Daxun 317 and 317L stainless steel PIPE and TUBE China supplier
As China’s leading Stainless Steel pipe and tube supplier and exporter, Daxun provides stainless steel PIPEs to the world.
- Grade: AISI 317/317L-S31700-S31703
- Manufacturing: hot-rolled, cold-drawn, forged, welded
- Normes : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Type: both seamless and welded pipes
- Diameter: from small diameter to large diameter pipes
- Thickness: thin-walled pipes and thick-walled pipes
- Surface: pickled, polished, bright annealed
- Length: 3000mm, 6000mm, 9000mm, etc.
Global leader in stainless steel pipe and tube fabrication services
Daxun is an exporter and supplier of 317L Stainless Steel Pipe and UNS S31703 Welded Pipe in various sizes, thicknesses and standards, Check online China SS Grade 1.4438 Stainless Steel Pipe Price
Daxun Alloy is a major maker of stainless steel pipes, and its SS 317/317L seamless pipes are unique. They are renowned for their durability and dimensional correctness. The domestic and worldwide nature of steel raw materials allows for the production of SS 317l pipes in a variety of sizes and thicknesses to meet the individual requirements of business customers. 317L alloy is a low carbon stainless steel with higher chromium, nickel, and molybdenum content than 316L for improved corrosion resistance. This steel is resistant to sulphurous acid, acetic acid, formic acid, citric acid, and tartaric acid, as well as pitting corrosion when exposed to phosphoric acid, chlorides, bromides, and iodides. 317L Stainless Steel Seamless Pipe, 317L Stainless Steel ERW Pipe, 317L Stainless Steel EFW Pipe, and 317L Stainless Steel Welded Pipe and Tube (Conforming to ASTM A213 / A312 / A269 / A358 Standards)
Daxun Alloys has been producing Type 317L Stainless Steel in various sizes and shapes for many years.
We sell 317L alloy that meets or surpasses numerous important international standards, including ASTM, ASME, UNS, DIN, and EN. We also offer SS 317L Tube in a variety of sizes, thicknesses, and specifications based on our customers’ specific needs. Stainless Steel Cold Drawn 317L Tube is a molybdenum-rich austenitic stainless steel, identical to SS 317 but with a greater molybdenum content. SS 317 Tube is available in cut-to-length sizes and can be manufactured or machined to match your specific piping needs. Contact Daxun today.
Données
- TECHNICAL PARAMETERS
- Information
- INGREDIENTS
- MECHANICAL PROPERTIES
- PROPRIÉTÉS PHYSIQUES
- EQUIVALENT GRADE
- PIPE TYPE
| AISI 317 pipe Material | SA213 TP 317 – ALLOY 317 – UNS S31700 – WNR 1.4438 |
| UNS S31700 Tube Standards | ASTM A213, ASTM A249, ASTM A269, ASME SA213, ASME SA249, ASME SA269, EN 10216-5 TC1 / TC2, PED 97/23/EC, AD 2000, NACE MR0175/ISO 15156 |
| 317 Stainless Steel Seamless Pipes & Tubes Manufacturing Specifications | ASME B36.19 |
| ASTM A213 | |
| ASTM A312 | |
| ASTM A269 | |
| ASTM A632 | |
| ASME SA213 | |
| NFA 49-117 | |
| BS 10216 | |
| Or as per customer specifications | |
| Seamless Tube Size | 3.35 mm OD To 101.6 mm OD |
| Welded Tube Size | 6.35 mm OD To 152 mm OD |
| Stainless Steel 317 Seamless Tube Swg & Bwg | 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg. |
| SS 317 ERW Pipe Wall thickness | 0.020″ –0.220″, (special wall thicknesses available) |
| ASTM A312 TP317 Pipe Length | Single Random, Double Random, Standard & Cut length |
| SS DIN 1.4438 / 1.4436 Rectangular Welded Pipes Finish | Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF |
| AMS 5573 Tube Form | Straight, Coiled, Seamless, Round Pipes/ Tubes, Square Pipes/ Tubes, Rectangular Pipe/ Tubes, Coiled Tubes, “U” Shape, Pan Cake Coils, Hydraulic Tubes, Straight or ‘U’ bent Tubes, Hollow, LSAW Tubes Etc. |
