Discover a wide range of premium products designed to meet your needs. Browse through our carefully curated collection, offering quality, innovation, and reliability. Whether you’re looking for the perfect gift or upgrading your essentials, you’ll find exactly what you’re looking for here.
Check out Stainless Steel Product
Check out Titanium Product
Stainless Steel Product List
| United States | چین | جیآیاس | ISO Number | نماد | European | |
|---|---|---|---|---|---|---|
| بدون سرویس | (AISI) | GB | انگلیسی | |||
| S20100 | 201 | S35350 | SUS201 | 4372-201-00-I | X12CrMnNiN17-7-5 | 1.4372 |
| S20200 | 202 | S35450 | SUS202 | 4373-202-00-I | X12CrMnNiN18-9-5 | 1.4373 |
| S30100 | 301 | S30110 | SUS301 | 4319-301-00-I | X5CrNi17-7 | 1.4319 |
| S30153 | * | S30153 | SUS301L | 4318-301-53-I | X2CrNiN18-7 | 1.4318 |
| * | * | * | SUS301J1 | – | – | * |
| S30200 | 302 | S30120 | SUS302 | 4325-302-00-E | X9CrNi18-9 | 1.4325 |
| S30215 | 302B | S30240 | SUS302B | 4326-302-15-I | X12CrNiSi18-9-3 | * |
| S30300 | 303 | S30317 | SUS303 | 4305-303-00-I | X10CrNiS18-9 | 1.4305 |
| S30323 | 303Se | S30327 | SUS303Se | 4625-303-23-X | X12CrNiSe18-9 | * |
| – | * | – | SUS303Cu | 4667-303-76-J | X12CrNiCuS18-9-3 | * |
| S30400 | 304 | S30408 | SUS304 | 4301-304-00-I | X5CrNi18-10 | 1.4301 |
| – | * | S30488 | SUS304Cu | 4649-304-76-J | X6CrNiCu19-9-1 | * |
| اس۳۰۴۰۳ | ۳۰۴ال | اس۳۰۴۰۳ | SUS304L | 4307-304-03-I | X2CrNi18-9 | 1.4307 |
| اس۳۰۴۰۳ | ۳۰۴ال | اس۳۰۴۰۳ | 4306-304-03-I | X2CrNi19-11 | 1.4306 | |
| – | * | اس۳۰۴۰۳ | 4650-304-75-E | X2CrNiCu19-10 | 1.465 | |
| S30451 | 304N | S30458 | SUS304N1 | 4315-304-51-I | X5CrNiN19-9 | 1.4315 |
| S30452 | * | * | SUS304N2 | – | – | * |
| S30453 | ۳۰۴ الان | S30453 | SUS304LN | 4311-304-53-I | X2CrNiN18-9 | 1.4311 |
| – | * | S30480 | SUS304J1 | 4567-304-76-I | X6CrNiCu17-8-2 | 1.4567 |
| – | * | – | SUS304J2 | 4617-201-76-J | X6CrNiMnCu17-8-4-2 | * |
| S30431 | * | S30480 | SUS304J3 | 4567-304-98-X | X6CrNiCu18-9-2 | 1.4567 |
| S30500 | 305 | S30510 | SUS305 | 4303-305-00-I | X6CrNi18-12 | 1.4303 |
| * | * | * | SUS305J1 | – | – | * |
| S30908 | ۳۰۹ اس | S30908 | SUS309S | 4950-309-08-E | X6CrNi23-13 | 1.495 |
| S31008 | ۳۱۰اس | S31008 | SUS310S | 4951-310-08-I | X6CrNi25-20 | 1.4951 |
| S31008 | ۳۱۰اس | S31008 | 4845-310-08-E | X8CrNi25-21 | 1.4845 | |
| اساس ۳۱۲۵۴ | * | S31252 | SUS312L | 4547-312-54-I | X1CrNiMoCuN20-18-7 | 1.4547 |
| – | * | – | SUS315J1 | 4660-315-77-I | X6CrNiCuSiMo19-10-3-2 | * |
| – | * | – | SUS315J2 | 4648-315-77-I | X6CrNiSiCuMo19-13-3-3-1 | * |
| اس۳۱۶۰۰ | 316 | S31608 | SUS316 | 4401-316-00-I | X5CrNiMo17-12-2 | 1.4401 |
| اس۳۱۶۰۰ | 316 | S31608 | 4436-316-00-I | X3CrNiMo17-12-3 | 1.4436 | |
| – | * | – | SUS316F | 4494-316-74-J | X6CrNiMoS17-12-3 | * |
| S31603 | ۳۱۶ ال | S31603 | SUS316L | 4404-316-03-I | X2CrNiMo17-12-2 | 1.4404 |
| S31603 | ۳۱۶ ال | S31603 | 4432-316-03-I | X2CrNiMo17-12-3 | 1.4432 | |
