Daxun is a 310S stainless steel sheet supplier from China
As China’s leading stainless steel plate supplier and exporter, Daxun provides 310S stainless steel plates to the world.
- Grade: AISI 310-310S-S31008
- Manufacturing: cold-rolled plate, hot-rolled plate, forged plate
- Standard: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Type: cold-rolled thin plate, hot-rolled thick plate
- Surface: 2B, NO.1, NO.4, HL, BA, 8K, etc.
- Length: 2438mm3048mm6000mm can be customized
- Origin: TISCO, Baosteel, Pohang, Tsingshan, Delong
The global leader in stainless steel sheet fabrication services
S31008 (310S) Sheet and Plate, Austenitic stainless steel alloy 310S (UNS S31008) is designed for applications requiring high-temperature corrosion resistance. The alloy resists oxidation up to 2010°F (1100°C) with room temperature cycling. Alloy 310 can be used in moderate carburizing environments and is resistant to sulfidation due to its high chromium content and moderate nickel content. More severe carburizing environments in heat-treating equipment typically require a nickel alloy such as 330 (UNS N08330). Alloy 310S can be used in bonding, nitriding, mild oxidation, and thermal cycling processes; however, a reduced maximum service temperature is required. Alloy 310 can also be used in cryogenic applications because it has low magnetic permeability and remains strong down to -450°F (-268°C). When heated to 1202–1742, the alloy precipitates the sigma phase (650–950°C). Hardness is partially restored by solution annealing at 2012–2102°F (1100–1150°C). This alloy is also available as a low-carbon alloy, 310S (UNS S31008). It is easily fabricated. A high carbon modification, 310H (UNS S31009), is designed to improve creep resistance. In most cases, the grain size and carbon content of the plate can meet both 310S and 310H standards. Standard shop fabrication procedures can be used to easily weld and process alloy 310.
Stainless Steel 310S Plate has trace amounts of silicon, sulfur, phosphorus, manganese, and up to 24% chromium, 19% nickel, and up to 0.08% carbon. Heat resistance, corrosion resistance, strength, and even high-temperature oxidation resistance are just a few of the many benefits of this popular stainless steel alloy. It can be utilized in many different applications, including burners, oil burners, and evaporator pipes and tubes. Because of its affordability, it’s perfect for a range of applications requiring low-cost maintenance supplies.
Because of its exceptional resilience to high temperatures, the 310S stainless steel plate is a great option for a wide range of industries, including petrochemical and chemical production, food processing, power plants, dairy farms, sugar mills, breweries, and energy generation. 310S Stainless Steel Plate is capable of withstanding oxidizing environments up to 2100°F (1149°C) due to its high chromium concentration. Its ductility, toughness, and weldability are all excellent. Its exceptional low-temperature performance, even down to -20°F (-29°C), combined with its resistance to heat and corrosion make it the perfect material for cryogenic applications. In conclusion, it is an excellent option for high-temperature industrial applications due to its strong resistance to oxidation and ability to prevent scaling at temperatures as high as 2000°F (1093°C).
Technical Data
- Parameter
- Element
- Mechanical properties
- Standard
Product Parameters: 310(UNS S31008) Stainless Steel Sheet/Plate | |||
Width | 10mm~2500mm | ||
Thickness | 0.2mm~100mm | Thickness tolerance | +/-0.03mm |
Standard | ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2 | ||
Surface | 2B,BA,8K,NO.1,NO.4,NO.3,hairline,checkered,gold ,black ,rose gold,etc | ||
specification | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
Mill Origin | TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc. | ||
Certification | ISO, SGS, BV, TUV,CE etc |
Element | % Present (in product form) | |
C, H, P, L | TW* / TS* | |
Carbon (C) | ≤0.10 | ≤0.15 |
Silicon (Si) | ≤1.50 | ≤0.75 |
Manganese (Mn) | ≤2.00 | ≤2.00 |
Phosphorous (P) | ≤0.045 | ≤0.045 |
Sulfur (S) | ≤0.015 | ≤0.030 |
Chromium (Cr) | 24.00 – 26.00 | 24.00 – 26.00 |
Nickel (Ni) | 19.00 – 22.00 | 19.00 – 22.00 |
Nitrogen (N) | ≤0.11 | – |
Iron (Fe) | Balance | Balance |
Product Form | |||||
C, H, P | L | TW* / TS* | |||
Thickness a or diamter d (mm) | a ≤ 12 | d ≤ 25 | – | ||
Hardness HB max. 1) 2) 3) | 192 | 192 | – | ||
Proof Strength3) | Rp0.2 N/mm2 | 210 | 210 | 230 | |
Rp1.0 N/mm2 | 230 | 230 | 270 | ||
Tensile Strength | Rm N/mm2 | 500 – 700 | 500 – 700 | min. 500 | |
Elongation min. in % | Long Products | 351) | 351) | 334) / 355) | |
Flat Products | 0.5 ≤ a/d < 3 | 334)5) | 334)5) | 354)5)6) | |
3 ≤ a/d | 354)5) | 354)5) | 354)5)6) |
310 | 310S | 310H |
---|---|---|
UNS S31000 | UNS S31008 | UNS S31009 |
ASTM A240 | ASTM A240 | ASTM A240 |
ASTM A480 | ASTM A480 | ASTM A480 |
ASME SA240 | ASME SA240 | ASME SA240 |
AMS 5521 | AMS 5521 | AMS 5521 |
Choose Daxun and make your customers satisfied.
