Daxun is a 430 stainless steel sheet supplier in China

As China’s leading stainless steel plate supplier and exporter, Daxun provides 430 stainless steel plates to the world.
  • Grade: AISI 430-Martensite
  • Manufacturing: cold-rolled plate, hot-rolled plate, forged plate
  • Standard: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Type: cold-rolled thin plate, hot-rolled thick plate
  • Surface: 2B, NO.1, NO.4, HL, BA, 8K, etc.
  • Length: 2438mm3048mm6000mm can be customized
  • Origin: TISCO, Baosteel, Pohang, Tsingshan, Delong

Global leader in stainless steel sheet fabrication services

430 (1.4016) Stainless Steel Sheet is a ferritic stainless steel classified based on its high chromium content. Chromium content ranges from 12 to 180, and the increased chromium content gives this stainless steel good ductility and formability. It also resists corrosion from strong acids and, due to the high chromium content, has good oxidation resistance. The corrosion resistance of stainless steel is maximized when it is polished or ground. The metal is annealed in order to eliminate its brittleness at room temperature after heating. Please refer to specific product pages for unique sizes. Contact us today to get a quote for any custom size 430 Stainless Steel Sheet order.

One of the producers, exporters, and suppliers of ss 430 stainless steel plate is Daxun; its product quality is superior to that of other 43O stainless steel plate suppliers, and its pricing is competitive. Daxun Warehouse has a sizable inventory of normal size 430 stainless steel plate and can ensure delivery in less than ten days. Please feel free to contact us if you require the price of ss 430 stainless steel plate. Since we have been producing and manufacturing stainless steel plates for almost 20 years, we are able to provide a tight guarantee for the quality of our work. I’m excited that you will select our business as one of your sources for 430 stainless steel plate.

Read More

Technical Data

Product Parameters:   Stainless Steel Sheet/Plate
Width 10mm~2500mm
Thickness 0.2mm~100mm Thickness tolerance +/-0.03mm
Standard ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2
Surface 2B,BA,8K,NO.1,NO.4,NO.3,hairline,checkered,gold ,black ,rose gold,etc
specification 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L
 Mill Origin TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc.
Certification ISO, SGS, BV, TUV,CE etc
Element % Present (in product form)
C, H, P L
Carbon (C) ≤0.08 ≤0.08
Silicon (Si) ≤1.00 ≤1.00
Manganese (Mn) ≤1.00 ≤1.00
Phosphorous (P) ≤0.040 ≤0.040
Sulfur (S) ≤0.015 ≤0.0301)
Chromium (Cr) 16.00 – 18.00 16.00 – 18.00
Iron (Fe) Balance Balance
Product Form Thickness t or diameter4) d mm max Yield Strength Rp0.2 Tensile Strength Elongation min. in %
N/mm2 N/mm2 Rm N/mm2 A80mm1) ˂3mm thickness (longitudinal and transverse)
(longitudinal) (transverse)
C 8 260 280 450 – 600 20
H 13.5 240 260 450 – 600 18
P 252) 240 260 430 – 630 20
L3) 100 240 400 – 630 20 (longitudinal)
Density at 20°C kg/m3 7,700
Modulus of Elasticity kN/mm2 at 20°C 220
200°C 210
400°C 195
500°C
Thermal Conductivity W/m K at 20°C 25
Specific Thermal Capacity at 20°C J/kg K 460
Electrical Resistivity at 20°C Ω mm2 /m 0.6
UNS S43000 1.4016 BS 430S17
ASTM A240 ASTM A240 ASTM A240
ASTM A480 ASTM A480 ASTM A480
ASME SA240 ASME SA240 ASME SA240
AMS 5521 AMS 5521 AMS 5521

Choose Daxun and make your customers satisfied.

Contact Daxun now

Fast delivery

We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.