| S31603 | ۳۱۶ ال | S31603 | 4436-316-91-I | X2CrNiMo18-14-3 | 1.4435 | |
| S31651 | 316N | S31658 | SUS316N | 4495-316-51-J | X6CrNiMoN17-12-3 | * |
| S31653 | 316LN | S31653 | SUS316LN | 4406-316-53-I | X2CrNiMoN17-11-2 | 1.4406 |
| S31653 | 316LN | S31653 | 4429-316-53-I | X2CrNiMoN17-12-3 | 1.4429 | |
| S31635 | * | S31668 | SUS316Ti | 4571-316-35-I | X6CrNiMoTi17-12-2 | 1.4571 |
| – | * | – | SUS316J1 | 4465-316-76-J | X6CrNiMoCu18-12-2-2 | * |
| – | * | S31683 | SUS316J1L | 4647-316-75-X | X2CrNiMoCu18-14-2-2 | * |
| S31700 | 317 | S31708 | SUS317 | 4445-317-00-U | X6CrNiMo19-13-4 | * |
| S31703 | 317L | S31703 | SUS317L | 4438-317-03-I | X2CrNiMo19-14-4 | 1.4438 |
| S31753 | * | S31753 | SUS317LN | 4434-317-53-I | X2CrNiMoN18-12-4 | 1.4434 |
| – | * | S31794 | SUS317J1 | 4476-317-92-X | X3CrNiMo18-16-5 | * |
| – | * | – | SUS317J2 | 4496-309-51-J | X4CrNiMoN25-14-1 | * |
| N08367, | * | – | SUS836L | 4478-083-67-U | X2NiCrMoN25-21-7 | * |
| S32053 | ||||||
| N08904 | * | S39042 | SUS890L | 4539-089-04-I | X1NiCrMoCu25-20-5 | 1.4539 |
| اس۳۲۱۰۰ | 321 | S32168 | SUS321 | 4541-321-00-I | X6CrNiTi18-10 | 1.4541 |
| اس۳۲۱۰۹ | * | * | X7CrNiTi18-10 | 1.4541 | ||
| S34700 | 347 | S34778 | SUS347 | 4550-347-00-I | X6CrNiNb18-10 | 1.455 |
| S34709 | * | * | X7CrNiNb18-10 | 1.4912 | ||
| S38400 | 384 | S38408 | SUS384 | 4389-384-00-I | X3NiCr18-16 | * |
| S30430 | S30430 | S30488 | SUSXM7 | 4567-304-30-I | X3CrNiCu18-9-4 | 1.4567 |
| S30500 | * | S38148 | SUSXM15J1 | 4884-305-00-X | X6CrNiSi18-13-4 | * |
| S82122 | * | * | SUS821L1 | * | * | – |
| S32304 | * | S23043 | SUS323L | 4362-323-04-1 | X2CrNiN23-4 | 1.4362 |
| S32900 | 329 | – | SUS329J1 | 4480-329-00-U | X6CrNiMo26-4-2 | * |
| S32205, | * | S22053 | SUS329J3L | 4462-318-03-I | ایکس۲کرنیامونایپی۲۲-۵-۳ | 1.4462 |
| S31803 | ||||||
| S31260, | * | S22583 | SUS329J4L | 4481-312-60-J | X2CrNiMoN25-7-3 | * |
| S32506 | ||||||
| اس۳۲۷۵۰ | * | S25073 | SUS327L | 4410-327-50-E | ایکس۲کرنیامونایاِیان۲۵-۷-۴ | 1.441 |
| S40500 | 405 | S11348 | SUS405 | 4002-405-00-I | X6CrAl13 | 1.4002 |
| – | * | S11203 | SUS410L | 4030-410-90-X | X2Cr12 | * |
| S42900 | 429 | S11510 | SUS429 | 4012-429-00-X | X10Cr15 | * |
| S43000 | 430 | S11710 | SUS430 | 4016-430-00-I | X6Cr17 | 1.4016 |
| S43020 | 430F | S11717 | SUS430F | 4004-430-20-I | X7CrS17 | * |
| – | * | – | SUS430LX | 4520-430-70-I | X2CrTi17 | 1.452 |
| S43940 | * | S11873 | 4509-439-40-X | X2CrTiNb18 | 1.4509 | |
| S43035 | 439 | S11863 | 4510-430-35-I | X3CrTi17 | 1.451 | |
| – | * | – | 4511-430-71-I | X3CrNb17 | 1.4511 | |
| – | * | – | SUS430J1L | 4664-430-75-J | X2CrCuTi18 | * |
| S43400 | 434 | S11790 | SUS434 | 4113-434-00-I | X6CrMo17-1 | 1.4113 |
| S43600 | 436 | S11862 | SUS436L | 4513-436-00-J | X2CrMoNbTi18-1 | * |
| – | * | – | SUS436J1L | 4609-436-77-J | X2CrMo19 | * |
| – | * | * | SUS443J1 | – | – | – |
| S44400 | 444 | S11972 | SUS444 | 4521-444-00-I | X2CrMoTi18-2 | 1.4521 |
| * | * | * | SUS445J1 | – | – | * |
