x
Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat

Saluran baja tahan karat

  • Daxun is a world-leading stainless steel channel supplier and manufacturer.
  • We produce high-quality stainless steel channels.

Daxun stainless steel channel steel is suitable for engineering and structure.

China stainless steel channel supplier.
Daxun has 10,000 tons of stainless steel channel in stock
Daxun can provide channel surface processing services

Introduction to Daxun stainless steel channel steel

Product Parameters:   Stainless Steel channel bar
Ukuran 5#、6#、6.3#、8#、10#、12#、14#、16#、18#、20#、22#、25#etc.
Please see the technical information below for detailed dimensions.
Permukaan Pickling 8K, NO.1, NO.4,hairline, etc
length 6000mm or  Customized
Kelas 304 201 304L 310S 316L 321 904L 2205 2507 S32750 S32760 etc
Standards ASTM A276, ASTM A484M, DIN 1028, EN10056, GB4227
Fitur Anti-corrosion (the degree is susceptible to the alloys contained), heat-resistance, good cold and hot working properties, good toughness, good comprehensive performances and wide application.

Daxun stainless steel channels are available in a variety of grades. We produce them by laser fusion and hot rolling, and are available in metric and imperial sizes. Daxun can provide custom sizes, shapes and grades upon request.
Send us a message now!

Baca Lebih Lanjut

Stainless Steel channel Steel Grade

Each type of stainless steel channel steel has its own different usage scenarios.

Click on the image to see more information about this product

Click on the image to see more information about this product

Click on the image to see more information about this product

Click on the image to see more information about this product

Click on the image to see more information about this product

Stainless Steel Channel
321 stainless steel channel

Click on the image to see more information about this product

Stainless Steel Channel
310S stainless steel channel

Click on the image to see more information about this product

Stainless Steel Channel
2205 stainless steel channel

Click on the image to see more information about this product

12 Products Found.

Performance of stainless steel channel steel

Ketahanan Korosi

The chemical composition on stainless steel channel bars protects them from rust. Their corrosion resistance is enhanced by the necessary polished finish, making them ideal for architectural use.

Low-Cost

Since stainless steel channel have a low melting point, no special tools are required. They are also durable and long-lasting materials, allowing industries to save on work and maintenance costs.

Valuable Metal

The smarter option material SS channel have far lesser drawbacks than other alloys. They provide excellent value, cost-effectiveness, and durability. SS is an easy-to-clean metal material.

Workability

Stainless steel channel material is an excellent choice for a variety of applications such as manufacturing. They are simple to use and ideal for large-scale industrial and complex uses.

Huge Stock Choiceable Material

With choiceable material from the very start comes our high quality stainless steel products.Daxun have stainless steel inventories for common grades and common sizes to ensure fast response to our customers’ demand.Mill Origin: TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc.

Stainless steel channel
Stainless steel channel

Stainless Steel Channel Manufacturing Process

Daxun stainless steel channels and C-channels are available in a variety of grades. We produce them by laser fusion and hot rolling, and are available in metric and imperial sizes. Daxun can provide custom sizes, shapes and grades upon request.Send us a message now!

About Daxun

1. Competitive price and quality from our own factory
2. Approved by ISO9001, CE, SGS every year
3. Best service with 24 hour`s reply
4. Flexible payment with T/T,L/C , paypal, etc
5. Smooth production ability
6. Quick delivery and standard exporting package
7. OEM/ODM

Stainless steel channel

Technical Information

Packing method

At Daxun, we choose different packaging for different stainless steel products, including: kraft paper, wooden boxes, woven bags, wooden pallets, based on the highest industry standards to ensure that the goods arrive in your hands in good condition.

Material Test Certification

All our stainless steel materials are certified by different industry standards such as ISO9001:2008, ISO14001:2014, AAA Certification, CQGC Certifications, and more. Our company also have certifications from ISO9001:2015 quality management system.

Actual Weight & Good Quality

At Daxun, we have testing laboratory and equipment to ensure that our stainless steel materials are in actual weight and good quality before shipment. Our strict quality control team also performs strict and 100% inspection on all production stages.

Excellent After-Sales Services

Our support and services are not only limited from the beginning of our transactions. Even if you have received your orders, Daxun will continue to provide excellent after-sales services. We will continue providing assistance and warranty to your orders.

Application cases of stainless steel channel steel in different industries

Dekorasi Bangunan

Stainless steel channels are widely used in the construction field. They can be used for exterior wall support, interior decoration, roofing materials, building structures, etc. Stainless steel is corrosion-resistant and has high strength, and can meet the design requirements of different buildings.

Mechanical equipment

Stainless steel has the advantages of corrosion resistance, no rust, no discoloration, easy removal of attached food, and good high and low temperature mechanical properties. Widely used in food machinery, such as sanitary systems, fluid pipe tanks, food storage tanks, heat exchangers, vacuum containers, etc.

Dirgantara

Stainless steel has good strength, toughness and corrosion resistance and is widely used in aircraft structural parts. For example, the wing structure, fuselage supports, seats and other components are all made of stainless steel.

Petrochemical

Stainless steel channel are also used in the manufacture and maintenance of oil refining equipment, and the brackets used in the petrochemical industry are all made of stainless steel channel.

military armor

Main application parts: wing skin, wing stringers, upper and lower edge strips of wing spar, web, fuselage stringers, seat rails, keel beam, side frames, fuselage skin, lower fuselage wall panels, Main floor stringers, etc.

