x
همین امروز استعلام خود را ارسال کنید
استعلام سریع

CP Grade 4 Titanium Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:UNS R50700
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Standards:ASTM B338
  • Softest Ti,High ductility, Very corrosion resistant, good cold formability

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

CP Grade 4 Titanium Pipe Manufacturer

Grade 4 titanium pipe is recognized as the strongest among commercially pure titanium grades, delivering exceptional mechanical performance combined with superior corrosion resistance. Its high tensile strength and excellent ductility allow it to endure demanding operational environments, making it an ideal solution for industries where reliability and durability are critical. Unlike lower grades, Grade 4 titanium pipe provides a higher strength-to-weight ratio without sacrificing formability, ensuring versatility in both fabrication and end-use applications.

The advantages of grade 4 titanium pipe

In industrial settings, Grade 4 titanium pipe is widely used in chemical processing, marine engineering, and aerospace sectors due to its outstanding resistance to aggressive media, including chlorides and acids. Its ability to withstand high pressure and extreme temperatures makes it suitable for critical fluid transport, heat exchangers, and hydraulic systems. Additionally, its biocompatibility extends its utility to medical applications where long-term structural integrity and resistance to bodily fluids are essential.

The technical advantages of Grade 4 titanium pipe are further highlighted by its low maintenance requirements and extended service life, even under cyclic loading and exposure to corrosive environments. This translates to reduced downtime and lifecycle costs for operators, reinforcing its value as a premium material choice. For projects demanding uncompromised performance and resilience, Grade 4 titanium pipe stands out as a benchmark in high-performance piping solutions.

Grade 4 titanium pipe is the strongest among commercially pure titanium grades, offering an impressive combination of high tensile strength, excellent ductility, and superior corrosion resistance. With a minimum yield strength of 480 MPa and ultimate tensile strength exceeding 550 MPa, it outperforms Grades 1-3 in load-bearing applications while maintaining the renowned resistance to chloride-induced pitting and crevice corrosion. Its chemical composition, primarily titanium with trace amounts of oxygen, iron, and carbon, contributes to its robustness and biocompatibility, making it suitable for both industrial and medical environments.

When compared to other materials, Grade 4 titanium pipe surpasses stainless steel in corrosion resistance and offers a better strength-to-weight ratio than many nickel-based alloys. Although its initial cost is higher, its extended service life, reduced maintenance, and reliability in harsh environments often result in lower lifecycle costs. For projects requiring uncompromised performance—such as offshore oil rigs, chemical reactors, or high-performance aerospace systems—Grade 4 titanium pipe represents the optimal choice.

بیشتر بخوانید

داده‌ها

عنصر
Maximum Content (%)
نیتروژن (N) 0.05
Carbon © 0.08
Hydrogen (H) 0.015
آهن (Fe) 0.5
Oxygen (O) 0.4
Titanium (Ti) تعادل
مالکیت ارزش
تراکم
4.51 g/cm³ (0.163 lb/in³)
نقطه ذوب
1660°C (3020°F)
هدایت حرارتی
~16.4 W/m·K (114 BTU·in/hr·ft²·°F)
مقاومت الکتریکی
5.4 × 10⁻⁵ Ω·cm
Coefficient of Thermal Expansion (20–100°C) 8.6 µm/m·°C
مالکیت ارزش
Tensile Strength, Ultimate
550 MPa (80,000 psi) min
Tensile Strength, Yield
480 MPa (70,000 psi) min
نرخ کشش در شکست 15–25%
ماژول ارتجاعی
~104 GPa (15,100 ksi)
سختی، ویکرز ~280 HV

داکسون را انتخاب کنید تا به پروژه‌تان کمک کند اوج بگیرد.

همین حالا با داکسون تماس بگیرید

Advanced Production:Titanium seamless pipe

  • CP Grade 4 titanium pipes are typically manufactured according to major international standards such as ASTM B338, ASME SB338, ASTM B861 (for seamless pipes), and ASTM B862 (for welded pipes). They are readily available in a variety of sizes, with diameters ranging from 3.35mm to 152mm and wall thicknesses from 0.020″ to 0.220″, accommodating diverse project requirements.
همین حالا با داکسون تماس بگیرید

CP Grade 4 Titanium Tube Features

  • Balanced Properties: As a commercially pure titanium, it offers a great balance of moderate strength and excellent corrosion resistance, stronger than Grade 1 and 2.
  • Superior Corrosion Resistance: Exceptionally resistant to chloride and seawater environments, making it ideal for marine and chemical processing applications.
  • Good Fabricability: It is well-suited for forming, welding, and machining, allowing for easy manufacturing of complex components.
  • Biocompatible: Safe for use in medical implants and food processing equipment due to its non-toxic and hypoallergenic nature.
  • Cost-Effective: Provides better performance than lower grades without the high cost of titanium alloys, offering a practical solution for many industrial uses.
همین حالا با داکسون تماس بگیرید

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

همین حالا با داکسون تماس بگیرید

گزارش‌های آزمون

The test reports we provide include: Factory test certificate for CP Grade 4 titanium welded pipe and CP Grade 4 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

همین حالا با داکسون تماس بگیرید

Applications and standards

CP Grade 4 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
همین حالا با داکسون تماس بگیرید

کیفیت، تحویل، بازرسی

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Titanium Welded Pipe and  Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • زمان تحویل ما دقیقاً مطابق قرارداد است.
  • از آژانس‌های ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
  • از نمونه‌های رایگان برای آزمایش مشتری پشتیبانی کنید.
  • حمایت از بازرسی کارخانه‌ای حضوری یا ویدیویی
همین حالا با داکسون تماس بگیرید

