Daxun Super Duplex 2507 Stainless Steel Alloys PIPE and TUBE China supplier

As China’s leading Stainless Steel pipe and tube supplier and exporter, Daxun provides stainless steel PIPEs to the world.
  • Grade: AISI 2507/S2507-S32750
  • Manufacturing method: hot rolling, cold rolling, forging, welding
  • Norme : ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Type: general seamless steel pipe
  • Diameter: from small diameter to large diameter tube
  • Thickness: thin wall tube and thick wall tube
  • Surface: pickled AP, polished, bright EP, annealed BA, etc.
  • Length: 3000mm, 6000mm, 9000mm, etc.

Global leader in stainless steel pipe and tube fabrication services

Daxun Alloys provides Duplex 2507 Stainless Steel Pipes – 2507 Stainless Steel Welded Pipes – 2507 Stainless Steel Seamless Pipes in a variety of shapes and sizes that meet industry standards such as ASTM, ASME, EURONORM, and AFNOR. AS 9100D Certified ASTM A790, UNS S32750, and UNS S32760 Seamless Pipe Supplier from China
Duplex 2507 stainless steel is a super duplex material with low carbon (up to 0.03%), chromium (~25%), nickel (~7%), and molybdenum (~4%) content. Duplex 2507 stainless steel is intended to meet the rigorous requirements of applications that demand high strength and corrosion resistance. These applications include chemical process equipment, the petrochemical industry, and seawater equipment. This steel is very resistant to chloride-induced stress corrosion cracking. Because of its high chromium, molybdenum, and nitrogen content, it offers exceptional resistance to pitting, crevice corrosion, and other types of corrosion.

Daxun Alloy understands the international specifications for super duplex seamless pipes and has the product knowledge to supply appropriate goods to our customers. We are one of China’s best super duplex pipe suppliers because to our competitive pricing, excellent quality, and timely delivery.
Super duplex seamless pipes are utilized in the oil and gas industry, as well as in naturally existing high-salinity horizontal wells or brine injection wells to improve oil recovery. Super duplex pipes are also very strong and resistant to corrosion, fatigue, and erosion. Astm A790 S32750 pipes are also resistant to uniform corrosion caused by organic acids like acetic and formic acids. Astm A790 Super Duplex Stainless Steel Seamless Pipes exhibit strong thermal conductivity and energy absorption. Furthermore, Super Duplex Hollow Pipes are easily machinable and weldable. WerkstoffWhen heated, pipes with the number 1.4410 deform less significantly. Deformation of super duplex pipes might lead to faulty flanges or connections. 2507 Super Duplex Pipes are utilized in heat exchangers in chemical processing, offshore oil and gas processing, and petrochemical manufacturing. Our 2507 Super Duplex Stainless Steel Pipes are compliant with international standards. Our Super Duplex 2507 Seamless Pipes are provided to a number of industries worldwide.

