310S-310-31008 stainless steel bars and round bars China supplier
En tant que principal fournisseur et exportateur d'acier inoxydable en Chine, Daxun fournit des barres d'acier inoxydable.(barres rondes) dans le monde entier.
- High temperature resistance
- Haute résistance
- Résistance à la corrosion
- Reliability
- Grade: 310S-2520
Fabrication : laminage à chaud, étirage à froid, forgeage
Standards: ASTM, ASME, GB, DIN, JIS, ISO
For over 20 years, Daxun Alloys has been the premier supplier of heat resistant, high temperature 310 or 310S stainless steel bar. Contact Daxun to learn more about how 310S SS can best suit your specific application.
310S Global leader in stainless rod and Round Bar fabrication services
Daxun Alloys is a reputable manufacturer of high-quality SS 310 / 310S Round Bars with a variety of characteristics. Stainless Steel 310 / 310S Round Bars are austenitic stainless steel that is based on chromium and nickel. SS310/310S Round Bars/Rods have exceptional properties such as durability, flexibility, workability, machinability, weldability, ductility, fabricability, high strength, and hardness. These rods are mostly useful for industrial chemistry and nut manufacture. These rods are most likely the most popular on the market due to their anti-corrosion qualities. These rods and bars withstand extreme temperatures. These rods may be simply utilized at annealing temperatures without deforming the rod. We supply Stainless Steel Round Bars to our valued clients at market-leading costs. We can customize round bars in a variety of finishes, lengths, and shapes to meet our clients’ specific wants or specifications. We sell circular bars that may be conveniently used in industrial applications.
Notre réseau de centres de service stocke des produits en barres d'acier inoxydable pour un approvisionnement rapide en barres de tailles et d'alliages courants.Nous produisons également des barres d'acier inoxydable de taille personnalisée et pouvons organiser des programmes d'inventaire pour une rotation rapide si les quantités sont inférieures aux minimums de l'usine.Daxun Alloys stocke des barres rondes en acier inoxydable avec des diamètres allant de 1/16″ à 26″. Les barres rondes sont disponibles dans presque toutes les nuances d'acier inoxydable, y compris 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205, et Alloy 20. Les barres rondes en acier inoxydable traitées thermiquement sont proposées en 17-4PH, H900 (sur demande), H1025, H1150, Double H1150 et H1150M. D'autres températures de traitement thermique peuvent être fabriquées sur demande. Nous stockons les aciers inoxydables de la série 400 suivants : 410, 430 et 416. Nous avons également en stock des barres rondes en acier inoxydable de précision et de qualité roulement 303, 304 et 316/L. La majeure partie de notre stock est constituée de nos barres usinées uniques : des barres rondes en acier inoxydable qui sont fondues selon des normes cohérentes afin d'augmenter leur usinabilité et de réduire le coût total par composant. Nos machines de traitement des barres en acier inoxydable permettent à Daxun Alloys de produire selon les spécifications exactes de nos clients.
Données
- Paramètres
- Ingrédients
- Propriétés mécaniques
- PROPRIÉTÉS PHYSIQUES
- Tous les équivalents
- Les types
| Paramètres du produit : Tige en acier inoxydable | |
| Spécifications | ASTM A276, ASME SA276 / ASTM A479 ASME SA479 |
| Dimensions | EN, DIN, JIS, ASTM, BS, ASME, AISI |
| SS 310/310S Round Bars | Diamètre extérieur de 4 mm à 500 mm |
| SS 310/310S Bright Bars | Diamètre extérieur de 4 mm à 100 mm |
| SS 310/310S Hex Bars | 18mm - 57mm (11/16″ à 2-3/4″) |