Fast delivery
We provide timely and fast delivery of 310S stainless steel plate products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Benefits of Stainless Steel 310S Plates :
- Corrosion resistance: The main benefit of 310S stainless steel plates is their excellent corrosion resistance. They resist corrosion from a wide range of environments, including acidic and alkaline solutions, making them suitable for a wide range of applications.
- High-temperature strength: 310S stainless steel plates exhibit excellent strength at elevated temperatures. This property is critical in applications that are frequently exposed to high temperatures, ensuring structural integrity and performance in demanding conditions.
- Durability and lifespan: The durability of 310S stainless steel plates gives them a long service life, making them an affordable choice for many applications. The material is resistant to wear and tear, minimizing the need for frequent replacement.
Benefits of Stainless Steel 310S Plates :
310S/2520 Plate Features:
- High-temperature resistance
- Excellent oxidation resistance
- Improved creep/rupture properties
- Excellent corrosion resistance
- Not susceptible to thermal fatigue and cyclic heating
- Good strength at temperatures up to 2100°F
Quality, delivery, inspection
- Daxun strictly controls product quality. Before placing an order, we will send you the product warranty, or if you need samples for testing, we can also send samples for free.
- During the production process, we carefully measure the diameter, thickness, and surface quality of each product to ensure it meets exacting standards. Our standard delivery time is typically 7 to 15 days. However, for special-sized products, the delivery time may be extended to 20 days to accommodate the additional customization and processing required.
Our delivery time is strictly in accordance with the contract. - Support customer third-party agencies to go to the factory for inspection
- Support free samples to customers for testing
- Support on-site or video factory inspection
Applications
- Cryogenic Components: Designed to withstand extremely low temperatures, ensuring optimal performance in critical applications.
- Food Processing: Reliable materials and components tailored for hygienic and efficient food production systems.
- Furnaces: Durable solutions for burners, doors, fans, ducting, and liners, supporting high-temperature industrial processes.
- Fluidized Bed Furnaces: Robust components including coal burners, grates, ducting, and bellows for enhanced operational efficiency.
- Ore Processing and Steel Mills: High-performance equipment for smelting, steelmaking, and continuous casting operations.
- Petroleum Refining: Specialized systems such as catalytic recovery units, flares, heat exchangers, and tube hangers for maximum efficiency in refining processes.
- Power Generation: Precision-engineered components like gas furnace internals, pulverized coal burners, and tube hangers to support energy production.
- Sintering and Cement Plants: Reliable burners, burner hoods, feed and discharge systems, and bellows for seamless operation in harsh environments.
- Heat Treating: Advanced solutions, including annealing covers and boxes, burner grates, doors, fans, muffle furnaces, retorts, heat exchangers, and walking beams for consistent performance in thermal processing.
SS 310S Plate Surface Treatment
1D: The surface is matte with a discontinuous particle shape.
2D: White with a silvery tone.
2B: Silver gray with better gloss and flatness than the 2D surface.
Ba: Close to mirror surface with excellent gloss and reflectivity.
No.3: Good gloss and rough surface.
No.4: The surface has fine lines and good gloss.
HL: Silver gray with golden hair.
8K: Mirror surface.
