Daxun 310-310S-S31008 stainless steel PIPE and TUBE China supplier

As China’s leading Stainless Steel pipe and tube supplier and exporter, Daxun provides stainless steel PIPEs to the world.
  • Grade: AISI 310S/310-S31008
  • Manufacturing: hot-rolled, cold-drawn, forged, welded
  • Standards: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Type: general seamless steel pipe
  • Diameter: from small diameter to large diameter pipe
  • Thickness: thin-walled pipe and thick-walled pipe
  • Surface: pickled AP, polished, bright EP, annealed BA, etc.
  • Length: 3000mm, 6000mm, 9000mm, etc.

Global leader in stainless steel pipe and tube fabrication services

ASTM A312 / A358 Stainless Steel 310 Pipe Supplier, 310S Stainless Steel Seamless Pipe, Call us for ASME SA312 310 Stainless Steel Pipe.

310s grade stainless steel pipes are commercially used in various industries due to their high temperature operation and corrosion resistance in various environmental conditions. 310s grade stainless steel pipes are low carbon alloys that provide temporary operating values ​​up to 1050 degrees Celsius in intermittent services. Daxun Alloys is one of the leading producers, suppliers and stockists of 310s grade stainless steel pipes.

310S Stainless Steel Seamless Pipe | 310S Stainless Steel Seamless Pipe | 310S Stainless Steel ERW Pipe | 310S Stainless Steel EFW Pipe | 310S Stainless Steel Welded Pipe and Tube (Conforming to ASTM A213 / A312 / A269 / A358 Standards)

Type 310S is a low carbon austenitic stainless steel. Type 310S is a low carbon version of Type 310 and is noted for its ability to tolerate high temperature applications. The 310S alloy, like 309S, is best suited for high temperature applications. Both alloys function well in temperatures up to 2000°F, especially where oxidation resistance is necessary. 309 and 310S are the best high temperature performance of the typical stainless grades in our collection. 310S stainless steel has strong corrosion resistance and resists carburization, oxidation, and other conditions. It delivers good performance in industrial grade high temperature situations where great resistance to carburization and thermal cycling corrosion is required. It remains austenitic throughout the full temperature range and does not get embrittled. Its great strength and high temperature oxidation resistance make it valuable in commercial incinerators, kilns and food processing equipment.

