304/304L/304LN Stainless steel bars and round bars China supplier
As a leading stainless steel supplier and exporter in China, Daxun supplies stainless steel barsRod (Round Bar) all over the world.
- Good machinability
- Excellent corrosion resistance
- Excellent forming and welding properties
- Relatively susceptible to stress cracking corrosion (SCC)
- Medium strength, ductility, hardness and toughness stability
- The most common variant, used in almost all applications
A global leader in stainless rod and Round Bar fabrication services
304 Stainless Steel Bar (ASTM A276) 304 Stainless Steel Round Bar, SS UNS S30400 Bright Bar, 304 Austenitic Stainless Steel Bar Suppliers and Manufacturers in China. Daxun Alloys’ stainless steel bars meet the standards of ASTM A276 (Standard Specification for Stainless Steel Bars and Shapes), and the majority of sizes meet ASTM A484 (Standard Specification for General standards for Stainless Steel Bars, Billets, and Forgings). The diameters meet the criteria of ISO 683/13. All supplied materials come with test certificates in line with ASTM A276 standards. Daxun Alloys supplies stainless steel bars that meet the AS2837-1986 specification.
Our network of service centers stocks stainless steel bar products for a fast, ready supply of bars in common sizes and alloys.We also produce custom-sized stainless steel rods and can arrange inventory schedules for quick turnaround promptly if quantities are below factory minimums—Daxun Alloys stocks stainless steel round bars with diameters ranging from 1/16″ to 26″. Round bars are available in nearly every grade of stainless steel, including 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205, and Alloy 20. Heat-treated stainless steel round bars are offered in 17-4PH, H900 temper (on request), H1025, H1150, Double H1150, and H1150M. Other heat-treated tempers can be manufactured upon request. We stock the following 400 series stainless steels: 410, 430, and 416. We also carry 303, 304, and 316/L precision and bearing quality stainless steel round bars. Most of our inventory consists of our unique machined bar grades: stainless steel round bars that are melted to consistent standards to increase machinability and lower total cost per component. Our stainless steel bar processing machinery allows Daxun Alloys to produce to our customers’ exact specifications.
Data
- Parameter
- Ingredients
- Mechanical Properties
- All equivalent
- Types
Product Parameters: Stainless Steel rod | |
Specifications | ASTM A276, ASME SA276 / ASTM A479 ASME SA479 |
Dimensions | EN, DIN, JIS, ASTM, BS, ASME, AISI |
SS 304 Round Bars | Outside Diameter in the range of 4mm to 500mm |
SS 304 Bright Bars | Outside Diameter in the range of 4mm to 100mm |
SS 304 Hex Bars | 18mm – 57mm (11/16″ to 2-3/4″) |
Finish | Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
Length | 1 to 6 Meters, Custom Cut Lengths |
Form | Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc. |
Composition of 304/304L/304LN/304H rod and bar | ||||
Grade | 304 | 304L | 304LN | 304H |
UNS Designation | S30400 | S30403 | S30453 | S30409 |
Carbon (C) Max. | 0.08 | 0.030* | 0.03 | 0.04 – 0.10 |
Manganese (Mn) Max. | 2 | 2 | 2 | 2 |
Phosphorous (P) Max. | 0.045 | 0.045 | 0.045 | 0.045 |
Sulphur (S) Max. | 0.03 | 0.03 | 0.03 | 0.03 |
Silicon (Si) Max. | 1 | 1 | 1 | 1 |
