x
همین امروز استعلام خود را ارسال کنید
استعلام سریع

Daxun is an experienced manufacturer of CP-1 grade titanium tubes

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:CP-1(Grade 1)- UNS R50250
  • Titanium tube types: Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of grade 1 titanium is 4.51 g/cm3
  • Standards: ASTM B861、B862、B338 / ASME SB861、SB862、SB338
  • Softest Ti,High ductility, Very corrosion resistant, good cold formability

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

A global leader in commercially pure titanium tube fabrication services

Commercially Pure Titanium Grade 1 Tube is one of the softest and most ductile types with excellent formability. Grade 1 Titanium Tube is primarily used in the maritime and chemical industries where parts are exposed to extremely harsh conditions. The ultimate tensile strength of SB 338 Gr 1 Tube is 35 KSI min (240 MPa min), while the yield strength (0.2% variation) of Cp Grade 1 Tube is 25 – 45 KSI (170 – 310 MPa). Ti Cp Grade 1 Seamless Tube is also known as TA1, Titan Grade 1, and Gr 1. Grade 1 Titanium Tube is a non-alloyed, low-strength titanium tube product with low oxygen concentration and excellent formability; it is used in the chemical industry, heat exchangers, and desalination facilities.

Grade 1 Titanium Tube is also well suited for manufacturing exhaust systems, charge air pipes, and water pipes. We offer Titanium Tube with a thickness equivalent to 1.2 mm and diameters ranging from 51 mm to 102 mm (the most common exhaust system sizes). Therefore, these tubes are more stable and stronger even at higher exhaust gas temperatures.

Daxun certifies and tests titanium alloy tubes according to ASME SB/ASTM, B861 and B862, including hardness testing, hydrostatic testing, eddy current testing, ultrasonic defect identification, tensile testing, flattening, expansion testing, annealing, tempering, stress relief, etc.

Titanium Grade 1 Tube, Titanium UNS R50250 Tube, Titanium Alloy DIN 3.7025 Seamless Tube, Titanium Alloy Grade 1 Tube, Titanium Grade 1 Seamless Tube, Titanium UNS R50250 Seamless Tube, Titanium Alloy Grade 1 Tube, Titanium Tube Suppliers, Welded Titanium Tubes, Titanium Tubes for Sale, Titanium Seamless Tubes, Titanium Tube Suppliers, Titanium Werkstoff Nr. 3.7025 Tube, Titanium UNS R50250 Seamless Tube, Titanium Alloy R50250 Tube, Titanium R50250 Welded Tube, Titanium Gr1 Tube, Titanium Alloy DIN 3.7025 Welded Tube, Titanium Gr.1 Tube Suppliers in China.

Are you looking to purchase titanium tubes for your project or order a range of tubes? Daxun produces a wide range of titanium tubes including Grade 1 (3.7025), Grade 2 (3.7035), Grade 3 (3.7055), Grade 7 (3.7235), Grade 9 (3.7195) and Grade 12 (3.7105).

Buy titanium tubes at Daxun Alloys.
We offer a wide range of sizes starting from 1.0 mm in diameter with multiple variations, available directly from stock or custom made to your specifications through our network. We have wrought titanium tubes, seamless titanium tubes and longitudinally welded titanium tubes immediately available from stock for a wide range of applications.

We offer heat exchanger tubing in standard specifications such as ASTM B 338, ASME SB 338, DIN 17866 and VD TÜV welded titanium tubes or seamless titanium tubes. When it comes to titanium tubes, we have a large supply of titanium welded tubes and titanium seamless tubes in China in standard sizes up to 100 mm thick. We will supply welded titanium tubes for larger pipe sizes. The most common specifications used in the industry are ASTM B 861, ASFM B 862, NACE and NORSOK and VD TÜV Tube 230/2, depending on the specifications of the plant designer.

Titanium tube surface treatment options include bright annealing, pickling and grinding. Material parameters vary depending on the application and product requirements. The corrosion and mechanical properties of titanium alloy tubes vary. We are happy to assist you in evaluating your needs. If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee price and quantity for a specified period.