| UNS S31700 Square Pipes Type | Seamless, ERW, EFW, Welded, Fabricated |
| SS 317 Pipe Schedule | SCH5, SCH10, SCH10S, SCH20, SCH30, SCH40, SCH40S, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| 317 Stainless Steel Tube Electropolished | (EP) Electropolished for Ultra High Purity Systems |
| ASTM A312 TP317 Pipe Non-Electropolished | (BA) Bright Annealed or (AP) Annealed & Pickled for High-Purity, (CFOS) Cleaned for Oxygen Grade Service or Corrosive Systems |
| Stainless Steel 317 Seamless Tube & Pipe I.D. Surface Finish Options | 5, 7 & 10 µin. Ra |
| 317 Rectangular tubing JIS | 8A to 250A |
| SS 317 Tube Tolerances | In accordance with: ASTM: A269 & A632, JIS: G 3459 |
| 317 stainless steel tubing End | Plain End, Beveled End, Treaded, Ends are suitable for orbital welding |
| AMS 5573 Tube Marking | All 317 Stainless Steel tubes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.) |
| 317 stainless steel tubing Application | Oil Tube, Gas Tube, Fluid Tube, Boiler and Heatexchanger |
| SS 317 welded round tubes Value Added Service | Draw & Expansion as per required Size & Length, Polish (Electro & Commercial) Annealed & Pickled Bending, Machining Etc. |
| AMS 5584 Seamless/ welded tube Specialize in | Stainless Steel 317 Capillary Tube & Other Odd Size |
| Stainless Steel 317 Heat Exchanger & Condenser Tubes | |
| Stainless Steel 317 Hydraulic tubing with OD up to 50.8 mm (2.0 in.) are delivered in bright annealed condition | |
| Stainless Steel 317 hydraulic tube with OD larger than 50.8 mm are supplied in the annealed and pickled condition, Or in polished condition | |
| SS 317 welded square tubes Marking & Traceability | Each Stainless Steel 317 Tubing is traceable to its producing mill and heat by an identification number etched within 24″ (610mm) of one end. |
| 317 stainless steel tubing Test Certificate | Manufacturer Test Certificate according to EN 10204 3.1 B |
| Laboratory Test Certificate from Govt. Approved Lab. | |
| Under Third Party Inspection | |
| 317 stainless steel tubing Testing & Inspection | Visual inspection • Surface roughness measurement • Helium-leak testing • Scanning Electron Microscopy (SEM) • Auger Electron Microscopy (AES) • Election Spectroscopy for Chemical Analysis (ESCA or XPS) • Particle testing • Moisture testing |
| 317/317L Pipe and Tubing | |||||||
| Tailles | Standard Tolerances | ||||||
| Produits | OD | Wall | Lengths and/or coils | Notes | OD | Wall | Lengths |
| Welded Austenitic Steel Boiler, Super Heater, Heat-Exchangers & Condenser Tubes | 3/16″ (4.76 mm) to 4″ (101.6 mm) | 0.020″ (0.51 mm) to 0.220″ (5.59 mm) | Random or cut lengths up to 90′ (27.4 m) Coils to 1-1/2″ OD | 317/317L | Under 1″ (25.4 mm) ±0.004″ (0.10 mm) | ±10% | Randoms up to +2″ (50.8 mm) Cuts +1/8″ (3 mm) -0″ Coils to 80,000′ (24,384 m) |
| Specifications: ASTM-A249, ASME-SA249, ASTM-A688, ASME-SA688 | Metric sizes available | 1″ (25.4 mm) to 1-1/2″ (38.1 mm) ±0.006″ (0.15 mm) | |||||
| >1-1/2″ (38.1 mm) to 2″ (50.8 mm) ±0.008″ (0.20 mm) | |||||||
| >2″ (50.8 mm) to 2-1/2″ (63.5 mm) ±0.010″ (0.25 mm) | |||||||
| >2-1/2″ (63.5 mm) to 3″ (76.2 mm) ±0.012″ (0.30 mm) | |||||||
| 3″ (76.2 mm) to 4″ (101.6 mm) ±0.015″ (0.38 mm) | |||||||
| Pressure & Corrosion Tubing | 1/16″ (1.59 mm) to 4″ (101.6 mm) | 0.010″ (0.25 mm) to 0.220″ (5.59 mm) | Random or cut lengths up to 90′ (27.4 m) | 317/317L | <1-1/2″ (38.1 mm) ±0.005″ (0.13 mm) 1-1/2″ (38.1 mm) to 3″ (76.2 mm) ±0.010″ (0.25 mm) | ±10% | Randoms up to +2″ (50.8 mm) |