Chromium (Cr) | 18.0–20.0 | 18.0–20.0 | 18.0–20.0 | 18.0–20.0 |
Nickel (Ni) | 8.0–11.0 | 8.0–11.0 | 8.0–11.0 | 8.0–11.0 |
Molybdenum (Mo) | — | — | — | — |
Nitrogen (N) | — | — | 0.10–0.15 | — |
Iron (Fe) | Bal. | Bal. | Bal. | Bal. |
Other Elements | — | — | — | — |
Tensile Strength | Yield Strength | |||||||||||||
Alloy | UNS Designation | Spec. | psi | MPa | ksi | psi | MPa | ksi | Elongation in 2 inches (min.) % | Grain Size Req. | Max. Hardness | Modulus of Elasticity (x106 psi) | Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) | Thermal Conductivity (BTU-in/ft2-h-°F) |
304 | S30400 | A249, A312 | 75,000 | 515 | 75 | 30,000 | 205 | 30 | 35 | — | 90 Rb | 28 | 9.2 | 116 |
304L | S30403 | A270 A312 | 70,000 | 485 | 70 | 25,000 | 170 | 25 | 35 | — | 90 Rb | 28 | 9.2 | 116 |
304LN | S30453 | A249, A688 | 75,000 | 515 | 75 | 30,000 | 205 | 30 | 35 | — | 90 Rb | 28 | 9.2 | 116 |
304H | A30409 | A249, A312 | 75,000 | 515 | 75 | 30,000 | 205 | 30 | 35 | 7 or coarser | 90 Rb | 28 | 9.2 | 116 |
Alloy | UNS Designation | Werkstoff NR. | Specifications* |
304 | S30400 | 1.4301 | A269, A/SA249, A/SA312, A632, A/SA688, A270 |
304L | S30403 | 1.4306 | A269, A/SA249, A/SA312, A629, A632, A/SA688, A270 |
304LN | S30453 | 1.4311 | A/SA249, A/SA688 |
304H | S30409 | 1.4948 | A269, A/SA249, A/SA312, A/SA688 |
*Note: The specifications noted including ASTM, ASME, or other applicable authorities are correct at the time of publication. Other specifications may apply for use of these materials in different applications. |
Stainless Steel 304 Bright Bar | SS 304 Bright Bar |
304 SS Bright Bar | |
Stainless Steel 304 Bright Bar | |
UNS S30400 SS Bright Bar | |
WERKSTOFF NR. 1.4301 Bright Bar | |
ASTM A276 304 Stainless Steel Bright Bar | |
Stainless Steel 304 Hex Bar | SS 304 Hex Bar |
304 SS Hexagonal Bar | |
304 Stainless Steel Hex Bar | |
UNS S30400 SS Hexagonal Bar | |
ASTM A276 304 Stainless Steel Hex Bar | |
Stainless Steel 304 Square Bar | SS 304 Square Bar |
304 SS Square Bars | |
304 Stainless Steel Square Bar | |
UNS S30400 SS Square Bar | |
WERKSTOFF NR. 1.4301 Square Bar | |
ASTM A479 304 Stainless Steel Square Bars | |
Stainless Steel 304 Rectangular Bar | SS 304 Rectangular Bar |
304 SS Rectangular Bars | |
304 Stainless Steel Rectangular Bar | |
UNS S30400 SS Rectangular Bars | |
WERKSTOFF NR. 1.4301 Rectangular Bar | |
ASTM A276 304 Stainless Steel Rectangular Bar | |
Stainless Steel 304 Flat Bars | SS 304 Flat Bar |
304 SS Flat Bars | |
304 Stainless Steel Flat Bars | |
UNS S30400 SS Flat Bars | |
WERKSTOFF NR. 1.4301 Flat Bars | |
ASTM A276 304 Stainless Steel Flat Bars | |
Stainless Steel 304 Polished Bar | SS 304 Polished Bar |
304 SS Polished Bars | |
304 Stainless Steel Polished Bar | |
UNS S30400 SS Polished Bars | |
WERKSTOFF NR. 1.4301 Polished Bar | |
ASTM A476 304 Stainless Steel Polished Bar | |
Stainless Steel 304 Threaded Bar | SS 304 Threaded Bar |
304 SS Threaded Bars | |
304 Stainless Steel Threaded Bar | |
UNS S30400 SS Threaded Bar | |
WERKSTOFF NR. 1.4301 Threaded Bar | |
ASTM A276 304 Stainless Steel Threaded Bar |
Choose Daxun and make your customers satisfied
Quick response-304 Stainless Steel Rod
We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Advantages
- Varieties: We offer a wide range of sizes and grades, including 300 series, 400, 600 series, and more.
