x
همین امروز استعلام خود را ارسال کنید
استعلام سریع
banner-p

لوله و تیوب فولادی ضد زنگ

  • Daxun is the world’s leading stainless steel pipe manufacturer
  • Large and small diameters, from straight to rolled tubes
  • Welded and drawn tubes, or seamless tubes and tubes.

لوله و تیوب فولادی ضد زنگ

Welded Tube

Stainless steel welded tube products made from strip are roll formed and fusion welded along a longitudinal seam. The welding processes employed by Daxun does not use any filler metals during the welding process.

Welded & Drawn Tubing

Tubular products are welded and then redrawn to a final size. Welded and drawn is ideal to produce heavy wall to diameter tubes that cannot be welded directly to size, but still enjoy the lower cost savings vs. seamless tubes. All Daxun welded and drawn tubes are bright annealed.

Seamless Tubing

Stainless steel seamless tubing products are drawn from tube hollows, which are made by piercing a billet or by a hot extrusion process. Seamless is ideal for very heavy diameter to wall ratios and offers very good outside dimensional tolerances.

Daxun is located in Wuxi, Jiangsu, China

Product Parameters:   Stainless Steel Pipe/Tube
OD 3mm~2000mm ضخامت 0.3mm~100mm
استاندارد ASTM A312 A249 A213 A269 A268 etc
DATA SeamlessTube weldedTube precisionTube polishTube picklingTube hairlineTube etc
shape Round square rectangle Hexagonal Special-shaped etc
نمره 304 304DQ 201 301 304L 304H 309S 310S 316L 316TI 317L 321 347 347H 430 410 410S 420 420J2 430 430LNT 430J1L 434 436L 439 441 443

444  904L 2205 2507 S32750 S32760 445J2 442etc

Daxun is a Chinese stainless steel tube manufacturer that produces precision seamless cylindrical shapes and components, including standard tube specifications and tight tolerances, thin-walled tubes, and stainless steel tubes in a variety of materials, including standard tube specifications and titanium alloy tubes, stainless steel tubes , high-strength steel pipes and nickel-based alloy pipes.

Backed by a global service and support network, our Daxun stainless steel seamless pipe and stainless steel welded pipe product lines set the standard for the large diameter, stainless steel pipe requirements of the power, petrochemical, nuclear, aerospace and defense industries.

بیشتر بخوانید

Brands and characteristics of various stainless steel pipes

Our unparalleled resources, technical expertise and highly skilled workforce produce consistently high quality stainless steel pipe

Stainless steel seamless square tube

Stainless steel square tubes are often used in the construction field and structural parts.

17 Products Found.

Commonly used grades

4 Products Found.

Manufacturing Methods

Each tube is manufactured to the strictest regulatory and internal specifications. Daxun’s proprietary forming, welding and finishing processes produce pipe and pipe with superior performance. Some of the stages of manufacturing are randomly listed below.

Main features of stainless steel pipes

Preservative

Excellent corrosion resistance in extreme environments

مقاومت بالا

Many types of stainless steel pipes have very high strengthMany types of stainless steel pipes have very high strength

غیرمغناطیسی

Suitable for situations where magnetic field interference is avoided

Temperature Resistant

The ability to withstand very high temperatures makes nickel alloys perfect for onshore, offshore and power generation applications.

Daxun stainless steel pipe manufacturing capabilities

Forming capabilities include state-of-the art extrusion and cold working assets for manufacturing tube and pipe products, one of the world’s largest pilger mills, and a unique hydroforming processes to manufacture fittings.

Daxun’s pipe processing capabilities

As a vertically integrated manufacturer, we offer a one-stop shop and we have the ability to handle anything, whether it’s an entire project or just a machining job.Straightening、Drilling、Honing、Trepanning、Cutting、Testing、Boring、Machining、Laser Weld、Polishing、Turning、Specialized Services.

Bigger, Better Pipe Solutions

With vertical and horizontal presses ranging from 12,000 tons to 35,000 tons, Daxun has the most comprehensive pipe extrusion capabilities in the world. Capabilities enable us to manufacture the longest lengths and largest diameter pipes in the industry.

