Duplex 2507/S32750 Stainless Steel Bars and Round Bars China Supplier

Leading stainless steel rod and bar Suppliers in China

    • Daxun Alloy offers Duplex 2507 in Round Bar and Flat Bar forms
    • Available in cold rolled and hot rolled options
    • Composition: 25% chromium, 4% molybdenum, 7% nickel
    • High strength and excellent corrosion resistance
    • Used in chemical processing, petrochemical, and seawater equipment
    • Resistant to chloride stress corrosion cracking
    • Good thermal properties, including low thermal expansion, making it suitable for high-temperature applications

Global leader in stainless rod and Round Bar fabrication services

GENERAL PROPERTIES

Duplex 2507 (UNS S32750) is a super duplex stainless steel bar. Its composition includes 25% chromium, 4% molybdenum, and 7% nickel. This alloy excels in challenging environments, offering remarkable strength and corrosion resistance. It’s the go-to choice for chemical processing and petrochemical industries. Seawater equipment also benefits from its exceptional properties. Duplex 2507 stands strong against chloride stress corrosion cracking. Its thermal properties are impressive, with high conductivity and low thermal expansion, making it ideal for high-temperature applications. The alloy’s unique blend of elements ensures top-notch corrosion resistance. For tough conditions demanding both strength and durability, Duplex 2507 delivers.

Our network of service centers stock stainless steel bar products for fast, ready supply of bar in common sizes and alloys.We also produce custom-sized stainless steel rods and can arrange inventory schedules for quick turnaround in a timely manner if quantities are below factory minimums.Daxun Alloys stocks stainless steel round bars with diameters ranging from 1/16″ to 26″. Round bars are available in nearly every grade of stainless steel, including 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205, and Alloy 20. Heat treated stainless steel round bars are offered in 17-4PH, H900 temper (on request), H1025, H1150, Double H1150, and H1150M. Other heat-treated tempers can be manufactured upon request. We stock the following 400 series stainless steels: 410, 430, and 416. We also carry 303, 304, and 316/L precision and bearing quality stainless steel round bars. The majority of our inventory consists of our unique machined bar grades: stainless steel round bars that are melted to consistent standards to increase machinability and lower total cost per component. Our stainless steel bar processing machinery allows Daxun Alloys to produce to our customers’ exact specifications.

