Daxun-A Professional Supplier of 430 Stainless Steel Coil
As a leading stainless steel coil supplier and exporter in China, Daxun supplies stainless steel coils all over the world.
- Coil grade: Ferrite-SS 430
- Coil features: Easy to process, corrosion resistant.
- Coil thickness: 0.4 mm to 12.00 mm
- Coil width: 1000 mm, 1250 mm, 1500 mm and 2000 mm.
- Coil surface: 2B, BA, matte, polished, 8k mirror. If necessary, stainless steel coils will come with a protective film to protect the metal surface from unnecessary damage.
Global leader in stainless steel Coil fabrication services
430 stainless steel coil is a high-quality alloy with good corrosion resistance and strength.
They have higher thermal conductivity than austenite-grade stainless steel coils, a lower thermal expansion coefficient than austenite strip, and are heat fatigue resistant.
430 stainless steel coils are available in various widths and thicknesses from our stock. Known for its excellent formability and weldability, it experiences minimal distortion or warping during welding processes. Additionally, 430 stainless steel can harden during cold working, enhancing its formability and ductility compared to other grades.
Typical applications of 430 stainless steel coil include automotive trim and appliances.
Daxun provides a wide selection of ASTM A240 430 stainless steel coils, including UNS S43000 coils, with both cold-rolled and hot-rolled variations available. As a prominent manufacturer and supplier in China, we take pride in offering high-quality 430 stainless steel coils for diverse applications.
Dah Hsun, an ISO 9001:2008 certified company, stands out as a trusted supplier and exporter of ASTM A240 stainless steel coils, known for our commitment to excellence and customer satisfaction. Stainless steel coils can be cut to your requirements and include a full set of mill test results. Custom lengths and widths are available up to 2000mm. Exporting is our specialty! We can obtain several hard-to-find grades and/or non-standard sizes to satisfy our customers’ specific needs. We have vast experience processing steel coil goods and can divide all stainless steel coils to the desired sizes. Introducing our extensive line of Dah Hsun Stainless Steel goods – the pinnacle of dependability, durability, and performance. We are glad to provide a wide selection of grades and varieties to fulfill the diverse needs of industrial and architectural applications.
Our stainless steel coil goods, which range from the Austenitic series to the Ferritic series and other special categories, are well-known for their high performance and extensive requirements. The austenitic series includes grades such as 304/304L/304J1, 321, and 316/316L/317L/316Ti/310/309, offering a range of thickness options and various surface finishes, including 2B, BA, NO.4, 8K, SB, HL, NO.1, and more.
Our ferritic range, which includes 430, ultra-pure ferrite 443, and 436L/439/444/441, is designed to meet the needs of customers seeking specialized properties and applications. These materials can accommodate thicknesses ranging from 0.4mm to 3.0mm and offer a variety of surface treatment options such as 2B, BA, NO.4, 8K, SB, HL, and so on.
By selecting our stainless steel coils, you are investing in a material that ensures long service life, great reliability, and exceptional performance. Don’t compromise on quality; choose our stainless steel solutions and see the impact they can make on your project. Contact Daxun today for additional information or to place an order for the stainless steel coil specs and quantities that you require.
