Daxun is an excellent manufacturer of CP-2-grade titanium rods
As China’s leading supplier of titanium and titanium alloy rods, Daxun provides high-performance titanium rods to the world.
- Titanium Rod Grade:CP-2(Grade 2)- UNS R50400-3.7035-TA2
- Types: Hot rolled rod, forged rod, cold drawn rod, extruded rod etc
- Shape: Titanium round bar, titanium square bar、Ti hexagonal bar
- Density of Titanium Rod: Density of Grade 2 Titanium Rod is 4.51g/cm3
- Standards: ASTM B 348,ASME SB348,DIN 17862,ASTM F67,ASTM 265
- Dimensions: GB, GJB, EN, ASTM, JIS, ASME, BS, AISI, DIN, ISO, etc.
پیشرو جهانی در خدمات تولید میلههای تیتانیوم خالص تجاری
Grade 2 Titanium Rod is the workhorse among titanium alloy rods, offering an excellent balance of strength and weight for weight-sensitive applications. As a commercially pure (CP) titanium alloy, it achieves an ideal combination of strength and ductility, making it suitable for a wide range of demanding uses. It provides high impact strength, is easily weldable, and is extremely corrosion-resistant in oxidizing conditions, alkaline media, brine solutions, weakly reducing environments, nitric acid, and wet chlorine. Additionally, its excellent resistance to seawater and saline solutions further enhances its versatility.
The Grade 2 Titanium Rod stands out for its lightweight nature, impressive strength-to-weight ratio, and outstanding resistance to corrosion, making it highly versatile and ideal for numerous industrial uses. From general industrial uses to military and aerospace applications, this material delivers reliable performance in challenging environments.
Daxun Alloys stocks Grade 2 Titanium Rods in a variety of diameters to meet the specific requirements of different projects. Our inventory includes sizes ranging from 1 mm to 300 mm, with the ability to accommodate custom orders for larger dimensions. All rods are certified to ASTM B348 and ASTM B381 standards.
For those seeking reliable suppliers, Daxun Alloys offers a comprehensive range of Grade 2 Titanium products, including ASTM B348 Titanium Grade 2 Round Bars, UNS R50400 Bright Bars, and WERKSTOFF NR. 3.7035 Round Bars. Whether you need round, forged, or square bars, we ensure consistent quality and competitive pricing.
Feel free to contact Daxun Alloys for inquiries or to request a quote. Our team is committed to providing high-quality Grade 2 Titanium Rods and is happy to assist with any questions or project-specific needs.
دادهها
- پارامتر
- مادهٔ تشکیلدهنده
- خواص مکانیکی
- خواص فیزیکی
- جستجوهای داغ
| مشخصات | جزئیات |
| مواد | Titanium rod and bar Grade 2 (UNS R50400) |
| استاندارد | ASTM B348, ASTM SB348, AMS 4921, AMS 4902 |
| ابعاد | EN, ASTM, JIS, ASME, BS, AISI |
| محدوده قطر | 0.125″ – 14″ (3.175mm – 355.6mm)، سفارشی |
| محدوده طول | تا ۲۴۰ اینچ (۶۰۹۶ میلیمتر)، سفارشی |
| پایان | سرد (درخشان) کشیده، بدون مرکز سنگزنی، نورد گرم، تراش صاف، پوستکنی، لبهی نورد شکافدار، نورد گرم و انیل، تراش زبر، درخشان، پولیش، سنگزنی، بدون مرکز سنگزنی و سیاه |
| پایانکاری سطح | کشیده شده سرد، بدون مرکز تراشیده شده، صیقلی، یا تراشخورده خام، مشکی، پرداخت شماره ۴، پرداخت BA، پرداخت مات، و غیره. |