Read More

Data

Product Parameters:   Stainless Steel rod
Specifications ASTM A276, ASME SA276 / ASTM A479  ASME SA479
Dimensions EN, DIN, JIS, ASTM, BS, ASME, AISI
Duplex 2507- S32750 Round Bars Outside Diameter in the range of 4mm to 500mm
Duplex 2507- S32750 Round Bars Outside Diameter in the range of 4mm to 100mm
Duplex 2507- S32750 Round Bars 18mm – 57mm (11/16″ to 2-3/4″)
Finish Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish
Length 1 to 6 Meters, Custom Cut Lengths
Form Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc.
Grade Super Duplex 2507
UNS Designation S32750
Carbon (C) Max. 0.03
Manganese (Mn) Max. 1.2
Phosphorous (P) Max. 0.035
Sulphur (S) Max. 0.02
Silicon (Si) Max. 0.8
Chromium (Cr) 24.0–26.0
Nickel (Ni) 6.0–8.0
Molybdenum (Mo) 3.0–5.0
Nitrogen (N) 0.24–0.32
Iron (Fe) Bal.
Copper (Cu) 0.5
Other Elements
Physical Properties of Super Duplex 2507 Alloys in the Annealed Condition at -20°F to +100°F
Tensile Strength Yield Strength
Alloy UNS Designation Spec. psi MPa ksi psi MPa ksi Elongation in 2 in. (min.) % Grain Size Req. Max. Hardness Modulus of Elasticity (x106 psi) Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) Thermal Conductivity (BTU-in/ ft2-h-°F)
Super Duplex 2507 S32950 A789, A790 100,000 690 100 70,000 485 70 20 30.5 Rc
Super Duplex 2507 S32750 A789, A790 116,000 800 116 80,000 550 80 15 32 Rc 27.5 7.2 98
Density, lb/in3 0.28
Modulus of Elasticity, psi 29.0x 106
Coefficient of Thermal Expansion, 68-212˚F, /˚F 7.5 x 10-6
Thermal Conductivity, Btu/ft hr ˚F 8
Specific Heat, Btu/lb ˚F 0.12
Electrical Resistivity, Microhm-in 31.5
Super Duplex 2507 Product Range
Alloy UNS Designation Werkstoff NR. Specifications*
Super Duplex 2507 S32750                       1.4410 A/SA789, A/SA790
Stainless Steel 2507/S32750 Bright Bar SS 2507/S32750 Bright Bar
2507/S32750 SS Bright Bar
Stainless Steel 2507/S32750 Bright Bar
UNS S2507/S3275000 SS Bright Bar
WERKSTOFF NR. 1.4410 Bright Bar
ASTM A276 2507/S32750 Stainless Steel Bright Bar
Stainless Steel 2507/S32750 Hex Bar SS 2507/S32750 Hex Bar
2507/S32750 SS Hexagonal Bar
2507/S32750 Stainless Steel Hex Bar
UNS S2507/S3275000 SS Hexagonal Bar
ASTM A276 2507/S32750 Stainless Steel Hex Bar
Stainless Steel 2507/S32750 Square Bar SS 2507/S32750 Square Bar
2507/S32750 SS Square Bars
2507/S32750 Stainless Steel Square Bar
UNS S2507/S3275000 SS Square Bar
WERKSTOFF NR. 1.4410 Square Bar
ASTM A479 2507/S32750 Stainless Steel Square Bars
Stainless Steel 2507/S32750 Rectangular Bar SS 2507/S32750 Rectangular Bar
2507/S32750 SS Rectangular Bars
2507/S32750 Stainless Steel Rectangular Bar
UNS S2507/S3275000 SS Rectangular Bars
WERKSTOFF NR. 1.4410 Rectangular Bar
ASTM A276 2507/S32750 Stainless Steel Rectangular Bar
Stainless Steel 2507/S32750 Flat Bars SS 2507/S32750 Flat Bar
2507/S32750 SS Flat Bars
2507/S32750 Stainless Steel Flat Bars
UNS S2507/S3275000 SS Flat Bars
WERKSTOFF NR. 1.4410 Flat Bars
ASTM A276 2507/S32750 Stainless Steel Flat Bars
Stainless Steel 2507/S32750 Polished Bar SS 2507/S32750 Polished Bar
2507/S32750 SS Polished Bars
2507/S32750 Stainless Steel Polished Bar
UNS S2507/S3275000 SS Polished Bars
WERKSTOFF NR. 1.4410 Polished Bar
ASTM A476 2507/S32750 Stainless Steel Polished Bar
Stainless Steel 2507/S32750 Threaded Bar SS 2507/S32750 Threaded Bar
2507/S32750 SS Threaded Bars
2507/S32750 Stainless Steel Threaded Bar
UNS S2507/S3275000 SS Threaded Bar
WERKSTOFF NR. 1.4410 Threaded Bar
ASTM A276 2507/S32750 Stainless Steel Threaded Bar

Choose Daxun and make your customers satisfied.

Contact Daxun now-2507 Stainless Steel Rod

Quick response

We provide timely and fast delivery of 2507 stainless steel bars for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to ports and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

Contact Daxun now

Daxun Advantages

  • Varieties: We offer a wide range of sizes and grades, including 300 series, 400, 600 series, and more.
  • Flexibility: Whether you need hot-rolled or cold-drawn bars, our stainless steel bar lengths are designed to meet your specific project requirements.
  • Quality Standards: 2507 Stainless Steel Rod meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
  • Custom Orders: Looking for special sizes of stainless steel bars? We offer a variety of stainless steel bar customization options with competitive prices and convenient online ordering.
Contact Daxun now

2507 Stainless Steel Rod packaging

We pay attention to every process to ensure quality. The 2507 round bar packaging we usually adopt is to pack the stainless steel round bars with environmentally friendly plastic bags and then put them into fumigation-free wooden boxes or wooden pallets. Customized packaging, such as OEM, can also be negotiated. We provide almost everything to meet your round bar packaging requirements. We attach great importance to packaging. The round bars are packed in wooden corrugated boxes, wrapped with plastic packaging and bubble film on the outside.

