CP Grade 3 Titanium Pipe Manufacturer
As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
- Titanium tube Grade:R50550 / CP TI50A
- Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
- Standards:ASTM B338
- Softest Ti,High ductility, Very corrosion resistant, good cold formability
————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!
CP Grade 3 Titanium Pipe Manufacturer
CP Grade 3 titanium pipe is a commercially pure titanium product known for its balanced combination of moderate strength and excellent corrosion resistance. With titanium content of approximately 99.1% and controlled oxygen levels between 0.10-0.27%, Grade 3 offers higher mechanical properties than Grades 1 and 2. This specific oxygen content is the key differentiator, providing increased strength while retaining the inherent corrosion resistance of pure titanium.
In terms of mechanical performance, CP Grade 3 features a tensile strength around 450-485 MPa and a yield strength of 380-415 MPa, all while maintaining good ductility with 20-30% elongation. This makes it stronger than Grade 1 and Grade 2 but less strong than Grade 4 or titanium alloys like Grade 5, positioning it as a versatile “middle-strength” option within the commercially pure titanium series.
Applications of CP Grade 3 titanium
CP Grade 3 titanium pipes find extensive applications across various industries due to their excellent corrosion resistance and moderate strength. In the chemical processing industry, they are widely used for heat exchangers, condensers, and piping systems that handle corrosive chemicals and chlorides. The marine sector relies on these pipes for seawater cooling systems, desalination plants, and offshore platform components where resistance to saltwater corrosion is critical.
The oil and gas industry utilizes CP Grade 3 pipes for downhole tubing and surface equipment exposed to harsh environments. In power generation, particularly in geothermal and coastal plants, these pipes serve in condensers and heat transfer systems. The aerospace industry employs them for hydraulic systems and fuel lines where weight savings and corrosion resistance are priorities.
Medical applications include surgical implants and medical devices that benefit from titanium’s biocompatibility. Additionally, the food processing and pharmaceutical industries use CP Grade 3 pipes for equipment requiring sanitary conditions and resistance to cleaning chemicals. Their combination of weldability, formability, and durability makes them suitable for custom fabrication across these diverse applications.
Comparison of Grade 3 titanium pipes with other pure titanium grades
CP Grade 3 titanium pipe sits in a practical middle ground within the commercially pure titanium series. Think of it as a balance between strength and formability.
Grade 1 is the softest and most easily formed, perfect for complex deep-drawing applications, but it has the lowest strength. Grade 2 is the workhorse of the titanium industry—it’s slightly stronger than Grade 1 while still offering excellent corrosion resistance and weldability, which is why it’s the most commonly used grade.
This is where CP Grade 3 comes in. With a higher oxygen content, it provides significantly more strength than Grade 2, making it suitable for pressure vessels and piping systems where Grade 2 might not be robust enough. However, this extra strength means it’s slightly less formable than the lower grades.
Grade 4 is the strongest of all the commercially pure grades, but it sacrifices much of the ductility that makes the other grades easy to work with.
For most piping applications, the choice often comes down to Grade 2 versus Grade 3. If your project demands higher pressure ratings and mechanical strength, Grade 3 is the superior choice. If you need maximum formability for complex shapes, Grade 2 might be more suitable. Essentially, you choose Grade 3 when strength is a higher priority than ease of fabrication.
دادهها
- پارامتر
- خواص فیزیکی
- خواص مکانیکی
| عنصر | Content (%) |
| Titanium (Ti) |
Balance (~99.1%)
|
| Oxygen (O) | 0.10 – 0.27 |
| آهن (Fe) | ≤ 0.30 |
| Carbon © | ≤ 0.10 |
| نیتروژن (N) | ≤ 0.05 |
| Hydrogen (H) | ≤ 0.015 |
| مالکیت | ارزش |
| تراکم | ~4.51 g/cm³ |
| نقطه ذوب |
~1660–1670 °C
|
| ماژول ارتجاعی |
~103–107 GPa
|
| هدایت حرارتی |
~21.9 W/m·K (at 25°C)
|
| مقاومت الکتریکی | ~420 nΩ·m |
| مالکیت | ارزش |
| مقاومت کششی |
~450–485 MPa
|
| مقاومت تسلیم |
~380–415 MPa
|
| Elongation | ~20–30% |
| سختی (برینل) |
~200–240 HB
|
داکسون را انتخاب کنید تا به پروژهتان کمک کند اوج بگیرد.

Advanced Production:Titanium seamless pipe
- CP Grade 3 titanium pipes are typically manufactured according to major international standards such as ASTM B338, ASME SB338, ASTM B861 (for seamless pipes), and ASTM B862 (for welded pipes). They are readily available in a variety of sizes, with diameters ranging from 3.35mm to 152mm and wall thicknesses from 0.020″ to 0.220″, accommodating diverse project requirements.
CP Grade 3 Titanium Tube Features
- Balanced Properties: As a commercially pure titanium, it offers a great balance of moderate strength and excellent corrosion resistance, stronger than Grade 1 and 2.
- Superior Corrosion Resistance: Exceptionally resistant to chloride and seawater environments, making it ideal for marine and chemical processing applications.
- Good Fabricability: It is well-suited for forming, welding, and machining, allowing for easy manufacturing of complex components.
- Biocompatible: Safe for use in medical implants and food processing equipment due to its non-toxic and hypoallergenic nature.
- Cost-Effective: Provides better performance than lower grades without the high cost of titanium alloys, offering a practical solution for many industrial uses.