Data
- Parameter
- Element
- Mechanical Properties
- PHYSICAL PROPERTIES
- All equivalent
- 430 coil stock
430 Stainless Steel Coil Specification | ASTM A240 / ASME SA240 |
---|---|
430 Stainless Steel Coil Manufacturing Process | Hot Rolled (HR) / Cold Rolled (CR). Note: 430 stainless steel is less weldable compared to 304 due to its higher carbon content and lack of stabilizing elements, requiring post-weld heat treatment. |
430 Stainless Steel Coil Grades | 201 / 304 / 304L/ 430 / 309S / 420 / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L etc. |
UNS No. – UNS S430, UNS S31008, UNS S31600, UNS S31603, UNS S31603, UNS S31600, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904 | |
EN No. – 1.4301, 1.4307, 1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539 | |
430 Stainless Steel Coil Thickness | 0.6 MM TO 16 MM THICKNESS |
430 Stainless Steel Coil Width | 1250 MM / 1500 MM / 2000 MM / 04 Feet / 05 Feet and Custom Cut Width as Per Requirement |
430 Stainless Steel Coil Length | 2400 MM / 2420 MM / 6000 MM / 08 Feet / 10 Feet / Coil Cut and Custom Cut Length as Per Requirement |
430 Stainless Steel Coil Surface Finish | 2B, 2D, BA, MATT, MATT PVC, No.4, No.5, SB, HR, No.8, Mirror, Hairline, Brush, Textured, Oil base wet Polished, Both sides Polished available. |
430 Stainless Steel Coil Coating | PVC coating Normal / Laser, Film: 100 micrometers, Color: black/white. |
430 Stainless Steel Coil Other Testing | NACE MR0175, Ultrasound TEST, IGC TEST, Intergranular Corrosion Test as per ASTM A262 Practice E, Charpy Impact Test, Macro, Grain Size, Hardness, etc. |
Surface finish is crucial in preventing crevice corrosion, especially in thinner gauge materials, to ensure the longevity of the product. | |
430 Stainless Steel CoilValue Added Services | Gas Cutting / CNC Plasma Cutting / Profiling / Rolling / Bending / Sheet Metal Fabrication / Drill / Punch / Machining / Sand Blasting / Shot Blasting / Heat Treatment |
430 Stainless Steel Coil Packaging | Loose / Carrate / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps |
430 Stainless Steel Coil Shipment & Transportation | By Road – Truck / Train Partial Load, Full Load, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes |
430 Stainless Steel Coil Material Test Certificate | Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of Indian Standards BIS Approved ETC |
Manufacturer | POSCO, Aperam, Jindal Stainless, DKC Korea, Thyssenkrup, Baosteel, TISCO,Arcelor Mittal, VDM,Nippon Metal, Outokumpu,Qingshan,Delong. |
Shipping Port | Shanghai/Ningbo port/Tianjin/Qingdao |
Element | 430 |
Carbon | 0.12 |
Chromium | 16.0-18.0 |
Nickel | 0.75 |
Manganese | 1 |
Silicon | 1 |
Phosphorus | 0.04 |
Sulfur | 0.03 |
* Maximum, unless range is indicated |
Property | 430 |
Yield Strength, min. (ksi) | 30 |
Tensile Strength, min. (ksi) | 65 |
Elongation, min. (%) | 22 |
Hardness, max. (Rb) | 89 |
Property | 430 Data |
Density, lb/in3 | 0.276 |
Modulus of Elasticity, psi | 29.0 x 106 |
Coefficient of Thermal Expansion, 68-212˚F, /˚F | 5.7 x 10-6 |
Thermal Conductivity, Btu/ft hr ˚F | 13.8 |
Specific Heat, Btu/lb ˚F | 0.11 |
Electrical Resistivity, Microohm-in | 23.6 |
STANDARD | UNS | JIS | WERKSTOFF NR. | AFNOR | BS | GOST | EN |
SS 430 | S43000 | SUS 430 | 1.4016 | – | – | – | – |
• Tisco Stainless Steel 430 coil | • 430 Stainless Steel B. Q. Profile coil |
• SS 430 Perforated coil | • Best selling 4’x8′ mirror finished ss 430 coil |
• Stainless Steel 430 UNS S31635 coil | • Decorative hairline inox cold rolled ss 430 coil |
• A 240 Chequered 430 coil | • Hair Line Finish SS 430 coil |
• Aperam Stainless Steel 430 coil | • Laser cutting ss 430 coil |
• Stainless Steel 430 coil | • Tisco Supplier 3mm Thickness Stainless Steel 430 coil |
• A 240 430 coil | • Decorative Stainless Steel 430 coil |
• SS 430 Embossed coil | • Scotch Brite SS 430 coil |
• Outokumpu SS 430 coil | • Baosteel Stainless Steel 430 coil |
• SA 240 430 stainless steel coil | • Stainless Steel Cladding 430 coil |
