Stainless steel sheet
Daxun maintains a standing inventory of 30,000 tons of stainless steel plate, divided between cold-rolled thin plate and hot-rolled medium-to-heavy plate. Surface processing services are available, including polishing, brushing, and pickling. For common grades such as 304, 316L, and 321, this stock lets us confirm availability and quote turnaround on the same day you send your specification — no need to wait on a new mill run for standard sizes.
Daxun stainless steel plate introduction
| Product Parameters: Stainless Steel Sheet/Plate | |||
| نمره | 201,304,304L,316,316L,317,321,309,310S,2205,2507,904L,409,410,420,430,436,444,441,17-4 etc. | ||
| عرض | 10mm~2500mm | ||
| ضخامت | 0.2mm~100mm | Thickness tolerance | +/-0.03mm |
| استاندارد | ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2 | ||
| سطح | 2B,BA,8K,NO.1,NO.4,NO.3,hairline,checkered,gold ,black ,rose gold,etc | ||
| specification | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
| Mill Origin | TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc. | ||
| Certification | ISO, SGS, BV, TUV,CE etc | ||
A Wide Range of Steel Grades
Daxun Alloy supplies stainless steel sheet in cold-rolled and hot-rolled
form across the austenitic, ferritic, and duplex grade range — including
304, 316L, 321, 409, 430, and 2205. Send your grade, thickness, and
application, and we’ll confirm availability and lead time.
Excellent Flatness and Thickness Accuracy
Every coil is checked for flatness and thickness against the applicable
standard tolerance (e.g. ASTM A480) before shipment, under an in-process
quality control system. Consistent tolerance is what keeps formability and
corrosion performance predictable from sheet to sheet.
Surface Finishing
Automated rolling control keeps surface condition consistent across the
full range — from 2B mill finish to polished and brushed finishes.
Confirm the finish grade with your order and we’ll match it to the
applicable standard.
Stainless Steel Sheet — Grades and Finishes
Daxun supplies stainless steel sheet in austenitic grades — including 201,
304, 304L, 304J1, 321, 316, 316L, 317L, and 316Ti — with standard surface
finishes including 2B, BA, No.1, No.4, 8K, SB, and HL.
Send your grade, thickness, and finish requirement, and we’ll confirm
availability and lead time.
Stainless steel plate grades and characteristics
Each stainless steel plate material has its own different usage scenarios.
high strength,Suitable for chemical processing, petrochemical and subsea equipment
Super stainless steel, corrosion resistant,Able to resist erosion by a variety of chemical media。
Suitable for decorative materials, stainless steel for tableware, and many other industries.
Suitable for various industries such as mechanical equipment and mechanical parts.
Suitable for various industries such as machinery and equipment, auto parts and so on.
Suitable for heat exchanger shells, automotive panels and other industries. Complete specifications and abundant inventory.
Precipitation hardened stainless steel, used in a variety of industries such as the production of high-strength parts.
Suitable for floor anti-slip and decoration industries, such as elevators, stair slabs, etc.
Stainless steel plate form types
If the shape you need is not available here, please contact us.
Performance of stainless steel plate
Huge Stock Choiceable Material
Daxun keeps stainless steel sheet in stock across common grades and sizes, so most orders ship without waiting on a new production run — with additional grades and thicknesses available to source on request. Every order, whether from stock or sourced to spec, goes through the same inspection process and ships with a mill test certificate.
Stainless Steel Sheet Finishes Options
Daxun’s stainless steel sheet comes in a range of finishes: brushed (hairline/HL) for a uniform grain that hides scratches, sandblasted for an even matte surface, mirror (up to 8K) for high-gloss polish, laser-etched for permanent patterns, and embossed for raised decorative or anti-slip textures. Confirm the finish grade with your order.
Strict Quality Control
Daxun cuts and finishes stainless steel sheet to your exact size
specifications. Our quality management system is certified to ISO 9001, and
every shipment is accompanied by a mill test certificate. Material is
inspected on receipt and again before it leaves our warehouse, with full
traceability from source to delivery.
Stainless steel plate processing and customization
Daxun’s processing capability includes laser cutting, water jet cutting,CNC bending, and CNC shearing — covering both straight and contoured cuts, and forming to your specified angles and dimensions.Send us your drawing with the required dimensions and tolerances, and we’ll confirm feasibility, pricing, and lead time for cutting and bending to your specification.
Packaging of Stainless Plates
Daxun matches packaging to the product and shipping method — including kraft paper wrapping, wooden crates, woven bags, and wooden pallets — to protect surface finish and prevent damage in transit. Packaging is confirmed with you before shipment based on your order size and destination.
Daxun’s quality management system is certified to ISO 9001:2015. Every
shipment includes a mill test certificate, and material is traceable from
source to delivery.
Daxun maintains an in-house testing laboratory to verify that every shipment meets the specified weight and quality standard before delivery. Our quality control team performs 100% inspection at every production stage.
Our support doesn’t end when your order ships. Daxun continues to provide after-sales assistance and warranty support for every order.
Stainless Steel plate application cases in different industries
Stainless steel plate is widely used in construction, including exterior
wall cladding, interior decoration, roofing, and structural applications.
Its corrosion resistance and mechanical strength make it suitable for both
long-term exposed applications and structural load-bearing use, while
surface finish options (brushed, mirror, embossed) support a range of
architectural design requirements.
Corrosion resistance and a smooth, easy-to-clean surface make stainless
steel plate well suited to food machinery applications — including
sanitation systems, fluid pipe troughs, food storage tanks, heat
exchangers, and vacuum vessels. Mechanical properties remain stable across
a wide temperature range, supporting both hot processing and cold storage
equipment.
Stainless steel plate offers a combination of strength, toughness, and
corrosion resistance suited to demanding structural applications.