Lire la suite

Données

Spécifications Astm A790/ ASME SA790
Pipe Thickness 0.3mm – 50 mm
Pipe Standard EN, ASTM, ASME AISI, GB, JIS, DIN Super Duplex 2507 Pipe Supplier
Super Duplex 2507 Seamless Pipe Outer Diameter Sizes up to 12” NB/ 6.00 – 250 mm OD
Super Duplex 2507 Welded Pipe size 5.0 to 1219.2 mm
Super Duplex 2507 Welded Tube Size 6.35 – 810 mm OD
Super Duplex 2507 EFW Pipe size 5.0 – 1219.2 mm
Super Duplex 2507 tubing wall thickness 0.0020″ to 0.0220″ (custom wall thicknesses available)
Super Duplex 2507 Seamless Tube Size 15 NB – 508 NB IN/ 3.35 To 508 mm OD,
Super Duplex 2507 Pipe & Tube Finish AP (Annealed & Pickled), Polished, MF, BA (Bright & Annealed), NO.4, NO.1, BA, 2B, 8K, HL, Mirror finish,etc
Pipe & Tube Swg & Bwg 12 Swg., 10 Swg., 16 Swg., 14 Swg., 20 Swg, 18 Swg.
Super Duplex 2507 Pipe Schedule SCH10, SCH 5, SCH 80, SCH 40, , SCH 160, SCH 80S, SCH XS, SCH XXS
Super Duplex 2507 Pipe & Tube Form Hydraulic, Round, Rectangular, Hollow, Pan Cake Coils, Square, Coiled, “U” Shape, Straight Pipes etc.
Super Duplex 2507 Pipe & Tube Length Standard & Cut length, Single and Double Random,
Super Duplex 2507 Pipe & Tube Type Super Duplex 2507 ERW/ Seamless / Welded / EFW / CDW /Fabricated / CEW/ DOM Pipe
Pipe Value Added Service as per required Size & Length Draw & Expansion , Pickled Bending and Polish (Electro & Commercial) Annealed, Machining Etc.
Super Duplex 2507 Tube Application Oil Tube, Boiler and Heatexchanger, Gas Tube, Fluid Tube
Super Duplex 2507 Pipe & Tube End Beveled End, Plain End, Treaded Pipe.
Pipe Marking marked as follows All Super Duplex 2507 Pipes : Standard, Grade, Thickness, OD, Heat No. (Or according to the customer’s request.), Length
Material Test Certificates (MTC) 100% Radiography Test Report, Raw Materials Certificate
Material Test Certificates (MTC) as per EN 10204 3.1, EN 10204/3.1B and EN 10204 3.2
Manufacturer Test Certificate
Form A for Generalized System of Preferences (GSP)
Fumigation Certificates
Third Party Inspection Report
Heat Treatment Charts
Super Duplex 2507 Tubes HS Code Commercial Invoice
Laboratory Test Certificate from Govt. Approved Lab.
Spécialisé dans Super Duplex 2507 Heat Exchanger & Condenser Tubes
Super Duplex 2507 Capillary Tube & Other Odd Size
Large Diameter Super Duplex 2507 Pipe
Grade Super Duplex 2507
Désignation UNS S32750
Carbone (C) Max. 0.03
Manganèse (Mn) Max. 1.2
Phosphore (P) Max. 0.035
Soufre (S) Max. 0.02
Silicium (Si) Max. 0.8
Chrome (Cr) 24.0–26.0
Nickel (Ni) 6.0–8.0
Molybdène (Mo) 3.0–5.0
Azote (N) 0.24–0.32
Fer (Fe) Bal.
Copper (Cu) 0.5
Autres éléments
Physical Properties of Super Duplex 2507 Alloys in the Annealed Condition at -20°F to +100°F
Résistance à la traction Limite d'élasticité
Alliage Désignation UNS Spec. psi MPa ksi psi MPa ksi Elongation in 2 in. (min.) % Grain Size Req. Max. Hardness Modulus of Elasticity (x106 psi) Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) Thermal Conductivity (BTU-in/ ft2-h-°F)
Super Duplex 2507 S32950 A789, A790 100,000 690 100 70,000 485 70 20 30.5 Rc
Super Duplex 2507 S32750 A789, A790 116,000 800 116 80,000 550 80 15 32 Rc 27.5 7.2 98
Density, lb/in3 0.28
Modulus of Elasticity, psi 29.0x 106
Coefficient of Thermal Expansion, 68-212˚F, /˚F 7.5 x 10-6
Thermal Conductivity, Btu/ft hr ˚F 8
Specific Heat, Btu/lb ˚F 0.12
Electrical Resistivity, Microhm-in 31.5
Super Duplex 2507 Product Range
Alliage Désignation UNS Werkstoff NR. Specifications*
Super Duplex 2507 S32750 1.441 A/SA789, A/SA790
Super Duplex 2507 Exhaust Pipes Duplex2507 Super Duplex Round Pipes
Schedule 40 Alloy 2507 Pipes Nickel Super Duplex 2507 EFW Pipes
Alloy 2507 Pipes material Super Duplex 2507 Hexagonal Pipes
Alloy 2507 Capillary Pipes ASTM A790 SAF 2507 Custom Pipes
Small diameter Super Duplex 2507 Pipes Super Duplex 2507 Rectangular Pipes
High pressure 2507 Super Duplex Pipes Capillary Alloy 2507 Thin Pipes
WERKSTOFF NR. 2.4856 Clad Pipes Super Duplex 2507 Bush Hex Pipes
Super Duplex 2507 Thin Wall Pipes 2507 Alloy Square Pipes
Super Duplex 2507 Rectangular Tube Alloy 2507 elliptical and Oval Tube
Super Duplex 2507 SCH 80 Tube SAF 2507 Alloy SCH 40 Tube
Super Duplex 2507 Bellows Tubes Super Duplex 2507 High-strength capillary tubing
Super Duplex 2507 Transmission Tubes ASME SA790 SAF 2507 precision Tubes
ASME SA790 Super Duplex 2507 Electropolished Tube Super Duplex 2507 Instrumentation Tube
Super Duplex 2507 Electropolished Tube Super Duplex 2507 Seamless Hollow Tube
ASTM A790 SAF 2507 Oil & Gas Tubing Super Duplex 2507 Condenser Tube
Super Duplex 2507 SCH 80 Tube Super Duplex 2507 SCH 40 Tube
Super Duplex 2507 Aero engine Tubes Super Duplex 2507 cold drawn seamless Tubes
Super Duplex 2507 Furnace Tubes Super Duplex 2507 Gas Tubing
Super Duplex 2507 Cold drawn seamless tubing (CDS) Super Duplex 2507 Hot finished seamless tubing (HFS)
Super Duplex 2507 High Pressure Tubes SAF 2507 Alloy Precision Tubing
ASME SA790 SAF 2507 Capillary Tubing Super Duplex 2507 Bourdon Tubes
Alloy 2507 Finned Tubes Super Duplex 2507 Drawn over mandrel (DOM)
Super Duplex 2507 Furnace Tubes Super Duplex 2507 Aerospace Engine Tubes
Super Duplex 2507 seamless straight tubing Super Duplex 2507 seamless coil tubing

Choisissez Daxun et faites en sorte que vos clients soient satisfaits.

Contacter Daxun maintenant

Quick response 2507 Stainless Steel Pipe

  • Very strong resistance to uniform corrosion
  • Good resistance to inorganic acids/chlorides
  • For use with dilute hydrochloric acid
  • Improved machinability and weldability
  • Resistant to stress corrosion cracking in chloride-containing materials
  • Excellent resistance to pitting and crevice corrosion
  • Strong resistance to general corrosion
  • Extremely high mechanical strength
  • Good weldability
  • High impact strength
Contacter Daxun maintenant

2507 Stainless Steel Pipe quality policy

Daxun Alloy is committed to providing customers with defect-free products by:

Producing the highest quality and value 2507 stainless steel pipe products, quick response and on-time delivery, paying great attention to health, safety and environmental protection, and complying with laws. Use our experience and culture of continuous improvement to meet or exceed customer expectations and requirements for 2507 stainless steel pipes.