Contact Daxun now

Quality, delivery, inspection

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    Our delivery time is strictly in accordance with the contract.
  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples to customers for testing
  • Support on-site or video factory inspection
Contact Daxun now

Technical Support

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Contact Daxun now

2507 Stainless Steel Rod Ordering Information

2507 Round Bar Purchase orders shall include quantity, PSL grade, type or category, API5L reference, diameter, surface finish, length and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish or end treatment. Bars are solution bright annealed.

2507/S32750 Stainless Steel Rod Features

High strength
Corrosion resistance
Heat resistance
Low temperature resistance
Environmental protection
Welding performance

Daxun Alloy Let your brand improve rapidly

Delivery State Choice Surface Condition
Forged Black
Polished
Hot Rolled Black
Polished
Bright
Pickled
Cold Drawn Polished
Bright
Note:
1. If you require different deliver state than the above listed, kindly confirm with us.
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here.
Material in the solution annealed condition may be age hardened as follows:-*Denotes Double Overaged
Condition H900 (H480) H925 (H495) H1025 (H550) H1075 (H580) H1100 (H595) H1150 (H620) H1150M (H620M)* Plus H1150D (H620D)* Plus
Heat to ±15oF 900oF 925 oF 1025oF 1075oF 1100oF 1150oF 1400oF 1150oF 1150oF 1150oF
±9oC 480oC 495oC 550oC 580oC 595oC 620oC 760oC 620oC 620oC 620oC
Hold for Hours 1 4 4 4 4 4 2 4 4 4
Cool to Below Air Air Air Air Air Air Air Air Air Air
90oF (32oC)

Types of 2507/S32750 Stainless Steel Rods (6)

Information available for reference and download

Stainless Steel Rod Production

Daxun is a trustworthy stainless steel rod and bar manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless rod  are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 2507 Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

Recent hot case projects and products

2507/S32750 stainless steel rod
stainless steel rod
large diameter stainless steel rod
2507/S32750 stainless steel rod
Stainless Steel Polished rod
2507/S32750 bar
Stainless steel rod
stainless steel rod
Stainless steel rod
2507/S32750 stainless rod
Stainless steel precision rod
Stainless steel rod

Leading stainless steel rod and bar Suppliers in China


DUPLEX 2507 STAINLESS STEEL ROD AND BAR

  • Daxun Alloys Stainless Steels inventory currently contains Duplex 2507 Round Bar and Flat Bar, which isare available in both cold rolled and hot rolled forms. This super duplex stainless steel bar contains 25% chromium, 4% molybdenum and 7% nickel. The alloy is suitable for applications requiring high strength and corrosion resistance, such as chemical processing, petrochemical and seawater equipment. The steel has strong resistance to chloride stress corrosion cracking, good thermal conductivity and a low coefficient of thermal expansion. The high chromium, molybdenum and nickel content provides excellent resistance to pitting, crevice and general corrosion.

Applications

    • Oil and gas:
    • Offshore platforms, heat exchangers, water systems
    • Fire-fighting, injection, and ballast water systems
    • Chemical processing:
    • Heat exchangers, vessels, and piping
    • Desalination:
    • High-pressure RO systems and seawater piping
    • Mechanical and structural components:
    • High-strength, corrosion-resistant parts
    • Power industry:
    • FGD systems, scrubber systems, absorber towers
    • Ducting and piping
    • Export Destinations: Our 2507 stainless steel round bars are exported to various countries, including Costa Rica and South Korea, highlighting our global reach and the international demand for our high-quality products.

Standards

  • ASTM/ASME ………. A240 – UNS S32750
    EURONORM………… 1.4410 – X2 Cr Ni MoN 25.7.4
    AFNOR……………….. Z3 CN 25.06 Az

CORROSION RESISTANCE

General corrosion

SAF 2507™ exhibits excellent resistance to general corrosion. It is highly resistant to corrosion by organic acids. In 10% formic and 50% acetic acid, it experiences less than 0.05 mm/year. This outperforms ASTM 316L, which has a corrosion rate higher than 0.2 mm/year. SAF 2507™ remains resistant even in contaminated acids (see Figures 5 and 6).