| Meets or exceeds requirements for welded | Metric sizes available | Coils to 1-1/2″ OD | 3-1/2″ (88.9 mm) to 4″ (101.6 mm) ±0.015″ (0.38 mm) | Cuts +1/8″ (3 mm) -0″ | |||
| Specifications: ASTM-A269, ASTM-A1016, and ASTM-A632 | Coils to 80,000′ (24,384 m) | ||||||
| Instrumentation Tubing | 1/16″ (1.59 mm) to 1/2″ (12.7 mm) | 0.010″ (0.25 mm) to 0.065″ (1.65 mm) | Random or cut lengths up to 40′ (12.2 m) | 317/317L | ±0.005″ (0.13 mm) | ±10% | Randoms up to +2″ (50.8 mm) |
| Specifications: ASTM-A269 and ASTM-A632 | Metric sizes available | Cuts +1/8″ (3 mm) -0″ | |||||
| Composition of 317/317L tubing and pipe | ||
| Grade | 317 | 317L |
| Désignation UNS | S31700 | S31703 |
| Carbone (C) Max. | 0.08 | 0.035* |
| Manganèse (Mn) Max. | 2 | 2 |
| Phosphore (P) Max. | 0.04 | 0.04 |
| Soufre (S) Max. | 0.03 | 0.03 |
| Silicium (Si) Max. | 1 | 1 |
| Chrome (Cr) | 18.0-20.0 | 18.0-20.0 |
| Nickel (Ni) | 11.0–14.0 | 11.0–15.0 |
| Molybdène (Mo) | 3.0–4.0 | 3.0–4.0 |
| Azote (N) | — | — |
| Fer (Fe) | Bal. | Bal. |
| Autres éléments | — | — |
| *Maximum carbon content of 0.04% acceptable for drawn tubes | ||
| Physical Properties of 317/317L Alloys in the Annealed Condition at -20°F to +100°F | ||||||||||||||
| Résistance à la traction | Limite d'élasticité | |||||||||||||
| Alliage | Désignation UNS | Spec. | psi | MPa | ksi | psi | MPa | ksi | Elongation in 2 inches (min.) % | Grain Size Req. | Max. Hardness | Modulus of Elasticity (x106 psi) | Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) | Thermal Conductivity (BTU-in/ft2-h-°F) |
| 317 | S31700 | A249, A312 | 75,000 | 515 | 75 | 30,000 | 205 | 30 | 35 | — | 90 Rb | 28 | 9.2 | 116 |
| 317L | S31703 | A249, A312 | 70,000 | 485 | 70 | 25,000 | 170 | 25 | 35 | — | 90 Rb | 28 | 9.2 | 116 |
| Grade | Density (kg/m3) | Elastic Modulus (GPa) | Mean Coefficient of Thermal Expansion (m/m/0C) | Thermal Conductivity (W/m.K) | Specific Heat 0-1000C (J/kg.K) | Electrical Resistivity (n.m) | |||
| 0-1000C | 0-3150C | 0-5380C | at 1000C | at 5000C | |||||
| 317L | 8000 | 193 | 17.2 | 17.8 | 18.4 | 16.2 | 21.5 | 500 | 720 |
| 317 | 8000 | 193 | 17.2 | 17.8 | 18.4 | 16.2 | 21.5 | 500 | 720 |
| Grade | UNS No | Old British | Euronorm | Swedish SS | Japanese JIS | ||
| BS | En | No | Nom | ||||
| 317L | S31703 | – | – | 1.4438 | – | – | – |
| 317 | S31700 | – | – | 1.4449 | – | – | – |
| Din W.-Nr. 1.4438 Aisi 317L Corrugated Tube | Stainless Steel 317L Round Tube |
| UNS S31703 Seamless Pipe | Stainless Steel 317L Seamless Round Pipe |
| S31703 Stainless Steel U Shaped Tube | 317L Stainless Steel Square Tube Mirror Finish |
| Din 1.4438 Material Seamless Pipe | WERKSTOFF NR. 1.4438 Coaxial Tube |
| 317L Stainless Steel Rectangular Pipe | 317L Stainless Steel Hypodermic Pipe for Medical Needle |
| 317L Stainless Steel Oval Pipe | SS 317L Needle Tube |
| Din 1.4438 Stainless Steel Welded Pipe | ASTM A358 TP317L Coil Pipe Heat Exchanger |
| SAE J405 Uns S31703 Thin Wall Pipe | 317L Stainless Steel Metric Pipe |
| ASTM A312 TP317L Coiled Pipe | Stainless Steel Inox 317L Capillary Pipe |
| ASTM A312 gr TP 317L Aerospace tubes | ASTM A632 TP317L Electric Fusion Welding Pipe |
| Jis 317L Stainless Steel Coil Pipe | Stainless Steel 317L Seamless Pipe |
| Schedule 10 Type 317L Stainless Steel Pipe | Schedule 40 Type 317L Stainless Steel Pipe |
| Stainless Steel 317L Grade Pipe | Type 317L Stainless Steel Polished Pipe |
| ASTM A312 TP317L Elliptical Tubes | ASTM A213 SS TP 317L Stainless Steel Rectangular Tube |
| Material 1.4438 Aisi 317L Slotted Handrail Tube | SA312 TP317L Thin Wall Tube |
| Austenitic Stainless Steel 317L Pipe | DIN 1.4438 SS 317L Pipe |