• Bright Hammered Pattern Decorative SS 430 coil | • Black SS 430 coil 4mm Thick |
• Stainless Steel 430 coil | • Bright-pickled Stainless Steel 430 coil |
• SS DIN 1.4571 coil | • Cold rolled, heat treated 430 coil |
• ThyssenKrupp Stainless Steel 430 coil | • 3mm Cold Rolled AISI SS 430 coil |
• ASTM A240 Stainless Steel 430 coil | • Mill Supply SS 430 coil |
• Surface Polishing SS 430 coil | • Grade Prime SS 430 coil |
• 430 Stainless Steel HR coil | • Carpenter Custom 450 Stainless Steel 430 coil |
• 430 Stainless Steel Chequered coil | • Cut to Size Stainless Steel 430 coil |
• 430 Stainless Steel Golden Laser Pattern coil | • Non Magnetic Polishing Stainless Steel 430 coil |
• Super thin-Mirror surface BA ss 430 coil | • ASME SA240 430 coil |
• Super Austenitic SS 430 coil | • 430 Stainless Steel Blank coil |
• ASTM A240 430 coil | • 430 Stainless Steel Perforated coil |
• JMSS cold rolled ss 430 coil | • Embossed ss 430 coil |
• Cold Rolled No.1 Finish SS 430 coil | • Cheap cold rolled ss 430 coil with best price |
• SEW 400 Stainless Steel 430 coil | • Brush finish ss 430 coil price list |
• Hot Rolled Stainless Steel 430 coil | • SS URANUS B6 430 coil |
• Sales Promotion SS 430 coil | • 2B SUS SS 430 coil |
• Cr Stainless Steel 430 coil | • Food Grade Stainless Steel 430 coil |
• SS 430 Mill Test Certificate coil | • No. 4 PVC Coated SS 430 coil |
• ASTM A240 430 coil | • SS 430 coil Blasted Tin-Gold Rose |
• Cold rolled, bright annealed 430 coil | • 2mm ASTM SS 430 coil |
• Ground Stainless Steel 430 coil | • Stainless Steel Corrugated 430 coil |
• Hot Selling AISI SS 430 coil | • ASTM B625 430 coil |
• SS 430 Rose Golden coil | • Brushed or dull polished Stainless Steel 430 coil |
• Surface coated Stainless Steel 430 coil | • Cold rolled, heat treated, pickled 430 coil |
• Satin finish Stainless Steel 430 coil | • 10K Mirror Finish Surface SS 430 coil |
• AISI stainless steel 430 armor coil | • Gold Etched SS 430 coil |
• Satin finish Stainless Steel 430 coil | • 18 Gauge SS 430 coil |
• Mirror Finish SS 430 coil | • Patterned Stainless Steel 430 coil |
• SS 430 coil Gold Brush Finish | • #4 Finish Stainless Steel 430 coil |
• 430 Stainless Steel CR coil | • Patterned Stainless Steel 430 coil |
• 430 Stainless Steel 2B coil | • Passenger Elevator Cabin SS 430 coil |
Choose Daxun and make your customers satisfied.

Quick response
We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule. Daxun’s stainless steel materials are of reliable quality, and their varieties, specifications and delivery weights strictly comply with the standards.
Daxun Advantages
Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel achieves full traceability of each steel coil from the ERP system, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strict monitoring during sales, and provides worry-free service guarantees after sales.


Stainless steel coil packaging
Daxun Alloy ensures the best quality of packaging as it plays an important role in international freight where goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
• Boxes and crates
• Shrink wrap
• Wooden pallets
• Wooden boxes
Quality, delivery, inspection
- Daxun also performs a range of quality assurance tests, including flattening, pitting and resistance, mechanical, hardness, material identification, and expansion tests. These rigorous checks ensure that the material meets the necessary specifications for its intended application. For instance, 430 stainless steel, which lacks nickel, undergoes specific tests to assess its corrosion resistance and cost-effectiveness compared to 304 stainless steel, which contains about 8% nickel and offers enhanced durability and weldability.
- Throughout production, we carefully monitor the diameter, thickness, and surface quality of each product. Our standard delivery time ranges from 7 to 15 days. For custom or special-sized items, delivery may extend to 20 days. Rest assured, our delivery timelines are always adhered to as per the terms outlined in the contract.