Contacter Daxun maintenant

Qualité, livraison, inspection

  • 2507 Stainless Steel Pipe:
  • Daxun effectue également plusieurs tests d'assurance qualité. Ces tests comprennent le test d'aplatissement, le test de piqûre et de résistance, le test mécanique, le test de dureté, l'identification positive du matériau, le test d'expansion, etc. Tous ces tests garantissent que le matériau est adapté à l'application requise.
  • Au cours du processus de production, nous mesurons le diamètre, l'épaisseur et la surface du produit. Notre délai de livraison standard est de 7 à 15 jours, sauf pour certains produits de taille spéciale, pour lesquels le délai de livraison peut atteindre 20 jours.
    Nos délais de livraison sont strictement conformes au contrat.
  • Aider les agences tierces des clients à se rendre à l'usine pour l'inspection
  • Fournir des échantillons gratuits aux clients pour qu'ils les testent
  • Soutien à l'inspection sur site ou à l'inspection vidéo en usine
Contacter Daxun maintenant

2507 Stainless Steel Pipe packaging

  1. Woven bag bale cargo (hexagonal)
  2. Special crates for U-bend pipes, (steel/wood) divided
  3. Each bale is wrapped in plastic to protect against wind and rain.
  4. SS 2507 seamless pipes are protected by plastic covers.
  5. Plastic strips are used to secure the bale.
  6. Export-specific fumigation-free wooden crate packaging.
  7. Laminated packing slip attached to the bale or crate.
  8. Customized packaging as per customer needs.
Contacter Daxun maintenant

2507 Stainless Steel Pipe Ordering Information

Duplex 2507/S32750 stainless steel pipe The purchase order shall include quantity, PSL grade, type or class, API5L reference, outside diameter, wall thickness, length and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Pipe is solution bright annealed.

Contacter Daxun maintenant

Support technique

Si vous avez besoin d'une assistance technique supplémentaire, notre métallurgiste résident et notre personnel compétent se feront un plaisir de vous aider. En outre, Daxun dispose d'un laboratoire d'essai certifié, une première dans l'industrie des stocks multimétaux et plastiques. Ceci, à notre avis, démontre notre dévouement inébranlable à la qualité et notre philosophie en tant que fournisseur de services complets.

Super Duplex 2507 Stainless Steel Alloys pipe and tube Features

Haute résistance
Résistance à la corrosion
Résistance à la chaleur
Résistance aux basses températures
Protection de l'environnement
Performance de soudage

Do as countless other companies have done — rely on Daxun alloy.