Petroleum refining equipment manufacturing and maintenance uses medium-thick
plate and cold-rolled sheet in grades including 321 and 316L. Typical
specification for petrochemical vessel applications: SUS316, thickness
0.3-0.6mm, width 1219-1520mm, surface finish 2B/2D.
Stainless steel plate is used in shipbuilding for its resistance to
seawater corrosion, along with strength, toughness, and fatigue resistance
— properties suited to the demanding marine environment.
316L is a widely used austenitic stainless steel grade for offshore
installations, offering a stable combination of mechanical strength and
resistance to chloride-induced corrosion in marine environments.
Duplex stainless steels combine high mechanical strength with strong
resistance to stress corrosion cracking, making them well suited to
offshore applications. UNS S32205 is the most commonly used duplex grade
for offshore installations.
Stainless steel plate is used in power generation applications for its
corrosion resistance and mechanical strength, supporting components that
operate under demanding thermal and structural conditions.
Our stainless steel plate stock sizes
- Data Sheet
- Tolerances and Delivery State
- Surface finishes
| Thickness (mm) | Width (mm) | Length (mm) | Comment |
| 0.5 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 0.8 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 1.0 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 1.5 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 2.5 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 3.0 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 5.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 6-8.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 1.0-20.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 20.0-50.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 50.0+ | 1500/1800/2000 | 3000/6000/8000 | AAA |
| Tolerances | |||||
| رتبه تحمل | |||||
| اندازه | گروه ۱ | گروه ۲ | گروه ۳ | وضعیت تحویل | وضعیت سطح |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 | نورد سرد | دو بی دو بعدی کارشناسی هنر خط موی سر شمارهٔ ۳ شمارهٔ ۴ ۶ کیلومتر کیوکیو |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 | ||
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 | ||
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 | ||
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 | ||
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 | ||
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 | ||
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 | ||
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 | ||
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 | ||
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 | ||
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 | ||
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 | وضعیت تحویل | شمارهٔ یک شمارهٔ ۳ شمارهٔ ۴ ۶ کیلومتر کیوکیو شور شده |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 | ||
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 | ||
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 | ||
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 | ||
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 | ||
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 | ||
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 | ||
| توجه: ۱. در صورتی که به وضعیت تحویل متفاوتی از موارد فوق نیاز دارید، لطفاً با ما هماهنگ فرمایید. ۲. در صورت هرگونه پرسش یا سفارش، لطفاً ما را از هرگونه نیاز اضافی که در اینجا ذکر نشده است، مطلع سازید. |
|||||
| Finish Designation | Method and degree of finish |
| شمارهٔ یک | After hot rolling, heat treatment, pickling or other equivalent treatment is applied. |
| No.2D | Annealing and pickling are performed after cold rolling; material is soft with surface of silver-white luster; used for general applications and deep drawing. |
| No.2B | After 2D finish, skin pass rolling is performed to obtain a more suitable luster; the surface becomes very exquisite; used for general applications. |
| شمارهٔ ۳ | Intermediate 100-120 grit finish; used for applications in which surface polishing is performed after shaping. |
| شمارهٔ ۴ | General 150-180 grit finish; used for restaurants and kitchen equipment and tools. |
| #240 | 240 grit finish; used when a finer finish than No. 4 is required; typically for restaurants and kitchen equipment and tools. |
| #320 | 320 grit finish polished product. |
| HL | This finish is performed by continuous linear polishing using an abrasive of appropriate grain size; mainly used for architectural applications. |
| کارشناسی هنر | Achieved by performing bright annealing after cold rolling and then skin pass rolling to obtain even greater reflectance; provides excellent corrosion resistance; used for household appliances, kitchen equipment, and automobiles. |
| کیوکیو | Through multiple grinding, it achieves very high brightness and smoothness, like a mirror. |
Related Product
داکسون آلیاژ
We handle all types of stainless steel plate inquiries — send us your
requirements and we’ll recommend the right grade and specification for
your application.
Stainless Steel Sheet Supplier in China
Daxun supplies stainless steel sheet in a range of finishes, with free
cutting service and dependable delivery — so you can source everything you
need from a single supplier.
Surface Finishes
Available finishes include brushed (hairline), sandblasted, mirror (8K),
laser-etched, and embossed.
Protective Film
Daxun’s stainless steel sheet ships with a protective film on the finished
surface, which can be peeled off after installation or fabrication to
protect against scratches and marks during handling. The reverse side is
left unfilmed.
نمره
300-series stainless steel is the most commonly used type, offering good
formability, corrosion resistance, and weldability.
Sizing and Cutting
Daxun supplies stainless steel sheet across a wide range of thicknesses and
sheet sizes, with free cutting service included on every order to meet
your exact dimensions.
How to Order
Send us your specifications by email or phone, and our team will confirm
availability, pricing, and lead time.
ایمیل: daxunalloy@gmail.com
Phone: +86 133 8289 8899
We offer three shipping methods — sea, land, and air — to get your order
to you reliably.
Important Safety Note
Sheet edges are not polished, ground, or deburred and may be sharp, as with
any raw stainless steel plate. Please handle, install, and use with
appropriate care.
Yes, we have complete specifications and inventory and can quickly meet your needs.
Yes, it can be customized. You can contact us and send us the customized specifications and quantity.
Our transportation methods generally include sea transportation, land transportation, and sea transportation. Reach you quickly and safely.
Because our output is high, the cost will be much lower, so the price is low.
ما میتوانیم نمونههای ورق فولاد ضدزنگ را برای بررسی کیفیت در اختیار شما قرار دهیم. نمونه رایگان است و شما فقط هزینه حمل را پرداخت میکنید.
We attach great importance to product quality and have passed various quality system tests.