  • 6825b rev 1.png

Figure 4. Isocorrosion diagram in formic acid. The curves represent a corrosion rate of 0.1 mm/year (4 mpy) in stagnant test solution.

  • 6967b rev 1.png

Figure 5. Corrosion rate of various alloys in 80% acetic acid with 2000 ppm chloride ions at 90°C.

  • 6968b rev 1.png

Figure 6. Corrosion rate of various alloys in concentrated acetic acid with 200 ppm chloride ions.

SAF 2507™ exhibits excellent resistance to general corrosion. It is highly resistant to corrosion by organic acids. In 10% formic and 50% acetic acid, it experiences less than 0.05 mm/year. This outperforms ASTM 316L, which has a corrosion rate higher than 0.2 mm/year. SAF 2507™ remains resistant even in contaminated acids (see Figures 5 and 6).

 

  • 6827b-rev 1.png

Figure 7. Isocorrosion diagram in naturally aerated sulfuric acid. The curves represent a corrosion rate of 0.1 mm/year (4 mpy) in a stagnant test solution.

  • 6826b-rev 1.png

Figure 8. Isocorrosion diagram, 0.1 mm/year (4 mpy) in a naturally aerated sulfuric acid containing 2000 ppm chloride ions.

Figure 9. Isocorrosion diagram in hydrochloric acid. The curves represent a corrosion rate of 0.1 mm/year (4 mpy) in stagnant test solution.

 

SAF 2507™ excels in resisting inorganic acids, often surpassing high-alloy austenitic stainless steels. Isocorrosion diagrams reveal its strength against sulfuric and hydrochloric acids. The alloy thrives in terephthalic acid plants, proving its exceptional resistance. It offers a competitive edge over high-alloyed austenitics and nickel alloys. In environments where standard austenitic stainless steels falter, SAF 2507™ stands strong. Its performance in harsh chemical settings makes it a top choice. Industries dealing with corrosive acids find SAF 2507™ to be a reliable solution. The alloy’s versatility shines in various concentration ranges of inorganic acids.

To ensure the highest quality, all products undergo rigorous testing and third-party inspection before packaging.

Pitting and crevice corrosion

 

Stainless steel’s resistance to pitting and crevice corrosion hinges on key elements. Chromium, molybdenum, and nitrogen content significantly impact its performance. The manufacturing process plays a vital role in corrosion resistance. Welding and other fabrication methods can affect the steel’s durability. SAF 2507™’s composition is optimized for superior corrosion resistance. Its high alloy content ensures robust protection against localized corrosion. Proper manufacturing techniques enhance the material’s service life. In challenging environments, SAF 2507™ stands out for its resilience.

The PRE (Pitting Resistance Equivalent) number is a parameter used to compare the resistance to pitting in chloride environments. It is defined as PRE = %Cr + 3.3 x %Mo + 16 x %N (in weight-%). In duplex stainless steels, the pitting corrosion resistance is determined by the PRE value in both the ferrite and austenite phases. The phase with the lowest PRE value limits the actual pitting corrosion resistance. SAF 2507™ has been carefully balanced to achieve equal PRE values in both phases.

SAF 2507™ seamless tubes boast a minimum PRE value of 42.5. This surpasses other 25Cr duplex steels, like UNS S31260, significantly. The ASTM G48 test rigorously evaluates pitting and crevice corrosion resistance. It exposes steel to harsh 6% FeCI3 solutions, with and without crevices. A modified version increases temperature until pitting occurs. Figure 11 displays critical pitting and crevice temperatures from this test. Potentiostatic tests reveal performance in varied chloride and acidic environments. These tests use high potentials, exceeding typical seawater conditions. As a result, critical temperatures are lower than in most practical applications. SAF 2507™ consistently demonstrates superior corrosion resistance in these demanding tests.