بیشتر بخوانید

داده‌ها

Grade 1 Titanium pipe & Tubes Specification ASTM B338 / ASTM B861 / ASTM B862 / ASME SB338 / ASME SB861 / ASME SB862
Grade 1 Titanium pipe & Tubes Grades Commercially pure titanium Grade 1- TA1- USN 50250
Grade 1 Titanium pipe & Tubes Type ot Rolled / Cold Drawn / Welded / ERW
Grade 1 Titanium pipe & Tubes Outer Diameter Size Titanium seamless pipe – φ1.0mm to φ508.3mm
Titanium welded pipe – φ6.0mm to φ1219mm
Grade 1 Titanium pipe & Tubes Wall Thickness 0.3mm—50mm (customizable wall thickness)
Grade 1 Titanium pipe & Tubes Length 5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size.
Titanium pipe Form ‘ Hollow, U’ bent, LSAW, Hydraulic, Straight Tube, Boiler, Round, Tube Coil, Square, Rectangular Etc
Marking All Titanium Tubes Tubing are marked as follows: Grade, Standard, Thickness, OD, Heat No., Length (Or according to the customer’s request.)
Uses of Titanium Alloy Tubes Gas pipes, oil pipes, heat exchanger tubes, boiler tubes, fluid pipes, titanium exhaust pipes.
Grade 1 Titanium pipe & Tubes Pipe Ends Plain Ends / Beveled Ends
Grade 1 Titanium pipe & Tubes Delivery Conditions As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered
Grade 1 Titanium pipe & Tubes Coating Electropolish, Mechanical Polish, Satin Finish, Passivated
Grade 1 Titanium pipe & Tubes Other Testing ardness Test, Hydrostatic Test, Eddy Current test, Eddy Current, Tensile Test, Flattening, Flare Test, Annealed, Hydrostatic Test, Tempered, Stress Relieved etc.
Grade 1 Titanium pipe & Tubes Dimension All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME
Grade 1 Titanium pipe & Tubes Value Added Services Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment
Grade 1 Titanium pipe & Tubes Packaging Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector
Grade 1 Titanium pipe & Tubes Shipment & Transportation By Road – Truck / Train, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes
Grade 1 Titanium pipe & Tubes Material Test Certificate Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS ETC
عنصر Minimum (weight %) Maximum (weight %) Typical (weight %)
آهن 0.2
O 0.18
C 0.08
N 0.03
H 0.015
تیتانیوم تعادل
خواص فیزیکی متریک انگلیسی نظرات
تراکم 4.50 g/cc 0.163 lb/in³
a Lattice Constant 2.95 Å @Temperature 25.0 °C 2.95 Å @Temperature 77.0 °F alpha phase
3.29 Å @Temperature 900 °C 3.29 Å @Temperature 1650 °F beta phase
c Lattice Constant 4.683 Å 4.683 Å @Temperature 77.0 °F c/a = 1.587
Chemical Properties متریک انگلیسی نظرات
Thermal Neutron Cross Section 5.6 barns/atom 5.6 barns/atom Average for naturally occurring Ti
خواص مکانیکی متریک انگلیسی نظرات
سختی، برینل 120 120 annealed
سختی، نوپ 132 132 Estimated from Brinell.
Hardness, Rockwell B 70 70 annealed
سختی، ویکرز 122 122 Estimated from Brinell.
مقاومت کششی 124 – 138 MPa @Temperature 427 °C 18000 – 20000 psi @Temperature 801 °F
152 – 179 MPa @Temperature 316 °C 22000 – 26000 psi @Temperature 601 °F
193 – 207 MPa @Temperature 204 °C 28000 – 30000 psi @Temperature 399 °F
Tensile Strength, Ultimate ۲۴۰ مگاپاسکال ۳۴۸۰۰ پی‌اس‌آی
Tensile Strength, Yield 170 – 310 MPa 24700 – 45000 psi
76.0 – 90.0 MPa @Temperature 427 °C 11000 – 13100 psi @Temperature 801 °F 0.2% offset
83.0 – 103 MPa @Temperature 316 °C 12000 – 14900 psi @Temperature 601 °F 0.2% offset
110 – 124 MPa @Temperature 204 °C 16000 – 18000 psi @Temperature 399 °F 0.2% offset
نرخ کشش در شکست 24% 24%
25 – 30 % @Temperature 427 °C 25 – 30 % @Temperature 801 °F
30 – 35 % @Temperature 316 °C 30 – 35 % @Temperature 601 °F
40 – 50 % @Temperature 204 °C 40 – 50 % @Temperature 399 °F
کاهش مساحت 35% 35%
Tensile Modulus 103 GPa 14900 ksi
Compressive Modulus 110 GPa 16000 ksi
Poissons Ratio 0.37 0.37
ماژول برشی 45.0 GPa 6530 ksi
آزمایش ضربه چارپی 310 J 229 ft-lb V-نُچ
Impact Test 136 J 100 ft-lb Impact Strength
Coefficient of Friction, Dynamic 0.68 0.68 Ti sliding on Ti; 300 m/min
0.8 0.8 Ti sliding on Ti; 40 m/min
خواص الکتریکی متریک انگلیسی نظرات
مقاومت الکتریکی 0.0000420 ohm-cm 0.0000420 ohm-cm
نفوذپذیری مغناطیسی 1.00005 1.00005 at 1.6 kA/m
پذیری مغناطیسی 3.98E-08 3.98E-08 1/kg; Paramagnetic
خواص حرارتی متریک انگلیسی نظرات
Heat of Fusion 325 J/g 140 BTU/lb High Purity Ti.
CTE, linear 8.35 µm/m-°C @Temperature 15.0 °C 4.64 µin/in-°F @Temperature 59.0 °F
8.70 µm/m-°C @Temperature 100 °C 4.83 µin/in-°F @Temperature 212 °F
9.50 µm/m-°C @Temperature 300 °C 5.28 µin/in-°F @Temperature 572 °F
9.70 µm/m-°C @Temperature 0.000 – 540 °C 5.39 µin/in-°F @Temperature 32.0 – 1000 °F perpendicular to the c-axis
ظرفیت گرمایی ویژه 0.520 J/g-°C 0.124 BTU/lb-°F
0.560 J/g-°C @Temperature 200 °C 0.134 BTU/lb-°F @Temperature 392 °F
0.620 J/g-°C @Temperature 400 °C 0.148 BTU/lb-°F @Temperature 752 °F
0.690 J/g-°C @Temperature 600 °C 0.165 BTU/lb-°F @Temperature 1110 °F
هدایت حرارتی 16.0 W/m-K 111 BTU-in/hr-ft²-°F annealed
نقطه ذوب <= 1670 °C <= 3040 °F
مایع 1670 °C 3040 °F
بتا ترنسوس 882 °C 1620 °F
Optical Properties متریک انگلیسی نظرات
Emissivity (0-1) 0.3 @Temperature 710 °C 0.3 @Temperature 1310 °F High purity Ti
Reflection Coefficient, Visible (0-1) 0.56 0.56 High purity Ti; visible light.
Component Elements Properties متریک انگلیسی Comments
Carbon, C <= 0.10 % <= 0.10 %
Hydrogen, H <= 0.015 % <= 0.015 %
Iron, Fe <= 0.20 % <= 0.20 %
Nitrogen, N <= 0.030 % <= 0.030 %
سایر، کل <= 0.30 % <= 0.30 %
Oxygen, O <= 0.18 % <= 0.18 %
Titanium, Ti >= 99.175 % >= 99.175 %
Descriptive Properties
Alpha Phase Crystal Structure cph, below 882°C
Beta Phase Crystal Structure bcc, above 882°C