NPS Outside Diameter Épaisseur de la paroi Weight Weight
in mm in mm Sched kg/Mtr Lb/ft
1/2″ 0.84 21 0.109 2.769 40 STD 1.268 0.851
0.147 3.734 80 STD 1.621 1.088
3/4″ 1.05 27 0.113 2.87 40 STD 1.684 1.131
0.154 3.912 80 STD 2.195 1.474
1″ 1.315 33 0.133 3.378 40 STD 2.501 1.679
0.179 4.547 80 STD 3.325 2.172
1 1/4″ 1.66 42 0.14 3.556 40 STD 3.385 2.273
0.191 4.851 80 STD 4.464 2.997
1 1/2″ 1.9 48 0.145 3.683 40 STD 4.048 2.718
0.2 5.08 80 STD 5.409 3.361
2″ 2.375 60 0.154 3.912 40 STD 5.441 3.653
0.218 5.537 80 STD 7.48 5.022
2 1/2″ 2.875 73 0.203 5.516 40 STD 8.629 5.793
0.276 7.01 80 STD 11.411 7.661
3″ 3.5 89 0.216 5.486 40 STD 11.284 7.576
0.3 7.62 80 STD 15.272 10.253
4″ 4.5 114 0.237 6.02 16.073 10.79
0.337 8.56 22.318 14.983
6″ 6.625 168 0.188 4.775 19.252 12.924
0.203 5.516 20.739 13.923
0.219 5.563 22.318 14.983
0.25 6.35 25.354 17.021
0.28 7.112 40 STD 58.263 18.974
0.312 7.925 31.334 21.036
0.375 9.525 37.285 25.031
0.432 10.973 80 XHY 42.561 28.573
0.5 12.7 48.719 32.708
8″ 8.625 219 0.188 4.775 25.233 16.94
0.203 5.156 27.198 18.259
0.219 5.563 29.286 19.661
0.25 6.35 20 33.308 22.361
0.277 7.036 30 36.786 24.696
0.322 8.179 40 42.352 28.554
0.375 9.525 49.216 33.041
0.406 10.312 60 53.085 35.638
0.5 12.7 80 XHY 64.627 43.388
10″ 10.75 273 0.188 4.775 31.588 21.207
0.219 5.563 36.689 24.631
0.25 6.35 20 41.759 28.035
0.307 7.798 30 51.002 34.24
0.344 8.738 56.946 38.231
0.365 9.271 40 STD 63.301 40.483
0.438 11.125 71.852 48.238
0.5 12.7 60 XHY 81.53 54.735
0.594 15.088 80 95.969 64.429
12″ 12.75 324 0.188 4.775 37.57 25.222
0.219 5.563 43.657 29.309
0.25 6.35 49.713 33.375
0.281 7.137 55.739 37.42
0.312 7.925 61.735 41.445
0.375 9.525 73.824 49.562
0.406 10.312 79.727 53.525
0.5 12.7 97.438 65.415
0.562 14.275 108.966 73.154
14″ 14 356 0.188 4.775 41.308 27.732
0.219 5.563 48.012 32.233
0.25 6.35 20 54.685 36.713
0.281 7.137 61.327 41.172
0.312 7.925 67.939 45.611
0.375 9.525 STD 81.281 54.568
0.438 11.125 40 94.498 63.441
0.5 12.7 XHY 107.381 72.09
0.625 15.875 132.983 89.278
16” 16 406 0.188 4.775 47.29 21.748
0.219 5.563 54.98 36.91
0.25 6.35 10 62.639 42.053
0.281 7.137 70.268 47.174
0.312 7.925 20 77.866 52.275
0.344 8.738 85.677 57.519
0.375 9.525 30 93.213 62.578
STD
0.438 11.125 108.433 72.797
0.5 12.7 40 123.289 82.77
XHY
18″ 18 457 0.219 5.563 61.948 41.588
0.25 6.35 70.593 47.393
0.281 7.137 79.208 53.176
0.312 7.925 20 87.792 58.939
0.375 9.525 STD 105.144 70.588
0.438 11.125 30 122.369 82.152
0.5 12.7 XHY 139.198 93.45
0.562 14.275 40 155.904 104.666
0.625 15.875 172.754 115.978
20″ 20 508 0.25 6.35 78.547 52.733
0.282 7.163 88.458 59.386
0.312 7.925 97.719 65.604
0.375 9.525 20 STD 117.075 78.598
0.438 11.125 136.305 91.508
0.5 12.7 30 XHY 155.106 104.13
0.594 15.088 40 183.378 123.11
0.625 15.875 192.64 129.328
0.688 17.475 211.368 141.901
24″ 24 610 0.25 6.35 94.456 63.413
0.281 7.137 106.029 71.183
0.312 7.925 117.573 18.932
0.375 9.525 20 STD 140.938 64.618
0.438 11.125 164.176 110.219
0.5 12.7 XHY 186.923 125.49
0.625 15.875 232.41 156.028
0.688 17.475 40 255.148 171.293
0.75 19.05 277.401 186.233
30″ 30 762 0.25 6.35 118.318 79.433
0.281 7.137 132.851 89.189
0.312 7.925 10 147.353 98.925
0.375 9.525 STD 176.731 118.648
0.438 11.125 205.983 138.286
0.5 12.7 20 XHY 234.647 157.53
0.625 15.875 30 292.066 196.078
0.688 17.475 320.817 215.38
0.75 19.05 348.988 234.293
36″ 36 914 0.25 6.35 142.18 95.453
0.281 7.137 159.672 107.196
0.312 7.925 10 177.133 118.918
0.375 9.525 STD 215.525 142.678
0.438 11.125 247.79 166.353
0.5 12.7 20 XHY 282.372 198.57
0.625 15.875 351.723 236.128
0.688 17.475 386.487 259.467
0.75 19.05 420.576 282.353
42″ 42 1067 0.312 7.925 206.914 138.911
0.375 9.525 STD 248.319 166.708
0.5 12.7 XHY 33.097 221.61
0.75 19.05 492.163 330.413
48″ 48 1219 0.375 9.525 STD 284.112 190.738
0.438 11.125 331.404 222.487
0.5 12.7 XHY 377.822 253.65
0.75 19.05 563.75 378.473
0.875 22.225 655.969 440.383
PRESSURE RATING (PSIG)
SIZES SCHEDULE (SCH) OUTSIDE WALL TEMPERATURE (OF)
(INCHES) DIA. THICK. 100 200 300 400 500 600 650 700 750
(IN) (IN) ALLOWABLE STRESS (PSI)
16700 16700 16700 15500 14400 13500 13200 12900 12600
1″ 40 1.315 0.133 2205 2205 2205 2047 1902 1783 1743 1703 1664
80 1.315 0.179 3061 3061 3061 2841 2640 2475 2420 2365 2310
160 1.315 0.25 4493 4493 4493 4170 3874 3632 3552 3471 3390
1 1/2″ 40 1.9 0.145 1629 1629 1629 1512 1404 1317 1287 1258 1229
80 1.9 0.2 2303 2303 2303 2138 1986 1862 1821 1779 1738
160 1.9 0.281 3362 3362 3362 3120 2899 2717 2657 2597 2536
2″ 40 2.375 0.154 1371 1371 1371 1272 1182 1108 1083 1059 1034
80 2.375 0.218 1985 1985 1985 1843 1712 1605 1569 1534 1498
160 2.375 0.344 3283 3283 3283 3047 2831 2654 2595 2536 2477
3″ 40 3.5 0.216 1301 1301 1301 1208 1122 1052 1028 1005 982
80 3.5 0.3 1844 1844 1844 1712 1590 1491 1458 1425 1391
160 3.5 0.438 2787 2787 2787 2587 2403 2253 2203 2153 2103
4″ 40 4.5 0.237 1102 1102 1102 1023 950 891 871 851 831
80 4.5 0.337 1596 1596 1596 1482 1377 1291 1262 1233 1204
160 4.5 0.531 2611 2611 2611 2424 2552 2111 2064 2017 1970
5″ 40 5.563 0.258 965 965 965 896 832 780 763 746 728
80 5.563 0.375 1428 1428 1428 1325 1231 1154 1129 1103 1077
160 5.563 0.625 2474 2474 2474 2296 2133 2000 1955 1911 1866
6″ 40 6.625 0.28 877 877 877 814 756 709 693 677 661
80 6.625 0.432 1379 1379 1379 1280 1189 1115 1090 1065 1040
160 6.625 0.719 2382 2382 2382 2211 2054 1925 1883 1840 1797
8″ 40 8.625 0.322 771 771 771 716 665 623 610 596 582
80 8.625 0.5 1218 1218 1218 1131 1050 985 963 941 919
160 8.625 0.906 2298 2298 2298 2133 1982 1858 1817 1775 1734
10″ 40 10.75 0.365 699 699 699 649 603 565 553 540 528
80 10.75 0.594 1159 1159 1159 1075 999 937 916 895 874
160 10.75 1.125 2289 2289 2289 2124 1974 1850 1809 1768 1727
Les types Out diameter Tailles Longueur
NB Sizes (in stock) .0035” ~ 20” 1/8″, 1/4″, 3/8″, 1/2″, 5/8″, 3/4″, 1″, 1.25″, 1.5″, 2″, 2.5″, 3″, 4″, 5″, 6″etc Cut to length
Stainless Steel 2507/S32750 Seamless Tube (Custom Sizes) 6.35 mm OD To 508 mm OD As per requirement Cut to length
Stainless Steel 2507/S32750 Welded Tube (ERW Tube) (in Stock + Custom Sizes) 6.35 mm OD To 1219 mm OD As per requirement Cut to length
Finition de la surface Internal Surface(ID) Exterbal Surface(OD)
Roughness Average(RA) Roughness Average(RA)
μ inch μm μ inch μm
AP Annealed & Pickled Not defined Not defined 40 or Not defined 1.0 or Not defined
BA Beight Annealed 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
MP Mechanical Polish 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
EP Electro Polish 15,10,7,5 0.38,0.25,0.20;0.13 32 0.8

The surface and shape of Duplex 2507/S32750 stainless steel plate (6)

Daxun is a trustworthy stainless steel pipe and tube manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the stainless steel tubes have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

Projets et produits récents

2507/S32750 stainless steel pipe
tube en acier inoxydable sans soudure
tube en acier inoxydable de grand diamètre
2507/S32750 stainless steel pipe
Tube en acier inoxydable poli
2507/S32750 seamless pipe
Tube en acier inoxydable
BA stainless steel pipe
Stainless steel tube / pipe
2507/S32750 stainless pipe
Stainless steel precision tube

Leading stainless steel tube and pipe Suppliers in China


DUPLEX 2507 STAINLESS STEEL

  • Daxun Alloy Stainless Steel inventory currently contains Duplex 2507 Stainless Steel Pipe, which is a super duplex stainless steel containing 25% chromium, 4% molybdenum and 7% nickel. The alloy is suitable for applications requiring high strength and corrosion resistance, such as chemical processing, petrochemical and seawater equipment. The steel has strong resistance to chloride stress corrosion cracking, good thermal conductivity and a low coefficient of thermal expansion. The high chromium, molybdenum and nickel content provides excellent resistance to pitting, crevice and general corrosion.

PROPRIÉTÉS GÉNÉRALES

  • Duplex 2507 (UNS S32750) is a super duplex stainless steel pipe containing 25% chromium, 4% molybdenum and 7% nickel. It is designed for demanding applications requiring high strength and corrosion resistance, such as chemical processing, petrochemical and seawater equipment. The steel has strong resistance to chloride stress corrosion cracking, high thermal conductivity and low coefficient of thermal expansion. The high chromium, molybdenum and nickel content provides excellent resistance to pitting, crevice and general corrosion.

Applications

  • Oil and gas industry equipment
  • Offshore platforms, heat exchangers, process and service water systems, fire-fighting systems, injection and ballast water systems
  • Chemical process industries, heat exchangers, vessels, and piping
  • Desalination plants, high pressure RO-plant and seawater piping
  • Mechanical and structural components, high strength, corrosion-resistant parts
  • Power industry FGD systems, utility and industrial scrubber systems, absorber towers, ducting, and piping

Normes

  • ASTM/ASME ………. A240 – UNS S32750
    EURONORM………… 1.4410 – X2 Cr Ni MoN 25.7.4
    AFNOR……………….. Z3 CN 25.06 Az

RÉSISTANCE À LA CORROSION

General corrosion

  • SAF 2507™ is highly resistant to corrosion by organic acids, e.g. experience less than 0.05 mm/year in 10% formic and 50% acetic acid where ASTM 316L has corrosion rate higher than 0.2 mm/year. Pure formic acid see Figure 4. Also in contaminated acid SAF 2507™ remains resistant.
  • Figure 5 and Figure 6 show results from tests of SAF™ 2507 and various stainless steels and nickel alloys in acetic acid contaminated with chlorides which in practice are frequently present in processes.
  • 6825b rev 1.png

Figure 4. Isocorrosion diagram in formic acid. The curves represent a corrosion rate of 0.1 mm/year (4 mpy) in stagnant test solution.

  • 6967b rev 1.png

Figure 5. Corrosion rate of various alloys in 80% acetic acid with 2000 ppm chloride ions at 90°C.

  • 6968b rev 1.png

Figure 6. Corrosion rate of various alloys in concentrated acetic acid with 200 ppm chloride ions.

Practical experience with SAF™ 2507 in organic acids, e.g. in terephthalic acid plants, has shown that this alloy is highly resistant to this type of environment. The alloy is therefore a competitive alternative to high alloyed austenitics and nickel alloys in applications where standard austenitic stainless steels corrode at a high rate.