  • 6247b-rev 1.png

Figure 10. Critical pitting and crevice temperatures in 6% FeCl3, 24h (similar to ASTM G48).

SAF 2507™ and 6Mo+N show similar pitting resistance in 6% FeCl3. Tests in natural seawater evaluated critical crevice corrosion temperatures. The potential applied was 150 mV vs SCE, with temperature increases every 24 hours. Results are presented in the accompanying table. Crevice corrosion propagation rates were also measured at different temperatures. SAF 2507™ demonstrated remarkably low propagation rates compared to 6Mo+N alloy. Its rates were approximately ten times lower, showcasing superior corrosion resistance. This performance highlights SAF 2507™’s effectiveness in challenging marine environments. The data underscores its suitability for applications requiring exceptional corrosion resistance.

Alloy CCT (°C)
SAF 2507 64
6Mo+N 61

In these tests the propagation rates of initiated crevice corrosion attacks, at 15-50°C (59-122°F) and an applied potential of 150 mV vs SCE were also determined. These were found to be around ten times lower for SAF™ 2507 than for the 6Mo+N alloy.

  • 6185b-rev 1.png

Figure 11. Critical pitting temperatures (CPT) at varying concentrations of sodium chloride, from 3 to 25%

The CPT values were determined potentiostatically at +600 mV SCE with surfaces ground using 600 grit paper.

  • 6828bcyan-rev 1.png

Figure 12 illustrates the critical pitting temperatures (CPT) in 3% NaCl solution with varying pH levels. These values were also determined potentiostatically at +600 mV SCE with surfaces ground using 600 grit paper.

SAF 2507™ showcases exceptional corrosion resistance in oxidizing chloride solutions. Tests in ‘Green death’ and ‘Yellow death’ solutions reveal its strength. The table presents critical pitting temperatures (CPT) for various alloys. SAF 2507™’s performance matches that of nickel alloy UNS N06625. This data correlates well with alloy rankings for reheater tubes. Flue gas desulfurization systems benefit from such corrosion-resistant materials. The test results highlight SAF 2507™’s versatility in harsh chemical environments. Its high CPT values indicate superior protection against pitting corrosion. This makes SAF 2507™ a top choice for demanding industrial applications. The alloy’s resistance to these aggressive solutions is truly impressive.

Alloy Critical pitting temperature (CPT), °C
‘Green death’
‘Yellow death’
SAF™ 2507 72.5 >90
6Mo+N 70 >90
UNS N06625 67.5 >90
ASTM 316 <25 20

Stress corrosion cracking

SAF 2507™ shows remarkable resistance to chloride-induced stress corrosion cracking (SCC). Figure 13 displays its performance in high-temperature chloride solutions. The alloy resists SCC in up to 1000 ppm Cl⁻ at 300°C. It also withstands 10000 ppm Cl⁻ at 250°C without cracking. U-bend tests in hot brine further prove its durability. SAF 2507™ maintains integrity in 40% CaCl₂ at high temperatures. Its threshold stress exceeds 90% of tensile strength for both base metal and welds. Figure 14 reveals its superiority in acidified conditions compared to SAF 2205™. Even in boiling 45% MgCl₂, SAF 2507™ retains half its proof strength. These results underscore SAF 2507™’s exceptional SCC resistance across various harsh environments, partly due to its low thermal expansion.

  • 6877b-rev 1.png

Figure 13. SCC resistance in oxygen-bearing (abt. 8 ppm) neutral chloride solutions. Testing time 1000 hours. Applied stress equal to proof strength at testing temperature.

  • 6139bcyan-rev 1.png

Figure 14. Results of SCC tests with constant load in 40% CaCl2, pH=1.5, at 100 °C (210°F) with aerated test solution.

  • 6140b-rev 1.png

Figure 15. Constant load SCC tests in NACE solution at room temperature (NACE TM 0177).