Ship field

Stainless steel channel steel is widely used in the shipbuilding industry. The stainless steel channels supplied by Daxun are used in the shipbuilding and petroleum industries. They have high strength, good toughness, and are resistant to seawater corrosion, fatigue, and wear.

Teknik Kelautan

SS316L is the primary austenitic stainless steel grade used in offshore installations, where it enhances strength at high temperatures and protects structures from severe acidic environments.There are also duplex stainless steels, which offer an excellent combination of mechanical properties and resistance to stress corrosion cracking, making them ideal for offshore applications. UNS S32205 steel is the most commonly used duplex stainless steel grade for offshore installations.

Electric power field

The main application of stainless steel channel steel in electricity is the support of power station equipment. The excellent corrosion resistance and high strength of stainless steel make it the preferred material for power generation components.

about-feature3
Let us be your trustworthy stainless steel channel supplier

Our stainless steel channel are fully certified and traceable. We provide the highest quality stainless steel channel for leading industries such as building decoration, industrial equipment, chemical energy, shipbuilding, and petrochemicals.

echnical Information

Size Range
Hot-rolled U channel bar
Section Designation Mass Section Designation Mass
UPE80 [80*50*4.5*8 8.89 UPN65 [65*42*5*7 7.09
UPE100 [100*55*5*8.5 10.9 UPN80 [80*45*6*8 8.64
UPE120 [120*60*5.5*9 13.2 UPN100 [100*50*6*8.5 10.6
UPE140 [140*65*6*9.5 15.7 UPN120 [120*55*7*9 13.4
UPE160 [160*70*6.5*10 18.6 UPN140 [140*60*7*10 16
UPE180 [180*75*7*10.5 21.6 UPN160 [160*65*7.5*10.5 18.8
UPE200 [200*80*7.5*11 24.8 UPN180 [180*70*8*11 22
UPE220 [220*85*8*12 28.8 UPN200 [200*75*8.5*11.5 25.3
UPE240 [240*90*8.5*13 33.4 UPN220 [220*80*9*12.5 29.4
UPE270 [270*95*9*14 38.8 UPN240 [240*85*9.5*13 33.2
UPE300 [300*100*9.5*15 44.5 UPN260 [260*90*10*14 37.9
UPE330 [330*105*11*16 53.3 UPN280 [280*95*10*15 41.8
UPE360 [360*110*12*17 61.2 UPN300 [300*100*10*16 46.2
UPE400 [400*115*13.5*18 72.3 UPN320 [320*100*14*17.5 59.5
UPN30 [30*33*5*7 4.27 UPN350 [350*100*14*16 60.6
UPN40 [40*35*5*7 4.87 UPN380 [380*102*13.5*16 63.1
UPN50 [50*38*5*7 5.59 UPN400 [400*110*14*18 71.8
Specified Size of Stainless Channels, mm Size Tolerances, Over and Under, mm.
Flange Depth Flange Width Web Thickness for Thickness Given Out-of-Square B of Either Flange, mm/ mm of Flange Width
To 5.00mm Over 5.00mm
To 38.00mm, incl. 1.2 1.2 0.41 0.6 1.2
Over 38.00 to 75.00mm, excl. 2.4 2.4 0.6 0.8 1.2
Pilihan Status Pengiriman Kondisi Permukaan
Canai Panas Acar
Sand Blasting
Welding Acar
Sand Blasting
Press Bending Acar
Sand Blasting
No.1 Finish
Catatan:
1. Jika Anda memerlukan status pengiriman yang berbeda dari yang tercantum di atas, mohon konfirmasi dengan kami.
2. Jika ada pertanyaan atau pesanan, mohon beritahukan kepada kami persyaratan tambahan yang tidak disebutkan di sini.
  • “Thank you Daxun for the extremely durable, world-class quality stainless steel channel. I also appreciate the professional customization service. I am happy to work with you for my stainless steel channel needs. Looking forward to working with you next time!”

    Testimonials from customers located in the Middle East
  • “Daxun has always been a trustworthy company when it comes to stainless steel channel. All the stainless steel channel I purchased are of very high quality. I ordered stainless steel channel at a very low price at Daxun. The staff was also happy to answer my questions .” Asked questions and was impressed with my needs! “

    Testimonials from customers located in Europe and the United States
  • “We were very impressed with the quality and superiority of Daxun stainless steel channel. There are a variety of sizes available that fit our needs perfectly. Additionally, we really appreciate the affordable price and service.”

    Testimonials from customers located in Russia

Paduan Daxun

Regarding stainless steel channel, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.

Do you have any stock in stock?

Yes, we have complete specifications and inventory and can quickly meet your needs.

Can it be customized?

Yes, it can be customized. You can contact us and send us the customized specifications and quantity.

How do you ship the goods?

Our transportation methods generally include sea transportation, land transportation, and sea transportation. Reach you quickly and safely.

What's your price like?

Because our output is high, the cost will be much lower, so the price is low.

Bisakah saya mendapatkan beberapa sampel?

We can provide stainless steel channel samples for you to check the quality. Sample is free and you just pay the freight.

Bagaimana kualitas Anda?

We attach great importance to product quality and have passed various quality system tests.

Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat