Daxun is a 310S stainless steel sheet supplier from China
As China’s leading stainless steel plate supplier and exporter, Daxun provides 310S stainless steel plates to the world.
- Grade: AISI 310-310S-S31008
- تولید: ورق نورد سرد، ورق نورد گرم، ورق آهنگری
- استاندارد: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- نوع: ورق نازک نورد سرد، ورق ضخیم نورد گرم
- سطح: 2B، NO.1، NO.4، HL، BA، 8K و غیره.
- طول: 2438 میلیمتر، 3048 میلیمتر، 6000 میلیمتر قابل سفارشیسازی
- Origin: TISCO, Baosteel, Pohang, Tsingshan, Delong
The global leader in stainless steel sheet fabrication services
S31008 (310S) Sheet and Plate, Austenitic stainless steel alloy 310S (UNS S31008) is designed for applications requiring high-temperature corrosion resistance. The alloy resists oxidation up to 2010°F (1100°C) with room temperature cycling. Alloy 310 can be used in moderate carburizing environments and is resistant to sulfidation due to its high chromium content and moderate nickel content. More severe carburizing environments in heat-treating equipment typically require a nickel alloy such as 330 (UNS N08330). Alloy 310S can be used in bonding, nitriding, mild oxidation, and thermal cycling processes; however, a reduced maximum service temperature is required. Alloy 310 can also be used in cryogenic applications because it has low magnetic permeability and remains strong down to -450°F (-268°C). When heated to 1202–1742, the alloy precipitates the sigma phase (650–950°C). Hardness is partially restored by solution annealing at 2012–2102°F (1100–1150°C). This alloy is also available as a low-carbon alloy, 310S (UNS S31008). It is easily fabricated. A high carbon modification, 310H (UNS S31009), is designed to improve creep resistance. In most cases, the grain size and carbon content of the plate can meet both 310S and 310H standards. Standard shop fabrication procedures can be used to easily weld and process alloy 310.
Stainless Steel 310S Plate has trace amounts of silicon, sulfur, phosphorus, manganese, and up to 24% chromium, 19% nickel, and up to 0.08% carbon. Heat resistance, corrosion resistance, strength, and even high-temperature oxidation resistance are just a few of the many benefits of this popular stainless steel alloy. It can be utilized in many different applications, including burners, oil burners, and evaporator pipes and tubes. Because of its affordability, it’s perfect for a range of applications requiring low-cost maintenance supplies.
Because of its exceptional resilience to high temperatures, the 310S stainless steel plate is a great option for a wide range of industries, including petrochemical and chemical production, food processing, power plants, dairy farms, sugar mills, breweries, and energy generation. 310S Stainless Steel Plate is capable of withstanding oxidizing environments up to 2100°F (1149°C) due to its high chromium concentration. Its ductility, toughness, and weldability are all excellent. Its exceptional low-temperature performance, even down to -20°F (-29°C), combined with its resistance to heat and corrosion make it the perfect material for cryogenic applications. In conclusion, it is an excellent option for high-temperature industrial applications due to its strong resistance to oxidation and ability to prevent scaling at temperatures as high as 2000°F (1093°C).