| Alloy 317L Pipe | Stainless Steel 317L Seamless Pipe |
| Stainless Steel 317L EFW Pipe | Stainless Steel 317L Round Pipe |
| TP317L SS Welded Pipe | SS 317L Santiary Tube |
| ASTM A312 TP317L Pipe | SA312 TP317L square tubes |
| AISI 317l Stainless Steel Pipe | SS 317L Needle Tube |
| ASTM A269 TP317L Round Tube | ASTM A249 TP317L 317L hydraulic tube |
| Alloy 317L Pipe | NACE MR0175 |
| SA213 TP 317L Thick Wall Tube | En 1.4438 / Aisi 317L Hydraulic Pipe |
| Stainless Steel 317L Ornamental Pipe | Stainless Steel 317L Fin Tube / Finned Tube |
| 1.4438 Instrument Pipe | 317L Stainless Steel Square Pipe |
| Ultra-High Purity Electropolished Stainless Steel 317L Tube | Thin Wall S31703 Stainless Steel Pipe |
| 317L Stainless Steel ERW Pipe | Corrugated 317L Stainless Steel Tube (CSST) for Gas |
| SA 312 TP317L Seamless Pipe | Polished 317L Stainless Steel Pipe |
| 317L Stainless Steel Threaded Pipe | SAE 317L Stainless Steel Rectangular Tube |
| JIS SUS317L Seamless Tubes | Din 1.4438 Stainless Steel Tube |
| SA312 TP317L Welded Tubes | AISI 317L Seamless Tube |
| 317L Stainless Steel Seamless Square Pipe | Large Diameter 317L Stainless Steel Tube |
| SS 317L Erw Pipe | 317L Stainless Steel Instrumentation Pipe |
| High-pressure 317L Stainless Steel Water Pipe | Stainless Steel 317L Hexagonal Pipe |
| ASTM A358 TP317L Polished Pipe | 317L Stainless Steel Ornamental Tube |
| ASTM A312 TP317L erw | 317L Stainless Steel Spiral Pipe |
| ASME SA213 TP317L Perforated Tube | Din 1.4438 Material Tube |
| SA 688 TP317L Finned Tube | SA312 TP317L Dom Tube |
| Din 1.4438 AISI 317L Perforated Exhaust Tube | Stainless Steel 317L Hypodermic Pipe |
| ASTM A213 TP317L Condenser Tube | Stainless Steel 317L Welded Pipe & Tube |
| ASTM A269 TP317L straight tube | 317L Stainless Steel Welded Tube |
| ASTM A249 TP317L Mirror Tube | Jis 317L Stainless Steel Pipe |
| 317L Stainless Steel Seamless Pipe | SS UNS S31703 Welded Pipe |
| ASTM A312 TP 317L SS Seamless Pipe | 317L SS Electropolished Pipe |
| DIN 1.4438 SS 317L Pipe | Stainless Steel 317L Pipe |
| Stainless Steel 317L Seamless Pipe | WERKSTOFF NR.1.4449 SS 317L Pipe |
| SS 317L Hexagonal Pipe | 317L SS Hollow Pipe |
| SS 317L Bush Hex Pipe | SS 317L Welded Pipe |
| SS TP317L Seamless Pipe | TP317L SS Welded Pipe |
Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

Quick response-317 Stainless Steel pipe
- Provide seamless and welded pipes
- Bonne formabilité et soudabilité
- Increased resistance to chemical attack from acids
- Lower carbon content leads to resistance to sensitization when welded
- Excellent corrosion resistance in harsh environments.
- Higher creep strength, rupture stress and tensile strength.
- Pitting and crevice corrosion resistance
Avantages de Daxun
- Variety: From small to large diameter stainless steel pipe, we offer a wide range of sizes and grades, including 304L, 316L, 317L and more.
- Flexibility: Whether you need seamless or welded steel pipe, our stainless steel pipe lengths are designed to meet your specific project requirements.
Quality - Standards: Our stainless steel pipes meet stringent standards such as ISO9001, ABS, NSF/ANSI Standard 61, and NACE MR0175 to ensure reliability and performance.
- Custom Orders: Looking for special size stainless steel pipes? We offer a variety of stainless steel pipe custom options at competitive prices and convenient online ordering.


317 Stainless Steel pipe packaging
- Woven bag bale cargo (hexagonal)
- Special crates for U-bend pipes, (steel/wood) divided
- Each bale is wrapped in plastic to protect against wind and rain.
