Daxun is a 410 stainless steel sheet supplier in China
As China’s leading stainless steel plate supplier and exporter, Daxun provides 410 stainless steel plates to the world.
- Grade: AISI 410-Martensite
- Manufacturing: cold-rolled plate, hot-rolled plate, forged plate
- Standard: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Type: cold-rolled thin plate, hot-rolled thick plate
- Surface: 2B, NO.1, NO.4, HL, BA, 8K, etc.
- Length: 2438mm3048mm6000mm can be customized
- Origin: TISCO, Baosteel, Pohang, Tsingshan, Delong
Global leader in stainless steel sheet fabrication services
Martensitic 410 grade stainless steel can be toughened by a “quench and temper” heat treatment, like most non-stainless steels. It contains enough chromium (at least 11.5%) to resist corrosion. It has the highest corrosion resistance when it is polished after tempering and hardening. A general-purpose grade of stainless steel plate called 410 grade is usually hardened, but still machinable, and is used in applications that require moderate heat and corrosion resistance and high strength. The high hardness of martensitic stainless steel is its main feature, but some other characteristics are sacrificed. Poor weldability must be accommodated during manufacturing, and a final heat treatment is usually required. Martensitic stainless steels have lower corrosion resistance than ordinary austenitic stainless steels. They also lose ductility at temperatures below freezing and lose strength at temperatures above freezing due to over-tempering, which limits their useful operating temperature range. 410 alloy stainless steel plate is a widely used 12% chromium martensitic stainless steel plate that can be heat treated to produce a range of mechanical properties. 410 stainless steel plate has high strength and hardness while having good corrosion resistance. 410 Alloy Stainless Steel Plate is ductile and malleable. It is magnetic in all circumstances. Therefore, it is not recommended for use where severe corrosion may occur.
Stainless steel 410 plates are used in many different commercial applications. To meet the needs of their customers, Daxun Alloys producers acquire stainless steel plates in specified sizes and specifications. Because of the special qualities of 410 grade stainless steel, stainless steel plates can be used in steam, mild, and chemical environments. When stainless steel passes numerous, exacting quality tests, these qualities become highly valuable.
As a result, making sure the material is checked prior to delivery is crucial. Daxun Alloys carries out the required testing for any kind of application.
Technical Data
- Parameter
- Chemical Compositions
- Mechanical properties
- PHYSICAL PROPERTIES
- Standard
| Product Parameters: Stainless Steel Sheet/Plate | |||
| Width | 10mm~2500mm | ||
| Thickness | 0.2mm~100mm | Thickness tolerance | +/-0.03mm |
| Standard | ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2 | ||
| Surface | 2B,BA,8K,NO.1,NO.4,NO.3,hairline,checkered,gold ,black ,rose gold,etc | ||
| specification | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
| Mill Origin | TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc. | ||
| Certification | ISO, SGS, BV, TUV,CE etc | ||
| UNS No | S41000 |
| EN | 1.4006 |
| AISI | 410 |
| Carbon (C) | 0.08/0.15 |
| Silicon (Si) | 1 |
| Manganese (Mn) | 1 |
| Phosphorus (P) | 0.04 |
| Sulphur (S) | 0.03 |
| Chromium (Cr) | 11.5/13.5 |
| Molybdenum (Mo) | |
| Nickel (Ni) | 0.75 |
| Nitrogen (N) |
| Property | Value |
| Density | 7.8 g/cc |
| Yield Strength | 1,225 MPa at a strain of 0.2% |
| Ultimate Tensile Strength | 1,525 MPa |
| Hardness | 126–192 Brinell hardness (annealed condition) 201–255 Brinell hardness (when hardened and tempered) |
| Bulk Modulus | 200 GPa |
| Melting Point | 1,480–1,530 °C |
| Corrosion Resistance | Good corrosion resistance in mild atmospheric environments, water, and some mild chemical environments. It shows pitting corrosion and brown staining in salt water conditions and offers lower resistance to acidic environments than the austenitic stainless steel alternatives. |
| Magnetism | Permeability 700–1,000. Highly responsive to magnetic fields, act as a strong magnetic flux carrier due to its martensitic structure. |
| Density (lb./ in^2) @ RT | 0.28 | |
| Modulus of Elasticity in Tension (psi x 10^6) | 29 | |
| Specific Heat (BTU/o F/lb.) | 32 to 212 oF | 0.11 |
| Thermal Conductivity (BTU/hr/ft^2/ft) | 212oF | 14.4 |
| 932oF | 16.6 | |
| Mean Coefficient of Thermal Expansion (in. x 10^-6 per o F) | 32 to 212oF | 5.5 |
| 32 to 1,200oF | 6.5 | |
| Electrical Resistivity (micro ohms – cm) | at 70oF | 22.5 |
| UNS S41000 | ASTM A 276 |
| AMS 5504 | ASTM A 493 |
| AMS 5613 (Chemistry only) | ASTM F 899 |
| ASTM A 240 | ASME SA 240 |
| EN 1.4006 | B50991B |
| PWA-LCS | GE Aviation S-SPEC-35 AeDMS S-400 |
| GE Aircraft Engine (GT193) | RR SABRe Edition 2 |
Choose Daxun and make your customers satisfied.
