x
Envie hoje o seu pedido de informação
Orçamento rápido

Placa de aço inoxidável

Stainless steel plate and sheet supplier from Wuxi, China
Thickness 0.3mm to 100mm, width up to 3000mm
Hot rolled and cold rolled plate in a full range of grades

Chapa de aço inoxidável

Daxun maintains a standing inventory of 30,000 tons of stainless steel plate, divided between cold-rolled thin plate and hot-rolled medium-to-heavy plate. Surface processing services are available, including polishing, brushing, and pickling. For common grades such as 304, 316L, and 321, this stock lets us confirm availability and quote turnaround on the same day you send your specification — no need to wait on a new mill run for standard sizes.

Daxun stainless steel plate introduction

Product Parameters: Stainless Steel Sheet/Plate
Grau 201,304,304L,316,316L,317,321,309,310S,2205,2507,904L,409,410,420,430,436,444,441,17-4 etc.
Largura 10mm~2500mm
Espessura 0.2mm~100mm Thickness tolerance +/-0.03mm
Padrão ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2
Superfície 2B,BA,8K,NO.1,NO.4,NO.3,hairline,checkered,gold ,black ,rose gold,etc
specification 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L
 Mill Origin TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc.
Certification ISO, SGS, BV, TUV,CE etc

A Wide Range of Steel Grades

Daxun Alloy supplies stainless steel sheet in cold-rolled and hot-rolled
form across the austenitic, ferritic, and duplex grade range — including
304, 316L, 321, 409, 430, and 2205. Send your grade, thickness, and
application, and we’ll confirm availability and lead time.

Excellent Flatness and Thickness Accuracy

Every coil is checked for flatness and thickness against the applicable
standard tolerance (e.g. ASTM A480) before shipment, under an in-process
quality control system. Consistent tolerance is what keeps formability and
corrosion performance predictable from sheet to sheet.

Surface Finishing

Automated rolling control keeps surface condition consistent across the
full range — from 2B mill finish to polished and brushed finishes.
Confirm the finish grade with your order and we’ll match it to the
applicable standard.

Stainless Steel Sheet — Grades and Finishes

Daxun supplies stainless steel sheet in austenitic grades — including 201,
304, 304L, 304J1, 321, 316, 316L, 317L, and 316Ti — with standard surface
finishes including 2B, BA, No.1, No.4, 8K, SB, and HL.

Send your grade, thickness, and finish requirement, and we’ll confirm
availability and lead time.

Ler mais

Stainless steel plate grades and characteristics

Each stainless steel plate material has its own different usage scenarios.

high strength,Suitable for chemical processing, petrochemical and subsea equipment

Stainless Steel Plate/Stainless Steel Sheet

Super stainless steel, corrosion resistant,Able to resist erosion by a variety of chemical media。

Suitable for decorative materials, stainless steel for tableware, and many other industries.

Stainless Steel Plate/Stainless Steel Sheet

Suitable for various industries such as mechanical equipment and mechanical parts.

Stainless Steel Plate/Stainless Steel Sheet

Suitable for various industries such as machinery and equipment, auto parts and so on.

Stainless Steel Plate/Stainless Steel Sheet

Suitable for heat exchanger shells, automotive panels and other industries. Complete specifications and abundant inventory.

Stainless Steel Plate/Stainless Steel Sheet

Precipitation hardened stainless steel, used in a variety of industries such as the production of high-strength parts.

Stainless Steel Plate/Stainless Steel Sheet
Stainless steel pattern plate

Suitable for floor anti-slip and decoration industries, such as elevators, stair slabs, etc.

16 Products Found.

Stainless steel plate form types

If the shape you need is not available here, please contact us.

4 Produtos encontrados.

Performance of stainless steel plate

Resistência à corrosão
Low-Cost
Valuable Metal
Workability

Huge Stock Choiceable Material

Daxun keeps stainless steel sheet in stock across common grades and sizes, so most orders ship without waiting on a new production run — with additional grades and thicknesses available to source on request. Every order, whether from stock or sourced to spec, goes through the same inspection process and ships with a mill test certificate.

Stainless Steel Sheet Finishes Options

Daxun’s stainless steel sheet comes in a range of finishes: brushed (hairline/HL) for a uniform grain that hides scratches, sandblasted for an even matte surface, mirror (up to 8K) for high-gloss polish, laser-etched for permanent patterns, and embossed for raised decorative or anti-slip textures. Confirm the finish grade with your order.