Figure 13 highlights SAF 2507™’s stress corrosion cracking resistance in oxygen-rich chloride solutions. Tests ran for 1000 hours under high stress conditions. The alloy demonstrated impressive resilience across various temperatures and chloride concentrations. Figure 14 showcases SAF 2507™’s performance in acidic, hot calcium chloride. These tests reveal the alloy’s strength in harsh chemical environments. Figure 15 presents results from NACE solution tests at room temperature. SAF 2507™ showed no signs of cracking, regardless of applied stress. This exceptional performance underscores its suitability for demanding applications. The data consistently proves SAF 2507™’s superior resistance to stress corrosion cracking. These results make SAF 2507™ a top choice for industries facing corrosive challenges.

Hydrogen sulfide environments pose unique challenges for stainless steels. SAF 2507™ shows resilience in these conditions below 60°C (140°F). Acidity and chloride content influence the corrosivity of such solutions. Interestingly, ferritic stainless steels are more vulnerable than austenitic types. ISO 15156/NACE MR 0175 approves SAF 2507™ for sour environments. It’s suitable for oil and gas production up to 450°F (232°C). This applies when hydrogen sulfide partial pressure stays below 3 psi (0.20 bar). For sour petroleum refining, SAF 2507™ meets NACE MR0103 standards. The alloy must be solution annealed, rapidly cooled, and maintain a maximum hardness of 32 HRC. These specifications highlight SAF 2507™’s versatility in challenging industrial applications.

Hydrogen Induced Stress Cracking (HISC)

Hydrogen Induced Stress Cracking (HISC) poses a risk in subsea environments. It affects cathodically protected steel structures under high tensile stress. SAF 2507™, when connected to protected carbon steels, may face HISC risks. Low electrochemical potentials generate atomic hydrogen on steel surfaces. This hydrogen can diffuse into the metal, causing embrittlement. Ferrite phases in super duplex steels allow faster hydrogen diffusion. This makes SAF 2507™ more susceptible to HISC than austenitic steels. High mechanical stress exacerbates the problem. It increases hydrogen diffusion and crack propagation. Understanding these factors is crucial for safe subsea applications. Proper design and stress management can mitigate HISC risks in SAF 2507™ installations.

Super duplex stainless steels show unique HISC behavior. Cracks in SAF 2507™ propagate through the embrittled ferrite phase. They typically stop at ferrite-austenite boundaries. Austenite spacing plays a crucial role in HISC susceptibility. Coarser grains increase the risk of cracking. DNV RP-F112 recommends austenite spacing below 30 μm. Alleima’s tests confirm this reduces HISC tendency. Cold pilgered and solution annealed tubes perform exceptionally well. With 5-15 μm austenite spacing, they resist HISC up to 130% yield strength. Figure 16 shows how austenite spacing affects acceptable stress levels. This data helps engineers design safer subsea structures using SAF 2507™. Proper processing ensures optimal microstructure for HISC resistance.

 

HISC spacing

The acceptable stress without HISC occurring for products with different austenite spacing is illustrated in figure 16.

Intergranular corrosion

SAF 2507™ shows excellent resistance to intergranular corrosion. Its balanced composition allows quick austenite reformation in weld-affected zones. This microstructure ensures strong corrosion resistance. The alloy passes the ASTM A262 Practice E (Strauss test) without issues.

Erosion corrosion

SAF 2507™ excels in erosion corrosion resistance. Its mechanical properties and corrosion resistance contribute to this strength. Tests in sand-containing media prove its superiority over austenitic stainless steels. Figure 17 compares mass loss rates of different alloys. SAF 2507™ outperforms SAF 2205™ and 6Mo+N austenitic steel. These tests used synthetic seawater with silica sand at various velocities. The results highlight SAF 2507™’s durability in erosive environments. This makes it ideal for applications facing both corrosion and erosion challenges.

6830bcyan-rev 1.png

Figure 17. Relative mass loss rate after testing of the resistance against erosion corrosion.

Corrosion fatigue

SAF 2507™ demonstrates exceptional resistance to corrosion fatigue. Its high tensile strength contributes to an impressive fatigue limit. The alloy excels in both standard fatigue and corrosion fatigue scenarios. SAF 2507™’s superior mechanical properties explain its high fatigue strength. Rigorous testing in corrosive environments confirms its corrosion fatigue resistance. This dual strength makes SAF 2507™ ideal for cyclically loaded structures. Industries dealing with harsh, corrosive conditions benefit from its resilience. The alloy’s performance ensures longer service life in demanding applications. SAF 2507™ stands out among duplex stainless steels for its fatigue resistance.