| وضعیت | سختشده و تمپرشده، آنیلشده |
| بردباری | تolerance قطر: ± 0.005″ (0.127 میلیمتر)، tolerance طول: ± 0.125″ (3.175 میلیمتر) |
| فرم | میلههای مربعی تیتانیوم، شمشهای تیتانیوم، میلههای گرد تیتانیوم، میلههای مستطیلی تیتانیوم، میلههای مثلثی تیتانیوم، میلههای کوبیدهشده تیتانیوم، میلههای ششضلعی تیتانیوم و غیره. |
| خواص فیزیکی | تراکم: 0.163 پوند بر اینچ مکعب (4.51 گرم بر سانتیمتر مکعب)، نقطه ذوب: 3020 درجه فارنهایت (1660 درجه سانتیگراد)، افزایش طول: 20-30%، مدول الاستیسیته: 16.5 × 10^6 psi (114 GPa) |
| ترکیب شیمیایی | تیتانیوم (حداقل): 99.2%، اکسیژن (حداکثر): 0.25%، کربن (حداکثر): 0.08%، آهن (حداکثر): 0.30%، نیتروژن (حداکثر): 0.03%، هیدروژن (حداکثر): 0.015% |
| عنصر | Weight % |
| C | ≤0.08 |
| O | ≤0.25 |
| N | ≤0.03 |
| H | ≤0.015 |
| آهن | ≤0.30 |
| *OEE | ≤0.10 |
| *OET | ≤0.40 |
| تیتانیوم | Remaining |
| سختی، نوپ | 170 | 170 | |
| Hardness, Rockwell B | 80 | 80 | |
| سختی، ویکرز | 145 | 145 | |
| Tensile Strength, Ultimate | 344 MPa | 49900 psi | |
| Tensile Strength, Yield | 275 – 410 MPa | 39900 – 59500 psi | |
| نرخ کشش در شکست | 20 % | 20 % | |
| کاهش مساحت | 35 % | 35 % | |
| ماژول ارتجاعی | 105 GPa | 15200 ksi | In Tension |
| Compressive Modulus | 110 GPa | 16000 ksi | |
| Poisson’s Ratio | 0.37 | 0.37 | |
| Izod Impact | 114 – 171 J | 84.1 – 126 ft-lb | |
| مقاومت در خستگی | 300 MPa | 43500 psi | 1E+7 cycles, Unnotched |
| مقاومت در خستگی | 425 MPa | 61600 psi | 30,000 cycles, Unnotched |
| سختی شکست | 66 MPa-m½ | 60.1 ksi-in½ | K(Q); annealed |
| ماژول برشی | 45 GPa | 6530 ksi |
| تراکم | Melting Range | Modulus of Elasticity (Tension) | Specific Heat | Mean Coefficient of Expansion | Thermal conductivity | مقاومت الکتریکی |
| kg/m3 | °C | GPa | J/kg. °C | x10 -6 / °C | W / m. °C | micro-ohm.m |
| 4,507 | 1668± 10 | 103 | 519 | 8.41 | 11.4 | 0.42 |
| ASTM B348 Alloy Gr 2 Hex Bar Polished | grade 2 titanium Hexagonal Bar |
| ASTM B348 Alloy Gr 2 Rectangular Bar | Titanium WERKSTOFF NR. 3.7035 Threaded Bar Black |
| Titanium UNS R50400 Round Bar | grade 2 titanium Din 3.7035 Flat Bar |
| Titanium Grade 2 Bar | Alloy grade 2 titanium Flat Bar Black |
| Alloy Gr 2 Rounds | ASME SB 338 gr 2 Flat Bar Bright |
| Titanium Alloy Grade 2 Bright Bar | Alloy Gr 2 Flat Bar Polished |
| Alloy grade 2 titanium Hex Bar Annealed | Titanium WERKSTOFF NR. 3.7035 Cold Drawn Round Bar |
| ASTM B348 grade 2 titanium Round Bars | Titanium Grade 2 Flat Bar stock |
| Titanium WERKSTOFF NR. 3.7035 Hex Bar | Alloy Gr 2 Threaded Bar |
| Titanium Grade 2 Square Bar Polished | Titanium UNS R50400 Bright Bar Hot Rolled |
| 3.7035 grade 2 titanium Hex Bar Bright | Alloy Gr 2 Alloy Hollow Bar |
| Gr 2 Titanium Rectangular Bar Annealed | Alloy grade 2 titanium Polished Hex Bar |
| ASME SB 338 gr 2 Forged Bar | Gr 2 Titanium Polished Bar |
| Alloy Gr 2 Alloy Rods | UNS R50400 Titanium Flat Bar Cold Drawn |
| Alloy Gr 2 Square Bar Cold Drawn | Titanium Grade 2 Bright Bar material |
| grade 2 titanium Rod | Titanium UNS R50400 Flat Bar Annealed |
داکسون را انتخاب کنید تا به پروژهتان کمک کند اوج بگیرد.