Resistance to inorganic acids is comparable to, or even better than that of high alloy austenitic stainless steels in certain concentration ranges. Figures 7 to 9 show isocorrosion diagrams for sulfuric acid, sulfuric acid contaminated with 2000 ppm chloride ions, and hydrochloric acid, respectively.

  • 6827b-rev 1.png

Figure 7. Isocorrosion diagram in naturally aerated sulfuric acid. The curves represent a corrosion rate of 0.1 mm/year (4 mpy) in a stagnant test solution.

  • 6826b-rev 1.png

Figure 8. Isocorrosion diagram, 0.1 mm/year (4 mpy) in a naturally aerated sulfuric acid containing 2000 ppm chloride ions.

Figure 9. Isocorrosion diagram in hydrochloric acid. The curves represent a corrosion rate of 0.1 mm/year (4 mpy) in stagnant test solution.

Pitting and crevice corrosion

The pitting and crevice corrosion resistance of stainless steel is primarily determined by the content of chromium, molybdenum and nitrogen. The manufacturing and fabrication practices, e.g. welding, are also of vital importance for the actual performance in service.

A parameter for comparing the resistance to pitting in chloride environments is the PRE number (Pitting Resistance Equivalent).
The PRE is defined as, in weight-%
PRE = %Cr + 3.3 x %Mo + 16 x %N

For duplex stainless steels the pitting corrosion resistance is dependent on the PRE value in both the ferrite phase and the austenite phase, so that the phase with the lowest PRE value will be limiting for the actual pitting corrosion resistance. In SAF™ 2507 the PRE value is equal in both phases, which has been achieved by a careful balance of the elements.

The minimum PRE value for SAF™ 2507 seamless tubes is 42.5. This is significantly higher than e.g. the PRE values for other duplex stainless steels of the 25Cr type which are not super-duplex. As an example, UNS S31260 25Cr3Mo0.2N has a minimum PRE-value of 33.

One of the most severe pitting and crevice corrosion tests applied to stainless steel is ASTM G48, i.e. exposure to 6% FeCI3 with and without crevices (method A and B respectively). In a modified version of the ASTM G48 A test, the sample is exposed for periods of 24 hours. When pits are detected together with a substantial weight loss (>5 mg), the test is interrupted. Otherwise, the temperature is increased by 5 °C (9 °F) and the test is continued with the same sample. Figure 11 shows critical pitting and crevice temperatures (CPT and CCT) from the test.

Potentiostatic tests in solutions with different chloride contents are presented in Figure 11. Figure 12 shows the effect of increased acidity. In both cases the applied potential is 600 mV vs SCE, a very high value compared with that normally associated with natural unchlorinated seawater, thus resulting in lower critical temperatures compared with most practical service conditions.

  • 6247b-rev 1.png

Figure 10. Critical pitting and crevice temperatures in 6% FeCl3, 24h (similar to ASTM G48).

The scatter band for SAF™ 2507 and 6Mo+N illustrates the fact that both alloys have similar resistance to pitting, and CPT-values are within the range shown in the figure.

Tests were performed in natural seawater to determine the critical crevice corrosion temperature of samples with an applied potential of 150 mV vs SCE. The temperature was raised by 4°C (7oF) steps every 24 hours until crevice corrosion occurred. The results are shown in the table below.

Alliage CCT (°C)
SAF 2507 64
6Mo+N 61

In these tests the propagation rates of initiated crevice corrosion attacks, at 15-50°C (59-122°F) and an applied potential of 150 mV vs SCE were also determined. These were found to be around ten times lower for SAF™ 2507 than for the 6Mo+N alloy.

  • 6185b-rev 1.png

Figure 11. Critical pitting temperatures (CPT) at varying concentrations of sodium chloride, from 3 to 25% (potentiostatic determination at +600 mV SCE with surface ground with 600 grit paper).

  • 6828bcyan-rev 1.png

Figure 12. Critical pitting temperatures (CPT) in 3% NaCl with varying pH (potentiostatic determination at +600 mV SCE with surface ground with 600 grit paper).

The corrosion resistance of SAF™ 2507 in oxidizing chloride solutions is illustrated by critical pitting temperatures (CPT) determined in a ‘Green death’ -solution (1% FeCI3 + 1% CuCl2 +11% H2SO4 + 1.2% HCI) and in a ‘Yellow death’ -solution (0.1 % Fe2(SO4)3 + 4% NaCl + 0.01 M HCI). The table below shows CPT-values for different alloys in these solutions. It is clear that the values for SAF™ 2507 are on the same level as those for the nickel alloy UNS N06625. The tests demonstrate a good correlation with the ranking of alloys for use as reheater tubes in flue gas desulfurization systems.

Critical pitting temperature (CPT) determined in different test solutions.

Alliage Critical pitting temperature (CPT), °C
‘Green death’
‘Yellow death’
SAF™ 2507 72.5 >90
6Mo+N 70 >90
UNS N06625 67.5 >90
ASTM 316 <25 20

Stress corrosion cracking

SAF™ 2507 has excellent resistance to chloride induced stress corrosion cracking (SCC).

The SCC resistance of SAF™ 2507 in chloride solutions at high temperatures is illustrated in Figure 13. There were no signs of SCC up to 1000 ppm Cl-/300°C and 10000 ppm Cl-/250°C.

