW Tube) (in Stock + Custom Sizes) 6.35 mm OD To 1219 mm OD As per requirement Cut to length
Finition de la surface Internal Surface(ID) Exterbal Surface(OD)
Roughness Average(RA) Roughness Average(RA)
μ inch μm μ inch μm
AP Annealed & Pickled Not defined Not defined 40 or Not defined 1.0 or Not defined
BA Beight Annealed 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
MP Mechanical Polish 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
EP Electro Polish 15,10,7,5 0.38,0.25,0.20;0.13 32 0.8

The surface and shape of 321/321H stainless steel pipe (6)

Daxun is a trustworthy stainless steel pipe and tube manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 321 Stainless Steel pipe have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

Projets et produits récents

321/321H stainless steel pipe
tube en acier inoxydable sans soudure
321/321H stainless steel pipe
tube en acier inoxydable de grand diamètre
Tube en acier inoxydable poli
321/321H seamless pipe
BA stainless steel pipe
Tube en acier inoxydable
Stainless steel tube / pipe
321/321H stainless pipe
Stainless steel precision tube
Puis-je obtenir des échantillons ?

We can provide 321 Stainless Steel pipe samples for you to check the quality. Sample is free and you just pay the freight.

Quels sont les pays que vous avez déjà exportés ?

Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.

Quel est votre MOQ ?

Our MOQ is 1 ton for 321 Stainless Steel pipe.

Quel est le délai de livraison ?

Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.

Envoyez votre demande dès aujourd'hui
Devis rapide