Daxun stainless steel channel steel is suitable for engineering and structure.
China stainless steel channel supplier.
Daxun has 10,000 tons of stainless steel channel in stock
Daxun can provide channel surface processing services
Introduction to Daxun stainless steel channel steel
| Product Parameters: Stainless Steel channel bar | |
| Размер | 5#、6#、6.3#、8#、10#、12#、14#、16#、18#、20#、22#、25#etc. |
| Please see the technical information below for detailed dimensions. | |
| Поверхность | Pickling 8K, NO.1, NO.4,hairline, etc |
| length | 6000mm or Customized |
| Класс | 304 201 304L 310S 316L 321 904L 2205 2507 S32750 S32760 etc |
| Стандарты | ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227 |
| Характеристики | Anti-corrosion (the degree is susceptible to the alloys contained), heat-resistance, good cold and hot working properties, good toughness, good comprehensive performances and wide application. |
Daxun stainless steel channels are available in a variety of grades. We produce them by laser fusion and hot rolling, and are available in metric and imperial sizes. Daxun can provide custom sizes, shapes and grades upon request.
Send us a message now!
Stainless Steel channel Steel Grade
Each type of stainless steel channel steel has its own different usage scenarios.
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Click on the image to see more information about this product
Stainless steel channel steel surface
If the surface you need is not available here, you can contact Daxun.
Common sizes of stainless steel channel steel
Choose Daxun’s reliable stainless steel channels, available in a variety of sizes to suit your application.
Performance of stainless steel channel steel
The chemical composition on stainless steel channel bars protects them from rust. Their corrosion resistance is enhanced by the necessary polished finish, making them ideal for architectural use.
Since stainless steel channel have a low melting point, no special tools are required. They are also durable and long-lasting materials, allowing industries to save on work and maintenance costs.
The smarter option material SS channel have far lesser drawbacks than other alloys. They provide excellent value, cost-effectiveness, and durability. SS is an easy-to-clean metal material.
Stainless steel channel material is an excellent choice for a variety of applications such as manufacturing. They are simple to use and ideal for large-scale industrial and complex uses.
Огромный запас выбираемого материала
With choiceable material from the very start comes our high quality stainless steel products.Daxun have stainless steel inventories for common grades and common sizes to ensure fast response to our customers’ demand.Mill Origin: TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc.
Stainless Steel Channel Manufacturing Process
Daxun stainless steel channels and C-channels are available in a variety of grades. We produce them by laser fusion and hot rolling, and are available in metric and imperial sizes. Daxun can provide custom sizes, shapes and grades upon request.Send us a message now!
About Daxun
1. Competitive price and quality from our own factory
2. Approved by ISO9001, CE, SGS every year
3. Best service with 24 hour`s reply
4. Flexible payment with T/T,L/C , paypal, etc
5. Smooth production ability
6. Quick delivery and standard exporting package
7. OEM/ODM
Technical Information

В Daxun мы выбираем различные виды упаковки для различных изделий из нержавеющей стали, включая: крафт-бумагу, деревянные коробки, тканые мешки, деревянные поддоны, основываясь на самых высоких промышленных стандартах, чтобы гарантировать, что товары попадут к вам в руки в хорошем состоянии.
Все наши материалы из нержавеющей стали сертифицированы по различным отраслевым стандартам, таким как ISO9001:2008, ISO14001:2014, AAA Certification, CQGC Certifications и др. Наша компания также имеет сертификаты системы управления качеством ISO9001:2015.
В Daxun, у нас есть испытательная лаборатория и оборудование, чтобы убедиться, что наши материалы из нержавеющей стали имеют фактический вес и хорошее качество перед отправкой. Наша строгая команда контроля качества также осуществляет строгий и 100% контроль на всех этапах производства.
Our support and services are not only limited from the beginning of our transactions. Even if you have received your orders, Daxun will continue to provide excellent after-sales services. We will continue providing assistance and warranty to your orders.
Application cases of stainless steel channel steel in different industries
Stainless steel channels are widely used in the construction field. They can be used for exterior wall support, interior decoration, roofing materials, building structures, etc. Stainless steel is corrosion-resistant and has high strength, and can meet the design requirements of different buildings.
Stainless steel has the advantages of corrosion resistance, no rust, no discoloration, easy removal of attached food, and good high and low temperature mechanical properties. Widely used in food machinery, such as sanitary systems, fluid pipe tanks, food storage tanks, heat exchangers, vacuum containers, etc.
Stainless steel has good strength, toughness and corrosion resistance and is widely used in aircraft structural parts. For example, the wing structure, fuselage supports, seats and other components are all made of stainless steel.
Stainless steel channel are also used in the manufacture and maintenance of oil refining equipment, and the brackets used in the petrochemical industry are all made of stainless steel channel.
Основные детали: обшивка крыла, стрингеры крыла, верхние и нижние планки лонжерона крыла, полотно, стрингеры фюзеляжа, поручни сидений, килевая балка, боковые рамы, обшивка фюзеляжа, нижние панели стенок фюзеляжа, стрингеры пола и т.д.