- SS 317 seamless pipes are protected by plastic covers.
- Plastic strips are used to secure the bale.
- Export-specific fumigation-free wooden crate packaging.
- Laminated packing slip attached to the bale or crate.
- Customized packaging as per customer needs.
317 Stainless Steel pipe Ordering Information
317 stainless steel pipe The purchase order shall include quantity, PSL grade, type or class, API5L reference, outside diameter, wall thickness, length and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Pipe is solution bright annealed.


Qualité, livraison, inspection
- Daxun effectue également plusieurs tests d'assurance qualité. Ces tests comprennent le test d'aplatissement, le test de piqûre et de résistance, le test mécanique, le test de dureté, l'identification positive du matériau, le test d'expansion, etc. Tous ces tests garantissent que le matériau est adapté à l'application requise.
- Au cours du processus de production, nous mesurons le diamètre, l'épaisseur et la surface du produit. Notre délai de livraison standard est de 7 à 15 jours, sauf pour certains produits de taille spéciale, pour lesquels le délai de livraison peut atteindre 20 jours.
Nos délais de livraison sont strictement conformes au contrat. - Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
- Fournir des échantillons gratuits aux clients pour qu'ils les testent
- Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Support technique
Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.

317 and 317L Stainless Steel pipe and tube Features
Daxun Alloy Permettez à votre marque de s'améliorer rapidement
- Galerie
- 317/317L STEEL PIPE DATA TUBE
- PRESSURE RATING
- SIZE
- Surface finish
| NPS | Outside Diameter | Épaisseur de la paroi | Weight | Weight | |||
| in | mm | in | mm | Sched | kg/Mtr | Lb/ft | |
| 1/2″ | 0.84 | 21 | 0.109 | 2.769 | 40 STD | 1.268 | 0.851 |
| 0.147 | 3.734 | 80 STD | 1.621 | 1.088 | |||
| 3/4″ | 1.05 | 27 | 0.113 | 2.87 | 40 STD | 1.684 | 1.131 |
| 0.154 | 3.912 | 80 STD | 2.195 | 1.474 | |||
| 1″ | 1.315 | 33 | 0.133 | 3.378 | 40 STD | 2.501 | 1.679 |
| 0.179 | 4.547 | 80 STD | 3.325 | 2.172 | |||
| 1 1/4″ | 1.66 | 42 | 0.14 | 3.556 | 40 STD | 3.385 | 2.273 |
| 0.191 | 4.851 | 80 STD | 4.464 | 2.997 | |||
| 1 1/2″ | 1.9 | 48 | 0.145 | 3.683 | 40 STD | 4.048 | 2.718 |
| 0.2 | 5.08 | 80 STD | 5.409 | 3.361 | |||
| 2″ | 2.375 | 60 | 0.154 | 3.912 | 40 STD | 5.441 | 3.653 |
| 0.218 | 5.537 | 80 STD | 7.48 | 5.022 | |||
| 2 1/2″ | 2.875 | 73 | 0.203 | 5.516 | 40 STD | 8.629 | 5.793 |
| 0.276 | 7.01 | 80 STD | 11.411 | 7.661 | |||
| 3″ | 3.5 | 89 | 0.216 | 5.486 | 40 STD | 11.284 | 7.576 |
| 0.3 | 7.62 | 80 STD | 15.272 | 10.253 | |||
| 4″ | 4.5 | 114 | 0.237 | 6.02 | 16.073 | 10.79 | |
| 0.337 | 8.56 | 22.318 | 14.983 | ||||
| 6″ | 6.625 | 168 | 0.188 | 4.775 | 19.252 | 12.924 | |
| 0.203 | 5.516 | 20.739 | 13.923 | ||||
| 0.219 | 5.563 | 22.318 | 14.983 | ||||
| 0.25 | 6.35 | 25.354 | 17.021 | ||||
| 0.28 | 7.112 | 40 STD | 58.263 | 18.974 | |||