Powerful Pipe Solutions

Daxun supplies the power generation market with ductwork, boiler tubes, main steam tubes, thermal reheat tubes, flue gas desulfurization units and other products for nuclear, coal-fired, renewable energy and combined cycle applications.

Technical Information

We supply pipe and tubing products to the defense industry, as well as a variety of mechanical and structural applications where tubing products are used. High alloy nickel casing and mechanical tube products are used in the world’s most technically demanding industries and applications, including sour environments, high pressures and temperatures.

Chemical processing products include pipe and tube for ethylene production, caustic soda production and heat exchanger tubes. We also make a variety of products for the medical and general industrial industries, including x-ray machines, thermocouple sheathing tubes for industrial furnaces, and boiler tubes.

Actual Weight & Good Quality

At Daxun, we have testing laboratory and equipment to ensure that our stainless steel materials are in actual weight and good quality before shipment. Our strict quality control team also performs strict and 100% inspection on all production stages.

Excellent After-Sales Services

Our support and services are not only limited from the beginning of our transactions. Even if you have received your orders, TuoLian will continue to provide excellent after-sales services. We will continue providing assistance and warranty to your orders.

Application cases of stainless steel pipes in different industries

5ff7292d-1af6-473d-b0d9-bfd49aed751f.jpg_560xaf
Coal chemical industry

Daxun Stainless has developed R&D and manufacturing technology for N08825 alloy pipes for high-pressure hydrogen applications. The product and various mechanical, physical and chemical properties have reached the international advanced level, meeting the requirements for the use of alloy seamless pipes for high-pressure hydrogen applications, and realizing high-pressure hydrogen applications. The engineering development of alloy seamless pipe products has formed independent intellectual property rights and industrialization capabilities. It meets the pipe requirements for petroleum hydrogenation units, and also meets the needs of special pipes for nuclear power, petrochemical, coal-to-liquids, chemical industry, aerospace and other major equipment and high-end equipment manufacturing.

dianzhanguolu
Power station boiler

In thermal power generation, the use of supercritical units and ultra-supercritical units has increased. The supercritical unit improves the thermal efficiency of the unit by increasing the pressure and temperature of the steam in the boiler. Its steam and water pipelines include reheater tubes, superheater tubes, water wall tubes, economizer tubes, air preheating tubes, heat transfer tubes, and downcomers. And various header pipes are exposed to high temperature and high pressure conditions for a long time, so the steel pipes are required to have high lasting strength, high resistance to oxidation and corrosion and good structural stability. Usually, the number of high-pressure boiler tubes such as Super304H and HR3C consumed per million kilowatts of super (super)critical units is about 1,250 tons.

hanyangogngxheng
marine pipeline

Daxun developed the manufacturing technology of large-diameter super duplex stainless steel seamless pipes, realized the transformation of scientific and technological achievements into high-tech products for marine engineering, and served as a demonstration for the industrialization of key equipment and systems in high-end ship and marine engineering manufacturing.

hedian
nuclear power

Daxun joined the ranks of qualified suppliers and developed the core technology of N08367 seamless and welded steel pipe manufacturing for third-generation nuclear power AP1000, achieving major industrialization goals. Reaching the international advanced and leading level, the implementation of the project will effectively promote the independence of the nuclear power industry, meet the development needs of domestic and foreign advanced nuclear power equipment manufacturing, and ensure the safe operation of nuclear power plants.

lng
گاز طبیعی مایع

Focusing on the performance requirements of welded pipes for LNG, Daxun broke through the key technologies of welding and heat treatment during product processing and manufacturing, and developed large-diameter stainless steel welded pipes for LNG with excellent corrosion resistance, low-temperature toughness and good low-temperature strength.

هوافضا

Can be used in fuselage parts, aerospace equipment, rockets, artificial satellites, missiles, spacecraft shells, pipeline systems, etc.

Petrochemical

Serving the petrochemical industry, it can be used in: reaction towers, heat exchangers, pressure shafts, distillation towers, valves, pumps, various pipeline systems, etc. When you choose Daxun as your stainless steel pipe supplier, you know we truly understand the oil and gas industry, contact Daxun today.

military armor

When you choose Daxun as your stainless steel pipe supplier, you know we truly understand the armor and automotive industries, contact Daxun today.