Ti. Alloy Grade Titanium Alloy Grade 1 Round Tubes Titanium Grade 1 Oil and gas tubes distributor
Titanium Alloy Grade 1 Round Tubing ASME Titanium Grade 1 Seamless Tube
Titanium Grade 1 Round Tube suppliers Seamless Titanium Grade 1 Tubing
UNS R50250 Round Tubes distributor 1 Nickel Chromium Tubing
Titanium Alloy Grade 1 Round Tube suppliers Titanium Grade 1 Nuclear tubes suppliers
Titanium Alloy Grade 1 Welded Tube suppliers Titanium Grade 1 Chemical process tubes traders
Titanium Alloy Grade 1 Round Tubes stockist Titanium Grade 1 Medical tubes manufacturers
Titanium Grade 1 Seamless Tube Titanium Grade 1 Heat exchanger tubes stockist
Grade 1 Titanium Welded Tube Titanium Grade 1 Control lines manufacturers
Titanium Alloy Grade 1 Coil Tubes Titanium Grade 1 Umbilicals suppliers
Alloy WERKSTOFF NR. 3.7025 Welded Tubes Titanium Grade 1 Hydraulic tubes traders
Titanium Grade 1 Triangle Tube exporter in CHINA Titanium Grade 1 Electropolished Tubes
Titanium Grade 1 Hexagonal Tube distributor Titanium Grade 1 SCH 40 Tube exporter in CHINA
Titanium Grade 1 Hollow Tubes Suppliers Titanium Grade 1 SCH 80 Tube distributor
exporter of Titanium Grade 1 thermocouple Tube Titanium Grade 1 Oil & Gas Tubing distributor
Trader of ASTM Titanium Grade 1 Polish Tube Titanium Grade 1 SCH 40 Tube distributor
Titanium Grade 1 Cold Drawn Tube stockist Titanium Grade 1 SCH 80 Tube manufacturers
Titanium Grade 1 ERW Tube manufacturers Titanium Grade 1 Seamless Hollow Tubes
High Quality Titanium Grade 1 Seamless Tube Stockist of Titanium Grade 1 Electropolished Tubes
Titanium Grade 1 Square Tube manufacturers ASTM/ASME Titanium Grade 1 Capillary Tubes
Titanium Grade 1 Round Tube exporter in CHINA Titanium Grade 1 U Shaped Tube distributor
Titanium Grade 1 Rectangular Tube traders Titanium Grade Titanium Alloy Grade 1 Tube suppliers
ASTM Titanium Grade 1 Round Tubes stockist ASTM Titanium Grade 1 Decorative Tubes
exporter of Titanium Grade 1 Colour Coated Tube Titanium Grade 1 Tubing exporter in CHINA
Titanium Grade 1 Welded Tube stockist Titanium Grade 1 Oil Tube suppliers
Titanium Grade 1 Secondary & Surplus Tube ASTM Titanium Grade 1 Instrumentation Tubes
Titanium Grade 1 Outside Polished Tube Titanium Grade 1 Triangle Tube distributor
ASTM/ASME Titanium Grade 1 Capillary Tubes Titanium Grade 1 High-strength capillary tubing
Titanium Grade 1 EFW Tube suppliers Titanium Grade 1 Bellows Tubes exporter in CHINA
Titanium Grade 1 Boiler Tubes distributor Titanium Grade 1 precision tubes stockist
Titanium Grade 1 Cold Drawn Tube wholesaler Titanium Grade 1 Transmission tubes importers
Titanium Grade 1 U Shaped Tube suppliers Titanium Grade 1 Pitot tubes exporter in CHINA
Titanium Grade 1 exhaust tubing manufacturers Titanium Grade 1 encapsulated coiled tubing
Titanium Grade 1 Condensers tubes stockholder Titanium Grade 1 High pressure tubes stockist
Titanium Grade 1 Super Heaters exporter in CHINA Titanium Grade 1 Nuclear Fuel tubes manufacturers
distributor of Titanium Grade 1 Tubes for Heat Exchangers Titanium Grade 1 EFW Tubes Suppliers
Titanium Grade 1 redrawn tubing suppliers distributor of Titanium Grade 1 Instrumentation tubes
Titanium Grade 1 seam-welded tubing stockist exporter of Titanium Grade 1 high precision tubes
supplier of Titanium Grade 1 cold-drawn coiled tubing Titanium Grade 1 Nuclear Control Rod Tubes
Titanium Grade 1 Chemical Process Tubes stockist Titanium Grade 1 Seamless Tubing stockist
Titanium Grade 1 Welded coiled tubing distributor Stockholder of Titanium Grade 1 Gas Tube Ar 15
Titanium Alloy Grade 1 heat resistant tubing Titanium Grade 1 Bourdon Tube importers
custom Titanium Grade 1 tubing Distributor of Titanium Grade 1 Capillary Tubing
Titanium Grade 1 header tubing Supplier of Titanium Grade 1 Furnace Tube
Titanium Grade 1 rectangular tubing Titanium Grade 1 Gas Tubing manufacturers
Titanium Grade 1 Cold Rolled Coiled Tubing Titanium Grade 1 seamless coil tubing wholesaler
Titanium Grade 1 Heat-resistant capillary Tube Titanium Grade 1 seamless straight tubing
Titanium Grade 1 Square Tubing manufacturers Titanium Grade 1 cold drawn seamless tubes
ASTM Titanium Grade 1 Heat Exchager Tubes Titanium Grade 1 Aerospace Engine Tubes stockist
Titanium Grade 1 Tubing Titanium Grade 1 Furnace Tubes manufacturers
Grade 1 Titanium Instrumentation Tubes Titanium Grade 1 Precision Tubing exporter in CHINA
Titanium Alloy Grade 1 coiled tubing Titanium Grade 1 Hot finished seamless tubing (HFS)
Titanium Alloy Grade 1 straight tube heat exchanger Titanium Grade 1 Cold drawn seamless tubing (CDS)
Titanium Grade 1 umbilical tubing Titanium Grade 1 Drawn over mandrel (DOM)
Titanium Grade 1 extreme environment gas tube supplier of Grade 1 Titanium Finned Tube
Titanium Grade 1 tube stock Titanium Grade 1 Tubes for Precision Components
Titanium Grade 1 welded tubing stockist Titanium Alloy Grade 1 Seamless Tube
Titanium Grade 1 tubing bends Grade 1 Titanium Seamless Tubes
Titanium Grade 1 thin wall tubing UNS R50250 Seamless Tube
custom Titanium Grade 1 tubing Grade 1 Titanium Welded Tubes
Titanium Grade 1 tube sizes Titanium Alloy UNS R50250 Welded Tube
Titanium Grade 1 cannula Tubes Ti. Alloy Grade 1 Welded Tubes
Titanium Grade 1 pyrometer tubes WERKSTOFF NR. 3.7025 Seamless Tubes
Titanium Grade 1 protective tubes ASME SB338 Ti. Alloy Grade 1 Seamless Tube
Titanium Grade 1 hypodermic tubing ASME SB338 Ti. Alloy Grade 1 Round Tubes
Titanium Grade 1 capillary tube Titanium Grade 1 Mortar Tube stockholder