| 0.312 | 7.925 | 31.334 | 21.036 | ||||
| 0.375 | 9.525 | 37.285 | 25.031 | ||||
| 0.432 | 10.973 | 80 XHY | 42.561 | 28.573 | |||
| 0.5 | 12.7 | 48.719 | 32.708 | ||||
| 8″ | 8.625 | 219 | 0.188 | 4.775 | 25.233 | 16.94 | |
| 0.203 | 5.156 | 27.198 | 18.259 | ||||
| 0.219 | 5.563 | 29.286 | 19.661 | ||||
| 0.25 | 6.35 | 20 | 33.308 | 22.361 | |||
| 0.277 | 7.036 | 30 | 36.786 | 24.696 | |||
| 0.322 | 8.179 | 40 | 42.352 | 28.554 | |||
| 0.375 | 9.525 | 49.216 | 33.041 | ||||
| 0.406 | 10.312 | 60 | 53.085 | 35.638 | |||
| 0.5 | 12.7 | 80 XHY | 64.627 | 43.388 | |||
| 10″ | 10.75 | 273 | 0.188 | 4.775 | 31.588 | 21.207 | |
| 0.219 | 5.563 | 36.689 | 24.631 | ||||
| 0.25 | 6.35 | 20 | 41.759 | 28.035 | |||
| 0.307 | 7.798 | 30 | 51.002 | 34.24 | |||
| 0.344 | 8.738 | 56.946 | 38.231 | ||||
| 0.365 | 9.271 | 40 STD | 63.301 | 40.483 | |||
| 0.438 | 11.125 | 71.852 | 48.238 | ||||
| 0.5 | 12.7 | 60 XHY | 81.53 | 54.735 | |||
| 0.594 | 15.088 | 80 | 95.969 | 64.429 | |||
| 12″ | 12.75 | 324 | 0.188 | 4.775 | 37.57 | 25.222 | |
| 0.219 | 5.563 | 43.657 | 29.309 | ||||
| 0.25 | 6.35 | 49.713 | 33.375 | ||||
| 0.281 | 7.137 | 55.739 | 37.42 | ||||
| 0.312 | 7.925 | 61.735 | 41.445 | ||||
| 0.375 | 9.525 | 73.824 | 49.562 | ||||
| 0.406 | 10.312 | 79.727 | 53.525 | ||||
| 0.5 | 12.7 | 97.438 | 65.415 | ||||
| 0.562 | 14.275 | 108.966 | 73.154 | ||||
| 14″ | 14 | 356 | 0.188 | 4.775 | 41.308 | 27.732 | |
| 0.219 | 5.563 | 48.012 | 32.233 | ||||
| 0.25 | 6.35 | 20 | 54.685 | 36.713 | |||
| 0.281 | 7.137 | 61.327 | 41.172 | ||||
| 0.312 | 7.925 | 67.939 | 45.611 | ||||
| 0.375 | 9.525 | STD | 81.281 | 54.568 | |||
| 0.438 | 11.125 | 40 | 94.498 | 63.441 | |||
| 0.5 | 12.7 | XHY | 107.381 | 72.09 | |||
| 0.625 | 15.875 | 132.983 | 89.278 | ||||
| 16” | 16 | 406 | 0.188 | 4.775 | 47.29 | 21.748 | |
| 0.219 | 5.563 | 54.98 | 36.91 | ||||
| 0.25 | 6.35 | 10 | 62.639 | 42.053 | |||
| 0.281 | 7.137 | 70.268 | 47.174 | ||||
| 0.312 | 7.925 | 20 | 77.866 | 52.275 | |||
| 0.344 | 8.738 | 85.677 | 57.519 | ||||
| 0.375 | 9.525 | 30 | 93.213 | 62.578 | |||
| STD | |||||||
| 0.438 | 11.125 | 108.433 | 72.797 | ||||
| 0.5 | 12.7 | 40 | 123.289 | 82.77 | |||
| XHY | |||||||
| 18″ | 18 | 457 | 0.219 | 5.563 | 61.948 | 41.588 | |
| 0.25 | 6.35 | 70.593 | 47.393 | ||||
| 0.281 | 7.137 | 79.208 | 53.176 | ||||
| 0.312 | 7.925 | 20 | 87.792 | 58.939 | |||
| 0.375 | 9.525 | STD | 105.144 | 70.588 | |||
| 0.438 | 11.125 | 30 | 122.369 | 82.152 | |||
| 0.5 | 12.7 | XHY | 139.198 | 93.45 | |||
| 0.562 | 14.275 | 40 | 155.904 | 104.666 | |||
| 0.625 | 15.875 | 172.754 | 115.978 | ||||
| 20″ | 20 | 508 | 0.25 | 6.35 | 78.547 | 52.733 | |
| 0.282 | 7.163 | 88.458 | 59.386 | ||||
| 0.312 | 7.925 | 97.719 | 65.604 | ||||
| 0.375 | 9.525 | 20 STD | 117.075 | 78.598 | |||
| 0.438 | 11.125 | 136.305 | 91.508 | ||||
| 0.5 | 12.7 | 30 XHY | 155.106 | 104.13 | |||
| 0.594 | 15.088 | 40 | 183.378 | 123.11 | |||
| 0.625 | 15.875 | 192.64 | 129.328 | ||||
| 0.688 | 17.475 | 211.368 | 141.901 | ||||
