x
همین امروز استعلام خود را ارسال کنید
استعلام سریع

Grade 12 Ti-0.3Mo-0.8Ni Alloy Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:Grade 12 UNS R53400
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of grade 12 titanium is approximately 4.51 g/cm3
  • Standards:ASTM B338、ASTM B861
  • Softest Ti,High ductility, Very corrosion resistant, good cold formability

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

Grade 12 Titanium Alloy Pipe Manufacturer - Daxun Alloy

Provide High Quality Grade 12 Titanium Pipe to Customers Around The World
Grade 12 titanium pipe is a specialized tubing made from Ti-0.3Mo-0.8Ni titanium alloy, which belongs to a specific grade in the titanium alloy pipe family. This material is created by adding 0.3% molybdenum and 0.8% nickel to pure titanium, significantly enhancing its corrosion resistance, particularly in acidic environments and chloride media. Grade 12 titanium pipe complies with international standards such as ASTM B338 or ASTM B861, featuring a density of approximately 4.51 g/cm³, tensile strength of about 483 MPa, and yield strength of around 345 MPa, while maintaining the lightweight characteristics typical of titanium materials.

Where is Grade 12 titanium pipe used?
Compared to pure titanium, Grade 12 titanium pipe offers superior resistance to crevice corrosion and stress corrosion cracking, making it particularly suitable for chemical processing equipment, heat exchangers, oil and gas industries, and seawater treatment systems. This material provides longer service life and lower maintenance costs while maintaining excellent mechanical properties, making it highly favored in high-end industrial applications and an ideal choice for handling corrosive fluids.
Chemical processing plants utilize it for heat exchangers, reactor vessels, and piping systems handling aggressive acids and chlorides. Marine and offshore installations employ it in seawater cooling systems, desalination equipment, and subsea components, leveraging its exceptional resistance to saltwater corrosion and biofouling. In the oil and gas sector, it serves in downhole tubing, Christmas tree components, and production equipment exposed to sour environments with H₂S and CO₂. Power generation facilities specify Grade 12 titanium for condenser tubes and heat exchangers in cooling systems, while industrial pollution control systems incorporate it in scrubbers and flue gas desulfurization units that handle corrosive gases and acidic condensates.

Key Performance

Strength-Ductility Balance:

  • Tensile Strength: 483 MPa (annealed state) – Matches Grade 2 but with superior corrosion resistance.
  • Yield Strength: 345 MPa (min) – Exceeds Grade 2 (275 MPa), suitable for pressure-containing components.
  • Elongation: 18% (min) – Exceptional ductility for cold forming, flaring, and high fatigue resistance.
  • Density: 4.51 g/cm³ – 60% lighter than steel, ideal for weight-sensitive applications.

Corrosion Resistance:

  • Core Mechanism: Synergistic effect of Molybdenum (0.3%) and Nickel (0.8%) stabilizes the passive oxide layer.
  • Pitting/Crevice Corrosion Resistance:
    • Outstanding performance in seawater, chloride solutions (e.g., NaCl, MgCl₂), and sour gas (H₂S) environments.
    • Resists reducing acids (e.g., H₂SO₄, HCl) where stainless steels fail.
  • Advantages vs. Other Grades:
    • Outperforms Grade 2 in reducing acids and chlorides.
    • Superior to Grade 9 in high-temperature acidic media (e.g., chemical processing).
    • Immune to corrosion in oxidizing media (e.g., HNO₃) and aggressive chemical environments.
  • Optimal Heat Treatment: Annealed at 595°C to maximize corrosion resistance and ductility.
بیشتر بخوانید

داده‌ها

عنصر Minimum (%) Maximum (%)
Titanium (Ti) تعادل تعادل
مولیبدن (Mo) 0.25 0.40
نیکل (Ni) 0.60 0.90
آهن (Fe) 0.30
Oxygen (O) 0.25
Carbon © 0.08
نیتروژن (N) 0.03
Hydrogen (H) 0.015
عناصر دیگر 0.40 (total)
مالکیت Value/Range Unit
تراکم 4.48 g/cm³
نقطه ذوب 1650 ± 20 °C
هدایت حرارتی 7.2 (at 25°C) W/m·K
Specific Heat 560 (at 25°C) J/kg·K
مقاومت الکتریکی 1.7 μΩ·m
پذیری مغناطیسی Paramagnetic
مالکیت Minimum Requirement Typical Value Unit Test Method
مقاومت کششی 483 520–620 مگاپاسکال ASTM E8/E8M
Yield Strength (0.2% offset) 345 380–480 مگاپاسکال ASTM E8/E8M
Elongation 18 22–30 % ASTM E8/E8M
Hardness ≤ 200 (HV) 150–180 (HV) Vickers ASTM E10
Impact Toughness Not specified 40–60 J ASTM E23

Elevated Temperature Performance

Temperature (°C) مقاومت کششی (مگاپاسکال) Yield Strength (MPa) افزایش طول (%)
100 450–500 320–370 20–25
200 400–450 280–330 18–23
300 350–400 240–290 15–20

 

داکسون را انتخاب کنید تا به پروژه‌تان کمک کند اوج بگیرد.