دادههای فنی
- پارامتر
- عنصر
- خواص مکانیکی
- استاندارد
| Product Parameters: 310(UNS S31008) Stainless Steel Sheet/Plate | |||
| عرض | 10mm~2500mm | ||
| ضخامت | 0.2mm~100mm | Thickness tolerance | +/-0.03mm |
| استاندارد | ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2 | ||
| سطح | 2B,BA,8K,NO.1,NO.4,NO.3,hairline,checkered,gold ,black ,rose gold,etc | ||
| specification | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
| Mill Origin | TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc. | ||
| Certification | ISO, SGS, BV, TUV,CE etc | ||
| عنصر | % Present (in product form) | |
| C, H, P, L | TW* / TS* | |
| کربن (C) | ≤0.10 | ≤0.15 |
| سیلیکون (Si) | ≤1.50 | ≤0.75 |
| منگنز (Mn) | ≤2.00 | ≤2.00 |
| فسفر (P) | ≤0.045 | ≤0.045 |
| گوگرد (S) | ≤0.015 | ≤0.030 |
| کروم (Cr) | 24.00 – 26.00 | 24.00 – 26.00 |
| نیکل (Ni) | 19.00 – 22.00 | 19.00 – 22.00 |
| نیتروژن (N) | ≤0.11 | – |
| آهن (Fe) | تعادل | تعادل |
| Product Form | |||||
| C, H, P | L | TW* / TS* | |||
| Thickness a or diamter d (mm) | a ≤ 12 | d ≤ 25 | – | ||
| Hardness HB max. 1) 2) 3) | 192 | 192 | – | ||
| Proof Strength3) | Rp0.2 N/mm2 | 210 | 210 | 230 | |
| Rp1.0 N/mm2 | 230 | 230 | 270 | ||
| مقاومت کششی | Rm N/mm2 | 500 – 700 | 500 – 700 | min. 500 | |
| Elongation min. in % | Long Products | 351) | 351) | 334) / 355) | |
| Flat Products | 0.5 ≤ a/d < 3 | 334)5) | 334)5) | 354)5)6) | |
| 3 ≤ a/d | 354)5) | 354)5) | 354)5)6) | ||
| 310 | ۳۱۰اس | 310H |
|---|---|---|
| UNS S31000 | UNS S31008 | UNS S31009 |
| استم اِی۲۴۰ | استم اِی۲۴۰ | استم اِی۲۴۰ |
| استم اِی۴۸۰ | استم اِی۴۸۰ | استم اِی۴۸۰ |
| ASME SA240 | ASME SA240 | ASME SA240 |
| AMS 5521 | AMS 5521 | AMS 5521 |
داکسون را انتخاب کنید و مشتریان خود را راضی کنید.

تحویل سریع
We provide timely and fast delivery of 310S stainless steel plate products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Benefits of Stainless Steel 310S Plates :
- Corrosion resistance: The main benefit of 310S stainless steel plates is their excellent corrosion resistance. They resist corrosion from a wide range of environments, including acidic and alkaline solutions, making them suitable for a wide range of applications.
- High-temperature strength: 310S stainless steel plates exhibit excellent strength at elevated temperatures. This property is critical in applications that are frequently exposed to high temperatures, ensuring structural integrity and performance in demanding conditions.
- Durability and lifespan: The durability of 310S stainless steel plates gives them a long service life, making them an affordable choice for many applications. The material is resistant to wear and tear, minimizing the need for frequent replacement.

Benefits of Stainless Steel 310S Plates :
310S/2520 Plate Features:
- High-temperature resistance
- مقاومت عالی در برابر اکسیداسیون
- Improved creep/rupture properties
- مقاومت عالی در برابر خوردگی
- Not susceptible to thermal fatigue and cyclic heating
- Good strength at temperatures up to 2100°F
کیفیت، تحویل، بازرسی
- داکسون کیفیت محصولات را بهطور دقیق کنترل میکند. پیش از ثبت سفارش، ضمانتنامه محصول را برای شما ارسال خواهیم کرد، یا اگر برای آزمایش نیاز به نمونه دارید، میتوانیم نمونهها را بهصورت رایگان ارسال کنیم.
- During the production process, we carefully measure the diameter, thickness, and surface quality of each product to ensure it meets exacting standards. Our standard delivery time is typically 7 to 15 days. However, for special-sized products, the delivery time may be extended to 20 days to accommodate the additional customization and processing required.
زمان تحویل ما دقیقاً مطابق قرارداد است. - از آژانسهای ثالث مشتری برای انجام بازرسی به کارخانه پشتیبانی کنید.
- از ارائه نمونههای رایگان به مشتریان برای آزمایش پشتیبانی کنید.
- حمایت از بازرسی کارخانهای حضوری یا ویدیویی

کاربردها
- Cryogenic Components: Designed to withstand extremely low temperatures, ensuring optimal performance in critical applications.
- Food Processing: Reliable materials and components tailored for hygienic and efficient food production systems.
- Furnaces: Durable solutions for burners, doors, fans, ducting, and liners, supporting high-temperature industrial processes.
- Fluidized Bed Furnaces: Robust components including coal burners, grates, ducting, and bellows for enhanced operational efficiency.
- Ore Processing and Steel Mills: High-performance equipment for smelting, steelmaking, and continuous casting operations.
- Petroleum Refining: Specialized systems such as catalytic recovery units, flares, heat exchangers, and tube hangers for maximum efficiency in refining processes.