Read More

Data

Stainless Steel 310 Specification Stainless Steel 310 / 310S, ASTM A312 Stainless Steel
SS UNS S31008 Pipe 310s Stainless Steel Pipe
ASTM A312 TP 310 – 310S SS Seamless Pipe Size 4 to 510mm W. T.: 0.5 to 50mm
WERKSTOFF NR. 1.4841 Welded Pipe Size 5.0 mm – 1219.2 mm
ASTM A312 TP 310 – 310S Stainless Steel EFW Pipe size 5.0 mm – 1219.2 mm
Stainless Steel WERKSTOFF NR. 1.4841 Pipe Swg & Bwg 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg.
310 – 310S Stainless Steel Pipe Schedule SCH5, SCH10, SCH10S, SCH20, SCH30, SCH40, SCH40S, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
SS UNS S31008 Swg & Bwg 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg.
310s Stainless Steel Tube wall thickness 0.020″ –0.220″, (special wall thicknesses available)
TP310 SS Length Single Random, Double Random, Standard & Cut length Pipe & Tube
ASTM A 358 SS 310 – 310S Finish Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF
ASTM A 312 SS 310 – 310S Form Round, Hydraulic, ‘U’ bent or Hollow,LSAW, Boiler, Straight Pipe, Clad Pipe, Rectangular, Square Pipe Etc
Stainless Steel 310 / 310S Type Welded, Seamless, ERW, EFW, Fabricated Pipe, ‘U’ bent or Hollow, Hydraulic, LSAW, Boiler, Straight Tube, Tube Coil, Round, Rectangular, Square Tube etc
TP310 SS End Plain End, Beveled End, Treaded Pipe
ASTM A312 TP 310 – 310S SS Marking All 310s Stainless Steel Pipe are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.)
SS TP310 – 310S Application Oil Pipe & Tube, Gas Pipe & Tube, Fluid Pipe & Tube, Boiler Pipe & Tube, Heat exchanger Tube
ASTM A312 Stainless Steel Value Added Service Draw & Expansion as per required Size & Length, Polish (Electro & Commercial) Annealed & Pickled Bending, Machining Etc.
Marking All 310s Stainless Steel tubes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.)
310s stainless steel tubing Testing & Inspection Visual inspection • Surface roughness measurement • Helium-leak testing • Scanning Electron Microscopy (SEM) • Auger Electron Microscopy (AES) • Election Spectroscopy for Chemical Analysis (ESCA or XPS) • Particle testing • Moisture testing
SS WERKSTOFF NR. 1.4841 Specialize in Alloy 310 / 310S Large Diameter Pipe
Stainless Steel 310 Capillary Tube
Stainless Steel 310S Heat Exchanger &
310 SS Condenser Tube
Stainless Steel 310S Test Certificate Manufacturer Test Certificate
Laboratory Test Certificate from Govt. Approved Lab.
Under Third Party Inspection
Manufacturers of 310 / 310S Stainless Steel Pipe TISCO stainless steel pipes
Baosteel stainless steel pipes
Qingshan stainless steel pipes
ATI stainless steel, USA
Tubacex Tubos Inoxidables S.A., Spain
Schoeller Bleckmann, Austria
Seah Steel Corporation, South Korea
(AS1449 / ASTM A240 – Flat Products)
Grade Carbon Manganese Silicon Phosphorus Sulphur Chromium Nickel
310 0.25 max 2.00 max 1.50 max 0.045 max 0.030 max 24.00 – 26.00 19.00 – 22.00
310S-S31008 0.08 max 2.00 max 1.50 max 0.045 max 0.030 max 24.00 – 26.00 19.00 – 22.00
Tensile Strength Yield Strength
Alloy UNS Designation Spec. psi MPa ksi psi MPa ksi Elongation in 2 inches (min.) % Grain Size Req. Maximum Hardness Modulus of Elasticity (x106 psi) Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) Thermal Conductivity(BTU-in/ft2-h-°F)
310S S31008 A249, A312 75,000 515 75 30,000 205 30 35 90 Rb 29 9.2 116
310H S31009 A249, A312 75,000 515 75 30,000 205 30 35 6 or coarser 90 Rb 29 9.2 116
Property At Value unit
Density 8,000 kg/m³
Melting Range 1400 – 1450 °C
Modulus of Elasticity 20°C 200 GPa
Shear Modulus 20°C 77 GPa
Poisson’s Ratio 20°C 0.3
Thermal Conductivity 100°C 14.2 W / m. °C
Electrical Resistivity 25°C 0.78 micro-ohm . m
Electrical Conductivity 25°C 1.25 % IACS
Specific Heat 500 J/kg. °C
Relative Magnetic Permeability 1.02
Coefficient of Expansion 0 – 100°C 15.9 /°C
0 – 315°C 16.2 /°C
0 – 540°C 17 /°C
Grade CHINA UNS No Old British Euronorm Swedish SS Japanese JIS GOST
BS En No Name
310S 00Cr25Ni20 S31008 304S31 58E 1.4845 X5CrNi18-10 2332 SUS 310S 20Ch23N18
ASTM A312 TP310S Elliptical and Oval Tubes TP310S Pipe
ASTM A213 TP310S Condenser Tube A312 TP 310S pipe
ASTM A269 TP310S straight tube boiler Grade 310S stainless steel pipe
Schedule 10 Type 310S Stainless Steel Pipe Schedule 40 Type 310S Stainless Steel Pipe
SA312 TP310S Seamless Tubing Polished 310S Stainless Steel Tubing
310S Stainless Steel Threaded Pipe SAE 30310S Stainless Steel Rectangular Tube
JIS SUS310S Seamless Tubes 310S SS Round Tube
SS 310S Welded Tubes Seamless pipe 310s
ASTM A312 TP310S Coiled Tubing Stainless Steel Inox 310S Capillary Tubing
ASTM A312 gr TP 310S Aerospace tubes 310S Stainless Steel Pipe
SA213 TP 310S Sighting Tube Type 310S Stainless Steel Polished Pipes
ASTM A249 TP310S Mirror Tube 310S Stainless Steel Seamless Pipe
UNS S31008 Pitot Tube stockist Stainless Steel 310S Seamless Round Tubing
ASTM A358 TP310S Polished Tubing 310S Stainless Steel Ornamental Tube
Stainless Steel 310S Exhaust Pipe 310S Stainless Steel Spiral Pipe
ASME SA213 TP310S Perforated Tube WERKSTOFF NR. 1.4841/1.4845 Flexible Tube
SA 688 TP310S Finned Tube S31008 Stainless Steel Dom Tube
S31008 Stainless Steel U Shaped Tube 310S Stainless Steel Square Tube Mirror Finish
Din 1.4841/1.4845 Material Vacuum Tube WERKSTOFF NR. 1.4841/1.4845 Coaxial Tube
Schedule 40 Type 310S Stainless Steel Pipe SS 310S Needle Tube
310S Stainless Steel Rectangular Pipe 310S Stainless Steel Hypodermic Tubing for Medical Needle
Ultra-High Purity Electropolished Stainless Steel 310S Tube Thin Wall Stainless Steel 310S Tube
Din 1.4841/1.4845 Stainless Steel Annealed Tubing Type 310S Stainless Steel Coil Tubing Heat Exchanger
SAE J405 Uns S31008 Thin Wall Tubing 310S Stainless Steel Metric Tubing
310S Stainless Steel Seamless Square Tubing Large Diameter 310S Stainless Steel Tube
310S Stainless Steel Lined Pipe Corrugated 310S Stainless Steel Tube (CSST) for Gas
Z6 Cn 18.09 Woven Mesh Tube SS 2332 Sweden Stainless Steel Hollow Section
1.4841/1.4845 X 5 Crni 18 10 Instrument Tubing 310S Stainless Steel Square Tubing
High-pressure 310S Stainless Steel Water Pipe Stainless Steel 310S Hexagonal Pipe
Jis 310S Stainless Steel Coil Tubing JIS SUS310S Pipe
Din 1.4841/1.4845 AISI 310S Perforated Exhaust Tube Stainless Steel 310S Hypodermic Tubing
Din W.-Nr. 1.4841/1.4845 Aisi 310S Corrugated Tube SS 310S Box Pipe
Material 1.4841/1.4845 Aisi 310S Slotted Pipe SS 310S Thin Wall Tube
En 1.4841/1.4845 / Aisi 310S Thick Wall Tube 310S Stainless Steel Threaded Pipe
Stainless Steel 310S Ornamental Pipe Stainless Steel 310S Fin Tube / Finned Tube