DAXUN® Grade 2 Titanium Rod Features
DAXUN® Ti Grade 2 is a commercially pure (CP) titanium bar known for its standout features:
- Excellent general corrosion resistance in seawater
- Resistant to stress corrosion cracking in chloride and sour gas environments
- Excellent resistance to pitting, crevice, and erosion-corrosion
- High heat transfer efficiency
- قابلیت شکلپذیری و جوشپذیری خوب
- Extremely low thermal expansion
- Moderate strength
مزایای کارخانه داکسون
Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.
Grade 2 Titanium Rod Production Method
Daxun specializes in producing high-quality titanium bars known for their exceptional performance. Additionally, we offer customized manufacturing services to meet specific requirements as outlined in the customer’s agreement.
- Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
گزارشهای آزمون
گزارشهای آزمایشی که ما ارائه میدهیم شامل موارد زیر است: گواهی آزمایش کارخانهای میلهی تیتانیوم گرید ۲ و میلهی گرد تیتانیوم گرید ۲، EN 10204 3.1، گزارش شیمیایی، گزارش مکانیکی، گزارش آزمون PMI، گزارش بازرسی چشمی، گزارش بازرسی شخص ثالث، گزارش آزمایشگاه مورد تأیید NABL، گزارش آزمون مخرب و گزارش آزمون غیرمخرب. (داکسون بر اساس نیاز مشتری ارائه خواهد کرد)
Grade 2 Rods Applications and Standards
Grade 2 Titanium Rods are widely used in the following industries under extreme corrosive conditions:
- Aerospace, military, oil and gas industry, marine engineering, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
- Specifications: ASTM B861, B862, B338 / ASME SB861, SB862, SB338
- استانداردها: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
کیفیت، تحویل، بازرسی
Daxun ensures the reliability of Grade 2 Titanium Rods and Round Bars through rigorous quality assurance tests. These include tensile testing, chemical analysis, PMI for material consistency, micro and macro testing, IGC testing for corrosion resistance, ultrasonic flaw detection, and hardness and expansion evaluations.
Throughout production, Daxun carefully measures diameter, thickness, and surface quality, guaranteeing materials meet the highest standards and application requirements.
- زمان تحویل ما دقیقاً مطابق قرارداد است.
- از آژانسهای ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
- از نمونههای رایگان برای آزمایش مشتری پشتیبانی کنید.
- حمایت از بازرسی کارخانهای حضوری یا ویدیویی
بستهبندی
داکسون آلیاژ بهترین کیفیت بستهبندی را تضمین میکند، زیرا بستهبندی نقش مهمی در حملونقل بینالمللی دارد که کالاها از مسیرهای مختلف عبور میکنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژهای به بستهبندی داریم. ما کالاهای خود را بسته به محصول به روشهای مختلف بستهبندی میکنیم. روشهای بستهبندی محصولات ما عبارتند از:
• جعبهها و صندوقها
• Shrinkwrap
• پالتهای چوبی
• جعبههای چوبی
پشتیبانی فنی
If you require additional technical assistance, our resident metallurgist and knowledgeable staff are ready to support you. At Daxun, we take pride in our certified testing laboratory, a first in the multi-metal and plastic inventory industry. This reflects our unwavering commitment to quality and reinforces our philosophy as a full-service supplier dedicated to meeting your needs.