داکسون را انتخاب کنید تا به پروژه‌تان کمک کند اوج بگیرد.

همین حالا با داکسون تماس بگیرید

Advanced Production:Titanium seamless pipe

  • Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.
  • (The above is agreed upon by the manufacturer and the customer based on the specific situation)
همین حالا با داکسون تماس بگیرید

Grade 1 Titanium Tube Features

Grade 1 Titanium Tube is the softest form of titanium and has the highest ductility. It has good cold forming characteristics and offers excellent corrosion resistance. It also has excellent welding properties and high impact toughness.

  • Softest Titanium
  • Highest Ductility
  • Excellent Corrosion Resistance
  • Good Cold Formability
همین حالا با داکسون تماس بگیرید

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

همین حالا با داکسون تماس بگیرید

گزارش‌های آزمون

The test reports we provide include: Factory test certificate for Grade 1 titanium welded pipe and Grade 1 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

همین حالا با داکسون تماس بگیرید

Applications and standards

Titanium Grade 1 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
همین حالا با داکسون تماس بگیرید

کیفیت، تحویل، بازرسی

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 1 Titanium Welded Pipe and Grade 1 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • زمان تحویل ما دقیقاً مطابق قرارداد است.
  • از آژانس‌های ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
  • از نمونه‌های رایگان برای آزمایش مشتری پشتیبانی کنید.
  • حمایت از بازرسی کارخانه‌ای حضوری یا ویدیویی
همین حالا با داکسون تماس بگیرید

بسته‌بندی

داکسون آلیاژ بهترین کیفیت بسته‌بندی را تضمین می‌کند، زیرا بسته‌بندی نقش مهمی در حمل‌ونقل بین‌المللی دارد که کالاها از مسیرهای مختلف عبور می‌کنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژه‌ای به بسته‌بندی داریم. ما کالاهای خود را بسته به محصول به روش‌های مختلف بسته‌بندی می‌کنیم. روش‌های بسته‌بندی محصولات ما عبارتند از:
• جعبه‌ها و صندوق‌ها
• سلفون منقبض‌شونده
• پالت‌های چوبی
• جعبه‌های چوبی