Choose Daxun and make your customers satisfied.

Contact Daxun now

310S Stainless Steel pipe Quick response

  • Improved resistance to cyclic oxidation
  • Improved resistance to sulfidation
  • Better high temperature strength
  • Improved resistance to intergranular corrosion
  • Good resistance to aqueous corrosion
  • Not susceptible to thermal fatigue and cyclic heating
  • Good strength up to 2100°
Contact Daxun now

310S Stainless Steel pipe Daxun Advantages

  • Variety: From small to large diameter stainless steel pipe, we offer a wide range of sizes and grades, including 304L, 316L, 317L ,321,310S,347,2205and more.
  • Flexibility: Whether you need seamless or welded steel pipe, our stainless steel pipe lengths are designed to meet your specific project requirements.
    Quality
  • Standards: Our stainless steel pipes meet stringent standards such as ISO9001, ABS, NSF/ANSI Standard 61, and NACE MR0175 to ensure reliability and performance.
  • Custom Orders: Looking for special size stainless steel pipes? We offer a variety of stainless steel pipe custom options at competitive prices and convenient online ordering.
Contact Daxun now

Steel tube packaging

  1. Woven bag bale cargo (hexagonal)
  2. Special crates for U-bend pipes, (steel/wood) divided
  3. Each bale is wrapped in plastic to protect against wind and rain.
  4. SS 310S seamless pipes are protected by plastic covers.
  5. Plastic strips are used to secure the bale.
  6. Export-specific fumigation-free wooden crate packaging.
  7. Laminated packing slip attached to the bale or crate.
  8. Customized packaging as per customer needs.
Contact Daxun now

310S Stainless Steel pipe Ordering Information

310S stainless steel pipe The purchase order shall include quantity, PSL grade, type or class, API5L reference, outside diameter, wall thickness, length and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Pipe is solution bright annealed.