| Finition | Noir, poli brillant, brut de décolletage, finition NO.4, finition mate, finition BA |
| Longueur | 1 à 6 mètres, longueurs de coupe personnalisées |
| Formulaire | Ronde, carrée, hexagonale (A/F), rectangulaire, billette, lingot, forgeage, etc. |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Fe |
| SS 310 | 0.015 max | 2.0 max | 0.15 max | 0.020 max | 0.015 max | 24.00 – 26.00 | 0.10 max | 19.00 – 21.00 | 54.7 min |
| SS 310S | 0.08 max | 2.0 max | 1.00 max | 0.045 max | 0.030 max | 24.00 – 26.00 | 0.75 max | 19.00 – 21.00 | 53.095 min |
| Densité | Point de fusion | Résistance à la traction | Yield Strength (0.2%Offset) | Élongation |
| 7.9 g/cm3 | 1402 °C (2555 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 40% |
| Propriété | Au | Valeur | unit |
| Densité | 8,000 | kg/m³ | |
| Plage de fusion | 1400 – 1450 | °C | |
| Module d'élasticité | 20°C | 200 | GPa |
| Module de cisaillement | 20°C | 77 | GPa |
| Rapport de Poisson | 20°C | 0.3 | |
| Conductivité thermique | 100°C | 14.2 | W / m. °C |
| Résistivité électrique | 25°C | 0.78 | micro-ohm . m |
| Electrical Conductivity | 25°C | 1.25 | % IACS |
| Chaleur spécifique | 500 | J/kg. °C | |
| Relative Magnetic Permeability | 1.02 | ||
| Coefficient of Expansion | 0 – 100°C | 15.9 | /°C |
| 0 – 315°C | 16.2 | /°C | |
| 0 – 540°C | 17 | /°C |
| Grade | CHINA | UNS No | Old British | Euronorm | Swedish SS | Japanese JIS | GOST | ||
| BS | En | No | Nom | ||||||
| 310S | 00Cr25Ni20 | S31008 | 304S31 | 58E | 1.4845 | X5CrNi18-10 | 2332 | SUS 310S | 20Ch23N18 |
| Stainless Steel 310/310S Bright Bar | SS 310/310S Bright Bar |
| 310/310S SS Bright Bar | |
| Stainless Steel 310/310S Bright Bar | |
| UNS S310/310S00 SS Bright Bar | |
| WERKSTOFF NR. 1.4845 Bright Bar | |
| ASTM A276 310/310S Stainless Steel Bright Bar | |
| Stainless Steel 310/310S Hex Bar | SS 310/310S Hex Bar |
| 310/310S SS Hexagonal Bar | |
| 310/310S Stainless Steel Hex Bar | |
| UNS S310/310S00 SS Hexagonal Bar | |
| ASTM A276 310/310S Stainless Steel Hex Bar | |
| Stainless Steel 310/310S Square Bar | SS 310/310S Square Bar |
| 310/310S SS Square Bars | |
| 310/310S Stainless Steel Square Bar | |
| UNS S310/310S00 SS Square Bar | |
| WERKSTOFF NR. 1.4845 Square Bar | |
| ASTM A479 310/310S Stainless Steel Square Bars | |
| Stainless Steel 310/310S Rectangular Bar | SS 310/310S Rectangular Bar |
| 310/310S SS Rectangular Bars | |
| 310/310S Stainless Steel Rectangular Bar | |
| UNS S310/310S00 SS Rectangular Bars | |
| WERKSTOFF NR. 1.4845 Rectangular Bar | |
| ASTM A276 310/310S Stainless Steel Rectangular Bar | |
| Stainless Steel 310/310S Flat Bars | SS 310/310S Flat Bar |
| 310/310S SS Flat Bars | |
| 310/310S Stainless Steel Flat Bars | |
| UNS S310/310S00 SS Flat Bars | |
| WERKSTOFF NR. 1.4845 Flat Bars | |
| ASTM A276 310/310S Stainless Steel Flat Bars | |
| Stainless Steel 310/310S Polished Bar | SS 310/310S Polished Bar |
| 310/310S SS Polished Bars | |
| 310/310S Stainless Steel Polished Bar | |
| UNS S310/310S00 SS Polished Bars | |
| WERKSTOFF NR. 1.4845 Polished Bar | |
| ASTM A476 310/310S Stainless Steel Polished Bar | |
| Stainless Steel 310/310S Threaded Bar | SS 310/310S Threaded Bar |
| 310/310S SS Threaded Bars | |
| 310/310S Stainless Steel Threaded Bar | |
| UNS S310/310S00 SS Threaded Bar | |
| WERKSTOFF NR. 1.4845 Threaded Bar | |
| ASTM A276 310/310S Stainless Steel Threaded Bar |
Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

Quick response-310S Stainless Steel Rod
We provide timely and fast delivery of stainless steel rod products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Avantages de Daxun
- Variétés : Nous proposons une large gamme de tailles et de qualités, y compris les séries 300, 400, 600, etc.