همین حالا با داکسون تماس بگیرید

پشتیبانی فنی

اگر به هرگونه پشتیبانی فنی اضافی نیاز دارید، متالورژیست مقیم ما و کارکنان آگاه ما با کمال میل آماده کمک‌رسانی هستند. علاوه بر این، داکسون دارای آزمایشگاه آزمون معتبر است—نخستین در صنعت موجودی چندفلزی و پلاستیکی. به نظر ما، این امر تعهد تزلزل‌ناپذیر ما به کیفیت و فلسفه ما به‌عنوان یک تأمین‌کننده تمام‌خدمت را نشان می‌دهد.

Grade 1 Titanium TUBE Features

مقاومت بالا
مقاومت در برابر خوردگی
مقاومت در برابر حرارت
مقاومت در برابر دمای پایین
حفاظت از محیط زیست
سبک‌وزن

Daxun Grade 1 Titanium TUBE Let your brand improve rapidly

به جز محصولات فهرست‌شده در زیر، سایر محصولات فلزی موجود در اینجا ذکر نشده‌اند. سایر محصولات فلزی که DAXUN می‌تواند تولید و عرضه کند شامل تانتال، نیوبیوم، زیرکونیوم، هافنیوم، نیکل، مس و غیره هستند که عمدتاً به شکل ورق، شمش و لوله عرضه می‌شوند.
محصولات/استاندارد فرآوری رتبه/اندازه
Titanium pipe, tube, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7, GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3 (ضخامت: (0.0197”-6”)حداکثر عرض: ۱۲ فوت، حداکثر طول: ۵۰ فوت)
AMS-T-9046
Titanium and Titanium alloy tube
تیتانیوم خالص تجاری (CP)
نشانه‌گذاری کد مقاومت تسلیم
حداقل، ksi ۱ /
سی‌پی-۱ 70
سی‌پی-۲ 55
سی‌پی-۳ 40
سی‌پی-۴ 25
آلیاژهای تیتانیوم آلفا (الف)
نشانه‌گذاری کد ترکیب
الف-۱ ۵A۱-۲.۵Sn
الف-۲ ۵A۱-۲.۵Sn(ELI) ۲ /
الف-۳ ۶A۱-۲Cb-۱Ta-۰.۸Mo
الف-۴ ۸A۱-۱Mo-۱V
آلیاژهای تیتانیوم آلفا-بتا (AB)
نشانه‌گذاری کد ترکیب
ای‌بی-۱ ۶A۱-۴V
AB-2 ۶A۱-۴V(ELI)
AB-3 ۶A۱-۶V-۲Sn
AB-4 ۶آی۱-۲اس‌ان-۴زیر-۲موی
AB-5 ۳A۱-۲.۵V
AB-6 ۸ منگنز
آلیاژهای تیتانیوم بتا (B)
نشانه‌گذاری کد ترکیب
بی-یک ۱۳V-۱۱Cr-۳A1
بی-۲ ۱۱.۵ مولی‌بروم-۶ زِیرکونیم-۴.۵ قلع
بی-۳ ۳A۱-۸V-۶Cr-۴Mo-۴Zr
بی-۴ ۸ منگنز-۸ تیتانیوم-۲ آهن-۳ آلومینیوم
پردازش:
نورد گرم نورد سرد
مراحل در دسترس:
رتبه ۱ CP Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2)
رتبهٔ ۲ CP Grade 6Al-4V ELI (پیش‌تر Grade 23)
پایه هفتم Grade 6Al-6V-2Sn (6-62)
کلاس نوزدهم پایه ۸، ال-۱ مو-۱ وی (۸-۱-۱)
کلاس پنجم (۶آلومینیوم-۴ونادیوم) کلاس ۹ (۳ آل-۲.۵ ولت)
کلاس ۶ (۵آلومینیوم-۲.۵ قلع) CP درجه ۳
کاربرد
صنعت شیمیایی شیرین‌سازی آب دریا
صنعت پتروشیمی هوافضا
حوزه ماشین‌کاری، حوزه خودروسازی میدان قطعه تلفن همراه.
urface Finish Internal Surface(ID) Exterbal Surface(OD)
Roughness Average(RA) Roughness Average(RA)
μ inch μm μ inch μm
کارشناسی هنر Beight Annealed 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
EP Electro Polish 15,10,7,5 0.38,0.25,0.20;0.13 32 0.8
MP Mechanical Polish 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
AP Annealed & Pickled Not defined Not defined 40 or Not defined 1.0 or Not defined
Titanium Grade 1 Seamless Pipe Titanium DIN 3.7025 Seamless Pipe
Titanium UNS R50250 Seamless Pipe
Titanium Grade 1 Seamless Pipes
Titanium Alloy Gr.1 Seamless Pipe
ASTM B337 Titanium Grade 1 Seamless Pipe
ASME SB337 Ti Alloy Gr.1 Seamless Pipes
Titanium Grade 1 Welded Pipe Titanium DIN 3.7025 Welded Pipe
Titanium UNS R50250 Welded Pipe
Titanium Grade 1 Welded Pipes
Titanium Alloy Gr.1 Welded Pipe
ASTM B337 Titanium Grade 1 Welded Pipes
ASME SB337 Ti Alloy Gr.1 Welded Pipes
Titanium Grade 1 Round Pipe Titanium DIN 3.7025 Round Pipe
Titanium UNS R50250 Round Pipes
Titanium Grade 1 Round Pipes
Titanium Alloy Gr.1 Round Pipe
Titanium Grade 1 Round Pipe
Ti Alloy Gr.1 Round Pipes
Titanium Gr.1 Seamless Tubes Titanium DIN 3.7025 Seamless Tubes
Titanium UNS R50250 Seamless Tubes
Titanium Grade 1 Seamless Tubing
Titanium Alloy Gr.1 Seamless Tubes
ASTM B338 Titanium Gr.1 Seamless Tubing
ASME SB338 Ti Alloy Grade 1 Seamless Tubes
Titanium Grade 1 Welded Tubes Titanium DIN 3.7025 Welded Tubes
Titanium UNS R50250 Welded Tubes
Titanium Grade 1 Welded Tubing
Titanium Alloy Gr.1 Welded Tubes
ASTM B338 Titanium Grade 1 Welded Tubing
ASME SB338 Ti Alloy Gr.1 Welded Tubes
Titanium Grade 1 Round Tubes Titanium DIN 3.7025 Round Tubes
Titanium UNS R50250 Round Tubes
Titanium Grade 1 Round Tubing
Titanium Alloy Gr.1 Round Tubes
Titanium Grade 1 Round Tubing
Ti Alloy Gr.1 Round Tubes
Titanium Grade 1 Pipe Titanium DIN 3.7025 Pipe
Titanium UNS R50250 Pipes
Titanium Grade 1 Pipe
Titanium Alloy Gr.1 Pipes
Titanium Grade 1 Pipes
Ti Alloy Gr.1 Pipe