Contact Daxun now

Quality, delivery, inspection

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    Our delivery time is strictly in accordance with the contract.
  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples to customers for testing
  • Support on-site or video factory inspection
Contact Daxun now

Technical Support

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

310/310S Stainless Steel pipe and tube Features

High strength
Corrosion resistance
Heat resistance
Low temperature resistance
Environmental protection
Welding performance

Daxun Alloy Let your brand improve rapidly

NPS Outside Diameter Wall Thickness Weight Weight
in mm in mm Sched kg/Mtr Lb/ft
1/2″ 0.84 21 0.109 2.769 40 STD 1.268 0.851
0.147 3.734 80 STD 1.621 1.088
3/4″ 1.05 27 0.113 2.87 40 STD 1.684 1.131
0.154 3.912 80 STD 2.195 1.474
1″ 1.315 33 0.133 3.378 40 STD 2.501 1.679
0.179 4.547 80 STD 3.325 2.172
1 1/4″ 1.66 42 0.14 3.556 40 STD 3.385 2.273
0.191 4.851 80 STD 4.464 2.997
1 1/2″ 1.9 48 0.145 3.683 40 STD 4.048 2.718
0.2 5.08 80 STD 5.409 3.361
2″ 2.375 60 0.154 3.912 40 STD 5.441 3.653
0.218 5.537 80 STD 7.48 5.022
2 1/2″ 2.875 73 0.203 5.516 40 STD 8.629 5.793
0.276 7.01 80 STD 11.411 7.661
3″ 3.5 89 0.216 5.486 40 STD 11.284 7.576
0.3 7.62 80 STD 15.272 10.253
4″ 4.5 114 0.237 6.02 16.073 10.79
0.337 8.56 22.318 14.983
6″ 6.625 168 0.188 4.775 19.252 12.924
0.203 5.516 20.739 13.923
0.219 5.563 22.318 14.983
0.25 6.35 25.354 17.021
0.28 7.112 40 STD 58.263 18.974
0.312 7.925 31.334 21.036
0.375 9.525 37.285 25.031
0.432 10.973 80 XHY 42.561 28.573
0.5 12.7 48.719 32.708
8″ 8.625 219 0.188 4.775 25.233 16.94
0.203 5.156 27.198 18.259
0.219 5.563 29.286 19.661
0.25 6.35 20 33.308 22.361
0.277 7.036 30 36.786 24.696
0.322 8.179 40 42.352 28.554
0.375 9.525 49.216 33.041
0.406 10.312 60 53.085 35.638
0.5 12.7 80 XHY 64.627 43.388
10″ 10.75 273 0.188 4.775 31.588 21.207
0.219 5.563 36.689 24.631
0.25 6.35 20 41.759 28.035
0.307 7.798 30 51.002 34.24
0.344 8.738 56.946 38.231
0.365 9.271 40 STD 63.301 40.483
0.438 11.125 71.852 48.238
0.5 12.7 60 XHY 81.53 54.735
0.594 15.088 80 95.969 64.429
12″ 12.75 324 0.188 4.775 37.57 25.222
0.219 5.563 43.657 29.309
0.25 6.35 49.713 33.375
0.281 7.137 55.739 37.42
0.312 7.925 61.735 41.445
0.375 9.525 73.824 49.562
0.406 10.312 79.727 53.525
0.5 12.7 97.438 65.415
0.562 14.275 108.966 73.154
14″ 14 356 0.188 4.775 41.308 27.732
0.219 5.563 48.012 32.233
0.25 6.35 20 54.685 36.713
0.281 7.137 61.327 41.172
0.312 7.925 67.939 45.611
0.375 9.525 STD 81.281 54.568
0.438 11.125 40 94.498 63.441
0.5 12.7 XHY 107.381 72.09
0.625 15.875 132.983 89.278
16” 16 406 0.188 4.775 47.29 21.748
0.219 5.563 54.98 36.91
0.25 6.35 10 62.639 42.053
0.281 7.137 70.268 47.174
0.312 7.925 20 77.866 52.275
0.344 8.738 85.677 57.519
0.375 9.525 30 93.213 62.578
STD
0.438 11.125 108.433 72.797
0.5 12.7 40 123.289 82.77
XHY
18″ 18 457 0.219 5.563 61.948 41.588
0.25 6.35 70.593 47.393
0.281 7.137 79.208 53.176
0.312 7.925 20 87.792 58.939
0.375 9.525 STD 105.144 70.588
0.438 11.125 30 122.369 82.152
0.5 12.7 XHY 139.198 93.45
0.562 14.275 40 155.904 104.666
0.625 15.875 172.754 115.978
20″ 20 508 0.25 6.35 78.547 52.733
0.282 7.163 88.458 59.386
0.312 7.925 97.719 65.604
0.375 9.525 20 STD 117.075 78.598
0.438 11.125 136.305 91.508
0.5 12.7 30 XHY 155.106 104.13
0.594 15.088 40 183.378 123.11
0.625 15.875 192.64 129.328
0.688 17.475 211.368 141.901
24″ 24 610 0.25 6.35 94.456 63.413
0.281 7.137 106.029 71.183
0.312 7.925 117.573 18.932
0.375 9.525 20 STD 140.938 64.618