PROCESSING

2507 super duplex stainless steel can be processed using both hot and cold forming techniques. Each method requires specific considerations to ensure optimal results.

Hot Forming: 2507 can be hot formed at temperatures between 1875°F and 2250°F. After hot forming, a solution anneal should be performed at a minimum temperature of 1925°F. This is followed by a rapid air or water quench to maintain the desired properties.

Cold Forming: Cold working of 2507 super duplex steel is possible using most typical stainless steel forming processes. However, due to its higher yield strength and lower ductility compared to austenitic steels, some adjustments may be necessary. Due to its low thermal expansion, 2507 super duplex steel maintains dimensional stability during cold forming processes.

Fabricators may need to use higher forming forces, larger bend radii, and allow for greater springback when cold forming 2507. Deep drawing, stretching, and other similar processes are more challenging for 2507 than for austenitic stainless steels.

When the forming process requires more than 10% cold deformation, solution annealing and quenching are recommended to restore the material’s properties.

Heat TreatmentHeat treatment for 2507 consists of solution annealing and quenching after hot or cold forming. Solution annealing should be performed at a minimum temperature of 1925°F. Annealing should be followed immediately by a rapid air or water quench. Heat treated items that are pickled and rinsed have excellent corrosion resistance. Savoy Piping Inc. is a leading supplier of 2507 Super Duplex Round Bars, known for their high quality and excellent customer service.

Welding2507 is weldable and can be joined to other materials using SMAW, GTAW, PAW, FCW, or SAW. When welding 2507, a 2507/P100 filler metal is recommended to ensure proper duplex weld construction.

2507 does not require preheating except to prevent condensation on cold metal. Interpass welding temperatures should not exceed 300°F or weld integrity will be compromised. To maximize corrosion resistance, root protection should be applied using either argon or 90% N2/10% H2 purge gas. The latter provides higher corrosion resistance.

2507-S32750 grade stainless steel round bars

Stainless steel round bars can be easily ordered in a wide range of sizes. Simply select the grade of steel you require and we will provide bars in lengths ranging from 500mm to 6 meters, and diameters ranging from 3mm to 500mm. We even give you the option of ordering in metric or imperial sizes. If you want something that is not a standard size, that’s no problem. We offer unlimited free cuts to length. Using state-of-the-art bandsaws to ensure accuracy and repeatability, we can precisely meet your requirements every time. Just let us know when ordering.

Wide Range of Sizes to Choose From

Daxun Alloys offers an extensive selection of stainless steel round bar sizes. Choose your preferred grade and customize your order. We provide lengths from 500mm to 6 meters. Diameters range from 3mm to 500mm. You can order in metric or imperial units for your convenience. Need a non-standard size? No problem. We offer unlimited free cuts to length. Our state-of-the-art bandsaws ensure precise, repeatable results. We’ll meet your exact specifications every time. Just specify your requirements when ordering. Daxun’s flexibility caters to diverse project needs. Our cutting service saves you time and effort. Experience hassle-free ordering with Daxun Alloys’ custom sizing options.

Contact Your Stainless Steel Round Bar Supplier

Daxun Alloy is your go-to supplier for top-quality stainless steel round bars. We cater to both one-time orders and long-term inventory plans. Our diverse grade selection meets various manufacturing needs. Power your production with Daxun’s superior metal solutions. Ordering is easy through our user-friendly website. Prefer personal assistance? Call our sales team at +8613382898899. For inquiries, email us at [email protected]. Our team ensures prompt responses. We’re ready to tailor solutions to your specific requirements. Choose Daxun for reliability, quality, and customer-focused service. Contact us today to elevate your manufacturing process with premium stainless steel round bars.

Can I get some samples?

We can provide 2507 Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

What is your MOQ?

Our MOQ is 1 ton for 2507 Stainless Steel Rod.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.

Send Your Inquiry Today
Quick Quote