Titanium Grade 1 Tube Titanium DIN 3.7025 Tubes
Titanium UNS R50250 Tube
Titanium Grade 1 Tubing
Titanium Alloy Gr.1 Tubes
Titanium Grade 1 Tubes
Ti Alloy Gr.1 Tubes
NPS Outside Diameter Wall Thickness Weight Weight
in mm in mm Sched kg/Mtr Lb/ft
1/2″ 0.84 21 0.109 2.769 40 STD 1.268 0.851
0.147 3.734 80 STD 1.621 1.088
3/4″ 1.05 27 0.113 2.87 40 STD 1.684 1.131
0.154 3.912 80 STD 2.195 1.474
1″ 1.315 33 0.133 3.378 40 STD 2.501 1.679
0.179 4.547 80 STD 3.325 2.172
1 1/4″ 1.66 42 0.14 3.556 40 STD 3.385 2.273
0.191 4.851 80 STD 4.464 2.997
1 1/2″ 1.9 48 0.145 3.683 40 STD 4.048 2.718
0.2 5.08 80 STD 5.409 3.361
2″ 2.375 60 0.154 3.912 40 STD 5.441 3.653
0.218 5.537 80 STD 7.48 5.022
2 1/2″ 2.875 73 0.203 5.516 40 STD 8.629 5.793
0.276 7.01 80 STD 11.411 7.661
3″ 3.5 89 0.216 5.486 40 STD 11.284 7.576
0.3 7.62 80 STD 15.272 10.253
4″ 4.5 114 0.237 6.02 16.073 10.79
0.337 8.56 22.318 14.983
6″ 6.625 168 0.188 4.775 19.252 12.924
0.203 5.516 20.739 13.923
0.219 5.563 22.318 14.983
0.25 6.35 25.354 17.021
0.28 7.112 40 STD 58.263 18.974
0.312 7.925 31.334 21.036
0.375 9.525 37.285 25.031
0.432 10.973 80 XHY 42.561 28.573
0.5 12.7 48.719 32.708
8″ 8.625 219 0.188 4.775 25.233 16.94
0.203 5.156 27.198 18.259
0.219 5.563 29.286 19.661
0.25 6.35 20 33.308 22.361
0.277 7.036 30 36.786 24.696
0.322 8.179 40 42.352 28.554
0.375 9.525 49.216 33.041
0.406 10.312 60 53.085 35.638
0.5 12.7 80 XHY 64.627 43.388
10″ 10.75 273 0.188 4.775 31.588 21.207
0.219 5.563 36.689 24.631
0.25 6.35 20 41.759 28.035
0.307 7.798 30 51.002 34.24
0.344 8.738 56.946 38.231
0.365 9.271 40 STD 63.301 40.483
0.438 11.125 71.852 48.238
0.5 12.7 60 XHY 81.53 54.735
0.594 15.088 80 95.969 64.429
12″ 12.75 324 0.188 4.775 37.57 25.222
0.219 5.563 43.657 29.309
0.25 6.35 49.713 33.375
0.281 7.137 55.739 37.42
0.312 7.925 61.735 41.445
0.375 9.525 73.824 49.562
0.406 10.312 79.727 53.525
0.5 12.7 97.438 65.415
0.562 14.275 108.966 73.154
14″ 14 356 0.188 4.775 41.308 27.732
0.219 5.563 48.012 32.233
0.25 6.35 20 54.685 36.713
0.281 7.137 61.327 41.172
0.312 7.925 67.939 45.611
0.375 9.525 STD 81.281 54.568
0.438 11.125 40 94.498 63.441
0.5 12.7 XHY 107.381 72.09
0.625 15.875 132.983 89.278
16” 16 406 0.188 4.775 47.29 21.748
0.219 5.563 54.98 36.91
0.25 6.35 10 62.639 42.053
0.281 7.137 70.268 47.174
0.312 7.925 20 77.866 52.275
0.344 8.738 85.677 57.519
0.375 9.525 30 93.213 62.578
STD
0.438 11.125 108.433 72.797
0.5 12.7 40 123.289 82.77
XHY
18″ 18 457 0.219 5.563 61.948 41.588
0.25 6.35 70.593 47.393
0.281 7.137 79.208 53.176
0.312 7.925 20 87.792 58.939
0.375 9.525 STD 105.144 70.588
0.438 11.125 30 122.369 82.152
0.5 12.7 XHY 139.198 93.45
0.562 14.275 40 155.904 104.666
0.625 15.875 172.754 115.978
20″ 20 508 0.25 6.35 78.547 52.733
0.282 7.163 88.458 59.386
0.312 7.925 97.719 65.604
0.375 9.525 20 STD 117.075 78.598
0.438 11.125 136.305 91.508
0.5 12.7 30 XHY 155.106 104.13
0.594 15.088 40 183.378 123.11
0.625 15.875 192.64 129.328
0.688 17.475 211.368 141.901
24″ 24 610 0.25 6.35 94.456 63.413
0.281 7.137 106.029 71.183
0.312 7.925 117.573 18.932
0.375 9.525 20 STD 140.938 64.618
0.438 11.125 164.176 110.219
0.5 12.7 XHY 186.923 125.49
0.625 15.875 232.41 156.028
0.688 17.475 40 255.148 171.293
0.75 19.05 277.401 186.233
30″ 30 762 0.25 6.35 118.318 79.433
0.281 7.137 132.851 89.189
0.312 7.925 10 147.353 98.925
0.375 9.525 STD 176.731 118.648
0.438 11.125 205.983 138.286
0.5 12.7 20 XHY 234.647 157.53
0.625 15.875 30 292.066 196.078
0.688 17.475 320.817 215.38
0.75 19.05 348.988 234.293
36″ 36 914 0.25 6.35 142.18 95.453
0.281 7.137 159.672 107.196
0.312 7.925 10 177.133 118.918
0.375 9.525 STD 215.525 142.678
0.438 11.125 247.79 166.353
0.5 12.7 20 XHY 282.372 198.57
0.625 15.875 351.723 236.128
0.688 17.475 386.487 259.467
0.75 19.05 420.576 282.353
42″ 42 1067 0.312 7.925 206.914 138.911
0.375 9.525 STD 248.319 166.708
0.5 12.7 XHY 33.097 221.61
0.75 19.05 492.163 330.413
48″ 48 1219 0.375 9.525 STD 284.112 190.738
0.438 11.125 331.404 222.487
0.5 12.7 XHY 377.822 253.65
0.75 19.05 563.75 378.473
0.875 22.225 655.969 440.383