0.438 11.125 164.176 110.219
0.5 12.7 XHY 186.923 125.49
0.625 15.875 232.41 156.028
0.688 17.475 40 255.148 171.293
0.75 19.05 277.401 186.233
30″ 30 762 0.25 6.35 118.318 79.433
0.281 7.137 132.851 89.189
0.312 7.925 10 147.353 98.925
0.375 9.525 STD 176.731 118.648
0.438 11.125 205.983 138.286
0.5 12.7 20 XHY 234.647 157.53
0.625 15.875 30 292.066 196.078
0.688 17.475 320.817 215.38
0.75 19.05 348.988 234.293
36″ 36 914 0.25 6.35 142.18 95.453
0.281 7.137 159.672 107.196
0.312 7.925 10 177.133 118.918
0.375 9.525 STD 215.525 142.678
0.438 11.125 247.79 166.353
0.5 12.7 20 XHY 282.372 198.57
0.625 15.875 351.723 236.128
0.688 17.475 386.487 259.467
0.75 19.05 420.576 282.353
42″ 42 1067 0.312 7.925 206.914 138.911
0.375 9.525 STD 248.319 166.708
0.5 12.7 XHY 33.097 221.61
0.75 19.05 492.163 330.413
48″ 48 1219 0.375 9.525 STD 284.112 190.738
0.438 11.125 331.404 222.487
0.5 12.7 XHY 377.822 253.65
0.75 19.05 563.75 378.473
0.875 22.225 655.969 440.383
SS 310s Pipe Pressure Rating (psig)
310s Pipe Size(inches) 310s Pipe Schedule Temperature(F)
100 200 300 400 500 600 650 700 750
1″ 40 3048 2629 2362 2171 2019 1924 1867 1824 1810
80 4213 3634 3265 3002 2791 2659 2580 2528 2501
160 6140 5296 4759 4375 4068 3876 3761 3684 3646
1 1/2″ 40 2257 1947 1750 1608 1496 1425 1383 1354 1340
80 3182 2744 2466 2267 2108 2009 1949 1909 1889
160 4619 3984 3580 3291 3060 2916 2829 2772 2743
2″ 40 1902 1640 1474 1355 1260 1201 1165 1141 1129
80 2747 2369 2129 1957 1820 1734 1682 1648 1631
160 4499 3880 3486 3205 2980 2840 2755 2699 2671
3″ 40 1806 1558 1400 1287 1196 1140 1106 1084 1072
80 2553 2202 1979 1819 1691 1612 1564 1532 1516
160 3840 3312 2976 2736 2544 2424 2352 2304 2280
4″ 40 1531 1321 1187 1091 1014 967 938 919 909
80 2213 1909 1715 1577 1466 1397 1355 1328 1314
160 3601 3106 2791 2566 2386 2273 2206 2161 2138
5″ 40 1342 1158 1040 956 889 847 822 805 797
80 1981 1709 1535 1411 1312 1250 1213 1189 1176
160 3414 2945 2646 2433 2262 2155 2091 2049 2027
6 40 1219 1052 945 869 808 770 747 732 724
80 1913 1650 1483 1363 1267 1208 1172 1148 1136
160 3289 2836 2549 2343 2179 2076 2014 1973 1953
8″ 40 1073 926 832 765 711 678 657 644 637
80 1692 1459 1311 1205 1121 1068 1036 1015 1005
160 3175 2738 2460 2262 2103 2004 1944 1905 1885
10″ 40 974 840 755 694 645 615 596 584 578
80 1609 1388 1247 1147 1066 1016 986 966 56
160 3147 2714 2439 2242 2085 1986 1927 1880 1868
1 psi (lb/in2) = 6,894.8 Pa (N/m2) = 6.895×10-2 bar
Notes:
Maximum safe working pressure is calculated per ASME B 31.3-2012, paragraph 304.1.2 (formula 3a). Calculations assume maximum allowable O.D. and minimum allowable wall thickness (worst case scenario).
Temperature Range = -20°F to +300F, -28.8°C to 148.9°C
Types Out diameter Sizes Length
NB Sizes (in stock) .0035” ~ 20” 1/8″, 1/4″, 3/8″, 1/2″, 5/8″, 3/4″, 1″, 1.25″, 1.5″, 2″, 2.5″, 3″, 4″, 5″, 6″etc Cut to length
Stainless Steel 310/310S Seamless Tube (Custom Sizes) 6.35 mm OD To 508 mm OD As per requirement Cut to length
Stainless Steel 310/310S Welded Tube (ERW Tube) (in Stock + Custom Sizes) 6.35 mm OD To 1219 mm OD As per requirement Cut to length
Surface Finish Internal Surface(ID) Exterbal Surface(OD)
Roughness Average(RA) Roughness Average(RA)
μ inch μm μ inch μm
AP Annealed & Pickled Not defined Not defined 40 or Not defined 1.0 or Not defined
BA Beight Annealed 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
MP Mechanical Polish 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
EP Electro Polish 15,10,7,5 0.38,0.25,0.20;0.13 32 0.8