310 plate stainless steel Features
Daxun Let your brand improve rapidly
- Gallery
- Tolerance
- Delivery state
- Other product series
Tolerance for 2B Sheet | |||
Size | Tolerance Rank | ||
Group 1 | Group 2 | Group 3 | |
0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
Tolerance for No.1 Hot Rolled Plate | |||
Size | Tolerance Rank | ||
Group 1 | Group 2 | Group 3 | |
3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
Delivery State Choice | Surface Condition |
Cold Rolled | 2B |
2D | |
BA | |
Hairline | |
No.3 | |
No.4 | |
6K | |
8K | |
Note: | |
1. If you require different deliver state than the above listed, kindly confirm with us. | |
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here. | |
Delivery State | |
Delivery State Choice | Surface Condition |
Hot Rolled | No.1 |
No.3 | |
No.4 | |
6K | |
8K | |
Pickled | |
Note: | |
1. If you require different deliver state than the above listed, kindly confirm with us. | |
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here. |
Grade | Type | Thickness | Surface |
Austenitic | 304/304H/304L/304J1 | 0.25-150mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
321 | 0.4-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
316/316L/317L/316Ti | 0.3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
Ferrite | 430 | 0.4-3.0mm | 2B/BA/NO.4/8K/SB/HL |
Ultra Pure Ferrite | 443 | 0.4-2.0mm | 2B |
436L/439/444/441 | 0.5-3.0mm | 2B、2D | |
409L | 0.4-2.5mm | 2B、2D | |
Grade | Type | Thickness | Original |
Heat-resistant Steel | 309S | 0.5-40mm | CHN |
310S | 0.5-40mm | CHN | |
Duplex Steel | 2101 | 1.5-50mm | CHN |
2304 | 3.0-50mm | CHN | |
2205 | 0.5-60mm | CHN | |
2507 | 1.0-60mm | SWE / JPN / CHN | |
Super Austenitic Steel | N08904 | 0.6-50mm | SWE / JPN / CHN |
S31254 | 0.5-50mm | SWE / JPN / CHN | |
N08926 | 0.5-50mm | SWE / JPN / CHN | |
N08367 | 0.5-50mm | SWE / JPN / CHN | |
Nickel Base Alloy | N08031 | 1.0-50mm | US / JPN / GER |
N08810/N08800 | 0.8-50mm | US / JPN / CHN | |
N08028 | 1.0-20mm | US / GER / JPN | |
N08020 | 1.0-20mm | US / GER / JPN | |
N08825 | 0.8-40mm | US / GER / SWE / JPN / CHN | |
N10276 | 0.5-50mm | US / GER / JPN | |
N06022 | 1.0-50mm | US / GER / JPN | |
N06625 | 0.8-20mm | US / GER / CHN | |
N04400 | 1.0-20mm | US / GER / JPN | |
N06600 | 1.0-50mm | US / GER / JPN / CHN | |
N02201 | 0.5-20mm | US / JPN | |
Titanium | TA1/Gr1 | 0.5-50mm | JPN / CHN |
TA2/Gr2 | 0.5-50mm | JPN / CHN | |
Welding Material | ERNiCrMo-13 | 1.2、2.4mm | GER |
ERNiCrMo-3 | 2.4mm | GER | |
ERNiCrMo-4 | 2.4mm | US |
The surface and shape of 310S stainless steel plate (7)
Information available for reference and download
Daxun is a trustworthy stainless steel plate manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the stainless steel plates have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
Recent hot case projects and products
Related Products (13)
Leading Stainless Steel Sheet Suppliers in China
ASTM A240 Stainless Steel 310 / 310S Plate Suppliers and Exporters
Da Xun Alloy specializes in manufacturing and exporting premium-quality 310S Stainless Steel Plates, 310 Stainless Steel Plates, and Stainless Steel 310 Coils. These products are available in a wide range of thicknesses, from 0.3 mm to 120 mm, to meet diverse industrial requirements.
Our offerings include:
- Stainless Steel UNS S31000 / S31008 Plates and Sheets
- 310S Stainless Steel Plates
- ASME SA 240 Stainless Steel Plates
- DIN 1.4301 / 1.4306 / 1.4307 Plates
What is the density of 310S Stainless Steel Plates?
- Density: 8.0 g/cm³ (0.289 lb/in³)
While not the lightest material available, the relatively low density of 310S stainless steel contributes to its versatility. It is lightweight enough to be easily formed into complex shapes and sizes, yet robust enough to maintain superior performance in a variety of industrial applications. - Strength and Resilience: The alloy’s chromium-nickel structure provides excellent mechanical strength and resistance to both high-temperature oxidation and aqueous corrosion.
310S Grade Stainless Steel Sheets in a Variety of Finishes
Our stainless steel sheets (sometimes called steel sheets) are available in a range of beautiful finishes: brushed finish, 2B smooth finish or 8K mirror finish.
The finished side of each stainless steel sheet we supply is coated with a film. This film is easily peeled off after fabrication or installation and protects the surface of the material from wear and marks. The back side is unfinished.
310S Grade Stainless Steel Sheet is the most commonly used variety. It is easily weldable, formable, and has good corrosion resistance.
We can assist in providing stainless steel sheets in any required size.
To meet your specific requirements, our stainless steel sheets are available in three finishes and a variety of sizes. We can readily provide any custom size you may need with our free unlimited cutting service.
We are able to meet any size needs between 0.3 and 30 mm in thickness and between 50 x 50 mm and 2500 x 1250 mm in size. In addition, we provide free unlimited cutting with every order, using a state-of-the-art cutting machine to precisely meet your requirements.
Order Stainless Steel Sheets Online.
There has never been an easier way to get stainless steel sheets. Simply refer to the simple and detailed instructions on our website. Alternatively, our sales staff will be happy to take your order or answer any questions when you call +86 13382898899 or email [email protected].
Our delivery time is only one to two days.
Important Safety Note:
The edges of the metal sheets we sell are not polished, ground or finished, so they may be sharp, just like the edges of any stainless steel sheet. We remind users to use, install and handle these devices with care.8
We can provide stainless steel sheet samples for you to check the quality. Sample is free and you just pay the freight.
We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.
Our MOQ is 1 ton for stainless steel sheet.
Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.