| 24″ | 24 | 610 | 0.25 | 6.35 | 94.456 | 63.413 | |
| 0.281 | 7.137 | 106.029 | 71.183 | ||||
| 0.312 | 7.925 | 117.573 | 18.932 | ||||
| 0.375 | 9.525 | 20 STD | 140.938 | 64.618 | |||
| 0.438 | 11.125 | 164.176 | 110.219 | ||||
| 0.5 | 12.7 | XHY | 186.923 | 125.49 | |||
| 0.625 | 15.875 | 232.41 | 156.028 | ||||
| 0.688 | 17.475 | 40 | 255.148 | 171.293 | |||
| 0.75 | 19.05 | 277.401 | 186.233 | ||||
| 30″ | 30 | 762 | 0.25 | 6.35 | 118.318 | 79.433 | |
| 0.281 | 7.137 | 132.851 | 89.189 | ||||
| 0.312 | 7.925 | 10 | 147.353 | 98.925 | |||
| 0.375 | 9.525 | STD | 176.731 | 118.648 | |||
| 0.438 | 11.125 | 205.983 | 138.286 | ||||
| 0.5 | 12.7 | 20 XHY | 234.647 | 157.53 | |||
| 0.625 | 15.875 | 30 | 292.066 | 196.078 | |||
| 0.688 | 17.475 | 320.817 | 215.38 | ||||
| 0.75 | 19.05 | 348.988 | 234.293 | ||||
| 36″ | 36 | 914 | 0.25 | 6.35 | 142.18 | 95.453 | |
| 0.281 | 7.137 | 159.672 | 107.196 | ||||
| 0.312 | 7.925 | 10 | 177.133 | 118.918 | |||
| 0.375 | 9.525 | STD | 215.525 | 142.678 | |||
| 0.438 | 11.125 | 247.79 | 166.353 | ||||
| 0.5 | 12.7 | 20 XHY | 282.372 | 198.57 | |||
| 0.625 | 15.875 | 351.723 | 236.128 | ||||
| 0.688 | 17.475 | 386.487 | 259.467 | ||||
| 0.75 | 19.05 | 420.576 | 282.353 | ||||
| 42″ | 42 | 1067 | 0.312 | 7.925 | 206.914 | 138.911 | |
| 0.375 | 9.525 | STD | 248.319 | 166.708 | |||
| 0.5 | 12.7 | XHY | 33.097 | 221.61 | |||
| 0.75 | 19.05 | 492.163 | 330.413 | ||||
| 48″ | 48 | 1219 | 0.375 | 9.525 | STD | 284.112 | 190.738 |
| 0.438 | 11.125 | 331.404 | 222.487 | ||||
| 0.5 | 12.7 | XHY | 377.822 | 253.65 | |||
| 0.75 | 19.05 | 563.75 | 378.473 | ||||
| 0.875 | 22.225 | 655.969 | 440.383 | ||||
| PRESSURE RATING (PSIG) | ||||||||||||
| SIZES | SCHEDULE (SCH) | OUTSIDE | WALL | TEMPERATURE (OF) | ||||||||
| (INCHES) | DIA. | THICK. | 100 | 200 | 300 | 400 | 500 | 600 | 650 | 700 | 750 | |
| (IN) | (IN) | ALLOWABLE STRESS (PSI) | ||||||||||
| 16700 | 16700 | 16700 | 15500 | 14400 | 13500 | 13200 | 12900 | 12600 | ||||
| 1″ | 40 | 1.315 | 0.133 | 2205 | 2205 | 2205 | 2047 | 1902 | 1783 | 1743 | 1703 | 1664 |
| 80 | 1.315 | 0.179 | 3061 | 3061 | 3061 | 2841 | 2640 | 2475 | 2420 | 2365 | 2310 | |
| 160 | 1.315 | 0.25 | 4493 | 4493 | 4493 | 4170 | 3874 | 3632 | 3552 | 3471 | 3390 | |
| 1 1/2″ | 40 | 1.9 | 0.145 | 1629 | 1629 | 1629 | 1512 | 1404 | 1317 | 1287 | 1258 | 1229 |
| 80 | 1.9 | 0.2 | 2303 | 2303 | 2303 | 2138 | 1986 | 1862 | 1821 | 1779 | 1738 | |
| 160 | 1.9 | 0.281 | 3362 | 3362 | 3362 | 3120 | 2899 | 2717 | 2657 | 2597 | 2536 | |
| 2″ | 40 | 2.375 | 0.154 | 1371 | 1371 | 1371 | 1272 | 1182 | 1108 | 1083 | 1059 | 1034 |
| 80 | 2.375 | 0.218 | 1985 | 1985 | 1985 | 1843 | 1712 | 1605 | 1569 | 1534 | 1498 | |
| 160 | 2.375 | 0.344 | 3283 | 3283 | 3283 | 3047 | 2831 | 2654 | 2595 | 2536 | 2477 | |
| 3″ | 40 | 3.5 | 0.216 | 1301 | 1301 | 1301 | 1208 | 1122 | 1052 | 1028 | 1005 | 982 |
| 80 | 3.5 | 0.3 | 1844 | 1844 | 1844 | 1712 | 1590 | 1491 | 1458 | 1425 | 1391 | |
| 160 | 3.5 | 0.438 | 2787 | 2787 | 2787 | 2587 | 2403 | 2253 | 2203 | 2153 | 2103 | |