The surface and shape of 310/310S stainless steel tube (6)

Information available for reference and download

Daxun is a trustworthy stainless steel pipe and tube manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 310S stainless steel pipe have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

Recent hot case projects and products

310/310S stainless steel pipe
stainless steel seamless pipe
310/310S stainless steel pipe
large diameter stainless steel pipe
Stainless Steel Polished Tube
310/310S seamless pipe
BA stainless steel pipe
Stainless steel tube
Stainless steel tube / pipe
Stainless steel welded pipe
310/310S stainless pipe
Stainless steel precision tube

Leading stainless steel tube and pipe Suppliers in China


GENERAL PROPERTIES

  • 310 Stainless Steel Tube is an austenitic stainless steel that has excellent high temperature properties while also being ductile and weldable. It is often used in high temperature applications due to its high chromium and nickel content, offering strong corrosion resistance, excellent oxidation resistance, and exceptional strength at temperatures up to 2100°F. Due to its high chromium and nickel content, it outperforms 304 or 309 stainless steel in most applications.

APPLICATIONS

  • Higher alloyed stainless steels often offer good strength at high temperatures, as well as exceptional resistance to creep deformation and environmental damage. As a result, Alloy 310 is widely employed in industries like heat treatment and chemical processing. Examples include:
  • Furnace Parts
  • Oil Burner Parts
  • Heat Exchangers
  • Welding Filler Wire and Electrodes
  • Annealing Covers
  • Combustion Tubes
  • Fire Box Sheets

RESISTANCE

Stainless Steel Alloy 310 Stainless Steel Tubes and Pipes offer excellent resistance to corrosion and heat, even in the most demanding environments.