Strict Quality Control

Daxun cuts and finishes stainless steel sheet to your exact size
specifications. Our quality management system is certified to ISO 9001, and
every shipment is accompanied by a mill test certificate. Material is
inspected on receipt and again before it leaves our warehouse, with full
traceability from source to delivery.

Stainless steel plate processing and customization

Daxun’s processing capability includes laser cutting, water jet cutting,CNC bending, and CNC shearing — covering both straight and contoured cuts, and forming to your specified angles and dimensions.Send us your drawing with the required dimensions and tolerances, and we’ll confirm feasibility, pricing, and lead time for cutting and bending to your specification.

Packaging of Stainless Plates

Packing method

Daxun matches packaging to the product and shipping method — including kraft paper wrapping, wooden crates, woven bags, and wooden pallets — to protect surface finish and prevent damage in transit. Packaging is confirmed with you before shipment based on your order size and destination.

Material Test Certification

Daxun’s quality management system is certified to ISO 9001:2015. Every
shipment includes a mill test certificate, and material is traceable from
source to delivery.

Peso real e boa qualidade

Daxun maintains an in-house testing laboratory to verify that every shipment meets the specified weight and quality standard before delivery. Our quality control team performs 100% inspection at every production stage.

Excelentes serviços pós-venda

Our support doesn’t end when your order ships. Daxun continues to provide after-sales assistance and warranty support for every order.

Stainless Steel plate application cases in different industries

Decoração de edifícios

Stainless steel plate is widely used in construction, including exterior
wall cladding, interior decoration, roofing, and structural applications.
Its corrosion resistance and mechanical strength make it suitable for both
long-term exposed applications and structural load-bearing use, while
surface finish options (brushed, mirror, embossed) support a range of
architectural design requirements.

Mechanical equipment

Corrosion resistance and a smooth, easy-to-clean surface make stainless
steel plate well suited to food machinery applications — including
sanitation systems, fluid pipe troughs, food storage tanks, heat
exchangers, and vacuum vessels. Mechanical properties remain stable across
a wide temperature range, supporting both hot processing and cold storage
equipment.

Aeroespacial

Stainless steel plate offers a combination of strength, toughness, and
corrosion resistance suited to demanding structural applications.

Petroquímica

Petroleum refining equipment manufacturing and maintenance uses medium-thick
plate and cold-rolled sheet in grades including 321 and 316L. Typical
specification for petrochemical vessel applications: SUS316, thickness
0.3-0.6mm, width 1219-1520mm, surface finish 2B/2D.

Campo de navios

Stainless steel plate is used in shipbuilding for its resistance to
seawater corrosion, along with strength, toughness, and fatigue resistance
— properties suited to the demanding marine environment.

Engenharia naval

316L is a widely used austenitic stainless steel grade for offshore
installations, offering a stable combination of mechanical strength and
resistance to chloride-induced corrosion in marine environments.

Duplex stainless steels combine high mechanical strength with strong
resistance to stress corrosion cracking, making them well suited to
offshore applications. UNS S32205 is the most commonly used duplex grade
for offshore installations.

Campo de energia eléctrica

Stainless steel plate is used in power generation applications for its
corrosion resistance and mechanical strength, supporting components that
operate under demanding thermal and structural conditions.

about-feature3
Let us be your trustworthy stainless steel plate supplier

Every shipment includes a mill test certificate and is traceable from
source to delivery, backed by our ISO 9001:2015-certified quality
management system. Daxun supplies stainless steel plate to a range of
industries, including building decoration, industrial equipment, chemical
processing, shipbuilding, and petrochemicals.