Contact Daxun now

430 plate features

  • 430 stainless steel plate has corrosion resistance
  • 430 stainless steel plate has special nitric acid resistance
  • 430 stainless steel plate has good formability
  • 430 stainless steel plate has easy welding performance
  • 430 stainless steel plate has good machinability
  • Can be easily manufactured by cold working
Contact Daxun now

Stainless Steel 430 Applications

Typical uses for 430 Stainless Steel include:

  • Low cost sinks
  • Decorative trim
  • White & brown Goods
  • Refrigerators
  • Stove element supports
  • Scientific apparatus
  • Fasteners
  • Flue linings
  • Automotive trim
  • Hinges
Contact Daxun now

Quality, delivery, inspection

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    Our delivery time is strictly in accordance with the contract.
  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples to customers for testing
  • Support on-site or video factory inspection
Contact Daxun now

PROCESSING

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Contact Daxun now

SS 430 Plate Surface Treatment

1D: The surface is matte with discontinuous particle shape.
2D: White with a silvery tone.
2B: Silver gray with better gloss and flatness than 2D surface.
Ba: Close to mirror surface with excellent gloss and reflectivity.
No.3: Good gloss and rough surface.
No.4: The surface has fine lines and good gloss.
HL: Silver gray with golden hair.
8K: Mirror surface.

430 plate stainless steel Features

High strength
Corrosion resistance
Heat resistance
Low temperature resistance
Environmental protection
Welding performance

Daxun Let your brand improve rapidly

Delivery State Choice Surface Condition
Cold Rolled 2B
2D
BA
Hairline
No.3
No.4
6K
8K
Note:
1. If you require different deliver state than the above listed, kindly confirm with us.
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here.
Delivery State
Delivery State Choice Surface Condition
Hot Rolled No.1
No.3
No.4
6K
8K
Pickled
Note:
1. If you require different deliver state than the above listed, kindly confirm with us.
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here.
Tolerance for 2B Sheet
Size Tolerance Rank
Group 1 Group 2 Group 3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
Tolerance for No.1 Hot Rolled Plate
Size Tolerance Rank
Group 1 Group 2 Group 3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
Grade Type Thickness Surface
Austenitic 304/304H/304L/304J1 0.25-150mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0.4-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0.3-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
Ferrite 430 0.4-3.0mm 2B/BA/NO.4/8K/SB/HL
Ultra Pure Ferrite 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
Grade Type Thickness Original
Heat-resistant Steel 309S 0.5-40mm CHN
310S 0.5-40mm CHN
Duplex Steel 2101 1.5-50mm CHN
2304 3.0-50mm CHN
2205 0.5-60mm CHN
2507 1.0-60mm SWE / JPN / CHN
Super Austenitic Steel N08904 0.6-50mm SWE / JPN / CHN
S31254 0.5-50mm SWE / JPN / CHN
N08926 0.5-50mm SWE / JPN / CHN
N08367 0.5-50mm SWE / JPN / CHN
Nickel Base Alloy N08031 1.0-50mm US / JPN / GER
N08810/N08800 0.8-50mm US / JPN / CHN
N08028 1.0-20mm US / GER / JPN
N08020 1.0-20mm US / GER / JPN
N08825 0.8-40mm US / GER / SWE / JPN / CHN
N10276 0.5-50mm US / GER / JPN
N06022 1.0-50mm US / GER / JPN
N06625 0.8-20mm US / GER / CHN
N04400 1.0-20mm US / GER / JPN
N06600 1.0-50mm US / GER / JPN / CHN
N02201 0.5-20mm US / JPN
Titanium TA1/Gr1 0.5-50mm JPN / CHN
TA2/Gr2 0.5-50mm JPN / CHN
Welding Material ERNiCrMo-13 1.2、2.4mm GER
ERNiCrMo-3 2.4mm GER
ERNiCrMo-4 2.4mm US

The surface and shape of 430 stainless steel plate (7)

Daxun is a trustworthy stainless steel plate manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the stainless steel plates have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

Recent hot case projects and products

430 plate stainless steel
astm a240 430 stainless steel plate
430 flat stainless steel plate
430 stainless steel sheet suppliers
430 2b stainless steel sheet
430 stainless steel sheet

Leading Stainless Steel Sheet Suppliers in China

General properties:

  • Ferritic, pure chromium, non-hardenable grade 430 has good formability and corrosion resistance in addition to practical mechanical qualities. Its ability to withstand nitric acid corrosion makes it helpful in some chemical applications; nonetheless, its main uses are in appliance parts and car trim.
  • For use in automatic screw machines, grade 430F is a more machineable variation of this grade that is offered in bar form. Grade 434 is a molybdenum-containing grade that shares the same beneficial characteristics as Grade 430. The molybdenum that was added enhances corrosion resistance.
  • ASTM A240/A240M specifies these 430 qualities for flat rolled goods (plate, sheet, and coil). Similar, though not often identical, qualities are listed in the specifications of other items, like bars and forgings. ASTM A582 specifies the Grade 430F characteristics for bars.