SAF™ 2507 U-bend specimens exposed for 1000 hours in hot brine (108°C, 226°F, 25% NaCl) showed no cracking.
The threshold stress for SAF 2507® in 40% CaCl2 at 100 °C (210 °F) and pH = 6.5 is above 90% of the tensile strength for both parent metal and welded joints (TIG-welded with Alleima® 25.10.4.L or MMA-welded with Alleima® 25.10.4.LR).

Figure 14 shows the result of testing in 40% CaCl2 at 100 °C (210 °F) acidified to pH = 1.5. Acidifying of the standard test solution to pH = 1.5 lowers the threshold stress for SAF™ 2205, but not for SAF™ 2507. This applies to both parent metal and welded joints.

The threshold stress for both parent metal and welded joints of SAF™ 2507 in boiling 45% MgCl2 , 155°C (311°F) (ASTM G36), is approximately 50% of the proof strength.

  • 6877b-rev 1.png

Figure 13. SCC resistance in oxygen-bearing (abt. 8 ppm) neutral chloride solutions. Testing time 1000 hours. Applied stress equal to proof strength at testing temperature.

  • 6139bcyan-rev 1.png

Figure 14. Results of SCC tests with constant load in 40% CaCl2, pH=1.5, at 100 °C (210°F) with aerated test solution.

  • 6140b-rev 1.png

Figure 15. Constant load SCC tests in NACE solution at room temperature (NACE TM 0177).

Figure 15 shows the results of SCC tests at room temperature in NACE TM0177 Test solution A (5% sodium chloride and 0.5% acetic acid saturated with hydrogen sulfide). No cracking occurred on SAF™ 2507, irrespective of the applied stress.

In aqueous solutions containing hydrogen sulfide and chlorides, stress corrosion cracking can also occur on stainless steels at temperatures below 60 °C (140 °F). The corrosivity of such solutions is affected by acidity and chloride content. In direct contrast to the case with ordinary chloride-induced stress corrosion cracking, ferritic stainless steels are more sensitive to this type of stress corrosion cracking than austenitic steels.

In accordance with ISO 15156/NACE MR 0175 solution annealed and rapid cooled wrought SAF™ 2507 is suitable for use at temperatures up to 450 °F (232 °C) in sour environments in oil and gas production, if the partial pressure of hydrogen sulphide does not exceed 3 psi (0.20 bar).

SAF™ 2507, with a maximum hardness of 32 HRC, solution annealed and rapidly cooled, according to NACE MR0103, is suitable for use in sour petroleum refining.

Hydrogen Induced Stress Cracking (HISC)

Hydrogen Induced Stress Cracking (HISC) is an embrittlement phenomenon that may occur in cathodically protected subsea steel constructions in the presence of high tensile stresses. When connected to cathodically protected carbon steels, super duplex stainless steels will also be cathodically protected even though this is not necessary. At the prevalent low electrochemical potentials, atomic hydrogen will be generated on the steel surfaces by the reduction of sea water. Embrittlement due to HISC may occur when hydrogen diffuses into the metal.

Hydrogen diffuses much faster in the ferrite phase than in the austenite phase. Therefore, ferritic steels and ferrite containing steels, e.g. super duplex stainless steels, are more susceptible to HISC than austenitic stainless steels. A high mechanical stress increases the risk of HISC by increasing the hydrogen diffusion rate, crack initiation and propagation in the material.

In super duplex stainless steels, cracks tend to propagate in the embrittled ferrite phase and arrest at ferrite-austenite phase boundaries. Susceptibility to HISC significantly increases with increasing austenite spacing. Coarse-grained microstructures are therefore more susceptible. A testing program performed at Alleima Materials Technology has confirmed that tendency to HISC is reduced when austenite spacing is less than 30 μm, as recommended by DNV RP-F112. Cold pilgered and solution annealed tubes with austenite spacing between 5-15 μm have shown very good resistance to HISC under applied stress up to 130% of the yield strength without cracking.

The acceptable stress without HISC occurring for products with different austenite spacing is illustrated in figure 16.

HISC spacing

Figure 16. Tolerable stress as a percentage of the actual yield strength at 4°C without HISC occurring is schematically shown for tube and bar products with different austenite spacing. SAF™ 2507 (UNS S32750) has been tested on hydrogen pre-charged tensile specimens, using constant load with a dead weight, with an applied potential of -1050 mV/SCE in a electrochemical cell with 3% NaCl solution at 4°C, 500 hours. [NACE paper no. 07498]

Intergranular corrosion

SAF™ 2507 is a member of the family of modern duplex stainless steels whose chemical composition is balanced to give quick reformation of austenite in the high temperature heat affected zone of a weld. This results in a microstructure that provides the material with good resistance to intergranular corrosion. SAF™ 2507 passes testing to ASTM A262 Practice E (Strauss test) without reservation.

Erosion corrosion

The mechanical properties combined with corrosion resistance give SAF™ 2507 a good resistance to erosion corrosion. Testing in sand containing media has shown that SAF™ 2507 has an erosion corrosion resistance better than corresponding austenitic stainless steels. Figure 17 below shows the relative mass loss rate of the duplex SAF™ 2507, SAF™ 2205 and an austenitic 6Mo+N type steel after exposure to synthetic seawater (ASTM D-1141) containing 0.025-0.25% silica sand at a velocity of 8.9-29.3 m/s (average of all tests is shown).

6830bcyan-rev 1.png

Figure 17. Relative mass loss rate after testing of the resistance against erosion corrosion.