- Flexibilité : Que vous ayez besoin de barres laminées à chaud ou étirées à froid, nos longueurs de barres en acier inoxydable sont conçues pour répondre aux exigences spécifiques de votre projet.
- Quality Standards: Our 310S Stainless Steel Rod meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
- Commandes personnalisées : Vous recherchez des barres en acier inoxydable de dimensions spéciales ? Nous offrons une variété d'options de personnalisation de barres en acier inoxydable à des prix compétitifs et une commande en ligne pratique.
310S Stainless Steel Rod packaging
We focus on every procedure to assure quality, the package we usually take is pack Stainless Steel Round Bar with environmental poly bags, and then in free fumigation wooden cases or wooden palte. Also can accept customized package such as OEM by negotiation. We offers just about everything to meet your Round Bar pack requirements. Lot of emphasis is placed on the packing and packaging. The Round Bar are packed in wooden corrugated boxes foiled in plastic wraps and bubble wraps.
Qualité, livraison, inspection
- Daxun effectue également plusieurs tests d'assurance qualité. Ces tests comprennent le test d'aplatissement, le test de piqûre et de résistance, le test mécanique, le test de dureté, l'identification positive du matériau, le test d'expansion, etc. Tous ces tests garantissent que le matériau est adapté à l'application requise.
- Au cours du processus de production, nous mesurons le diamètre, l'épaisseur et la surface du produit. Notre délai de livraison standard est de 7 à 15 jours, sauf pour certains produits de taille spéciale, pour lesquels le délai de livraison peut atteindre 20 jours.
Nos délais de livraison sont strictement conformes au contrat. - Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
- Fournir des échantillons gratuits aux clients pour qu'ils les testent
- Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Support technique
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.Stainless Steel rods
310S Stainless Steel Rod Ordering Information
Stainless Steel rods The purchase order shall include quantity, PSL grade, type or category, API5L reference, diameter, finish, length and any applicable attachments or additional requirements relating to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish or end finish. Bars are solution bright annealed.
310-310S Stainless Steel Rod Features
Daxun Alloy Permettez à votre marque de s'améliorer rapidement
- Galerie
- État de livraison
- Durcissement par l'âge
| Choix de l'État de livraison | État de surface |
| Forgé | Noir |
| Poli | |
| Laminés à chaud | Noir |
| Poli | |
| Lumineux | |
| Mariné | |
| Etiré à froid | Poli |
| Lumineux | |
| Remarque : | |
| 1. Si vous avez besoin d'un autre pays de livraison que ceux mentionnés ci-dessus, veuillez nous le confirmer. | |
| 2. En cas de demande ou de commande, veuillez nous faire part de toute exigence supplémentaire non indiquée ici. | |
| Les matériaux recuits par mise en solution peuvent être durcis par vieillissement comme suit:-*Dénote un double surstockage | ||||||||||||
| Condition | H900 (H480) | H925 (H495) | H1025 (H550) | H1075 (H580) | H1100 (H595) | H1150 (H620) | H1150M (H620M)* | Plus | H1150D (H620D)* | Plus | ||
| Chauffer jusqu'à | ±15oF | 900oF | 925 oF | 1025oF | 1075oF | 1100oF | 1150oF | 1400oF | 1150oF | 1150oF | 1150oF | |
| ±9oC | 480oC | 495oC | 550oC | 580oC | 595oC | 620oC | 760oC | 620oC | 620oC | 620oC | ||
| Tenir pendant des heures | 1 | 4 | 4 | 4 | 4 | 4 | 2 | 4 | 4 | 4 | ||
| Frais jusqu'en dessous | Air | Air | Air | Air | Air | Air | Air | Air | Air | Air | ||
| 90oF (32oC) | ||||||||||||
Types of 310-310S Stainless Steel Rods (3)
Informations disponibles pour référence et téléchargement
Daxun est un fabricant fiable de barres en acier inoxydable.
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless ros are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 310S Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
Projets et produits récents
Produits apparentés (11)
We can provide 310S Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.
Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.
Our MOQ is 1 ton for 310S Stainless Steel Rod.
Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.