- Support customer third-party agencies to go to the factory for inspection
- Support free samples to customers for testing
- Support on-site or video factory inspection


Ordering Information
When placing a purchase order, please include the quantity, grade, type or category, API5L references, thickness, width, length, and any relevant documentation or specific requirements—such as chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coatings, or end finishes. Reach out to Daxun today, and we’ll get back to you promptly with all the details you need.
Technical Support
If you require further technical support, our in-house metallurgist and expert team are always available to assist. Plus, Daxun is proud to offer a certified testing laboratory—the first of its kind in the multi-metal and plastic inventory sector. This commitment reflects our dedication to exceptional quality and underscores our approach as a comprehensive, full-service supplier.

SS 430 Stainless Steel Coil Features






Daxun Alloy Let your brand improve rapidly
- Gallery
- Product Series
- Main Equipment
Grade | Type | Thickness | Surface |
Austenitic | 304/304H/304L/304J1 | 0.25-150mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
321 | 0.4-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
316/316L/317L/316Ti | 0.3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
Ferrite | 430 | 0.4-3.0mm | 2B/BA/NO.4/8K/SB/HL |
Ultra Pure Ferrite | 443 | 0.4-2.0mm | 2B |
436L/439/444/441 | 0.5-3.0mm | 2B、2D | |
409L | 0.4-2.5mm | 2B、2D | |
Super Austenitic Steel | N08904 | 0.6-50mm | SWE / JPN / CHN |
S31254 | 0.5-50mm | SWE / JPN / CHN | |
N08926 | 0.5-50mm | SWE / JPN / CHN | |
N08367 | 0.5-50mm | SWE / JPN / CHN | |
Nickel Base Alloy | N08031 | 1.0-50mm | US / JPN / GER |
N08810/N08800 | 0.8-50mm | US / JPN / CHN | |
N08028 | 1.0-20mm | US / GER / JPN | |
N08020 | 1.0-20mm | US / GER / JPN | |
N08825 | 0.8-40mm | US / GER / SWE / JPN / CHN | |
N10276 | 0.5-50mm | US / GER / JPN | |
N06022 | 1.0-50mm | US / GER / JPN | |
N06625 | 0.8-20mm | US / GER / CHN | |
N04400 | 1.0-20mm | US / GER / JPN | |
N06600 | 1.0-50mm | US / GER / JPN / CHN | |
N02201 | 0.5-20mm | US / JPN | |
Titanium | TA1/Gr1 | 0.5-50mm | JPN / CHN |
TA2/Gr2 | 0.5-50mm | JPN / CHN | |
Welding Material | ERNiCrMo-13 | 1.2、2.4mm | GER |
ERNiCrMo-3 | 2.4mm | GER | |
ERNiCrMo-4 | 2.4mm | US |
Subsidiary | Main Equipments | Qty | Annual Capacity |
Daxun Stainless steel co.(JiangSu) | Slitting Machine | 1 | Decorative Sheet:60,000 tons |
Cutting Machine | 1 | ||
No.4 And Hairline Sheet To Sheet Polishing Machine | 1 | ||
No.4/Hairline Coil To Coil Polishing Machines | 1 | ||
8K/Super Mirror Sheet To Sheet Polishing Machines | 2 | ||
8K/Super Mirror Coil To Coil Polishing Machines | 3 | ||
PVD Color Coating Machines | 4 | ||
Liquid Chemical Coating Machines | 2 | ||
Anti Finger Printing Machines | 2 | ||
Auto Pick and Place machines | 16 | ||
Plate Washing Machine | 1 | ||
Daxun Stainless steel co.(Shanghai) | Cold Rolling Machine | 3 | 2B Coils:100,000 tons |
Annealing & Pickling Line | 2 | Decorative Sheet;30,000 tons | |
Slitting Machine | 1 | ||
Cut to Length Machine | 1 | ||
No.4/HL Polishing Machine(Sheet to Sheet) | 3 | ||
8K Polishing Machine(Sheet to Sheet) | 13 | ||
PVD Titanium Coating Machine | 4 | ||
Liquid Chemical Coating Machines | 1 | ||
Daxun Stainless steel co.(Shandong) | Cold Rolling Machine | 3 | 2B & BA Coil:220,000 tons |
Annealing & Pickling Line(2B & BA) | 2 | Decorative Sheet:60,000 tons | |
Tension Levering & Skin Pass | 1 | ||
Slitting Machine | 1 | ||
Cut to Length Machine | 1 | ||
No.4/HL Polishing Machine(Sheet to Sheet) | 1 | ||
8K Polishing Machine(Sheet to Sheet) | 11 | ||
Automatic Copper Coating Machine | 1 | ||
Digital Printing Machine | 1 | ||