Stainless steel channel steel is widely used in the shipbuilding industry. The stainless steel channels supplied by Daxun are used in the shipbuilding and petroleum industries. They have high strength, good toughness, and are resistant to seawater corrosion, fatigue, and wear.
SS316L - основная аустенитная марка нержавеющей стали, используемая в морских установках, где она повышает прочность при высоких температурах и защищает конструкции от воздействия агрессивных кислотных сред. Существуют также дуплексные нержавеющие стали, которые обеспечивают превосходное сочетание механических свойств и устойчивости к коррозионному растрескиванию под напряжением, что делает их идеальными для морских установок. Сталь UNS S32205 - наиболее часто используемая марка дуплексной нержавеющей стали для морских установок.
The main application of stainless steel channel steel in electricity is the support of power station equipment. The excellent corrosion resistance and high strength of stainless steel make it the preferred material for power generation components.
echnical Information
- Stock
- Толерантность
- Состояние доставки
| Size Range | |||||
| Hot-rolled U channel bar | |||||
| Section | Designation | Mass | Section | Designation | Mass |
| UPE80 | [80*50*4.5*8 | 8.89 | UPN65 | [65*42*5*7 | 7.09 |
| UPE100 | [100*55*5*8.5 | 10.9 | UPN80 | [80*45*6*8 | 8.64 |
| UPE120 | [120*60*5.5*9 | 13.2 | UPN100 | [100*50*6*8.5 | 10.6 |
| UPE140 | [140*65*6*9.5 | 15.7 | UPN120 | [120*55*7*9 | 13.4 |
| UPE160 | [160*70*6.5*10 | 18.6 | UPN140 | [140*60*7*10 | 16 |
| UPE180 | [180*75*7*10.5 | 21.6 | UPN160 | [160*65*7.5*10.5 | 18.8 |
| UPE200 | [200*80*7.5*11 | 24.8 | UPN180 | [180*70*8*11 | 22 |
| UPE220 | [220*85*8*12 | 28.8 | UPN200 | [200*75*8.5*11.5 | 25.3 |
| UPE240 | [240*90*8.5*13 | 33.4 | UPN220 | [220*80*9*12.5 | 29.4 |
| UPE270 | [270*95*9*14 | 38.8 | UPN240 | [240*85*9.5*13 | 33.2 |
| UPE300 | [300*100*9.5*15 | 44.5 | UPN260 | [260*90*10*14 | 37.9 |
| UPE330 | [330*105*11*16 | 53.3 | UPN280 | [280*95*10*15 | 41.8 |
| UPE360 | [360*110*12*17 | 61.2 | UPN300 | [300*100*10*16 | 46.2 |
| UPE400 | [400*115*13.5*18 | 72.3 | UPN320 | [320*100*14*17.5 | 59.5 |
| UPN30 | [30*33*5*7 | 4.27 | UPN350 | [350*100*14*16 | 60.6 |
| UPN40 | [40*35*5*7 | 4.87 | UPN380 | [380*102*13.5*16 | 63.1 |
| UPN50 | [50*38*5*7 | 5.59 | UPN400 | [400*110*14*18 | 71.8 |
| Specified Size of Stainless Channels, mm | Size Tolerances, Over and Under, mm. | ||||
| Flange Depth | Flange Width | Web Thickness for Thickness Given | Out-of-Square B of Either Flange, mm/ mm of Flange Width | ||
| To 5.00mm | Over 5.00mm | ||||
| To 38.00mm, incl. | 1.2 | 1.2 | 0.41 | 0.6 | 1.2 |
| Over 38.00 to 75.00mm, excl. | 2.4 | 2.4 | 0.6 | 0.8 | 1.2 |
| Выбор государства доставки | Состояние поверхности |
| Горячекатаный | Маринованные |
| Sand Blasting | |
| Сварка | Маринованные |
| Sand Blasting | |
| Press Bending | Маринованные |
| Sand Blasting | |
| No.1 Finish | |
| Примечание: | |
| 1. Если вам требуется другое состояние доставки, чем перечисленные выше, пожалуйста, подтвердите с нами. | |
| 2. В случае запроса или заказа, пожалуйста, сообщите нам о любых дополнительных требованиях, не указанных здесь. | |
Сопутствующий товар
Сплав Даксунь
Regarding stainless steel channel, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.
Да, у нас есть полные спецификации и инвентарь, и мы можем быстро удовлетворить ваши потребности.
Да, он может быть настроен. Вы можете связаться с нами и отправить нам настроенные спецификации и количество.
Наши способы транспортировки обычно включают морские перевозки, наземные перевозки и морские перевозки. Мы доставим вам груз быстро и безопасно.
Поскольку наша производительность высока, затраты будут гораздо ниже, поэтому цена низкая.
We can provide stainless steel channel samples for you to check the quality. Sample is free and you just pay the freight.
Мы придаем большое значение качеству продукции и прошли различные испытания системы качества.