همین حالا با داکسون تماس بگیرید

Advanced Production:Titanium seamless pipe

  • Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.
  • (The above is agreed upon by the manufacturer and the customer based on the specific situation)
همین حالا با داکسون تماس بگیرید

Grade 12 Titanium Tube Features

Grade 12 Titanium Tube is the softest form of titanium and has the highest ductility. It has good cold forming characteristics and offers excellent corrosion resistance. It also has excellent welding properties and high impact toughness.

  • Softest Titanium
  • Highest Ductility
  • Excellent Corrosion Resistance
  • Good Cold Formability
همین حالا با داکسون تماس بگیرید

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

همین حالا با داکسون تماس بگیرید

گزارش‌های آزمون

The test reports we provide include: Factory test certificate for Grade 12 titanium welded pipe and Grade 12 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

همین حالا با داکسون تماس بگیرید

Applications and standards

Titanium Grade 12 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
همین حالا با داکسون تماس بگیرید

کیفیت، تحویل، بازرسی

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 12 Titanium Welded Pipe and Grade 12 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • زمان تحویل ما دقیقاً مطابق قرارداد است.
  • از آژانس‌های ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
  • از نمونه‌های رایگان برای آزمایش مشتری پشتیبانی کنید.
  • حمایت از بازرسی کارخانه‌ای حضوری یا ویدیویی
همین حالا با داکسون تماس بگیرید

بسته‌بندی

داکسون آلیاژ بهترین کیفیت بسته‌بندی را تضمین می‌کند، زیرا بسته‌بندی نقش مهمی در حمل‌ونقل بین‌المللی دارد که کالاها از مسیرهای مختلف عبور می‌کنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژه‌ای به بسته‌بندی داریم. ما کالاهای خود را بسته به محصول به روش‌های مختلف بسته‌بندی می‌کنیم. روش‌های بسته‌بندی محصولات ما عبارتند از:
• جعبه‌ها و صندوق‌ها
• سلفون منقبض‌شونده
• پالت‌های چوبی
• جعبه‌های چوبی

همین حالا با داکسون تماس بگیرید

پشتیبانی فنی

اگر به هرگونه پشتیبانی فنی اضافی نیاز دارید، متالورژیست مقیم ما و کارکنان آگاه ما با کمال میل آماده کمک‌رسانی هستند. علاوه بر این، داکسون دارای آزمایشگاه آزمون معتبر است—نخستین در صنعت موجودی چندفلزی و پلاستیکی. به نظر ما، این امر تعهد تزلزل‌ناپذیر ما به کیفیت و فلسفه ما به‌عنوان یک تأمین‌کننده تمام‌خدمت را نشان می‌دهد.

Daxun Grade 12 Titanium TUBE Let your brand improve rapidly

Grade 12 titanium tube form (4)

پروژه‌ها و محصولات داغ اخیر

Grade 12 Titanium pipe and tube
Grade 12 Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
کدام گرید تیتانیوم بهترین است؟

رتبه آلیاژ تیتانیومی که نیاز دارید به پروژه‌ای که روی آن کار می‌کنید بستگی دارد، زیرا هر رتبه مزایای متفاوتی دارد.

تمام گریدهای آلیاژ تیتانیوم فوق‌العاده قوی و مقاوم در برابر خوردگی هستند، به این معنی که در سخت‌ترین شرایط نیز به خوبی کار خواهند کرد.

درجهٔ بالاتر آلیاژ تیتانیوم (۵–۱۲) آلیاژهایی هستند که برای مزایای خاص طراحی شده‌اند. برای مثال، آلیاژ تیتانیوم درجهٔ ۱۲ مقاومت حرارتی عالی دارد و آن را به گزینه‌ای ایده‌آل برای مبدل‌های حرارتی پوسته و لوله‌ای، لوله‌کشی هیدرولیک و تجهیزات صنعت شیمی تبدیل می‌کند.

درجه‌های ۱ تا ۴ آلیاژهای تیتانیوم خالص هستند و اگر به ماده‌ای جوش‌پذیر و چکش‌خوار برای سیستم‌های لوله‌کشی و تیوب‌ها نیاز داشته باشید، انتخابی ایده‌آل‌اند. درجه‌های پایین‌تر را در صنایع دریایی و صنعتی خواهید یافت.