PVD Titanium Coating Machine | 3 | ||
Liquid Chemical Coating Machines | 1 | ||
Anti-finger Machine | 1 | ||
Daxun Stainless steel co.(Sichuan) | Slitting Machine | 1 | 2B & BA Coil:180,000 tons |
Cutting Machine | 1 | Decorative Sheet:50,000 tons | |
No.4 And Hairline Sheet To Sheet Polishing Machine | 1 | ||
No.4/Hairline Coil To Coil Polishing Machines | 1 | ||
8K/Super Mirror Sheet To Sheet Polishing Machines | 1 | ||
8K/Super Mirror Coil To Coil Polishing Machines | 1 | ||
PVD Color Coating Machines | 1 | ||
Liquid Chemical Coating Machines | 1 | ||
Anti Finger Printing Machines | 1 |
SS 430 Surface Types of Stainless Steel Coils (6)
Information available for reference and download
Daxun is a trustworthy stainless steel coil manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel coils have fewer defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

Recent hot case projects and products
Related Products (10)
Leading stainless steel coil Suppliers in China
Daxun has been engaged in international business for more than ten years. In 2023, its export revenue exceeded US$100 million, and its export volume ranked among the top Chinese stainless steel manufacturers. Daxun continues to improve its service skills. In order to serve the global market, we have established three export service facilities in China and cooperated with engineering enterprises, steel mills and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relationships with dozens of well-known steel mills around the world. Its inventory includes 50,000 tons of conventional stainless steel coils and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of consistent quality. Types, specifications and delivery weights strictly comply with standards.
GENERAL PROPERTIES
- Grade 430 is a ferritic, straight chromium, non-hardenable grade that combines excellent corrosion resistance and formability with usable mechanical properties. Because of its resistance to nitric acid assault, it can be used in a variety of chemical applications, but automobile trim and appliance components are the most common.
- Grade 430F is the free-machining version of this grade, which comes in bar form for use in automatic screw machines. Grade 434 is the molybdenum-bearing counterpart of Grade 430, with the same useful set of characteristics. The molybdenum component increases corrosion resistance.
- ASTM A240/A240M specifies the characteristics of 430 for flat rolled products (plate, sheet, and coil). Other products, like as forgings and bar, have similar but not identical qualities, according to their specifications. The properties of Grade 430F are given for bar in ASTM A582.
Features of 430 stainless steel coils
430 stainless steel coil is the ferrite stainless steel which is used in a variety of applications due to its strength and ductility.
Features of 430 Stainless Steel Coils:
- High Strength
- Easy Formability
- Excellent Corrosion Resistance
- Good Weldability
- Resistance to Stress Corrosion Cracking (SCC)
APPLICATIONS:
Typical applications for 430 grade include:
- Linings for dish washers
- Refrigerator cabinet panels
- Automotive trim
- Lashing Wire
- Element Supports
- Stove trim rings
- Fasteners
- Chimney Liners
Typical applications for 430F grade include:
- Repetition machined components
SPECIFICATIONS:
- UNS: ASTM/ASTE S43000
- DIN:1.4016
CORROSION RESISTANCE:
- Grade 430 material exhibits good resistance to a wide range of corrosive environments such as nitric acid and some organic acids. Highest levels of corrosion resistance are achieved when highly polished or ground. Overall, its resistance to pitting and crevice corrosion is comparable to that of grade 304. Like all ferritic grades, 430 exhibits very high resistance to stress corrosion cracking.