APPLICATIONS:

Typical applications for 430 grade include:

  • Linings for dish washers
  • Refrigerator cabinet panels
  • Automotive trim
  • Lashing Wire
  • Element Supports
  • Stove trim rings
  • Fasteners
  • Chimney Liners

Typical applications for 430F grade include:

  • Repetition machined components

SPECIFICATIONS:

  • UNS: ASTM/ASTE S43000
  • DIN:1.4016

CORROSION RESISTANCE:

  • Grade 430 material exhibits good resistance to a wide range of corrosive environments such as nitric acid and some organic acids. ​​​​​​Highest levels of corrosion resistance are achieved when highly polished or ground. Overall, its resistance to pitting and crevice corrosion is comparable to that of grade 304. Like all ferritic grades, 430 exhibits very high resistance to stress corrosion cracking.
  • The non-free machining grade, 430F, exhibits significantly reduced resistance to pitting and crevice corrosion, as do the other high sulfur free machining grades.

HEAT RESISTANCE:

  • Up to 870°C in intermittent service and 815°C in continuous service, grade 430 resists oxidation. This grade may require extended heating in the 400–600°C range before becoming brittle at room temperature. Annealing can be used to get rid of this effect.

HEAT TREATMENT:

  • Solution Annealing – Heat to 815-845°C, hold for ½ hour per 25mm of thickness, slow furnace cool to 600°C and then quickly air cool. Slow cooling from 540-400°C will cause embrittlement.
  • Sub-Critical anneal – Heat to 760-815°C and then air cool or water quench.
  • This grade is not hardenable by thermal treatment.

WELDING:

  • Pre-heat at 150-200°C if welding is necessary.
  • Embrittlement in the weld metal and heat affected zone can be relieved by a post-weld anneal at 790-815°C
  • Grain refinement will not occur.

MACHINING:

  • Easier to machine than the standard austenitic grades such as 304.
  • Still a tendency for galling and pick-up on the cutting tool.
  • Bars that have been lightly drawn are easier to machine than those in the annealed condition.
  • Grade 430F, the free machining version of 430, is very much easier to machine.

FABRICATION:

  • Lower work hardening rate makes bending and forming somewhat easier than for grade 304
  • Lower ductility restricts very severe operations.
  • Severe bends should be made with the bend axis at right angles to the rolling direction.
  • Severe cold heading of 430 wire is possible.

430 Grade Stainless Steel Sheets in a Variety of Finishes

Our stainless steel sheets (sometimes called steel sheets) are available in a range of beautiful finishes: brushed finish, 2B smooth finish or 8K mirror finish.

The finished side of each stainless steel sheet we supply is coated with a film. This film is easily peeled off after fabrication or installation and protects the surface of the material from wear and marks. The back side is unfinished.

430 Grade Stainless Steel Sheet is the most commonly used variety. It is easily weldable, formable, and has good corrosion resistance.

We can assist in providing stainless steel sheets in any required size.

To meet your specific requirements, our stainless steel sheets are available in three finishes and a variety of sizes. We can readily provide any custom size you may need with our free unlimited cutting service.

We are able to meet any size needs between 0.3 and 30 mm in thickness and between 50 x 50 mm and 2500 x 1250 mm in size. In addition, we provide free unlimited cutting with every order, using a state-of-the-art cutting machine to precisely meet your requirements.

Order Stainless Steel Sheets by Phone or Online.

There has never been an easier way to get stainless steel sheets. Simply refer to the simple and detailed instructions on our website. Alternatively, our sales staff will be happy to take your order or answer any questions when you call +86 13382898899 or email [email protected].

Our delivery time is only one to two days.

Important Safety Note:

The edges of the metal sheets we sell are not polished, ground or finished, so they may be sharp, just like the edges of any stainless steel sheet. We remind users to use, install and handle these devices with care.

Can I get some samples?

We can provide stainless steel sheet samples for you to check the quality. Sample is free and you just pay the freight.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

What is your MOQ?

Our MOQ is 1 ton for stainless steel sheet.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.