Fast delivery
We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.
410 plate features
Corrosion Resistance
410 is resistant to dry air, fresh water, mild bases and acids, foods, steam and hot gases.
It must be hardened for maximum heat and corrosion resistance. Best performance when smooth.
Heat Resistance
Good resistance to scaling up to about 650°C, but not generally recommended for use at temperatures between 400 and 580°C as mechanical properties are reduced.
Heat Treatment
Fully anneal 815-900°C, slow furnace cool to 600°C, then air cool.
Process anneal 650-760°C and air cool.
Welding
Easily welded by all standard methods, but requires preheating to 150-260°C and post weld annealing to reduce the likelihood of cracking.


Stainless Steel 410 Applications
- Aerospace structures;
- Automobile exhaust pipes, engine parts;
- Medical devices;
- Knives and kitchen utensils;
- Petrochemical applications;
- Stainless steel cutlery, kitchen utensils;
- Manufacturing flat springs;
- Hand tools;
- Bolts, nuts, springs and fasteners;
Quality, delivery, inspection
- Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
- During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
Our delivery time is strictly in accordance with the contract. - Support customer third-party agencies to go to the factory for inspection
- Support free samples to customers for testing
- Support on-site or video factory inspection

SS 410 Plate Surface Treatment
1D: The surface is matte with discontinuous particle shape.
2D: White with a silvery tone.
2B: Silver gray with better gloss and flatness than 2D surface.
Ba: Close to mirror surface with excellent gloss and reflectivity.
No.3: Good gloss and rough surface.
No.4: The surface has fine lines and good gloss.
HL: Silver gray with golden hair.
8K: Mirror surface.
PROCESSING
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.
410 plate stainless steel Features
Daxun Let your brand improve rapidly
- Gallery
- Tolerance
- Delivery state
- Other product series
| Tolerance for 2B Sheet | |||
| Size | Tolerance Rank | ||
| Group 1 | Group 2 | Group 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Tolerance for No.1 Hot Rolled Plate | |||
| Size | Tolerance Rank | ||
| Group 1 | Group 2 | Group 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Delivery State Choice | Surface Condition |
| Cold Rolled | 2B |
| 2D | |
| BA | |
| Hairline | |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Note: | |
| 1. If you require different deliver state than the above listed, kindly confirm with us. | |
| 2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here. | |
| Delivery State | |
| Delivery State Choice | Surface Condition |
| Hot Rolled | No.1 |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Pickled | |
| Note: | |
| 1. If you require different deliver state than the above listed, kindly confirm with us. | |
| 2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here. | |
| Grade | Type | Thickness | Surface |
| Austenitic | 304/304H/304L/304J1 | 0.25-150mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0.4-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0.3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferrite | 430 | 0.4-3.0mm | 2B/BA/NO.4/8K/SB/HL |
| Ultra Pure Ferrite | 443 | 0.4-2.0mm | 2B |
| 436L/439/444/441 | 0.5-3.0mm | 2B、2D | |
| 409L | 0.4-2.5mm | 2B、2D | |
| Grade | Type | Thickness | Original |
| Heat-resistant Steel | 309S | 0.5-40mm | CHN |
| 310S | 0.5-40mm | CHN | |
| Duplex Steel | 2101 | 1.5-50mm | CHN |
| 2304 | 3.0-50mm | CHN | |
| 2205 | 0.5-60mm | CHN | |
| 2507 | 1.0-60mm | SWE / JPN / CHN | |
| Super Austenitic Steel | N08904 | 0.6-50mm | SWE / JPN / CHN |
| S31254 | 0.5-50mm | SWE / JPN / CHN | |
| N08926 | 0.5-50mm | SWE / JPN / CHN | |
| N08367 | 0.5-50mm | SWE / JPN / CHN | |
| Nickel Base Alloy | N08031 | 1.0-50mm | US / JPN / GER |
| N08810/N08800 | 0.8-50mm | US / JPN / CHN | |
| N08028 | 1.0-20mm | US / GER / JPN | |
| N08020 | 1.0-20mm | US / GER / JPN | |
| N08825 | 0.8-40mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0.5-50mm | US / GER / JPN | |
| N06022 | 1.0-50mm | US / GER / JPN | |
| N06625 | 0.8-20mm | US / GER / CHN | |
| N04400 | 1.0-20mm | US / GER / JPN | |
| N06600 | 1.0-50mm | US / GER / JPN / CHN | |
| N02201 | 0.5-20mm | US / JPN | |
| Titanium | TA1/Gr1 | 0.5-50mm | JPN / CHN |
| TA2/Gr2 | 0.5-50mm | JPN / CHN | |
| Welding Material | ERNiCrMo-13 | 1.2、2.4mm | GER |
| ERNiCrMo-3 | 2.4mm | GER | |
| ERNiCrMo-4 | 2.4mm | US |
The surface and shape of 410 stainless steel plate (7)
Information available for reference and download
Daxun is a trustworthy stainless steel plate manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the stainless steel plates have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
Recent hot case projects and products
Related Products (13)
We can provide stainless steel sheet samples for you to check the quality. Sample is free and you just pay the freight.
We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.
Our MOQ is 1 ton for stainless steel sheet.
Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.