- Power Generation: Precision-engineered components like gas furnace internals, pulverized coal burners, and tube hangers to support energy production.
- Sintering and Cement Plants: Reliable burners, burner hoods, feed and discharge systems, and bellows for seamless operation in harsh environments.
- Heat Treating: Advanced solutions, including annealing covers and boxes, burner grates, doors, fans, muffle furnaces, retorts, heat exchangers, and walking beams for consistent performance in thermal processing.
SS 310S Plate Surface Treatment
1D: The surface is matte with a discontinuous particle shape.
دو بعدی: سفید با تهرنگ نقرهای.
2B: Silver gray with better gloss and flatness than the 2D surface.
Ba: نزدیک به سطح آینه با درخشندگی و بازتاب عالی.
شمارهٔ ۳: براق خوب و سطح زبر.
شمارهٔ ۴: سطح دارای خطوط ریز و درخشش خوبی است.
HL: خاکستری نقرهای با موهای طلایی.
۸K: سطح آینهای.
310 plate stainless steel Features
داکسون: به برندتان امکان پیشرفت سریع دهید
- گالری
- بردباری
- وضعیت تحویل
- سایر سری محصولات
| تolerance برای 2B Sheet | |||
| اندازه | رتبه تحمل | ||
| گروه ۱ | گروه ۲ | گروه ۳ | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| تolerance برای ورق نمره ۱ نورد گرم | |||
| اندازه | رتبه تحمل | ||
| گروه ۱ | گروه ۲ | گروه ۳ | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| انتخاب ایالت تحویل | وضعیت سطح |
| نورد سرد | دو بی |
| دو بعدی | |
| کارشناسی هنر | |
| خط موی سر | |
| شمارهٔ ۳ | |
| شمارهٔ ۴ | |
| ۶ کیلومتر | |
| کیوکیو | |
| توجه: | |
| ۱. در صورتی که به وضعیت تحویل متفاوتی از موارد فوق نیاز دارید، لطفاً با ما هماهنگ فرمایید. | |
| ۲. در صورت هرگونه پرسش یا سفارش، لطفاً ما را از هرگونه نیاز اضافی که در اینجا ذکر نشده است، مطلع سازید. | |
| وضعیت تحویل | |
| انتخاب ایالت تحویل | وضعیت سطح |
| نورد گرم | شمارهٔ یک |
| شمارهٔ ۳ | |
| شمارهٔ ۴ | |
| ۶ کیلومتر | |
| کیوکیو | |
| شور شده | |
| توجه: | |
| ۱. در صورتی که به وضعیت تحویل متفاوتی از موارد فوق نیاز دارید، لطفاً با ما هماهنگ فرمایید. | |
| ۲. در صورت هرگونه پرسش یا سفارش، لطفاً ما را از هرگونه نیاز اضافی که در اینجا ذکر نشده است، مطلع سازید. | |
| نمره | نوع | ضخامت | سطح |
| آستنیتی | ۳۰۴/۳۰۴H/۳۰۴L/۳۰۴J1 | ۰.۲۵-۱۵۰ میلیمتر | 2B/BA/شماره ۴/۸K/SB/HL/شماره ۱ |
| 321 | ۰.۴-۸۰ میلیمتر | 2B/BA/شماره ۴/۸K/SB/HL/شماره ۱ | |
| ۳۱۶/۳۱۶L/۳۱۷L/۳۱۶Ti | 0.3-80 میلیمتر | 2B/BA/شماره ۴/۸K/SB/HL/شماره ۱ | |
| فریت | 430 | 0.4-3.0 میلیمتر | 2B/BA/NO.4/8K/SB/HL |
| فریت فوق خالص | 443 | ۰.۴-۲.۰ میلیمتر | دو بی |
| ۴۳۶L/۴۳۹/۴۴۴/۴۴۱ | ۰.۵-۳.۰ میلیمتر | دو ب، دو دی | |
| چهارصد و نه ال | ۰.۴-۲.۵ میلیمتر | دو ب، دو دی | |