- The non-free machining grade, 430F, exhibits significantly reduced resistance to pitting and crevice corrosion, as do the other high sulfur free machining grades.
HEAT RESISTANCE:
- Up to 870°C in intermittent service and 815°C in continuous service, grade 430 resists oxidation. This grade may require extended heating in the 400–600°C range before becoming brittle at room temperature. Annealing can be used to get rid of this effect.
HEAT TREATMENT:
- Solution Annealing – Heat to 815-845°C, hold for ½ hour per 25mm of thickness, slow furnace cool to 600°C and then quickly air cool. Slow cooling from 540-400°C will cause embrittlement.
- Sub-Critical anneal – Heat to 760-815°C and then air cool or water quench.
- This grade is not hardenable by thermal treatment.
WELDING:
- Pre-heat at 150-200°C if welding is necessary.
- Embrittlement in the weld metal and heat affected zone can be relieved by a post-weld anneal at 790-815°C
- Grain refinement will not occur.
MACHINING:
- Easier to machine than the standard austenitic grades such as 304.
- Still a tendency for galling and pick-up on the cutting tool.
- Bars that have been lightly drawn are easier to machine than those in the annealed condition.
- Grade 430F, the free machining version of 430, is very much easier to machine.
FABRICATION:
- Lower work hardening rate makes bending and forming somewhat easier than for grade 304
- Lower ductility restricts very severe operations.
- Severe bends should be made with the bend axis at right angles to the rolling direction.
- Severe cold heading of 430 wire is possible.
What are the commonly used surfaces of stainless steel coils?
The surface finish of 201 stainless steel coil might vary depending on the cold rolling processing methods used and the surface treatment used after rolling. Surface treatments for stainless steel coils include NO.1, 2B, 4, HL, 6, 8, BA, TR hard, heavy rolling bright 2H, polished bright, and other surface treatments:
- NO.1: The surface obtained after hot rolling, heat treatment and pickling of stainless steel strip. It is used to remove the black oxide scale formed by pickling or similar processes during hot rolling and heat treatment. It ranks first in surface treatment. The No. 1 surface is silvery white and matte. It is generally used in heat-resistant and corrosion-resistant industries that do not require high surface gloss, such as the alcohol industry, chemical industry, large containers, etc.
- 2B: Unlike the 2D surface, the 2B surface is smoothed by a light roller, and the surface is brighter. The surface roughness Ra value measured by the equipment ranges from 0.1 to 0.5μm, which is a typical value for most processing types. This stainless steel strip surface has the strongest adaptability and is suitable for industries such as chemical, papermaking, petroleum, medical, and a wide range of fields such as building curtain walls.
- TR hard surface: TR stainless steel is also called hard steel. Its characteristic steel grades include 304 and 301, which are used for items that require high strength and hardness, such as railway vehicles, conveyor belts, springs and washers. The idea is to use the work hardening characteristics of austenitic stainless steel to improve the strength and hardness of steel plates through cold working methods such as rolling. In order to replace the gentle flatness of the 2B base surface, the hard material is gently rolled by a few percent to tens of percent, and no annealing is performed after rolling. Therefore, the TR hard surface of the hard material is the rolled surface after the cold rolling process.
- Re-rolled bright 2H: After the rolling operation, the stainless steel strip will be bright annealed. A continuous annealing line can be used to quickly cool the strip. The stainless steel strip travels along the line at a speed of 60-80m/min. After this process, the surface finish will be 2H re-rolled bright.
- No. 4: The No. 4 surface has a good polishing effect and is brighter than No. 3. It can also be obtained by polishing the cold-rolled stainless steel plate with a 2D or 2B surface, and then polishing the processed surface with a sanding belt with a particle size of 150-180#. The tool measures the surface roughness (Ra) between 0.2 and 1.5μm. The No. 4 surface is widely used in restaurants and cooking equipment, medical equipment, architectural decoration, containers and other applications.