بسته‌بندی

داکسون آلیاژ بهترین کیفیت بسته‌بندی را تضمین می‌کند، زیرا بسته‌بندی نقش مهمی در حمل‌ونقل بین‌المللی دارد که کالاها از مسیرهای مختلف عبور می‌کنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژه‌ای به بسته‌بندی داریم. ما کالاهای خود را بسته به محصول به روش‌های مختلف بسته‌بندی می‌کنیم. روش‌های بسته‌بندی محصولات ما عبارتند از:
• جعبه‌ها و صندوق‌ها
• سلفون منقبض‌شونده
• پالت‌های چوبی
• جعبه‌های چوبی

همین حالا با داکسون تماس بگیرید

پشتیبانی فنی

اگر به هرگونه پشتیبانی فنی اضافی نیاز دارید، متالورژیست مقیم ما و کارکنان آگاه ما با کمال میل آماده کمک‌رسانی هستند. علاوه بر این، داکسون دارای آزمایشگاه آزمون معتبر است—نخستین در صنعت موجودی چندفلزی و پلاستیکی. به نظر ما، این امر تعهد تزلزل‌ناپذیر ما به کیفیت و فلسفه ما به‌عنوان یک تأمین‌کننده تمام‌خدمت را نشان می‌دهد.

Daxun CP Grade 4 Titanium TUBE Let your brand improve rapidly

CP Grade 4 titanium tube form (4)

پروژه‌ها و محصولات داغ اخیر

CP Grade 4 Titanium pipe and tube
CP Grade 4 Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
What are the main characteristics of Grade 4 titanium pipe?

Grade 4 titanium pipe is the strongest of the commercially pure titanium grades. Its key characteristics include high tensile strength, excellent ductility, and superior corrosion resistance, especially against chlorides and acids. It offers an outstanding strength-to-weight ratio, making it both durable and lightweight.

What is the difference between Grade 4 and Grade 2 titanium pipe?

The primary difference is strength. Grade 4 titanium has a significantly higher minimum yield strength (480 MPa) compared to Grade 2 (275 MPa). While Grade 2 is more formable and often used for general corrosion resistance, Grade 4 is chosen for applications requiring higher mechanical strength and pressure resistance, such as in aerospace or demanding chemical processing components.

What are the most common applications for Grade 4 titanium pipe?

Due to its robust properties, Grade 4 titanium pipe is commonly used in the aerospace industry for hydraulic and fuel lines, in chemical processing for heat exchangers and pressure vessels, and in marine engineering for desalination plants and offshore platforms. It is also found in medical implants where high strength and biocompatibility are essential.

Can Grade 4 titanium pipe be laser cut?

Absolutely. Laser cutting is an excellent method for fabricating Grade 4 titanium pipe, offering high precision, clean cuts, and a minimal heat-affected zone. This is particularly beneficial for creating complex shapes or preparing pipe ends for welding. It’s crucial to use optimized cutting parameters and an assist gas like argon or nitrogen to prevent oxidation and maintain the material’s corrosion resistance.

Why is Grade 4 titanium pipe more expensive than stainless steel?

The higher initial cost is due to the complex extraction and refining processes required for titanium. However, Grade 4 titanium pipe often provides a lower total cost of ownership. Its exceptional corrosion resistance leads to a much longer service life and significantly reduced maintenance and replacement costs, especially in harsh environments where stainless steel would fail quickly.

آیا درجه تیتانیوم بر هزینه تأثیر دارد؟

اگرچه درجه تیتانیوم کمی هزینه را افزایش می‌دهد، اما هزینه کل عمدتاً به شکل و فرم تیتانیومی که نیاز دارید بستگی دارد.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

متأسفانه بدون اطلاع کافی از پروژه شما و کاربرد تیتانیوم، تعیین قیمت به‌صورت آنلاین دشوار است.

خوشبختانه تیم کارشناسان ما همیشه در خدمت شماست تا در زمینه نیازهای تیتانیومی‌تان به شما کمک و مشاوره دهد. با ارسال ایمیل به [email protected]، ما قادر خواهیم بود با ارائه مشاوره و برآورد دقیق هزینه به شما پاسخ دهیم.

حتماً تا حد امکان اطلاعاتی دربارهٔ گرید، شکل و مقدار تیتانیومی که نیاز دارید ارائه دهید تا نیازهایتان بهتر درک شود.

چگونه سریعاً یک برآورد قیمت دریافت کنیم یا اطلاعات بازار را بفهمیم؟

لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتس‌اپ ما آنلاین است و ایمیل ([email protected]) ظرف ۶ ساعت بررسی می‌شود. به هر پرسش یا پیام به‌سرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک می‌گذاریم.

می‌توانم چند نمونه بگیرم؟

ما می‌توانیم نمونه‌های ورق فولاد ضدزنگ را برای بررسی کیفیت در اختیار شما قرار دهیم. نمونه رایگان است و شما فقط هزینه حمل را پرداخت می‌کنید.

تا کنون به کدام کشورها صادرات داشته‌اید؟

ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشته‌ایم.

زمان تحویل شما چقدر است؟

سفارش‌های آزمایشی را می‌توان ظرف یک هفته تحویل داد. برای سفارش‌های معمولی تقریباً دو هفته زمان لازم است.

همین امروز استعلام خود را ارسال کنید
استعلام سریع