Grade 2 bar and rod features
Daxun Grade 2 Titanium Rods help your brand improve quickly
- Titanium rod/bar
- Types of Grade 2 Titanium Rods
- Tolerances for Grade 2 Titanium Round Bars (BS EN ISO 286-2)
| Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of rod/bar, Bar and Tube. | |
| محصولات/استاندارد فرآوری | رتبه/اندازه |
| Titanium rod/bar— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1, GR2, GR3, GR4, GR5, GR7, GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3 (ضخامت: (0.0197”-6”)حداکثر عرض: ۱۲ فوت، حداکثر طول: ۵۰ فوت) |
| AMS-T-9046 | |
| Titanium and Titanium alloy rod/bar | |
| تیتانیوم خالص تجاری (CP) | |
| نشانهگذاری کد | مقاومت تسلیم |
| حداقل، ksi ۱ / | |
| سیپی-۱ | 70 |
| سیپی-۲ | 55 |
| سیپی-۳ | 40 |
| سیپی-۴ | 25 |
| آلیاژهای تیتانیوم آلفا (الف) | |
| نشانهگذاری کد | ترکیب |
| الف-۱ | ۵A۱-۲.۵Sn |
| الف-۲ | ۵A۱-۲.۵Sn(ELI) ۲ / |
| الف-۳ | ۶A۱-۲Cb-۱Ta-۰.۸Mo |
| الف-۴ | ۸A۱-۱Mo-۱V |
| آلیاژهای تیتانیوم آلفا-بتا (AB) | |
| نشانهگذاری کد | ترکیب |
| ایبی-۱ | ۶A۱-۴V |
| AB-2 | ۶A۱-۴V(ELI) |
| AB-3 | ۶A۱-۶V-۲Sn |
| AB-4 | ۶آی۱-۲اسان-۴زیر-۲موی |
| AB-5 | ۳A۱-۲.۵V |
| AB-6 | ۸ منگنز |
| آلیاژهای تیتانیوم بتا (B) | |
| نشانهگذاری کد | ترکیب |
| بی-یک | ۱۳V-۱۱Cr-۳A1 |
| بی-۲ | ۱۱.۵ مولیبروم-۶ زِیرکونیم-۴.۵ قلع |
| بی-۳ | ۳A۱-۸V-۶Cr-۴Mo-۴Zr |
| بی-۴ | ۸ منگنز-۸ تیتانیوم-۲ آهن-۳ آلومینیوم |
| پردازش: | |
| نورد گرم | نورد سرد |
| مراحل در دسترس: | |
| رتبه ۱ CP | Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2) |
| رتبهٔ ۲ CP | Grade 6Al-4V ELI (پیشتر Grade 23) |
| پایه هفتم | Grade 6Al-6V-2Sn (6-62) |
| کلاس نوزدهم | پایه ۸، ال-۱ مو-۱ وی (۸-۱-۱) |
| کلاس پنجم (۶آلومینیوم-۴ونادیوم) | کلاس ۹ (۳ آل-۲.۵ ولت) |
| کلاس ۶ (۵آلومینیوم-۲.۵ قلع) | CP درجه ۳ |
| کاربرد | |
| صنعت شیمیایی | شیرینسازی آب دریا |
| صنعت پتروشیمی | هوافضا |
| حوزه ماشینکاری، حوزه خودروسازی | میدان قطعه تلفن همراه. |
| Titanium Grade 2 Hex Bar | Titanium Gr 2 Hex Bar |
| Grade 2 Titanium Hexagonal Bar | |
| Gr 2 Titanium Alloy Hex Bar | |
| UNS R50400 Titanium Hexagonal Bar | |
| ASTM B348 Grade 2 Titanium Hex Bar | |
| Titanium Alloy Grade 2 Square Bar | Titanium Grade 2 Square Bar |
| Grade 2 Titanium Square Bars | |
| Gr 2Titanium Alloy Square Bar | |
| UNS R50400 Titanium Square Bar | |
| مادهٔ خام شمارهٔ ۳.۷۰۳۵ میلهای مربعی | |
| ASTM B348 Gr 2 Titanium Square Bars | |
| Titanium Grade 2 Rectangular Bar | Titanium Grade 2 Rectangular Bar |
| تی. آلیاژ Gr2 میلههای مستطیلی | |
| Gr 2 Titanium Alloy Rectangular Bar | |
| UNS R50400 Titanium Rectangular Bars | |
| مادهٔ خام شمارهٔ ۳.۷۰۳۵ میلهای مستطیلی | |
| ASTM B348 Gr 2 Titanium Rectangular Bar | |
| Titanium Grade 2 Flat Bars | Titanium Grade 2 Flat Bar |
| Gr 2Titanium Alloy Flat Bars | |
| Titanium Gr 2Flat Bars | |
| UNS R50400 Titanium Flat Bars | |
| مادهٔ خام شمارهٔ ۳.۷۰۳۵ میلههای تخت | |
| ASTM B348 Gr 2 Titanium Flat Bars | |
| Titanium Grade 2 Polished Bar | Titanium Grade 2 Polished Bar |
| Grade 2Titanium Polished Bars | |
| Gr 2Titanium Alloy Polished Bar | |
| UNS R50400 Titanium Polished Bars | |
| مادهٔ خام شمارهٔ ۳.۷۰۳۵ میلۀ صیقلیشده | |
| ASTM B348 Gr 2 Titanium Polished Bar | |
| Titanium Grade 2 Threaded Bar | Titanium Gr 2 Threaded Bar |
| Grade 2Titanium Threaded Bars | |
| Ti. Alloy Grade 2 Threaded Bar | |
| UNS R50400 Titanium Threaded Bar | |
| مادهٔ خام شمارهٔ ۳.۷۰۳۵ میلهٔ رزوهای | |
| ASTM B348 Gr 2 Titanium Threaded Bar |
| اندازه اسمی | سرتیتر | سربرگ | h7 | hatred | h9 | H10 | H11 | سرتیتر ۱۲ |
|---|---|---|---|---|---|---|---|---|
| قطر میلیمتر | ||||||||
| تا ۳ | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| بیش از ۳ تا ۶ | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| بیش از ۶ تا ۱۰ | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| بیش از ۱۰ تا ۱۸ | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| بیش از ۱۸ تا ۳۰ ساله | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| بیش از ۳۰ تا ۵۰ | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| بیش از ۵۰ تا ۸۰ | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| بیش از ۸۰ تا ۱۲۰ | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| بیش از ۱۲۰ تا ۱۸۰ | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| بیش از ۱۸۰ تا ۲۵۰ | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