Grade 1 titanium tube form (4)

Daxun is a trustworthy stainless steel tube manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel tubes have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

پروژه‌ها و محصولات داغ اخیر

Grade 1 Titanium pipe and tube
Grade 1 Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
Commercially Pure Titanium Tube Grade 1/UNS R50250

ASTM B338 | ASTM B265 | ASME SB265 | ASTM F67 | ISO 5832-2 | 3.7025 | UNS R50250

  • Pure titanium Grade 1 has excellent ductility and cold formability, making it ideal for deep drawing. Titanium Grade 1 is well-known for its good general and seawater corrosion resistance, as well as its great resistance to oxidising, neutral, and mildly reducing media (solutions), including chlorides.
  • Titanium’s low density (approximately half that of nickel-based alloys), high strength-to-weight ratio, and corrosion resistance make it an excellent choice for a variety of harsh chemical conditions.
کدام گرید تیتانیوم بهترین است؟

رتبه آلیاژ تیتانیومی که نیاز دارید به پروژه‌ای که روی آن کار می‌کنید بستگی دارد، زیرا هر رتبه مزایای متفاوتی دارد.

تمام گریدهای آلیاژ تیتانیوم فوق‌العاده قوی و مقاوم در برابر خوردگی هستند، به این معنی که در سخت‌ترین شرایط نیز به خوبی کار خواهند کرد.

درجهٔ بالاتر آلیاژ تیتانیوم (۵–۱۲) آلیاژهایی هستند که برای مزایای خاص طراحی شده‌اند. برای مثال، آلیاژ تیتانیوم درجهٔ ۱۲ مقاومت حرارتی عالی دارد و آن را به گزینه‌ای ایده‌آل برای مبدل‌های حرارتی پوسته و لوله‌ای، لوله‌کشی هیدرولیک و تجهیزات صنعت شیمی تبدیل می‌کند.