- Flexibility: Whether you need hot-rolled or cold-drawn bars, our stainless steel bar lengths are designed to meet your specific project requirements.
- Quality Standards: Our 304 Stainless Steel Rod meets strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
- Custom Orders: Looking for special sizes of stainless steel bars? We offer a variety of stainless steel bar customization options with competitive prices and convenient online ordering.
304 Stainless Steel Rod packaging
We pay close attention to every step to make sure everything’s top quality. We usually pack our 304 stainless steel round bars in eco-friendly poly bags, then put them in fumigation-free wooden cases or on wooden pallets. We’re also happy to do custom packaging, like OEM, if we work it out together. We can basically handle any packing you need for your 304 stainless steel round bars. We put a lot of effort into making sure the packing is done right. The AISI 304 round bars are packed in wooden boxes with corrugated cardboard, wrapped in plastic and bubble wrap.
Quality, delivery, inspection
- Daxun ensures the quality of its products by running them through various tests. These include checks for flattening, pitting resistance, mechanical performance, and hardness, as well as material identification and expansion tests, among others. This thorough testing guarantees that each product meets the standards needed for your project.
- Throughout production, we meticulously measure the diameter, thickness, and surface of each item to maintain precision. Orders are typically shipped within 7 to 15 days, though custom sizes might take a bit longer—up to 20 days—to ensure they meet your specifications.
Our delivery time is strictly in accordance with the contract. - Support customer third-party agencies to go to the factory for inspection
- Support free samples to customers for testing
- Support on-site or video factory inspection
Technical Support
If you need extra technical support, our in-house metallurgist and experienced team are ready to assist. Plus, Daxun is proud to have a certified testing lab—a groundbreaking achievement in the multi-metal and plastic inventory industry. We believe this highlights our commitment to quality and reflects our approach as a reliable, full-service supplier.
304 Stainless Steel Rod Ordering Information
The purchase order shall include quantity, PSL grade, type or category, API5L reference, diameter, finish, length and any applicable attachments or additional requirements relating to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish, or end finish. Bars are solution bright annealed.
304 Stainless Steel Rod Features
Daxun Alloy Let your brand improve rapidly
- Gallery
- Delivery State
- Age Hardening
Delivery State Choice | Surface Condition |
Forged | Black |
Polished | |
Hot Rolled | Black |
Polished | |
Bright | |
Pickled | |
Cold Drawn | Polished |
Bright | |
Note: | |
1. If you require different deliver state than the above listed, kindly confirm with us. | |
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here. |
Material in the solution annealed condition may be age hardened as follows:-*Denotes Double Overaged | ||||||||||||
Condition | H900 (H480) | H925 (H495) | H1025 (H550) | H1075 (H580) | H1100 (H595) | H1150 (H620) | H1150M (H620M)* | Plus | H1150D (H620D)* | Plus | ||
Heat to | ±15oF | 900oF | 925 oF | 1025oF | 1075oF | 1100oF | 1150oF | 1400oF | 1150oF | 1150oF | 1150oF | |
±9oC | 480oC | 495oC | 550oC | 580oC | 595oC | 620oC | 760oC | 620oC | 620oC | 620oC | ||
Hold for Hours | 1 | 4 | 4 | 4 | 4 | 4 | 2 | 4 | 4 | 4 | ||
Cool to Below | Air | Air | Air | Air | Air | Air | Air | Air | Air | Air | ||
90oF (32oC) |
Types of 304 Stainless Steel Rods (3)
Information available for reference and download
Daxun is a trustworthy stainless steel rod and bar manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all 304 Stainless Steel Rod are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the s304 Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
Recent hot case projects and products
Related Products (10)
Leading stainless steel rod and bar Suppliers in China
GENERAL PROPERTIES
- 304/304L Stainless Steel Rod alloy is an upgraded version of regular 304/304L that has been treated for better machinability and uniformity. This alloy will machine faster, with longer tool life, higher part quality, and lower overall cost of machined parts. 304/304L Stainless Steel Rod is not magnetic when annealed, but may be slightly magnetic after cold working or welding.