Ship field

Stainless steel pipes are used in the manufacture of ship piping systems, whip antennas, seawater pipes, condensers, heat exchangers, acoustic devices, fire piping, etc.

مهندسی دریایی

Deep-sea exploration equipment is one of the important directions in the field of marine engineering, and stainless steel pipes have become an ideal material for various deep-sea exploration equipment due to their corrosion resistance, high strength and other advantages. Deep-sea pipelines, detectors, sonar equipment, etc. can all be made of stainless steel pipes to ensure long-term reliable operation in harsh marine environments.

Pharmaceutical, biological

Serving the pharmaceutical and biopharmaceutical industries has been a welcome challenge for Daxun. From raw material selection to delivery, we have developed high purity and ultra-high purity services to meet and exceed industry standards. When only the best stainless steel tubing and stainless steel pipes can meet the demand, more and more pharmaceutical and biopharmaceutical companies trust Daxun.

Electric power field

Serving the power generation industry, Daxun is able to combine technical expertise and experience to produce the best pipe and pipe available today. When you choose the best, you get the best. Follow what countless other companies have done – trust Daxun. Highly demanding industries need Daxun

about-feature3
Let us be your trustworthy stainless steel pipe supplier

Customers from different industries trust Daxun for fast delivery of high-quality products. Seamless, welded and drawn tubing are produced at our factory in Wuxi, China. Strict production processes produce pipes that are homogeneous throughout their outer diameter and wall microstructure.

Technical Information

Diam (mm) Thickness(mm) Length (mm) Comment
φ3.0-12.0 0.3-1.0 6000 AAA
φ19.0-22.0 0.6-3.0 6000 AAA
φ25.0-27.2 0.8-10.0 6000 AAA
φ32.0-60.3 0.8-15.0 36000 AAA
φ76.3-102.1 0.8-205.0 36000 AAA
φ114.3-168.3 0.8-20.0 6000 AAA
φ180.0-219.2 3.0-20.0 6000 AAA
φ273.1-325.3 4.0-30.0 6000 AAA
φ377.2-426.3 5.0-30.0 6000 AAA
φ508.1-711.0 5.0-30.0 6000 AAA
711.0+

 

5.0-30.0

 

6000

 

AAA

 