درجه‌های ۱ تا ۴ آلیاژهای تیتانیوم خالص هستند و اگر به ماده‌ای جوش‌پذیر و چکش‌خوار برای سیستم‌های لوله‌کشی و تیوب‌ها نیاز داشته باشید، انتخابی ایده‌آل‌اند. درجه‌های پایین‌تر را در صنایع دریایی و صنعتی خواهید یافت.

اگر در حال شروع یک پروژه هستید و مطمئن نیستید کدام گرید آلیاژ تیتانیوم برای شما مناسب‌تر است، همین امروز با ما تماس بگیرید؛ ما با کمال میل به شما کمک خواهیم کرد.

کلاس‌های بالاتر تیتانیوم چه تفاوتی با کلاس‌های پایین‌تر دارند؟

در داکسون، ما طیف گسترده‌ای از گریدهای آلیاژ تیتانیوم از گرید ۱ تا گرید ۱۲ را ارائه می‌دهیم.

گریدهای ۱ تا ۴ تیتانیوم خالص هستند، در حالی که گریدهای بالاتر آلیاژ هستند.

کلاس‌های آلیاژ به‌خاطر نسبت بالای استحکام به وزن‌شان محبوب هستند.

رایج‌ترین گرید آلیاژ تیتانیومی که می‌یابیم، گرید ۵ است. اگرچه همچنان غنی از تیتانیوم است، این گرید یکی از قابل‌اعتمادترین‌هاست زیرا می‌تواند دماهای تا ۶۰۰ درجه فارنهایت را تحمل کند و در شرایط شدید دوام بیاورد.

در صنایعی مانند صنایع هوافضا و دریایی، به دلیل مقاومت در برابر سایش و خوردگی، گریدهای بالاتر ترجیح داده می‌شوند.

برعکس، گریدهای پایین‌تر عمدتاً به دلیل استحکام کمتر برای جوشکاری استفاده می‌شوند.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

آیا درجه تیتانیوم بر هزینه تأثیر دارد؟

اگرچه درجه تیتانیوم کمی هزینه را افزایش می‌دهد، اما هزینه کل عمدتاً به شکل و فرم تیتانیومی که نیاز دارید بستگی دارد.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

متأسفانه بدون اطلاع کافی از پروژه شما و کاربرد تیتانیوم، تعیین قیمت به‌صورت آنلاین دشوار است.

خوشبختانه تیم کارشناسان ما همیشه در خدمت شماست تا در زمینه نیازهای تیتانیومی‌تان به شما کمک و مشاوره دهد. با ارسال ایمیل به [email protected]، ما قادر خواهیم بود با ارائه مشاوره و برآورد دقیق هزینه به شما پاسخ دهیم.

حتماً تا حد امکان اطلاعاتی دربارهٔ گرید، شکل و مقدار تیتانیومی که نیاز دارید ارائه دهید تا نیازهایتان بهتر درک شود.

از کجا می‌توانم دربارهٔ گریدهای تیتانیوم بیشتر بیاموزم؟

تیم DAXUN باتجربه، آگاه و خوش‌برخورد است. با سال‌ها تجربه در این صنعت، آن‌ها همه چیز را درباره تیتانیوم، از کاربردها و مزایا گرفته تا گریدهای مختلف آن، می‌دانند.

برای دریافت به‌روزرسانی‌های منظم درباره تیتانیوم، کاربردها و مصارف آن در صنایع مختلف، حتماً وبلاگ ما را بررسی کنید. کارشناسان ما راهنماهای ساده‌ای نوشته‌اند که همیشه می‌توانید هنگام پرسش به آن‌ها مراجعه کنید.

اگر همچنان با مشکل مواجه هستید، با ما تماس بگیرید؛ خوشحال می‌شویم به شما کمک کنیم.

با ارسال ایمیل به [email protected]، پاسخ سریعی دریافت خواهید کرد. لطفاً در سؤال خود تا حد امکان جزئیات بیشتری درج کنید تا بتوانیم راه‌حل مناسبی پیشنهاد دهیم.

چگونه سریعاً یک برآورد قیمت دریافت کنیم یا اطلاعات بازار را بفهمیم؟

لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتس‌اپ ما آنلاین است و ایمیل ([email protected]) ظرف ۶ ساعت بررسی می‌شود. به هر پرسش یا پیام به‌سرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک می‌گذاریم.

می‌توانم چند نمونه بگیرم؟

ما می‌توانیم نمونه‌های ورق فولاد ضدزنگ را برای بررسی کیفیت در اختیار شما قرار دهیم. نمونه رایگان است و شما فقط هزینه حمل را پرداخت می‌کنید.

تا کنون به کدام کشورها صادرات داشته‌اید؟

ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشته‌ایم.

حداقل مقدار سفارش شما چیست؟

حداقل سفارش ما برای ورق فولاد ضد زنگ ۱ تن است.

زمان تحویل شما چقدر است؟

سفارش‌های آزمایشی را می‌توان ظرف یک هفته تحویل داد. برای سفارش‌های معمولی تقریباً دو هفته زمان لازم است.

همین امروز استعلام خود را ارسال کنید
استعلام سریع