2nd grade bar type (3)
اطلاعات موجود برای مرجع و دانلود
میل تیتانیوم
Daxun is a trustworthy titanium rod and bar manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium bars are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the Titanium rod have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
پروژهها و محصولات داغ اخیر
محصولات مرتبط (8)
What are Grade 2 Titanium rods?
Ti CP Grade 2 has greater tolerated levels of iron and oxygen and is frequently utilized due to its outstanding formability, moderate strength, and superior corrosion resistance. It has a minimum yield strength of 275 Mpa (40 ksi) and relatively low amounts of impurity elements, placing it in the strength range of Grades 1 to 3.
Grade 2 Titanium Rod Equivalent Grade
| nation | name | usually |
| Russia | VT1-0 (VT1-0) | Gorst 19807-91 |
| Germany | 3.7035 | Job Number (3.7035) |
| Europe | Titanium Grade 2 | ZH-10204 3.1 |
| Japan | Titanium Grade 2 | JIS H 4600 |
| People’s Republic of China | TA2 | GB/T 3621-2007 / GB/T 13810-2007 |
| USA | Titanium Grade 2 | ASTM B348 / B265 / B337,UNS R50400 |
مقاومت در برابر خوردگی
Commercially pure (CP) titanium offers remarkable resistance to crevice corrosion in salt solutions, outperforming stainless steel. It retains its integrity against crevice corrosion at temperatures under 80 °C (176 °F), regardless of pH levels, even in environments with high chlorine concentrations.
Stress Corrosion Cracking (SCC)
Grade 2 titanium exhibits remarkable resistance to stress corrosion cracking. It performs exceptionally well in hot chloride solutions and is entirely immune to SCC in seawater, making it a dependable material for harsh environments.
Erosion Corrosion
Titanium exhibits exceptional durability in flowing seawater, withstanding velocities as high as 130 ft/sec (40 m/sec) without significant degradation. Even in the presence of abrasive particles like sand, its corrosion resistance remains largely unaffected, highlighting its reliability in demanding environments.
Hydrogen Embrittlement
When exposed to seawater, titanium absorbs minimal hydrogen, even at higher temperatures. However, absorption typically takes place only under certain specific conditions:
- pH levels below 3 or above 12
- Temperatures exceeding 80 °C (176 °F)
- A mechanism for hydrogen generation, such as galvanic coupling or an impressed current.
Bio-Corrosion
Titanium alloys exhibit complete immunity to microbiologically influenced corrosion. However, because they are non-toxic to marine organisms, biofouling can develop in seawater. This can be effectively managed through chlorination or by increasing the flow rate of water through heat exchangers.
Corrosion Fatigue
Unlike many materials, titanium maintains its fatigue performance in seawater. Fatigue endurance limits and crack growth rates are consistent, whether tested in air or seawater, making it a reliable choice for marine applications.
Galvanic Corrosion
Titanium ranks among the noble materials in the galvanic series, positioned near stainless steels, and generally serves as the cathode when paired with other metals. As a result, titanium remains resistant to galvanic corrosion but can increase corrosion in less noble metals. When paired with more noble substances, such as graphite, its passive properties become even stronger.
Fatigue Properties
Grade 2 Titanium Rod maintains its exceptional fatigue properties even in seawater. Its fatigue endurance limits and crack growth rates remain unchanged regardless of whether testing occurs in air or seawater, highlighting its consistent performance under varied conditions.