Our stainless steel plate stock sizes

Thickness (mm) Width (mm) Comprimento (mm) Comentário
0.5 1000/1219/1500 2000/2438/3000 AAA
0.8 1000/1219/1500 2000/2438/3000 AAA
1.0 1000/1219/1500 2000/2438/3000 AAA
1.5 1000/1219/1500 2000/2438/3000 AAA
2.5 1000/1219/1500 2000/2438/3000 AAA
3.0 1000/1219/1500 2000/2438/3000 AAA
5.0 1500/1800/2000 3000/6000/8000 AAA
6-8.0 1500/1800/2000 3000/6000/8000 AAA
1.0-20.0 1500/1800/2000 3000/6000/8000 AAA
20.0-50.0 1500/1800/2000 3000/6000/8000 AAA
50.0+ 1500/1800/2000 3000/6000/8000 AAA
Tolerâncias
                                       Classificação de tolerância
Tamanho Grupo 1 Grupo 2 Grupo 3 Estado de entrega Estado da superfície
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39 Laminados a frio 2B
2D
BA
Fio de cabelo
N.º 3
N.º 4
6K
8K
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9 Estado de entrega N.º 1
N.º 3
N.º 4
6K
8K
Em conserva
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
Nota:
1. Se necessitar de um estado de entrega diferente do acima indicado, por favor confirme connosco.
2. Em caso de pedido de informação ou de encomenda, agradecemos que nos informe de qualquer requisito adicional não indicado aqui.
Finish Designation Method and degree of finish
N.º 1 After hot rolling, heat treatment, pickling or other equivalent treatment is applied.
No.2D Annealing and pickling are performed after cold rolling; material is soft with surface of silver-white luster; used for general applications and deep drawing.
No.2B After 2D finish, skin pass rolling is performed to obtain a more suitable luster; the surface becomes very exquisite; used for general applications.
N.º 3 Intermediate 100-120 grit finish; used for applications in which surface polishing is performed after shaping.
N.º 4 General 150-180 grit finish; used for restaurants and kitchen equipment and tools.
#240 240 grit finish; used when a finer finish than No. 4 is required; typically for restaurants and kitchen equipment and tools.
#320 320 grit finish polished product.
HL This finish is performed by continuous linear polishing using an abrasive of appropriate grain size; mainly used for architectural applications.
BA Achieved by performing bright annealing after cold rolling and then skin pass rolling to obtain even greater reflectance; provides excellent corrosion resistance; used for household appliances, kitchen equipment, and automobiles.
8K Through multiple grinding, it achieves very high brightness and smoothness, like a mirror.
  • Customer references and project case studies available on request.

Liga de Daxun

We handle all types of stainless steel plate inquiries — send us your
requirements and we’ll recommend the right grade and specification for
your application.

Stainless Steel Sheet Supplier in China

Daxun supplies stainless steel sheet in a range of finishes, with free
cutting service and dependable delivery — so you can source everything you
need from a single supplier.

Surface Finishes

Available finishes include brushed (hairline), sandblasted, mirror (8K),
laser-etched, and embossed.

Protective Film

Daxun’s stainless steel sheet ships with a protective film on the finished
surface, which can be peeled off after installation or fabrication to
protect against scratches and marks during handling. The reverse side is
left unfilmed.

Grau

300-series stainless steel is the most commonly used type, offering good
formability, corrosion resistance, and weldability.

Sizing and Cutting

Daxun supplies stainless steel sheet across a wide range of thicknesses and
sheet sizes, with free cutting service included on every order to meet
your exact dimensions.

How to Order

Send us your specifications by email or phone, and our team will confirm
availability, pricing, and lead time.

Correio eletrónico: daxunalloy@gmail.com
Phone: +86 133 8289 8899

We offer three shipping methods — sea, land, and air — to get your order
to you reliably.

Important Safety Note

Sheet edges are not polished, ground, or deburred and may be sharp, as with
any raw stainless steel plate. Please handle, install, and use with
appropriate care.

Têm algum stock em armazém?

Sim, dispomos de especificações e inventário completos e podemos responder rapidamente às suas necessidades.

Pode ser personalizado?

Sim, pode ser personalizado. Pode contactar-nos e enviar-nos as especificações personalizadas e a quantidade.

Como é que enviam as mercadorias?

Os nossos métodos de transporte incluem geralmente o transporte marítimo, o transporte terrestre e o transporte marítimo. Chegar até si de forma rápida e segura.

Qual é o vosso preço?

Uma vez que a nossa produção é elevada, o custo será muito inferior, pelo que o preço é baixo.

Podem dar-me algumas amostras?

Podemos fornecer amostras de chapas de aço inoxidável para que possa verificar a qualidade. A amostra é grátis e o cliente só paga o frete.

Qual é a vossa qualidade?

Damos grande importância à qualidade do produto e passámos vários testes de sistema de qualidade.

Envie hoje o seu pedido de informação
Orçamento rápido