Advanced Production: Titanium Welded Tube
Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.
گزارشهای آزمون
The test reports we provide include: Factory test certificate for CP Grade 3 titanium welded pipe and CP Grade 3 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)


Applications and standards
CP Grade 3 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:
- Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
- Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
Standard : ASTM, ASME and API
کیفیت، تحویل، بازرسی
Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Titanium Welded Pipe and Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.
- زمان تحویل ما دقیقاً مطابق قرارداد است.
- از آژانسهای ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
- از نمونههای رایگان برای آزمایش مشتری پشتیبانی کنید.
- حمایت از بازرسی کارخانهای حضوری یا ویدیویی


بستهبندی
داکسون آلیاژ بهترین کیفیت بستهبندی را تضمین میکند، زیرا بستهبندی نقش مهمی در حملونقل بینالمللی دارد که کالاها از مسیرهای مختلف عبور میکنند تا به مقصد نهایی برسند؛ بنابراین ما توجه ویژهای به بستهبندی داریم. ما کالاهای خود را بسته به محصول به روشهای مختلف بستهبندی میکنیم. روشهای بستهبندی محصولات ما عبارتند از:
• جعبهها و صندوقها
• سلفون منقبضشونده
• پالتهای چوبی
• جعبههای چوبی
پشتیبانی فنی
اگر به هرگونه پشتیبانی فنی اضافی نیاز دارید، متالورژیست مقیم ما و کارکنان آگاه ما با کمال میل آماده کمکرسانی هستند. علاوه بر این، داکسون دارای آزمایشگاه آزمون معتبر است—نخستین در صنعت موجودی چندفلزی و پلاستیکی. به نظر ما، این امر تعهد تزلزلناپذیر ما به کیفیت و فلسفه ما بهعنوان یک تأمینکننده تمامخدمت را نشان میدهد.

Daxun CP Grade 3 Titanium TUBE Let your brand improve rapidly
- گالری
CP Grade 3 titanium tube form (4)
پروژهها و محصولات داغ اخیر
محصولات مرتبط (8)
The primary difference is the oxygen content, which directly impacts strength. CP Grade 3 has a higher oxygen content (0.10-0.27%) than Grade 2, giving it approximately 20-30% higher tensile and yield strength. This makes Grade 3 suitable for applications requiring more robust pressure handling and mechanical performance, while Grade 2 is often chosen for its superior formability.
Yes, CP Grade 3 has excellent weldability using standard titanium welding procedures, most commonly TIG (GTAW) and MIG (GMAW) welding. It requires proper inert gas shielding (argon or helium) to prevent contamination of the weld pool, but it can be reliably welded to itself or other CP titanium grades.
You should choose CP Grade 3 when excellent corrosion resistance is your primary concern and the mechanical demands are moderate. Titanium alloys like Grade 5 offer much higher strength and are better for high-stress structural applications. CP Grade 3 is more cost-effective than titanium alloys and provides superior corrosion resistance in many environments, making it the ideal choice for piping, heat exchangers, and chemical processing equipment.
CP Grade 3 offers vastly superior corrosion resistance, especially in chloride environments like seawater, where 316L is prone to pitting and crevice corrosion. Titanium is also about 40% lighter than steel and has a much longer service life in aggressive environments. However, 316L has a lower initial material cost. The choice depends on whether long-term durability and corrosion resistance outweigh upfront cost.
اگرچه درجه تیتانیوم کمی هزینه را افزایش میدهد، اما هزینه کل عمدتاً به شکل و فرم تیتانیومی که نیاز دارید بستگی دارد.
At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.
متأسفانه بدون اطلاع کافی از پروژه شما و کاربرد تیتانیوم، تعیین قیمت بهصورت آنلاین دشوار است.
خوشبختانه تیم کارشناسان ما همیشه در خدمت شماست تا در زمینه نیازهای تیتانیومیتان به شما کمک و مشاوره دهد. با ارسال ایمیل به [email protected]، ما قادر خواهیم بود با ارائه مشاوره و برآورد دقیق هزینه به شما پاسخ دهیم.
حتماً تا حد امکان اطلاعاتی دربارهٔ گرید، شکل و مقدار تیتانیومی که نیاز دارید ارائه دهید تا نیازهایتان بهتر درک شود.
لطفاً فرم صفحه “تماس با ما” را پر کنید یا با مدیر فروش ما به شماره +86 13382898899 تماس بگیرید. ما در اسرع وقت با شما تماس خواهیم گرفت. واتساپ ما آنلاین است و ایمیل ([email protected]) ظرف ۶ ساعت بررسی میشود. به هر پرسش یا پیام بهسرعت پاسخ داده خواهد شد. علاوه بر این، ما هر هفته اطلاعات بازار را با مشتریان خود به اشتراک میگذاریم.
ما میتوانیم نمونههای ورق فولاد ضدزنگ را برای بررسی کیفیت در اختیار شما قرار دهیم. نمونه رایگان است و شما فقط هزینه حمل را پرداخت میکنید.
ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشتهایم.
سفارشهای آزمایشی را میتوان ظرف یک هفته تحویل داد. برای سفارشهای معمولی تقریباً دو هفته زمان لازم است.