قابلیت جوشکاری
CP2 Grade Titanium Rod is highly weldable when appropriate precautions are observed. Given its reactive nature, an inert gas shield must protect both the outer diameter (OD) and inner diameter (ID) during welding. Additionally, the rod should be completely free of grease or oil to ensure optimal weld integrity.
Grade 2 Titanium Rod is most often welded using either manual or automatic TIG methods, with or without filler wire. A low heat input is advised to limit the size of the heat-affected zone. Post-weld heat treatment is generally not required, simplifying the process while maintaining the rod’s key properties.
This revised version maintains the technical depth and original structure while improving clarity, readability, and flow. Let me know if you’d like further refinements!
| Working material: | 3.7035 / UNS R50400 |
| Diameter: | 3 – 400 mm |
| Lengths: | 2.000 – 4.000 mm |
| Versions: | Rolled, forged, annealed |
| Surfaces: | Turned, peeled, polished |
| Standards: | ASTM B 348, ASME SB 348, DIN 17862, ASTM F 67, NACE MR 0175, ISO 1515156-3, ISO 5832-2 |
Buy Grade 2 Titanium Rods/Rounds at Daxun
Are you in need of round rod material made from Grade 2 Titanium Alloy Rod-3.7035? At Daxun, we specialize in providing customized titanium rods tailored to your project’s specifications. As an experienced supplier, we are committed to supporting your needs with precision and reliability.
Our Grade 2 Titanium bars are available in diameters ranging from 2.0 mm to 400 mm. Tolerances and execution may vary based on the size of the bar. Smaller diameters are provided centerless ground with h7 tolerances, while larger sizes come with h9 or h11 tolerances. Contact Daxun to discuss your requirements or to request a customized project quote.
Buy Grade 2 Titanium Bars: Features and Specifications.
- Forged bars can be peeled or pre-machined. The material is available in a variety of specifications depending on the application and market needs.
- Our titanium bars typically meet various requirements and certifications, including ASTM B348 and ASTM F 67, DIN 17860, VD TÜV Table 230-3, and Nace MR 0175.
- Titanium round bars are often used where they have excellent corrosion resistance and good mechanical properties.
- Grade 2 titanium bars (3,7035) are therefore suitable for use as a construction material for equipment and devices, as they are easy to process.
خدمات مواد میلهای تیتانیوم ما
- بهعنوان یک مرکز خدمات با تجربه، ما میتوانیم ماده میلهی تیتانیومی شما را مطابق با مشخصاتتان سفارشی کنیم، با نهادهای مختلف صدور گواهی مانند TÜV Rheinland یا DNV برای تأیید مشخصات همکاری کنیم و فرایند ارتقای محصولات نیمهتمام تیتانیومی را برای پاسخگویی به کاربردهای مناسب آغاز کنیم.
- ما خوشحال میشویم مشاوره لازم را در اختیار شما قرار دهیم و همه چیزهایی را که باید در مورد تهیه مواد میلهای تیتانیوم بدانید، از جمله استانداردهایی که برای ساخت قطعات نیازمند توجه بیشتری هستند، برایتان توضیح دهیم.
- اگر تعهد تأمین بلندمدت دارید، میتوانید یک قرارداد چارچوبی با داکسون منعقد کنید. ما قیمتها و مقادیر را برای مدت زمان مشخصی تضمین میکنیم.
- Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about the Grade 2 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.
اطلاعات سفارش
When placing a purchase order, make sure to include the quantity, grade, type or category, API5L reference, as well as the thickness, width, and length of the product. If you have any specific requirements, like chemical composition, mechanical properties, heat treatment, additional testing, manufacturing methods, surface coatings, or end finishes, let us know so we can meet your needs.
Feel free to contact Daxun with your order details. We are committed to responding to your inquiry promptly.
رتبه آلیاژ تیتانیومی که نیاز دارید به پروژهای که روی آن کار میکنید بستگی دارد، زیرا هر رتبه مزایای متفاوتی دارد.
تمام گریدهای آلیاژ تیتانیوم فوقالعاده قوی و مقاوم در برابر خوردگی هستند، به این معنی که در سختترین شرایط نیز به خوبی کار خواهند کرد.