| نمره | نوع | ضخامت | اصلی |
| فولاد مقاوم در برابر حرارت | ۳۰۹ اس | ۰.۵-۴۰ میلیمتر | CHN |
| ۳۱۰اس | ۰.۵-۴۰ میلیمتر | CHN | |
| فولاد دوبلکس | 2101 | ۱.۵-۵۰ میلیمتر | CHN |
| 2304 | ۳.۰-۵۰ میلیمتر | CHN | |
| 2205 | ۰.۵-۶۰ میلیمتر | CHN | |
| 2507 | ۱.۰-۶۰ میلیمتر | SWE / JPN / CHN | |
| فولاد فوقآستنیتی | N08904 | ۰.۶-۵۰ میلیمتر | SWE / JPN / CHN |
| اساس ۳۱۲۵۴ | ۰.۵-۵۰ میلیمتر | SWE / JPN / CHN | |
| N08926 | ۰.۵-۵۰ میلیمتر | SWE / JPN / CHN | |
| N08367 | ۰.۵-۵۰ میلیمتر | SWE / JPN / CHN | |
| آلیاژ پایه نیکل | N08031 | ۱.۰-۵۰ میلیمتر | آمریکا / ژاپن / آلمان |
| N08810/N08800 | ۰.۸-۵۰ میلیمتر | ایالات متحده / ژاپن / چین | |
| N08028 | ۱.۰-۲۰ میلیمتر | ایالات متحده آمریکا / آلمان / ژاپن | |
| N08020 | ۱.۰-۲۰ میلیمتر | ایالات متحده آمریکا / آلمان / ژاپن | |
| N08825 | ۰.۸-۴۰ میلیمتر | ایالات متحده آمریکا / آلمان / سوئد / ژاپن / چین | |
| N10276 | ۰.۵-۵۰ میلیمتر | ایالات متحده آمریکا / آلمان / ژاپن | |
| N06022 | ۱.۰-۵۰ میلیمتر | ایالات متحده آمریکا / آلمان / ژاپن | |
| N06625 | ۰.۸-۲۰ میلیمتر | ایالات متحده / آلمان / چین | |
| N04400 | ۱.۰-۲۰ میلیمتر | ایالات متحده آمریکا / آلمان / ژاپن | |
| N06600 | ۱.۰-۵۰ میلیمتر | ایالات متحده آمریکا / آلمان / ژاپن / چین | |
| N02201 | ۰.۵-۲۰ میلیمتر | ایالات متحده / ژاپن | |
| تیتانیوم | TA1/Gr1 | ۰.۵-۵۰ میلیمتر | ژاپنی / چینی |
| TA2/Gr2 | ۰.۵-۵۰ میلیمتر | ژاپنی / چینی | |
| مواد جوشکاری | ERNiCrMo-13 | ۱.۲، ۲.۴ میلیمتر | GER |
| ERNiCrMo-3 | ۲.۴ میلیمتر | GER | |
| ERNiCrMo-4 | ۲.۴ میلیمتر | ایالات متحده آمریکا |
The surface and shape of 310S stainless steel plate (7)
اطلاعات موجود برای مرجع و دانلود
داکسون یک تولیدکننده قابل اعتماد ورق فولاد ضد زنگ است.
بهعنوان یک تولیدکننده حرفهای، داکسون تضمین میکند که تمامی محصولاتی که تولید میکند از کیفیت بالایی برخوردار باشند. بنابراین، ما اطمینان حاصل میکنیم که تمامی ورقهای فولاد ضدزنگ دارای گواهیهای ISO9001، SGS، CE، OQC و سایر استانداردهای بینالمللی کیفیت باشند. ما همچنین کنترل کیفیت سختگیرانهای داریم تا اطمینان حاصل کنیم که ورقهای فولاد ضدزنگ دارای عیوب کمتری باشند. در داکسون، مطمئن باشید که تمامی محصولات بادوام، باکیفیت و با کارایی بالا هستند.
پروژهها و محصولات داغ اخیر
محصولات مرتبط (13)
ما میتوانیم نمونههای ورق فولاد ضدزنگ را برای بررسی کیفیت در اختیار شما قرار دهیم. نمونه رایگان است و شما فقط هزینه حمل را پرداخت میکنید.
ما به بیش از ۴۲ کشور مانند کانادا، شیلی، کویت، آلمان، کرهٔ جنوبی، عربستان سعودی، سنگاپور و غیره صادرات داشتهایم.
حداقل سفارش ما برای ورق فولاد ضد زنگ ۱ تن است.
سفارشهای آزمایشی را میتوان ظرف یک هفته تحویل داد. برای سفارشهای معمولی تقریباً دو هفته زمان لازم است.