CORROSION RESISTANCE

  • Provides excellent corrosion resistance
  • High chromium content allows for good aqueous corrosion resistance
  • Excellent resistance at normal temperatures and also has good resistance to oxidizing and carburizing atmospheres

HEAT RESISTANCE

  • Good resistance to oxidation in intermittent service in air at temperatures up to 1040°C and 1150°C in continuous service.
  • Good resistance to thermal fatigue and cyclic heating.
  • Widely used where sulphur dioxide gas is encountered at elevated temperatures.
  • Continuous use in 425-860°C range not recommended due to carbide precipitation, if subsequent aqueous corrosion resistance is needed
  • Generally used at temperatures starting from about 800 or 900°C – above the temperatures at which 304H and 321 are effective.

 FABRICATION

  • Commonly used in the heat treatment and process industries due to high temperature and corrosive environments
  • Often fabricated into complex structures
  • Roller-forms, stamps and draws readily
  • Because 310 work hardens, severe forming operations should be followed by an anneal

WELDABILITY

  • Austenitic stainless steel is generally considered to be weldable
  • Generally considered to have weldability equivalent to 304 and 304L
  • Special consideration is needed to compensate for a higher coefficient of thermal expansion to avoid warping and distortion

Manufacturer of SS UNS S31008 Stainless Steel Welded Pipe, SS UNS S31008 Stainless Steel Seamless Pipe WERKSTOFF NR.1.4845, SS UNS S31008 Heat Exchanger Tubes, We stock different sizes and shapes of TP310s Welded Pipes, Austenitic Stainless Steel 310S Pipe Manufacturer

Find the stainless steel tube you need right here

  • We have a large inventory of high quality standard and specialty grade seamless and welded stainless steel pipes. Our 300 Series stainless steel pipes offer increased strength and corrosion resistance for use in high pressure and harsh conditions, making them perfect for your project. ASTM standard requirements include A213 seamless stainless steel pipe, A269 welded stainless steel pipe, A511 seamless mechanical stainless steel pipe, and A554 decorative stainless steel pipe, with fabrication options including annealed, pickled, or bright annealed.
  • Stainless steel tubes are offered in welded and seamless configurations, with annealed, pickled, and bright annealed manufacturing choices.
  • We carry and specialise in small and large outer diameter stainless steel tubes of various thicknesses and grades, all of which are in stock and available to be custom cut, polished, and supplied to you promptly. Our services for cutting and polishing stainless steel tubes can be tailored to your individual needs.
  • Daxun Alloys is the China leading supplier of stainless steel tubes. Our high quality products, fast delivery and free unlimited cutting make us the preferred stainless steel tube supplier for many domestic and international customers. Order online or by phone and receive stainless steel tubes cut to your specifications within 5-7 days.

310/310S grade stainless steel pipe

Wide choice of dimensions and free cutting

  • Whatever your needs, Daxun Alloys has the perfect stainless steel tube for you. We offer 3m and 6m lengths, with diameters from 3mm to 2000mm (Grade 310) and ¾” to 20″ (Grade 310S).
  • If you require a specific length, we offer a free unlimited cutting service with every purchase. Using state-of-the-art bandsaws, our precision cutting service can cut the tube to the exact length you require. Just let us know when ordering. It’s another reason why we are a leading stainless steel tube supplier to our domestic and international customers.

Contact your stainless steel tube suppliers

  • You can easily order stainless steel pipes online, in any size, in any quantity.
  • Alternatively, our friendly sales team will be happy to take your order. Simply call +86 13382898899 or email Daxunhejin@gmail and we will get back to you as soon as possible.
Can I get some samples?

We can provide stainless steel sheet samples for you to check the quality. Sample is free and you just pay the freight.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

What is your MOQ?

Our MOQ is 1 ton for stainless steel sheet.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.

Send Your Inquiry Today
Quick Quote