درجهٔ بالاتر آلیاژ تیتانیوم (۵–۱۲) آلیاژهایی هستند که برای مزایای خاص طراحی شدهاند. برای مثال، آلیاژ تیتانیوم درجهٔ ۱۲ مقاومت حرارتی عالی دارد و آن را به گزینهای ایدهآل برای مبدلهای حرارتی پوسته و لولهای، لولهکشی هیدرولیک و تجهیزات صنعت شیمی تبدیل میکند.
درجههای ۱ تا ۴ آلیاژهای تیتانیوم خالص هستند و اگر به مادهای جوشپذیر و چکشخوار برای سیستمهای لولهکشی و تیوبها نیاز داشته باشید، انتخابی ایدهآلاند. درجههای پایینتر را در صنایع دریایی و صنعتی خواهید یافت.
اگر در حال شروع یک پروژه هستید و مطمئن نیستید کدام گرید آلیاژ تیتانیوم برای شما مناسبتر است، همین امروز با ما تماس بگیرید؛ ما با کمال میل به شما کمک خواهیم کرد.
در داکسون، ما طیف گستردهای از گریدهای آلیاژ تیتانیوم از گرید ۱ تا گرید ۱۲ را ارائه میدهیم.
گریدهای ۱ تا ۴ تیتانیوم خالص هستند، در حالی که گریدهای بالاتر آلیاژ هستند.
کلاسهای آلیاژ بهخاطر نسبت بالای استحکام به وزنشان محبوب هستند.
رایجترین گرید آلیاژ تیتانیومی که مییابیم، گرید ۵ است. اگرچه همچنان غنی از تیتانیوم است، این گرید یکی از قابلاعتمادترینهاست زیرا میتواند دماهای تا ۶۰۰ درجه فارنهایت را تحمل کند و در شرایط شدید دوام بیاورد.
در صنایعی مانند صنایع هوافضا و دریایی، به دلیل مقاومت در برابر سایش و خوردگی، گریدهای بالاتر ترجیح داده میشوند.
برعکس، گریدهای پایینتر عمدتاً به دلیل استحکام کمتر برای جوشکاری استفاده میشوند.
To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.
اگرچه درجه تیتانیوم کمی هزینه را افزایش میدهد، اما هزینه کل عمدتاً به شکل و فرم تیتانیومی که نیاز دارید بستگی دارد.
At DAXUN, we offer a wide range of titanium products, including rod/bars, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.
متأسفانه بدون اطلاع کافی از پروژه شما و کاربرد تیتانیوم، تعیین قیمت بهصورت آنلاین دشوار است.
خوشبختانه تیم کارشناسان ما همیشه در خدمت شماست تا در زمینه نیازهای تیتانیومیتان به شما کمک و مشاوره دهد. با ارسال ایمیل به [email protected]، ما قادر خواهیم بود با ارائه مشاوره و برآورد دقیق هزینه به شما پاسخ دهیم.
حتماً تا حد امکان اطلاعاتی دربارهٔ گرید، شکل و مقدار تیتانیومی که نیاز دارید ارائه دهید تا نیازهایتان بهتر درک شود.
تیم DAXUN باتجربه، آگاه و خوشبرخورد است. با سالها تجربه در این صنعت، آنها همه چیز را درباره تیتانیوم، از کاربردها و مزایا گرفته تا گریدهای مختلف آن، میدانند.
برای دریافت بهروزرسانیهای منظم درباره تیتانیوم، کاربردها و مصارف آن در صنایع مختلف، حتماً وبلاگ ما را بررسی کنید. کارشناسان ما راهنماهای سادهای نوشتهاند که همیشه میتوانید هنگام پرسش به آنها مراجعه کنید.
اگر همچنان با مشکل مواجه هستید، با ما تماس بگیرید؛ خوشحال میشویم به شما کمک کنیم.
با ارسال ایمیل به [email protected]، پاسخ سریعی دریافت خواهید کرد. لطفاً در سؤال خود تا حد امکان جزئیات بیشتری درج کنید تا بتوانیم راهحل مناسبی پیشنهاد دهیم.
لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتساپ ما آنلاین است و ایمیل ([email protected]) ظرف ۶ ساعت بررسی میشود. به هر پرسش یا پیام بهسرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک میگذاریم.
We can provide Titanium rod. samples for you to check the quality. Sample is free and you just pay the freight.
ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشتهایم.
Our MOQ is 1 ton for Titanium rod.
سفارشهای آزمایشی را میتوان ظرف یک هفته تحویل داد. برای سفارشهای معمولی تقریباً دو هفته زمان لازم است.