| 4″ | 40 | 4.5 | 0.237 | 1102 | 1102 | 1102 | 1023 | 950 | 891 | 871 | 851 | 831 |
| 80 | 4.5 | 0.337 | 1596 | 1596 | 1596 | 1482 | 1377 | 1291 | 1262 | 1233 | 1204 | |
| 160 | 4.5 | 0.531 | 2611 | 2611 | 2611 | 2424 | 2552 | 2111 | 2064 | 2017 | 1970 | |
| 5″ | 40 | 5.563 | 0.258 | 965 | 965 | 965 | 896 | 832 | 780 | 763 | 746 | 728 |
| 80 | 5.563 | 0.375 | 1428 | 1428 | 1428 | 1325 | 1231 | 1154 | 1129 | 1103 | 1077 | |
| 160 | 5.563 | 0.625 | 2474 | 2474 | 2474 | 2296 | 2133 | 2000 | 1955 | 1911 | 1866 | |
| 6″ | 40 | 6.625 | 0.28 | 877 | 877 | 877 | 814 | 756 | 709 | 693 | 677 | 661 |
| 80 | 6.625 | 0.432 | 1379 | 1379 | 1379 | 1280 | 1189 | 1115 | 1090 | 1065 | 1040 | |
| 160 | 6.625 | 0.719 | 2382 | 2382 | 2382 | 2211 | 2054 | 1925 | 1883 | 1840 | 1797 | |
| 8″ | 40 | 8.625 | 0.322 | 771 | 771 | 771 | 716 | 665 | 623 | 610 | 596 | 582 |
| 80 | 8.625 | 0.5 | 1218 | 1218 | 1218 | 1131 | 1050 | 985 | 963 | 941 | 919 | |
| 160 | 8.625 | 0.906 | 2298 | 2298 | 2298 | 2133 | 1982 | 1858 | 1817 | 1775 | 1734 | |
| 10″ | 40 | 10.75 | 0.365 | 699 | 699 | 699 | 649 | 603 | 565 | 553 | 540 | 528 |
| 80 | 10.75 | 0.594 | 1159 | 1159 | 1159 | 1075 | 999 | 937 | 916 | 895 | 874 | |
| 160 | 10.75 | 1.125 | 2289 | 2289 | 2289 | 2124 | 1974 | 1850 | 1809 | 1768 | 1727 | |
| Les types | Out diameter | Tailles | Longueur |
| NB Sizes (in stock) | .0035” ~ 20” | 1/8″, 1/4″, 3/8″, 1/2″, 5/8″, 3/4″, 1″, 1.25″, 1.5″, 2″, 2.5″, 3″, 4″, 5″, 6″etc | Cut to length |
| Stainless Steel 317/317L Seamless Tube (Custom Sizes) | 6.35 mm OD To 508 mm OD | As per requirement | Cut to length |
| Stainless Steel 317/317L Welded Tube (ERW Tube) (in Stock + Custom Sizes) | 6.35 mm OD To 1219 mm OD | As per requirement | Cut to length |
| Finition de la surface | Internal Surface(ID) | Exterbal Surface(OD) | |||
| Roughness Average(RA) | Roughness Average(RA) | ||||
| μ inch | μm | μ inch | μm | ||
| AP | Annealed & Pickled | Not defined | Not defined | 40 or Not defined | 1.0 or Not defined |
| BA | Beight Annealed | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| MP | Mechanical Polish | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| EP | Electro Polish | 15,10,7,5 | 0.38,0.25,0.20;0.13 | 32 | 0.8 |
The surface and shape of 317/317L stainless steel PIPE (6)
Informations disponibles pour référence et téléchargement
Daxun is a trustworthy stainless steel pipe and tube manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel tube are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 317 Stainless Steel pipe and tube have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
Projets et produits récents
Produits apparentés (10)
We can provide 317 Stainless Steel pipe and tube samples for you to check the quality. Sample is free and you just pay the freight.
Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.
Our MOQ is 1 ton for stainless steel 317 Stainless Steel pipe and tube.
Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.