اگر در حال شروع یک پروژه هستید و مطمئن نیستید کدام گرید آلیاژ تیتانیوم برای شما مناسب‌تر است، همین امروز با ما تماس بگیرید؛ ما با کمال میل به شما کمک خواهیم کرد.

کلاس‌های بالاتر تیتانیوم چه تفاوتی با کلاس‌های پایین‌تر دارند؟

در داکسون، ما طیف گسترده‌ای از گریدهای آلیاژ تیتانیوم از گرید ۱ تا گرید ۱۲ را ارائه می‌دهیم.

گریدهای ۱ تا ۴ تیتانیوم خالص هستند، در حالی که گریدهای بالاتر آلیاژ هستند.

کلاس‌های آلیاژ به‌خاطر نسبت بالای استحکام به وزن‌شان محبوب هستند.

رایج‌ترین گرید آلیاژ تیتانیومی که می‌یابیم، گرید ۵ است. اگرچه همچنان غنی از تیتانیوم است، این گرید یکی از قابل‌اعتمادترین‌هاست زیرا می‌تواند دماهای تا ۶۰۰ درجه فارنهایت را تحمل کند و در شرایط شدید دوام بیاورد.

در صنایعی مانند صنایع هوافضا و دریایی، به دلیل مقاومت در برابر سایش و خوردگی، گریدهای بالاتر ترجیح داده می‌شوند.

برعکس، گریدهای پایین‌تر عمدتاً به دلیل استحکام کمتر برای جوشکاری استفاده می‌شوند.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

آیا درجه تیتانیوم بر هزینه تأثیر دارد؟

اگرچه درجه تیتانیوم کمی هزینه را افزایش می‌دهد، اما هزینه کل عمدتاً به شکل و فرم تیتانیومی که نیاز دارید بستگی دارد.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

متأسفانه بدون اطلاع کافی از پروژه شما و کاربرد تیتانیوم، تعیین قیمت به‌صورت آنلاین دشوار است.

خوشبختانه تیم کارشناسان ما همیشه در خدمت شماست تا در زمینه نیازهای تیتانیومی‌تان به شما کمک و مشاوره دهد. با ارسال ایمیل به [email protected]، ما قادر خواهیم بود با ارائه مشاوره و برآورد دقیق هزینه به شما پاسخ دهیم.

حتماً تا حد امکان اطلاعاتی دربارهٔ گرید، شکل و مقدار تیتانیومی که نیاز دارید ارائه دهید تا نیازهایتان بهتر درک شود.

از کجا می‌توانم دربارهٔ گریدهای تیتانیوم بیشتر بیاموزم؟

تیم DAXUN باتجربه، آگاه و خوش‌برخورد است. با سال‌ها تجربه در این صنعت، آن‌ها همه چیز را درباره تیتانیوم، از کاربردها و مزایا گرفته تا گریدهای مختلف آن، می‌دانند.

برای دریافت به‌روزرسانی‌های منظم درباره تیتانیوم، کاربردها و مصارف آن در صنایع مختلف، حتماً وبلاگ ما را بررسی کنید. کارشناسان ما راهنماهای ساده‌ای نوشته‌اند که همیشه می‌توانید هنگام پرسش به آن‌ها مراجعه کنید.

اگر همچنان با مشکل مواجه هستید، با ما تماس بگیرید؛ خوشحال می‌شویم به شما کمک کنیم.

با ارسال ایمیل به [email protected]، پاسخ سریعی دریافت خواهید کرد. لطفاً در سؤال خود تا حد امکان جزئیات بیشتری درج کنید تا بتوانیم راه‌حل مناسبی پیشنهاد دهیم.

چگونه سریعاً یک برآورد قیمت دریافت کنیم یا اطلاعات بازار را بفهمیم؟

لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتس‌اپ ما آنلاین است و ایمیل ([email protected]) ظرف ۶ ساعت بررسی می‌شود. به هر پرسش یا پیام به‌سرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک می‌گذاریم.

می‌توانم چند نمونه بگیرم؟

ما می‌توانیم نمونه‌های ورق فولاد ضدزنگ را برای بررسی کیفیت در اختیار شما قرار دهیم. نمونه رایگان است و شما فقط هزینه حمل را پرداخت می‌کنید.

تا کنون به کدام کشورها صادرات داشته‌اید؟

ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشته‌ایم.

حداقل مقدار سفارش شما چیست؟

حداقل سفارش ما برای ورق فولاد ضد زنگ ۱ تن است.

زمان تحویل شما چقدر است؟

سفارش‌های آزمایشی را می‌توان ظرف یک هفته تحویل داد. برای سفارش‌های معمولی تقریباً دو هفته زمان لازم است.

همین امروز استعلام خود را ارسال کنید
استعلام سریع