- Specifications: UNS S30400, UNS S30403
APPLICATIONS:
DAUXN 304/304L Stainless Steel Rods are versatile and commonly used in a wide range of residential and commercial applications, including:
- Chemical process equipment
- Food and beverage industry
STANDARDS:
- ASTM/ASME: UNS S30400 / S30403
- EURONORM: 1.4301 / 1.4307
CORROSION RESISTANCE:
- DAXUN 304/304L stainless steel bar is a really versatile, all-purpose stainless steel that holds up well against corrosion from the weather, lots of different chemicals (both organic and inorganic), and even food and drinks.
- It is also used in vacuum processing equipment and specialized instruments where high integrity is critical.
HEAT RESISTANCE:
- Good oxidation resistance in intermittent use to 1600°F and continuous use to 1690°F.
Continuous use of 304 round bars in the 800-1580°F range is not recommended if subsequent aqueous corrosion resistance is important.
WELDING CHARACTERISTICS:
- readily welded by a full range of conventional welding procedures except oxyacetylene.
- AWS E308L/ ER308L filler metal should be used with Prodec 304/304L steel.
MACHINABILITY:
- Gives you faster machining, longer-lasting tools, better quality parts, and a lower overall cost for machined parts.
VALUE-ADDED SERVICES
- In order to meet the exact specifications you require for your stainless steel rods, Daxun can provide the following value-added services.
HEAT TREATING & ANNEALING
- Daxun can heat treat some of our 400 series stainless steel bars. Heat treatment can cause stress because of the hardening process, depending on the metal’s makeup. We also use heat treating for tempering, quenching, normalizing, and solution annealing.
POSITIVE MATERIAL IDENTIFICATION (PMI)
- Sometimes, we might need to do extra material testing to be absolutely sure of what we’re working with. Daxun can do this in our own lab, or we can team up with an independent lab. Get in touch if you have specific requirements.
UT TESTING
- Ultrasonic Testing (UT) uses high-frequency sound waves to check and measure the stainless steel. This helps us find and assess any flaws and take accurate measurements.
Stainless Steel Round Bars are produced to the right size by Daxun
With high-quality products and free unlimited cutting service, Daxun Alloys has become the preferred supplier of stainless steel round bars for domestic and foreign customers. Order stainless steel round bars online or by phone and they can be shipped in as fast as 3-5 days.
304 and 304L grade stainless steel round bars
Stainless steel round bars are used everywhere—from construction to car parts. Because they’re so versatile, Daxun Alloys offers them in lots of different grades and sizes. And with our free precision cutting service, we can always get you exactly what you need.
Stainless steel round bars are available in a variety of grades. The most common grade 304 has easy weldability, good formability and corrosion resistance. Grade 316 has excellent corrosion resistance and is well suited to harsh environments such as salt water or highly industrialized areas. Like grade 304, it is also easy to weld, but it is more difficult to process. Finally, grade 303 is easier to process, drill and cut than other grades. However, it is less suitable for welding than grades 304 and 316.
Wide Range of Sizes to Choose From
Ordering stainless steel round bars is easy—we have tons of sizes available. Just pick the steel grade you need, and we can provide bars in lengths from 500mm to 6 meters and diameters from 3mm to 500mm. You can even order in metric or imperial measurements.
If you want something that is not a standard size, that’s no problem. We offer unlimited free cuts to length. Using state-of-the-art bandsaws to ensure accuracy and repeatability, we can precisely meet your requirements every time. Just let us know when ordering.
Connect with your local stainless steel round bar supplier
Ordering stainless steel round bars is simple. Our website provides a simple step-by-step process. Alternatively, you can call our sales team at +8613382898899. If you have any questions, please email us at [email protected] and our team will get back to you as soon as possible.
We can provide 304 Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.
We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.
Our MOQ is 1 ton for 304 Stainless Steel Rod.
Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.