If you need to know more about the size, please contact Daxun

ASTM A269
Group Size, Outside Diameter, in. Permissible Variations in Outside Diameter, in. (mm) Permissible Variations in Wall Thickness, % Permissible Variations in Cut Length, in. (mm) Thin Walled Tubes
Over Under
1 Up to ½ ±0.005(0.13) ±15 ⅛(3.2) 0
2 ½ to 1½, excl ±0.005(0.13) ±10 ⅛(3.2) 0 less than 0.065 in. (1.65 mm) nominal
3 1½ to 3½, excl ±0.010(0.25) ±10 3/16(4.8) 0 less than 0.095 in. (2.41 mm) nominal
4 3½ to 5½, excl ±0.015(0.38) ±10 3/16(4.8) 0 less than 0.150 in. (3.81 mm) nominal
5 5½ to 8, excl ±0.030(0.76) ±10 3/16(4.8) 0 less than 0.150 in. (3.81 mm) nominal
6 8 to 12, excl ±0.040(1.01) ±10 3/16(4.8) 0 less than 0.200 in. (5.08 mm) nominal
7 12 to 14, excl ±0.050(1.26) ±10 3/16(4.8) 0 less than 0.220 in. (5.59 mm) nominal
ASTM A554
OD Size, in. (mm) Wall Thickness OD, ±
in. mm in. mm
Under ½ (12.7) 0.020 to 0.049 0.51 to 1.24 0.004 0.1
½ to 1 (12.7 to 25.4) 0.020 to 0.065 0.51 to 1.65 0.005 0.13
½ to 1 (12.7 to 25.4) over 0.065 to 0.134 over 1.65 to 3.40 0.01 0.25
Over 1 to 1½ (25.4 to 38.1), incl 0.025 to 0.065 0.64 to 1.65 0.008 0.2
Over 1 to 1½ (25.4 to 38.1), incl over 0.065 to 0.134 over 1.65 to 3.40 0.01 0.25
Over 1½ to 2 (38.1 to 50.8), incl 0.025 to 0.049 0.64 to 1.24 0.01 0.25
Over 1½ to 2 (38.1 to 50.8), incl over 0.049 to 0.083 over 1.24 to 2.11 0.011 0.28
Over 1½ to 2 (38.1 to 50.8), incl over 0.083 to 0.149 over 2.11 to 3.78 0.012 0.3
Over 2 to 2½ (50.8 to 63.5), incl 0.032 to 0.065 0.81 to 1.65 0.012 0.3
Over 2 to 2½ (50.8 to 63.5), incl over 0.065 to 0.109 over 1.65 to 2.77 0.013 0.33
Over 2 to 2½ (50.8 to 63.5), incl over 0.109 to 0.165 over 2.77 to 4.19 0.014 0.36
Over 2½ to 3½ (63.5 to 88.9), incl 0.032 to 0.165 0.81 to 4.19 0.014 0.36
Over 2½ to 3½ (63.5 to 88.9), incl over 0.165 over 4.19 0.02 0.51
Over 3½ to 5 (88.9 to 127.0), incl 0.035 to 0.165 0.89 to 4.19 0.02 0.51
Over 3½ to 5 (88.9 to 127.0), incl over 0.165 over 4.19 0.025 0.64
Over 5 to 7½ (127.0 to 190.5), incl 0.049 to 0.250 1.24 to 6.35 0.025 0.64
Over 5 to 7½ (127.0 to 190.5), incl over 0.250 over 6.35 0.03 0.76
Over 7½ to 16 (190.5 to 406.4), incl all all 0.00125 in./in. or mm/mm of circumference
ASTM A312
NPS Designator Tolerance, % from Nominal
Over Under
⅛ to 2½ incl., all t/D ratios 20 12.5
3 to 18 incl., t/D up to 5% incl. 22.5 12.5
3 to 18 incl., t/D > 5% 15 12.5
20 and larger, welded, all t/D ratios 17.5 12.5
20 and larger, seamless, t/D up to 5% incl. 22.5 12.5
20 and larger, seamless, t/D > 5% 15 12.5
وضعیت تحویل
انتخاب ایالت تحویل وضعیت سطح
نورد گرم Silver Bright
Polished (320#, 400#, 600#, Mirror finish)
نورد سرد Silver Bright
Polished (320#, 400#, 600#, Mirror finish)
توجه:
۱. در صورتی که به وضعیت تحویل متفاوتی از موارد فوق نیاز دارید، لطفاً با ما هماهنگ فرمایید.
۲. در صورت هرگونه پرسش یا سفارش، لطفاً ما را از هرگونه نیاز اضافی که در اینجا ذکر نشده است، مطلع سازید.

  • “Thank you Daxun for providing extremely durable, world-class quality stainless steel pipe. I also appreciate the professional customization service. I am happy to work with you for my stainless steel pipe needs. Looking forward to working with you next time!”

    Testimonials from customers located in the Middle East
  • “Daxun has always been a trustworthy company when it comes to stainless steel pipes. All the stainless steel pipes I purchased are of very high quality. I ordered stainless steel pipes at a very low price at Daxun. The staff was also happy to answer my questions .” Asked questions and was impressed with my needs! “

    Testimonials from customers located in Europe and the United States
  • “We are very impressed with the quality and superiority of Daxun stainless steel pipes. They are available in a variety of sizes and are perfect for our needs. Additionally, we are very grateful for their affordable prices and service.”

    Testimonials from customers located in Russia

داکسون آلیاژ

Regarding stainless steel pipes, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.

Do you have any stock in stock?

Yes, we have complete specifications and inventory and can quickly meet your needs.

Can it be customized?

Yes, it can be customized. You can contact us and send us the customized specifications and quantity.

How do you ship the goods?

Our transportation methods generally include sea transportation, land transportation, and sea transportation. Reach you quickly and safely.

What's your price like?

Because our output is high, the cost will be much lower, so the price is low.

کیفیت شما چگونه است؟

We attach great importance to product quality and have passed various quality system tests.

همین امروز استعلام خود را ارسال کنید
استعلام سریع