x
Отправьте запрос сегодня
Быстрая цитата
Incoloy

Incoloy

  • Daxun Alloy is a Chinese lncoloy manufacturer.
  • Experienced lncoloy sales team and professional production factory.
  • Strict quality control and standard testing.
  • Incoloy Plate
  • Incoloy Pipe
  • Incoloy Coil
  • Incoloy Bar
  • Incoloy Plate
  • Incoloy Pipe
  • Incoloy Coil
  • Incoloy Bar

What is Incoloy

Incoloy is a nickel-based high-temperature alloy produced by Special Metals Corporation, known for its excellent corrosion resistance and high-temperature strength.

Properties of Incoloy alloy:

  • Corrosion resistance: Incoloy alloys show excellent corrosion resistance in various corrosive environments, especially in acidic, alkaline and saline media.
  • High-temperature strength: These alloys can still maintain good mechanical properties at high temperatures and are suitable for high-temperature equipment.
  • Oxidation resistance: The high content of chromium enables Incoloy alloys to quickly form a dense oxide film in a high-temperature oxidizing environment to prevent further oxidation.
  • Processing performance: Incoloy alloys are easy to process and are suitable for manufacturing complex parts.

 

Incoloy series alloys are widely used in multiple industrial fields for their excellent corrosion resistance and high temperature performance. The following is a detailed introduction to several commonly used Incoloy grades:

  • Incoloy 800
    Features: Incoloy 800 is a nickel-iron-chromium alloy with good corrosion resistance and heat resistance, suitable for high temperature environments up to 800°C. It has a high chromium content and sufficient nickel content, so it has excellent high temperature corrosion resistance.
    Application areas: Commonly used in petrochemical, chemical, heat treatment and aerospace fields to manufacture high temperature equipment such as furnace tubes, heaters, catalyst brackets, etc.
  • Incoloy 800H
    Features: Incoloy 800H is an improved version of Incoloy 800 with better oxidation resistance, high temperature resistance and creep resistance. It significantly improves its high temperature strength and creep rupture performance by optimizing the alloy composition and heat treatment process.
    Application areas: Widely used in the manufacture of steam generators in metallurgy, petrochemical and nuclear industries, and is one of the main candidate materials for heat transfer tubes of steam generators in nuclear power plants.
  • Incoloy 800HT
    Features: Incoloy 800HT is an improvement on 800 and 800H, with better creep resistance and ultra-high temperature durability. It has extremely low carbon content and improved Ti:C ratio, stable structure, maximum resistance to sensitization and intergranular corrosion.
    Application: Suitable for various heat treatment equipment in high temperature and corrosive environments, such as furnace silencers, containers, silos, brackets and burner components.
  • Incoloy 825
    Features: Incoloy 825 is an austenitic nickel-iron-chromium alloy with added elements such as molybdenum, copper and titanium, which has excellent corrosion resistance and oxidation resistance. It has high corrosion resistance to a variety of corrosive media, including sulfuric acid, hydrochloric acid and chlorides.
    Application: Widely used in the oil and gas industry for the manufacture of submarine pipelines, refining equipment, acid gas field mining equipment, etc.
  • Incoloy 925
    Features: Incoloy 925 is a high-strength, corrosion-resistant and high-temperature resistant nickel-iron-chromium alloy. Through precipitation hardening treatment, it can obtain extremely high tensile strength and yield strength, and is suitable for application environments that need to withstand high stress.
    Application areas: Widely used in the oil and gas industry, chemical industry, marine engineering, aerospace and other fields, used to manufacture key equipment such as oil well equipment, pipelines, valves, reactors, heat exchangers, etc.
  • Incoloy 926
    Features: High resistance to pitting, crevice corrosion and chloride ion stress corrosion in chloride and sulfur-containing acidic environments, good high temperature performance, high strength and good welding performance.
    Application areas: petrochemical, marine engineering, nuclear energy, electric power, aerospace and other fields.
lncoloy
Major Constituent Elements lncoloy Grades
800 800H 800HT 825 925 926
Ni: 30.0 – 35.0% 30.0 – 35.0% 30.0 – 35.0% 38 – 46% 42.0 – 46.0% 26.0%
Cr: 19.0 – 23.0% 19.0 – 23.0% 19.0 – 23.0% 19.5 – 23.5% 27.0 – 31.0% 21.0%
Fe: 30-35% 30-35% 39.5 – 46% 30 – 35% ≥22% 30-35%
C : ≤0.10% 0.75% 0.75% 1.5 – 3% 1.5 – 3.0% 1.50%
Mn: 1.0 – 1.7% ≤1.5% ≤1.5% ≤1% ≤1% ≤1.5%
Si: 0.20 – 0.80% ≤1.0% ≤1.0% ≤0,5% ≤0,5% ≤0,5%
S : ≤0,015% ≤0,015% ≤0,015% ≤0.015 ≤0.03% ≤0.01%
P : ≤0.030% ≤0,015% ≤0.02% ≤0.03% ≤0.03%
Al: 0.15 – 0.60% 0.15 – 0.60% 0.15 – 0.60% ≤0.2% ≤0,5%
Ti: 0.15 – 0.60% 0.15 – 0.60% 0.15 – 0.60% 0.6 – 1.2% 1.9 – 2.4% 1.50%
C : 0.05 – 0.10% 0.06 – 0.10% ≤0.05% ≤0.03% ≤0.04%
Mo: 2.5 – 3.5% 2.5 – 3.5% 6.00%
Nb: 0.50%
N : 0.15%

Incoloy 800

Найдено 4 продукта.

Incoloy 800H

Найдено 4 продукта.

Incoloy 800HT

Найдено 4 продукта.

Incoloy 825

Найдено 4 продукта.

Incoloy 925

Найдено 4 продукта.

Incoloy 926

Найдено 4 продукта.
Can't find the right grade or size? Contact us now!
Есть ли у вас в наличии?

Да, у нас есть полные спецификации и инвентарь, и мы можем быстро удовлетворить ваши потребности.

Можно ли его настроить?

Да, он может быть настроен. Вы можете связаться с нами и отправить нам настроенные спецификации и количество.

Как вы отправляете товары?

Наши способы транспортировки обычно включают морские перевозки, наземные перевозки и морские перевозки. Мы доставим вам груз быстро и безопасно.

Какова ваша цена?

Поскольку наша производительность высока, затраты будут гораздо ниже, поэтому цена низкая.

Могу я получить несколько образцов?

Мы можем предоставить вам образцы листов из нержавеющей стали для проверки качества. Образец бесплатен, и вы просто оплачиваете перевозку.

Как у вас обстоят дела с качеством?

Мы придаем большое значение качеству продукции и прошли различные испытания системы качества.

Отправьте запрос сегодня
Быстрая цитата