| * | * | * | SUS445J2 | – | – | * |
| S44700 | * | S13091 | SUS447J1 | 4135-447-92-C | X1CrMo30-2 | * |
| S44627 | * | S12791 | SUSXM27 | 4131-446-92-C | X1CrMo26-1 | * |
| S40300 | 403 | * | SUS403 | – | – | * |
| S41000 | 410 | S41010 | SUS410 | 4006-410-00-I | X12Cr13 | 1.4006 |
| – | * | – | 4024-410-09-E | X15Cr13 | 1.4024 | |
| S41008 | * | S41008 | SUS410S | 4000-410-08-I | X6Cr13 | 1.4 |
| – | * | – | SUS410F2 | 4642-416-72-J | X13CrPb13 | * |
| – | * | S45710 | SUS410J1 | 4119-410-92-C | X13CrMo13 | * |
| S41600 | 416 | S41617 | SUS416 | 4005-416-00-I | X12CrS13 | 1.4005 |
| S42000 | 420 | S42020 | SUS420J1 | 4021-420-00-I | X20Cr13 | 1.4021 |
| S42000 | 420 | S42030 | SUS420J2 | 4028-420-00-I | X30Cr13 | 14,028 |
| S42020 | 420F | S42037 | SUS420F | 4029-420-20-I | X33CrS13 | 1.4029 |
| – | * | – | SUS420F2 | 4643-420-72-J | X33CrPb13 | * |
| S43100 | 431 | S43120 | SUS431 | 4057-431-00-X | X17CrNi16-2 | 1.4057 |
| S44002 | 440A | S44070 | SUS440A | 4040-440-02-X | X68Cr17 | * |
| S44003 | 440B | S44080 | SUS440B | 4041-440-03-X | X85Cr17 | * |
| S44004 | 440C | S44096 | SUS440C | 4023-440-04-I | X110Cr17 | * |
| – | * | S44097 | SUS440F | 4025-440-74-X | X110CrS17 | * |
| S17400 | 630 | S51740 | SUS630 | 4542-174-00-I | X5CrNiCuNb16-4 | 1.4542 |
| S17700 | 631 | S51700 | SUS631 | 4568-177-00-I | X7CrNiAl17-7 | 1.4568 |
| * | * | * | SUS631J1 | – | – | * |
| * | * | * | SUS632J1 | – | – | * |
Titanium Product List
| نمره | شماره UNS | Composition/Description |
|---|---|---|
| پایهٔ اول | UNS R50250 | Unalloyed titanium |
| دوم | UNS R50400 | Unalloyed titanium |
| Grade 2H | UNS R50400 | Unalloyed titanium (Grade 2 with 58 ksi (400 MPa) minimum UTS) |
| پایه سوم | UNS R50550 | Unalloyed titanium |
| پایه چهارم | UNS R50700 | Unalloyed titanium |
| Grade 5 | UNS R56400 | Titanium alloy (6% aluminum, 4% vanadium) |
| Grade 6 | UNS R54520 | Titanium alloy (5% aluminum, 2.5% tin) |
| پایه هفتم | UNS R52400 | Unalloyed titanium plus 0.12 to 0.25% palladium |
| Grade 7H | UNS R52400 | Unalloyed titanium plus 0.12 to 0.25% palladium (Grade 7 with 58 ksi (400 MPa) minimum UTS) |
| Grade 9 | UNS R56320 | Titanium alloy (3.0% aluminum, 2.5% vanadium) |
| Grade 11 | UNS R52250 | Unalloyed titanium plus 0.12 to 0.25% palladium |
| Grade 12 | UNS R53400 | Titanium alloy (0.3% molybdenum, 0.8% nickel) |
| Grade 13 | UNS R53413 | Titanium alloy (0.5% nickel, 0.05% ruthenium) |
| Grade 14 | UNS R53414 | Titanium alloy (0.5% nickel, 0.05% ruthenium) |
| Grade 15 | UNS R53415 | Titanium alloy (0.5% nickel, 0.05% ruthenium) |
| Grade 16 | UNS R52402 | Unalloyed titanium plus 0.04 to 0.08% palladium |
| Grade 16H | UNS R52402 | Unalloyed titanium plus 0.04 to 0.08% palladium (Grade 16 with 58 ksi (400 MPa) minimum UTS) |
| Grade 17 | UNS R52252 | Unalloyed titanium plus 0.04 to 0.08% palladium |
| Grade 18 | UNS R56322 | Titanium alloy (3% aluminum, 2.5% vanadium) plus 0.04 to 0.08% palladium |