- HL: The HL surface is often called a hairline finish. The Japanese JIS standard specifies a continuous hairline abrasive surface obtained by polishing with a 150-240# abrasive belt. The restrictions under the Chinese GB3280 standard are unclear. HL surface finish is commonly used for architectural decoration, such as elevators, escalators, and exterior walls.
- No. 6: The No. 6 surface is further polished on the basis of No. 4 with a Tampico brush or a W63 grit abrasive material specified in the GB2477 standard. The surface has good metallic luster, softness, weak reflection, and no imaging. Due to its good performance, it is very suitable for curtain walls, tassel decoration, and cooking supplies.
- BA: BA is a surface that is brightly heat treated after cold rolling. Bright heat treatment is annealing in a protective atmosphere to ensure that the surface is not oxidized and retain the gloss of the cold-rolled surface, and then it is polished with a high-precision smooth roller to improve the surface brightness. The instrument evaluates the surface roughness to be 0.05-0.1μm, indicating that the surface is close to a mirror surface. BA surfaces can be used in a variety of applications, including food utensils, household appliances, medical equipment, automotive parts, and decorations.
- No. 8: Mirror surface, maximum reflectivity, no abrasive particles. The stainless steel deep processing industry also refers to 8K board. BA material is often used as raw material for mirror processing. It only needs to be polished. The surface is beautiful after mirror processing and is often used in building entrances and interior decoration.
What is the standard sea packaging stainless steel coil?
- Standard export sea packaging:
Waterproof Paper Winding+PVC Film+Strap Banding+Wooden Pallet or Wooden Case; - Customized packaging as your request (Logo or other contents accepted to be printed on the packaging);
- Other special packaging will be designed as customer’s request;
Eye to wall and eye to sky are both available; - By International Express: DHL/UPS/FEDEX/EMS and our own express line;
- By air, sea or land;
- Shipping Port: Shanghai, Ningbo, Qingdao, Tianjin or as your request.
Why choose Daxun’s stainless steel coils?
Reliable Stainless Steel Coils and Sheets Inventory Guarantee
- Have you ever been in a situation where you required a significant quantity of stainless steel coils right away, only to discover that the supplier was running low on stock? This condition may impair your workflow and plans.
- Our Advantages: With us, this situation will be a thing of the past. Our inventory is always ample, guaranteeing that even the largest orders are fulfilled quickly and in accordance with your business schedule.
Custom Stainless Steel Material Processing
- You may have experienced a circumstance in which bespoke processing is required, but locating the correct supplier to match your exact requirements might be difficult.
- Our Advantages: We have great processing capabilities to satisfy any of your specific needs. Whether it is size, stainless steel surface treatment, or other unique requirements, we offer expert one-stop service.
Competitive Stainless Steel Prices
- When looking for a stainless steel coil provider, price is typically a major factor. You may have to make a compromise with your chosen supplier due to excessive costs.
- Our Advantages: We keep pricing low by implementing excellent cost control and improved sourcing methods. This implies that by choosing us, you will not only receive high-quality products but also outstanding value for money.
Various Specifications of Stainless Steel Coils in Stock
- Finding stainless steel coils with exact specifications might be a challenge. It is critical to select a supplier who understands and serves these specific needs.
- Our Advantages: Our portfolio demonstrates versatility, with a wide choice of materials, thicknesses, and widths. We take pleasure in our ability to satisfy your project’s exact specifications.
Precision Stainless Steel Shearing Service.
- Precision shearing is required for the usage of stainless steel coils, but not all vendors offer this precise service.
- Our Advantages: Our shearing service is both professional and efficient, delivering precise cuts that fit your exact demands.
Contact your stainless steel coil suppliers
- You can easily order stainless steel coils in any size and quantity online.
Alternatively, our friendly sales team will be happy to take your order. Simply call +86 13382898899 or email Daxunhejin@gmail and we will get back to you as soon as possible.
Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email ([email protected]) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week
Samples can be provided free of charge, but the freight is borne by the customer, and will be refunded after cooperation.
We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.
Our MOQ is 1 ton for stainless steel sheet.
We have a complete organization from raw material purchasing to processing and shipment arranging. In the whole chain, the documentary people ad QC will look for and check it by precise requirements.The third party inspection is welcomed.
Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.