Corrosion fatigue

Duplex stainless steels which have a high tensile strength usually have a high fatigue limit and high resistance to both fatigue and corrosion fatigue.

The high fatigue strength of SAF™ 2507 can be explained by its good mechanical properties, while its high resistance to corrosion fatigue has been proven by fatigue testing in corrosive media.

TRAITEMENT

Hot Forming
2507 can be hot formed at temperatures ranging from 1875°F to 2250°F. This should be followed by a solution anneal at a minimum temperature of 1925°F, followed by a rapid air or water quench.

Cold Forming
Cold working 2507 can be accomplished using most typical stainless steel forming processes. Because the alloy has a higher yield strength than austenitic steels, but lower ductility, fabricators may need to use higher forming forces, larger bend radii, and springback allowances. Deep drawing, stretching, and other similar processes are more difficult for 2507 than for austenitic stainless steels. Solution annealing and quenching are recommended when the forming process requires more than 10% cold deformation.

Heat Treatment
Heat treatment for 2507 consists of solution annealing and quenching after hot or cold forming. Solution annealing should be performed at a minimum temperature of 1925°F. Annealing should be followed immediately by a rapid air or water quench. Heat treated items that are pickled and rinsed have excellent corrosion resistance.

Soudage
2507 is weldable and can be joined to other materials using SMAW, GTAW, PAW, FCW, or SAW. When welding 2507, a 2507/P100 filler metal is recommended to ensure proper duplex weld construction.

2507 does not require preheating except to prevent condensation on cold metal. Interpass welding temperatures should not exceed 300°F or weld integrity will be compromised. To maximize corrosion resistance, root protection should be applied using either argon or 90% N2/10% H2 purge gas. The latter provides higher corrosion resistance.

2507/S32750 grade stainless steel pipe

Wide choice of dimensions and free cutting

  • Whatever your needs, Daxun Alloys has the perfect stainless steel tube for you. We offer 3m and 6m lengths, with diameters from 3mm to 2000mm (Grade 2507) and ¾” to 20″ (Grade S32750).
  • If you require a specific length, we offer a free unlimited cutting service with every purchase. Using state-of-the-art bandsaws, our precision cutting service can cut the tube to the exact length you require. Just let us know when ordering. It’s another reason why we are a leading stainless steel tube supplier to our domestic and international customers.

Contact your stainless steel tube suppliers

  • You can easily order stainless steel pipes online, in any size, in any quantity.
  • Par ailleurs, notre sympathique équipe de vente se fera un plaisir de prendre votre commande. Il vous suffit d'appeler le +86 13382898899 ou d'envoyer un courriel à Daxunhejin@gmail et nous vous répondrons dans les plus brefs délais.
Oil & Gas

You’ll learn a lot when you work on a large number of downhole and umbilical projects with Daxun Alloys.

You’ll learn how to manufacture and supply stainless steel and nickel straight and coiled tubing that is both complete and cost-effective. You’ll learn how to ensure quality by employing multiple non-destructive testing techniques. You’ll learn how to develop process plans specifically for downhole and umbilical customers.

When you choose Daxun Alloys as your tubular supplier, you know we truly understand the oil and gas industry. Connect with Daxun Alloys today.

Production d'électricité

Serving the Power Generation Industry, only DEXON Alloys combines the technical expertise and experience to produce the finest pipe available on the market today. Choose the best and you get the best. Do as countless other companies do – trust DEXON Alloys. Demanding industries demand DEXON Alloys.

Chemical, Petrochemical

Serving the Chemical, Petrochemical Industry, only DEXON Alloys combines the technical expertise and experience to produce the finest pipe available on the market today. Choose the best and you get the best. Do as countless other companies do – trust DEXON Alloys. Demanding industries demand DEXON Alloys.

Food, Beverage and Dairy

Sometimes good ingredients get mixed in with the bad stuff. When your product flows through a DAIXUN Alloy pipe, the bad stuff is no longer there. That’s because the internal structure manufactured by DAIXUN limits the tiny gaps where pathogens can hide. Improve quality by connecting to DAIXUN Alloy.

Pharmaceutical, Biopharmaceutical

Serving the pharmaceutical and biopharmaceutical industries is a challenge for Daxun Alloys. From raw material selection to delivery, we formulate our high purity and ultra-high purity services to meet and exceed industry standards. When only the highest quality tubing and pipe will meet the needs, more and more pharmaceutical and biopharmaceutical companies trust Daxun Alloys.

General Commercial

Serving the specialty automotive industry by setting the standard for specialized exhaust applications. Daxun Alloy tubes and pipes are specially formulated to resist tearing, corrosion, and thermal oxidation. For consistent performance and unmatched service, contact Daxun Alloy.

Puis-je obtenir des échantillons ?

Nous pouvons vous fournir des échantillons de tôles d'acier inoxydable pour vous permettre de vérifier la qualité. L'échantillon est gratuit et vous ne payez que les frais de transport.

Quels sont les pays que vous avez déjà exportés ?

Nous avons exporté vers plus de 42 pays, tels que le Canada, le Chili, le Koweït, l'Allemagne, la Corée du Sud, l'Arabie saoudite, Singapour, etc.

Quel est votre MOQ ?

Notre MOQ est de 1 tonne pour les tôles d'acier inoxydable.

Quel est le délai de livraison ?

Les commandes d'essai peuvent être livrées dans un délai d'une semaine. Pour les commandes régulières, il faut compter environ deux semaines.

Envoyez votre demande dès aujourd'hui
Devis rapide